Pb-0.1% Ca Alloy

Alloy name: Pb-0.1% Ca
Diagram No.: 775
Type of diagram: TTH
Chemical composition in weight %: 0.1% Ca, balance is Pb
Alloy group: Lead-based alloys
Note: Typical micro-hardness and resistance curves for a Pb-0.1% Ca at 20 C. In black the value of the resistance over the resistance at initial time (oversaturated alloy). The points correspond to hardness measurements HV/0.1/5 on a single sample. As samples are inhomogeneous in hardness due to the presence of discontinuous transformations, fitted grey solid lines are added to represent the mean and the maximum, minimum curve to visualise the hardness amplitude.
Additional links: No. 775, No. 776, No. 777, No. 778, No. 779, No. 780
Reference: Not shown in this demo version.

Transformation Diagram

Price: 20.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT of Steels
Hardenability Diagrams of Steels
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Tempering Diagrams of Steels

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.





Copyright © 2024 by Steel Data. All Rights Reserved.