M35 Steel

Steel name: M35
Diagram No.: 853
JIS designation: SKH55
Mat.No. (Wr.Nr.) designation: 1.3243
AISI/SAE designation: M35
Chemical composition in weight %: 0.93% C, 4.20% Cr, 5.00% Mo, 1.80% V, 6.40% W, 4.80% Co
Steel group: High speed steels
Applications: M35 is a high-speed steel suitable for cutting tools such as, broaches, taps, milling, reamers, hobs, shapers cutters, saws etc. In terms of performance, M35 is an all-round steel to be used in cutting conditions where demands for hot hardness are of importance. M35 is also suitable for cold work applications, where exacting demands are imposed on wear resistance. The steel possesses an admirable combination of wear resistance and toughness and in these respects superior to the high alloyed cold work steels.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1050–1220oC/air
Tempering: See the diagram
Diagram note: Hardness after hardening, step quenching and tempering 2x1 h of a sample 25 mm Ø.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.