S15500 Steel

Steel name: S15500
Diagram No.: 817
AISI/SAE designation: A693 grade XM12
AFNOR designation: Z5CNU15-05
UNS designation: S15500
Chemical composition in weight %: 0.07% C, 15.00% Cr, 4.50% Ni, 3.50% Cu, 0.30% Nb
Steel group: Precipitation hardening martensitic stainless steels
Properties: Tempering diagram: Hardness/Temperature tempered for 4 hours after austenitizing at 1040°C (1904°F) for 30 min quenched 100°C/sec (212°F/sec).
Applications: The main applications are those of steel 17.4 PH grade i.e. mechanical components and offshore industry when considering heavy plates.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1038oC/oil, air
Tempering: See the diagram

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.