1.1167 Steel
Steel name: 1.1167
Diagram No.: 901
BS designation: 150M36
AFNOR designation: 35M5, 40M5
Mat.No. (Wr.Nr.) designation: 1.1167
AISI/SAE designation: 1335
Old name: VM 135
Chemical composition in weight %: 0.36% C, 0.25% Si, 1.25% Mn, + Pb
Steel group: Structural steels
Properties: No data
Applications: No data
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 820 - 850oC/water
Tempering: See the diagram
Diagram note: Sample size: dia 60 mm, hardening 840oC/water.
Diagram Tempering Temperature - Mechanical Properties
Click the image to enlarge the diagram.
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.