CoCr28Mo6 Alloy

Alloy name: CoCr28Mo6
Diagram No.: 640
Type of diagram: TTP
Chemical composition in weight %: 27.00-30.00% Cr, 5.00-7.00% Mo, max. 1.00% Mn, max. 1.00% Si, max. 0.75% Fe, max. 0.50% Ni, max. 0.35% C, max. 0.10% Al, max. 0.01% B, max. 0.25% N, max. 0.02% P, max. 0.01% S, max. 0.20% W, max. 0.10% Ti, balance is Co
Alloy group: Cobalt-based alloys
Note: The temperature-time-precipitation diagram (TTP diagram) clearly shows that carbon is only precipitated as very fine secondary (Cr, Mo) carbides in CoCr28Mo6 when exposed to very high cooling rates in excess of 230K/min as possible in the new VACUCAST HIP system. Temperature-time-precipitation diagram in the HIP process for the secondary (Cr, Mo) carbides in CoCr28Mo6
Reference: Not shown in this demo version.

Transformation Diagram

Price: 20.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT of Steels
Hardenability Diagrams of Steels
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Tempering Diagrams of Steels

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.