X3NiCoMoTi18-9-5 Steel

Steel name: X3NiCoMoTi18-9-5
Diagram No.: 643
DIN designation: X3NiCoMoTi18-9-5
Mat.No. (Wr.Nr.) designation: 1.2709
Chemical composition in weight %: 0.03% C, 0.10% Si, 0.15% Mn, 9.50% Co, 5.20% Mo, 18.00% Ni, 0.95% Ti, + special additions
Steel group: Nickel maraging steel
Applications: Die casting tools for aluminium and zinc alloys; press tools for aluminium alloys; plastic moulds; piercing tools; punches; bushings and shrink rings for cold extrusion and for tungsten carbide inserts; heavy duty pilger mandrels for the production of thin-walled copper alloy or steel tubes.
Reference: Not shown in this demo version.

Heat Treatment
Precipitation hardening: 490oC/6-8 h and still air cooling. This leads to a substantial increase in hardness.
Tempering: See the diagram
Diagram note: Sample diameter: 30 mm.

Diagram of Precipitation Hardening

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.