AMS 6257 Steel

Steel name: AMS 6257
Diagram No.: 682
AMS designation: 6257
Messier-Dowty designation: MTL-1201
Goodrich designation: LGMS 1000
Chemical composition in weight %: 0.42% C, 1.65% Si, 0.75% Mn, 0.80% Cr, 0.40% Mo, 0.07% V, 1.80% Ni
Steel group: High strength alloy steels
Properties: No data
Applications: The enhanced properties of AMS 6257 permit the design of lighter aircraft components that exhibit equivalent load carrying capacities compared to standard 300M components.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 871oC/oil
Tempering: See the diagram
Diagram note: Austenitized 871oC, oil quench, tempered 2 x 2h.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.