40CrMnMo7, 40CrMnMoS8-6, 40CrMnNiMo8-6-4 Steels

Steel name: 40CrMnMo7, 40CrMnMoS8-6, 40CrMnNiMo8-6-4
Diagram No.: 615
DIN designation: KTW: 40CrMnMo7, KTS: 40CrMnMoS8-6, KTW - Ni: 40CrMnNiMo8-6-4
Mat.No. (Wr.Nr.) designation: KTW: 1.2311, KTS: 1.2312, KTW - Ni: 1.2738
Chemical composition in weight %:
KTW: 0.42% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo
KTS: 0.42% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo, + S
KTW - Ni: 0.42% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo, 1.00% Ni
Steel group: Chromium magnese molybdenum steel
Applications: a) K TW: Medium size hammer forging dies for steel; extrusion tools such as mantles and intermediate liners, supporting tools and tool holders, frames for die casting moulds; plastic moulds; assembling plates and similar tools. b) K TW- Ni: Recommended for sizes > 400 mm because of its improved deep hardening properties.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 850 - 870oC/oil, hot bath, polymer
Tempering: See the diagram
Diagram note: Sample diameter: 30 mm.

Diagram Tempering Temperature - Mechanical Properties

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.