1.2343 mod. Steel
Steel name: 1.2343 mod.
Diagram No.: 935
DIN designation: X38CrMoV51 mod.
EN designation: X38CrMoV51 mod.
Mat.No. (Wr.Nr.) designation: 1.2343 mod.
AISI/SAE designation: H11 mod.
Chemical composition in weight %: 0.36% C, 0.20% Si, 0.30% Mn, 5.00% Cr, 1.35% Mo, 0.45% V
Steel group: Hot work tool steels
Properties: No data
Applications: Above all, this steel grade is designed for die casting of light metals and alloys (aluminium and aluminium alloys), for die forging of steel and non-ferous metals (e.g. cupper) and their alloys, for extrusion of tubes, barrels and sections made of light metals and alloys, for casting and processing of various plastics, and for glass processing. Characterics: Excellent homogeneity, high cleanliness, high level of isotrophy, good workability, high impact toughness, good polishability. Advantages: Lower cost due to: Lower tool life, lower tool wear, less tool repair, less tool changes and consistent heat treatment results.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 980-1000oC/oil, hot bath, air, vacuum
Tempering: See the diagram
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.