AMS 5749 Steel

Steel name: AMS 5749
Diagram No.: 705
AMS designation: 5749
Chemical composition in weight %: 1.15% C, 0.30% Si, 0.50% Mn, 14.50% Cr, 4.00% Mo, 1.20% V
Steel group: Stainless knife steels
Properties: Response to tempering BG42, M50, 440 C MOD, 440 C, 52100 steel.
Applications: When manufactured in sheet form, 5749 has proven to be an excellent knife steel. The very good wear resistance and corrosion resistance result in knife blades that exhibit excellent edge retention and long life.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1121oC/oil, gas, salt
Tempering: See the diagram

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.