AUD11 Steel

Steel name: AUD11
Diagram No.: 863
Chemical composition in weight %: 10.00% Cr with 13% carbides in the microstructure.
Steel group: Cold work tool steels
Properties: Steel SKD11: 13% Cr
Applications: Blanking dies, forming dies, trimming dies, thread rolling dies, shear blades.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1000-1050oC/air, gas, vacuum
Tempering: See the diagram

Tempering Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.