Wear resistant steel

Steel name: Wear resistant steel
Diagram No.: 857
Chemical composition in weight %:
Thickness 10-50 mm: 0.37% C, 0.50% Si, 1.30% Mn, 1.14% Cr, 0.60% Mo, 1.40% Ni, 0.004% B
Steel group: Wear resistant steels
Properties: No data
Applications: Steel has been successfully used as linings in various applications, i.e. conveyor systems, wear strips, feeders, chutes and concrete mixers. Within the recycling industry steel has been utilized in rotating hammers as well as in shredder knives.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: No data
Tempering: See the diagram

Tempering Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.