1.1730 Steel
Steel name: 1.1730
Diagram No.: 821
DIN designation: C45W
Mat.No. (Wr.Nr.) designation: 1.1730
Chemical composition in weight %: 0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
Steel group: Non-alloyed tool steel
Applications: Non-alloyed tool steel for the production of equipment and machine parts, as well as foundation plates and guide rails for tools - the standard material for basic machine parts.
Reference: Not shown in this demo version..
Heat Treatment
Hardening: 810oC/water
Tempering: See the diagram
Diagram note: Hardening temperature: 810°C, specimen size: square: 20 mm.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.