24Ni8 Steel

Steel name: 24Ni8
Diagram No.: 79
DIN designation: 24Ni8
Mat.No. (Wr.Nr.) designation: 1.5633
Chemical composition in weight %: 0.22% C, 0.28% Si, 0.70% Mn, 0.07% Cr, 0.25% Mo, 1.97% Ni, 0.010% V, 0.11% Cu
Steel group: Alloy special structural steels
Properties: No data
Applications: Parts of good tenacity for the construction of apparatus and in general mechanical engineering as well as for boilers and vessels, structural components for the aviation industry and refrigerators, for temperatures down to -100 °C.
Reference: Not shown in this demo version.

Heat Treatment
Hardening in water: 830-850oC
Hardening in oil: 830-850oC
Tempering: 500-650oC
Diagram note: No data

Diagram Tempering Temperature - Mechanical Properties

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.