1.7220, 1.7226 Steels

Steel name: 1.7220, 1.7226
Diagram No.: 928
BS designation: 708A37
AFNOR designation: 34CrMo4, 35CD4
Mat.No. (Wr.Nr.) designation: 1.7220, 1.7226
AISI/SAE designation: 4135, 4137
Old name: Mo35
Chemical composition in weight %:
34CrMo4: 0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo, <0.035% S, + Pb
34CrMoS4: 0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo, 0.020-0.035% S, + Pb
Steel group: Heat treatable steels
Properties: No data
Applications: No data
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 830 - 870oC/oil, water
Tempering: See the diagram
Diagram note: Sample size: dia 60 mm, hardening 850oC/oil, tempering time 2h.

Diagram Tempering Temperature - Mechanical Properties

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.