X32CrMoV3-3 Steel

Steel name: X32CrMoV3-3
Diagram No.: 634
DIN designation: X32CrMoV3-3
Mat.No. (Wr.Nr.) designation: 1.2365
Chemical composition in weight %: 0.32% C, 0.40% Si, 0.40% Mn, 3.00% Cr, 2.80% Mo, 0.60% V
Steel group: Hot work tool steels
Applications: Extrusion tools for aluminium, copper alloys and steel, such as dies and inserts, dummy blocks, die holders and mandrels; die casting tools for aluminium and copper alloys; die forging tools for copper alloys; tools for making bolts and nuts; die-inserts, punches, jaws etc. used on forging presses; piercing and other tools on push benches for steel tube production.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1020 - 1050oC/oil, hot bath, polymer
Tempering: See the diagram
Diagram note: Sample diameter: 60 mm, hardening: 1030oC/oil.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.