X32CrMoV3-3 Steel

Steel name: X32CrMoV3-3
Diagram No.: 635
DIN designation: X32CrMoV3-3
Mat.No. (Wr.Nr.) designation: 1.2365
Chemical composition in weight %: 0.32% C, 0.40% Si, 0.40% Mn, 3.00% Cr, 2.80% Mo, 0.60% V
Steel group: Hot work tool steels
Applications: Extrusion tools for aluminium, copper alloys and steel, such as dies and inserts, dummy blocks, die holders and mandrels; die casting tools for aluminium and copper alloys; die forging tools for copper alloys; tools for making bolts and nuts; die-inserts, punches, jaws etc. used on forging presses; piercing and other tools on push benches for steel tube production.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1020 - 1050oC/oil, hot bath, polymer
Tempering: See the diagram
Diagram note: Sample diameter: 30 mm.

Diagram Tempering Temperature - Mechanical Properties


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.