Tempering Diagrams and Tables (100 Examples)

0.10C-2.50Mn-3.00Cr-1.00Ni Steel
0.33C-16.70Cr Steel
0.54C-17.30Cr-1.10Mo Steel
0.60C-4.50Cr-0.50Mo-0.20V Steel
1.1133 Steel
1.1167 Steel
1.1191, 1.1201, 1.1193 Steels
1.1223 Steel
1.20C-12.00Cr-1.40Mo-1.70V-2.50W Steel
1.2208 Steel
1.2312 Steel
1.2365 Steel
1.2436 Steel
1.2601 Steel
1.2714 Steel
1.2714 Steel
1.2767 Steel
1.40C-4.60Cr-3.20Mo-3.70V Steel
1.40C-4.70Cr-3.50Mo-3.70V Steel
1.4542 Steel
1.60C-4.80Cr-2.00Mo-5.00V-10.50W-8.00Co Steel
1.6582 Steel
1.70C-18.00Cr-1.00Mo-3.00V Steel
1.7707 Steel
1.80C-4.25Cr-5.00V-12.25W-5.00Co Steel
1.8161 Steel
100CrMo5 Steel
100W4 Steel
1050 Steel
105Cr4 Steel
12Ni19 Steel
14-4CrMo Steel
140Cr2 Steel
15CrMoV6 Steel
25CrMo4 Steel
28NiCrV5 Steel
34Cr4 Steel
34CrAlNi7-10 Steel
34CrNiMo6 Steel
35NiCr18 Steel
35NiCrMo16 Steel
36NiCr6 Steel
37CrS4 Steel
42CrMo4 Steel
42CrMo4TT Steel
45CrMoV7 Steel
45NiCrMo16 Steel
45NiCrMo18 Steel
49CrMo4 Steel
54NiCrMoV6 Steel
55NiCrMoV7 Steel
73WCrMoV2-2 Steel
80MoCrV42-16 Steel
A2 Steel
AISI 2367 Steel
AUD11 Steel
C105W2 Steel
C20E2C Steel
C35 Steel
C4732 Steel
C60E Steel
C60U Steel
C70D Steel
Cf53 Steel
D2 Steel
D3 Steel
DURO-V2 Steel
H13 Tool Steel
HMT12 Steel
HS0-4-1 Steel
HS2-9-1 Steel
HS2-9-2 Steel
HS6-5-2 Steel
HS6-5-2C Steel
M2 Steel
M2 Steel
O1 Steel
O1 Steel
S18-1-2-10 Steel
SMR4 Steel
VH13-ISO Steel
VWM2 Steel
Wear resistant steel
X100CrMoV5 Steel
X105CrCoMo18-2 Steel
X105CrMo17 Steel
X105CrMo17 Steel
X110CrMoV8 Steel
X12Cr13 Steel
X155CrVMo12-1 Steel
X30Cr13 Steel
X32CrMoV3-3 Steel
X37CrMoV5-1 Steel
X40Cr14 Steel
X40CrMo15 Steel
X40CrMoV5-1 Steel
X45CrSi9-3 Steel
X50CrMoW9-1-1 Steel
X60WCrMoV 9-4 Steel
X6NiCrTi 26-15 Steel