Chemical Composition of Alloys in Weight %
0.0021% C, 0.04% Si, 0.12% Mn, 0.009% P, 0.006% S, balance is Fe
0.005-0.04% C, max. 0.005% Si, max. 0.005% B, max. 0.005% Zr, 0.3-1.6% Hf, max. 0.005% Ti, 5.3-5.7% Al, 8.0-8.8% Cr, 0.5-0.8% Mo, 2.8-3.3% Ta, 9.0-11.0% Co, 9.5-10.5% W, max. 0.002% S, max. 0.002% S, max. 0.1% Mn, max. 0.1% Fe, max. 0.1% Cu, max. 0.1% Nb, balance is Ni
0.005% N, max. 0.10% C, max. 0.015% H, max. 0.10% Fe, max. 0.20% O, 14.0-16.0% Mo, balance is Ti
0.005% N, max. 0.10% C, max. 0.015% H, max. 0.10% Fe, max. 0.20% O, 14.0-16.0% Mo, balance is Ti
0.009% C, 1.00% Mn, 0.05% Si, 0.010% S, 0.020% P, 14.50-17.50% Cr, 10.00-17.00% Mo, 0.70% Ti, 2.00% Co, balance is Ni
0.01% C, max. 0.08% Si, 21% Cr, 17% Mo, max. 1% W, max. 2% Fe, 0.006% B, balance is Ni
0.010% C, 1.00% Mn, 0.08% Si, 0.010% S, 0.025% P, 14.50-16.50% Cr, 15.00-17.00% Mo, 3.00-4.50% W, 4.00-7.00% Fe, 2.5% Co, 0.35% V, balance is Ni
0.010% C, 0.50% Mn, 0.08% Si, 0.015% S, 0.025% P, 2.00-6.00% Fe, 20.00-22.50% Cr, 12.50-14.50% Mo, 2.50-3.50% W, 2.50% Co, 0.35% V, balance is Ni
0.010% C, 0.50% Mn, 0.10% Si, 0.005% S, 0.015% P, 22.00-24.00% Cr, 15.00-16.50% Mo, 1.50% Fe, 0.30% Co, 0.10-0.40% Al, balance is Ni
0.015% C, 1.00% Mn, 1.00% Si, 21.50-23.50% Cr, 18.00-21.00% Fe, 6.00-8.00% Mo, 1.50-2.50% Cu, 5.00% Co, 0.20-0.50% Nb, 1.50% W, balance is Ni
0.015% C, 2.00% Mn, 0.30% Si, 0.010% S, 0.020% P, 30.00-32.00% Ni, 26.00-28.00% Cr, 6.00-7.00% Mo, 1.00-1.40% Cu, 0.15-0.25% N, balance is Fe
0.015% C, 2.00% Mn, 0.50% Si, 0.010% S, 0.020% P, 30.00-33.0% Ni, 31.00-35.00% Cr, 0.50-2.00% Mo, 0.30-1.20% Cu, 0.35-0.60% N, balance is Fe
0.016% C, 0.8% Si, 0.06% Mn, 0.006% P, 0.006% S, 21.8% Cr, 0.027% Co, 9.06% Mo, 0.2% Ti, 0.1% Al, 2.4% Fe, 0.023% Cu, 3.7% Nb+Ta, 1 ppm B, balance is Ni
0.02% C, max. 0.02% S, 0.15-0.25% N, 20.00-21.00% Cr, 24.00-26.00% Ni, max. 1.00% Mn, max. 0.50% Si, 6.00-7.00% Mo, 0.50-1.50% Cu, max. 0.030% P, balance is Fe
0.02% C, 0.40% Si, 0.020% P, 0.001% S, 20.50% Cr, 6.20% Mo, 24.00% Ni, 0.20% Cu, 0.22% Ni
0.02% Si, 0.05% Fe, 2.04% Cu, 0.04% Mn, 2.15% Mg, 0.33% Zn, 0.12% Zr, balance is Al
0.02% Si, 0.05% Fe, 2.04% Cu, 0.04% Mn, 2.15% Mg, 6.33% Zn, 0.001% Ti, balance is Al
0.02% C, 1.00% Mn, 0.50% Si, 0.010% S, 0.030% P, 24.00-26.00% Ni, 20.00-21.00% Cr, 6.00-7.00% Mo, 0.50-1.50% Cu, 0.15-0.25% N, balance is Fe
0.02% C, 20.7% Cr, 0.72%Fe, 3.75% Nb, 8.83% Mo, balance is Ni
0.025% C, 18.0% Cr, 2.70% Mo, 1.0% W, 9.0% Co, 10.0% Fe, 5.40% Nb, 0.70% Ti, 1.45% Al, 0.007% P, 0.004% B
0.025% C, 18.0% Cr, 2.70% Mo, 1.0% W, 9.0% Co, 10.0% Fe, 5.40% Nb, 0.70% Ti, 1.45% Al, 0.007% P, 0.004% B
0.025% C, 18.0% Cr, 2.70% Mo, 1.0% W, 9.0% Co, 10.0% Fe, 5.40% Nb, 0.70% Ti, 1.45% Al, 0.007% P, 0.004% B
0.025% C, 18.0% Cr, 2.70% Mo, 1.0% W, 9.0% Co, 10.0% Fe, 5.40% Nb, 0.70% Ti, 1.45% Al, 0.007% P, balance is Ni
0.025% C, 18.0% Cr, 2.70% Mo, 1.0% W, 9.0% Co, 10.0% Fe, 5.40% Nb, 0.70% Ti, 1.45% Al, 0.007% P, balance is Ni
0.025% C, 1.00% Mn, 0.50% Si, 0.010% S, 0.020% P, 38.00-46.00% Ni, 19.50-23.50% Cr, 2.50-3.50% Mo, 1.15-3.0% Cu, 0.60-1.20% Ti, 0.20% Al, balance is Fe
0.028% C, 17.42% Cr, 2.72% Mo, 1.04% W, 9.13% Co, 9.66% Fe, 5.48% Nb, 1.46% Al, 0.71% Al, 9.71% Ti, balance is Ni
0.029% C, 0.S4% Si, 0.S8% Mn, 0.009% P, 0.004% S, 22.67% Cr, 1.33% Fe, 8.75% Mo, 0.17% Ti, 3.72% Nb, 0.15% Al, 0.0071% N, balance is Ni
0.029% Si, 0.073% Fe, 2.152% Cu, 1.936% Mg, 8.542% Zn, 0.127% Zr, 87.06% Al
0.03% C, 18.8% Cr, 11.8 Co, 6.0% Mo, 0.9% W, 2.9% Ti, 2.1% Al, 0.02% B, balance is Ni
0.03% C, 25% Cr, 0.5% Mo, 20% Co, 1.35% Al, 1.35% Ti, 1.5% Nb, 0.3% Mn, 0.7% Fe, 0.15% Si, balance is Ni
0.03% C, 0.65% Mn, 29.59% Fe, 0.27% Si, 1.71% Cu, 21.18% Cr, 0.11% Al, O.99% Ti, 2.61% Mo, balance is Ni
0.03% C, 0.10% Mn, 0.25% Si, 0.008% S, 0.011% P, 22.1% Cr, 1.89% Fe, 0.20% Al, 0.22% Ti, 9.1% Mo, 3.35% Nb+Ta, 0.20% W, 40 ppm B, 50 ppm 0, 480 ppm N, balance is Ni
0.03% C, 0.65% Mn, 29.59% Fe, 0.27% Si, 1.71% Cu, 21.18% Cr, 0.11% Al, 0.99% Ti, 2.61% Mo, balance is Ni
0.03% C, 0.65% Mn, 29.59% Fe, 0.27% Si, 1.71% Cu, 21.18% Cr, 0.11% Al, O.99% Ti, 2.61% Mo, balance is Ni
0.03% C, 0.65% Mn, 29.59% Fe, 0.27% Si, 1.71% Cu, 21.18% Cr, 0.11% Al, O.99% Ti, 2.61% Mo, balance is Ni
0.03% C, 0.65% Mn, 29.69% Fe, 0.27% Si, 1.71% Cu, 21.18% Cr, 0.11% Al, 0.99% Ti, 2.61% Mo, balance is Ni
0.03% C, 18.04% Fe, 18.5% Cr, 53.21% Ni, 5.3% Mo, 1.00% Ti, 0.52% Al, 0.06% Si, 0.13% Co
0.03% C, 1.00% Mn, 0.50% Si, 0.03% S, 0.03% P, 42.00-46.00% Ni, 19.50-22.50% Cr, 22.0% Fe, 2.50-3.50% Mo, 1.50-3.0% Cu, 1.90-2.40% Ti, 0.10-0.50% Al, 0.50% Nb
0.04% Cr, 1.30-2.00% Cu, max. 0.08% Fe, 1.20-1.80% Mg, max. 0.04% Mn, max. 0.06% Si, max. 0.06% Ti, 7.00-8.00% Zn, 0.08-0.15% Zr, balance is Al
0.04% Cr, 2.0-2.6% Cu, max. 0.15% Fe, 1.90-2.60% Mg, max. 0.10% Mn, max. 0.12% Si, max. 0.06% Ti, 5.70-6.70% Zn, 0.08-0.15% Zr, balance is Al
0.04% C, 0.20% Mn, 0.30% Si, 28.6% Cr, 3.1% Mo, 5.0% Nb, 18.5% Fe, 0.9% Ti, 0.4% Al, balance is Ni
0.04% C, 19% Cr, 53% Ni, 5.1% Nb, 0.90% Ti, 0.50% Al, 3% Mo, 18.5% Fe, 6.50% Ti+Al+Nb, 0.27% (Ti+Al)/Nb
0.04% C, 0.10% Mn, 18.95% Fe, 0.003% S, 0.16% Si, 0.008% Cu, 52.42% Ni, 18.35% Cr, 0.50% Al, 1.00% Ti, 0.10% Co, 2.98% Mo, 5.22% Nb+Ta
0.04% C, 0.10% Mn, 18.95% Fe, 18.35% Cr, 0.60% Al, 1.00% Ti, 0.10% Co, 2.98% Mo, 5.22% Nb+Ta, 0.003% S, 0.08% Cu, balance is Ni
0.04% C, 0.20% Mn, 0.30% Si, 18.6% Cr, 3.1% Mo, 6.0% Nb, 18.6% Fe, 0.9% Ti, 0.4% Al, balance is Ni
0.04% C, 15.36% Cr, 9.98% Fe, 0.40% Mn, 0.11% Si, 0.30% Cu, 0.17% Al, 0.20% Ti, 0.05% Co, 0.011% S, balance is Ni
0.04% C, 53% Ni, 19% Cr, 3% Mo, 18% Fe, 0.5% Al, 0.9% Ti, 0.1% Cu, 5% Nb
0.04-0.08% C, 0.60% Mn, 0.40% Si, 0.007% S, 0.015% P, 19.00-21.00% Cr, 5.60-6.10% Mo, 19.00-21.00% Co, 0.20% Cu, 0.70% Fe, 0.30-0.60% Al, 1.90-2.40% Ti, 2.40-2.60% Al+Ti, 0.002% Pb, 0.0005% Ag, 0.02% Zr, balance is Ni
0.041% Si, 0.089% Fe, 6.41% Cu, 0.301% Mn, 0.006% Mg, 0.001% Cr, 0.031% Zn, 0.034% Ti, balance is Al
0.042% C, 21.77% Cr, 60.63% Ni, 0.19% Co, 8.79% Mo, 0.21% Al, 0.40% Ti, 3.68% Fe, 3.75% Nb, 0.12% Si, 0.20% Mn, 0.0006% S, 0.006% P, 0.06% Cu
0.05% C, 0.57% Mn, 6.56% Fe, 0.25% Si, 0.05% Cu, 15.66% Cr, 0.70% Al, 2.35% Ti, 0.92% Nb, balance is Ni
0.05% C, 19% Cr, 53% Ni, 5% Cb, 3% Mo, 1% Ti, 0.5% Al, 0.005% B, 18% Fe
0.05% C, 19% Cr, 53% Ni, 5% Cb, 3% Mo, 1% Ti, 0.5% Al, 0.005% B, 18% Fe
0.05% C, 19% Cr, 53% Ni, 5% Cb, 3% Mo, 1% Ti, 0.5% Al, 0.005% B, 18% Fe
0.05% C, 19% Cr, 53% Ni, 5% Cb, 3% Mo, 1% Ti, 0.5% Al, 0.005% B, 18% Fe
0.05-0.15% C, max. 3.0% Fe, max. 0.5% Si, 20.0-24.0% Cr, 10.0-15.0% Co, max. 0.6% Ti, 8.0-10.0% Mo, 0.8-1.5% Al, max. 0.006% B, balance is Ni
0.06% C, 0.39% Si, 1.55% Mn, 0.020% S, 0.01% Cr, 0.20% Ni, 0.003% Ti, 0.016% Al, 0.004% N, 0.0540% O
0.06% C, 0.39% Si, 1.55% Mn, 0.020% S, 0.01% Cr, 0.20% Ni, 0.003% Ti, 0.016% Al, 0.004% N, 0.0540% O
0.06% C, 0.39% Si, 1.55% Mn, 0.020% S, 0.01% Cr, 0.20% Ni, 0.003% Ti, 0.016% Al, 0.004% N, 0.0540% O
0.06% C, 0.39% Si, 1.55% Mn, 0.020% S, 0.01% Cr, 0.20% Ni, 0.003% Ti, 0.016% Al, 0.004% N, 0.0540% O
0.06% C, 17.7% Cr, 15.1% Co, 3.0% Mo, 1.4% W, 4.8% Ti, 2.4% Al, 0.02% B, balance is Ni
0.06% C, 3% Fe, 21.5% Cr, 9% Mo, 4% Nb, balance is Ni
0.06% Si, 0.14% Fe, 0.04% Cu, 0.19% Mn, 1.16% Mg, 0.17% Cr, 4.70% Zn, 0.04% Ti, 0.16% Zr, balance is Al
0.06% C, 0.67% Mn, 6.66% Fe, 0.26% Si, 0.06% Cu, 16.66% Cr, 0.70% Al, 2.36% Ti, 0.92% Nb, balance is Ni
0.06% C, 19.30% Cr, 14.60% Co, 4.39% Mo, 3.08% Ti, 1.42% Al, 0.051% Zr, balance is Ni
0.06% C, 19.60% Co, 20.1% Cr, 6.00% Mo, 2.00% Ti, 0.4% Al, 0.001% Cu, 0.0013% O, 0.006% N, balance is Ni
0.06% C, 20% Cr, 2.4% Ti, 1.4% Al, balance is Ni
0.06% Ca, balance is Pb
0.06% C, 20.06% Cr, 9.81% Ni, 14.88% W, 1.66% Mn, 0.86% Si, 0.23% Fe, balance is Co
0.066% C, 0.89% Mn, 0.29% Si, 25.09% Ni, 19.84% Cr, 1.51% Mo, <0.01% Ti, 0.26% Nb, 0.15% N, <0.001% S, <0.005% P, 0.0026% B, balance is Fe
0.07% C, 15.10% Cr, 18.30% Co, 5.33% Mo, 3.34% Ti, 4.29% Al, 0.024% B, balance is Ni
0.07% C, 15.10% Cr, 18.30% Co, 5.33% Mo, 8.84% Ti, 4.29% Al, 0.024% B, balance is Ni
0.071% C, 0.004s Si, 0.062% Mn, 0.002% P, 0.004% S, 19.36% Cr, 13.9% Co, 0.20% Fe, 4.40% Mo, 1.55% Al, 3.03% Ti, 0.062% Zr, balance is Ni
0.08% C, max. 0.35% Mn, max. 0.35% Si, max. 0.015% P, max. 0.015% S, 17.0-21.0% Cr, max. l.00% Co, 2.80-3.30% Mo, 4.75-5.50% Nb+Ta, 0.65-1.15% Ti, 0.20-0.80% Al, max. 0.30% Cu, 50.0-55.0 Ni+Co, max. 0.006% B, balance is Fe
0.08% C, 15.0% Cr, 18.5% Co, 5.2% Mo, 3.5% Ti, 4.3% Al, 0.030% B, balance is Ni
0.08% C, 16.0% Cr, 10.0% Co, 4.8% Mo, 2.0% W, 4.8% Nb, 2.7% Ti, 1.5% Ta, 1.0% Al, balance is Ni
0.08% C, 0.5% Mn, 8% Fe, 0.25% Cu, 15.5% Cr, balance is Ni
0.08% C, 0.5% Mn, 8% Fe, 0.25% Cu, 15.5% Cr, balance is Ni
0.08% C, 0.5% Mn, 8% Fe, 0.25% Cu, 15.5% Cr, balance is Ni
0.08% C, 0.5% Mn, 8% Fe, 0.25% Cu, 15.5% Cr, balance is Ni
0.08% C, 0.5% Mn, 8% Fe, 0.25% Cu, 15.5% Cr, balance is Ni
0.08% C, 0.50% Fe, 19.00% Cr, 11.00% Co, 9.75% Mo, 3.15% Ti, 1.50% Al, 0.006% B, balance is Ni
0.08% C, 0.6% Ti, 3.2% Al, 16.6% Cr, 1.0% max Fe, balance is Ni
0.08% C, 15.0% Cr, 18.5% Co, 5.2% Mo, 3.5% Ti, 4.3% Al, 0.030% B, balance is Ni
0.08% C, 18.86% Cr, 2.99% Mo, 0.93% Ti, 0.57% Al, 5.25% Nb, 17.48% Fe, balance is Ni
0.08% C, 19.31% Cr, 10.02% Co, 9.11% Mo, 3.23% Ti, 1.51% Al, 0.000% B, 2.34% Fe, balance is Ni
0.08% C, 19.31% Cr, 10.82% Co, 9.77% Mo, 2.34% Fe, 3.23% Ti, 1.51% Al, 0.006% B, balance is Ni
0.08% Ca, balance is Pb
0.08% C, max. 0.36% Mn, max. 0.36% Si, max. 0.016% P, max. 0.016% S, 17.0-21.0% Cr, max. 1.0% Co, 2.80-3.30% Mo, 4.76-6.60% Nb+Ta, 0.66-1.16% Ti, 0.20-0.80% Al, max. 0.30% Cu, 60.0-66.0 Ni+Co, max. 0.006% B, balance is Ni
0.10% C, 7.96% Cr, 9.70% Co, 5.89% Mo, 1.03% Ti, 0.06% Al, 0.015% B, 0.084% Zr, 4.25% Ta, balance is Ni
0.10% C, 8.25% Cr, 9.50% Co, 5.89% Mo, 1.07% Ti, 5.93% Al, 0.016% B, 0.10% Zr, 4.19% Ta, balance is Ni
0.10% Si, 0.26% Fe, 0.16% Cu, 0.25% Mn, 1.24% Mg, 0.17% Cr, 4.47% Zn, 0.03% Ti, 0.13% Zr, Zn/Mg=3.60, balance is Al
0.10% Si, 0.26% Fe, 0.16% Cu, 0.25% Mn, 1.24% Mg, 0.17% Cr, 4.47% Zn, 0.03% Ti, 0.13% Zr, Zn/Mg=3.60, balance is Al
0.10-0.30% Fe, 0.35-0.60% Mg, 0.30-0.60% Si, max. 0.10% Cu, max. 0.15% Zn, max. 0.10% Ti, max. 0.05% Cr, balance is Al
0.10% C, 20.0-23.0% Cr, 8.0-10.0% Mo, max. 5.0% Fe, max. 0.015% P, max. 0.5% Si, max. 0.015% S, max. 0.50% Mn, Cb+Ta: 3.15-4.15%, max. 0.40% Al, max. 0.40% Ti, balance is Ni
0.10% Mn, <0.05% Cr, <0.10% Si, <0.15% Fe, 2.60-3.30% Cu, 0.01-0.06% Ti, <0.25% Zn, 0.005-0.05% Ce, 0.08-0.14% Zr, <0.10% Mn, 0.008-0.10% Be, <0.002% Na, 1.80-2.30% Li, balance is Al
0.10% C, 20.5% Cr, 75.00% Ni, 2.35% Ti, 1.25% Al
0.10% Cr, 0.20% Fe, 1.40% Sn, 0.12% O, 98.18% Zr
0.10-0.30% Fe, 0.35-0.60% Mg, 0.30-0.60% Si, max. 0.10% Cu, max. 0.15% Zn, max. 0.10% Ti, max. 0.05% Cr, balance is Al
0.1% Ca, balance is Pb
0.1% Ca, balance is Pb
0.10% C, 0.50% Mn, 0.50% Si, 0.015% S, 0.015% P, 58.00% Ni, 20.00-23.00% Cr, 8.00-10.0% Mo, 5.00% Fe, 1.00% Co, 0.40% Ti, 0.40% Al, 3.15-4.14% Nb+Ta
0.10% C, max. 0.50% Si, max. 0.50% Mn, max. 0.015% P, max. 0.40% Al, 20.00-23.00% Cr, 8.00-10.00% Mo, max. 5.00% Fe, max. 0.40% Ti, 3.15-4.15% Nb/Ta, balance is Ni
0.1% Cr, max. 0.1% Cu, max. 0.35% Fe, 0.45-0.9% Mg, max. 0.1% Mn, max. 0.15% Others, 0.2-0.6% Si, max. 0.1% Ti, max. 0.1% Zn, balance is Al
0.10% C, 20.0-23.0% Cr, 8.0-10.0% Mo, max. 5.0% Fe, max. 0.015% P, max. 0.5% Si, max. 0.015% S, max. 0.50% Mn, Cb+Ta: 3.15-4.15%, max. 0.40% Al, max. 0.40% Ti, balance is Ni
0.10% C, 20.0-23.0% Cr, 8.0-10.0% Mo, max. 5.0% Fe, max. 0.015% P, max. 0.5% Si, max. 0.015% S, max. 0.50% Mn, Cb+Ta: 3.15-4.15%, max. 0.40% Al, max. 0.40% Ti, balance is Ni
0.10% C, 20.0-23.0% Cr, 8.0-10.0% Mo, max. 5.0% Fe, max. 0.015% P, max. 0.5% Si, max. 0.015% S, max. 0.50% Mn, Cb+Ta: 3.15-4.15%, max. 0.40% Al, max. 0.40% Ti, balance is Ni
0.11% Si, 0.24% Fe, 0.13% Cu, 0.06% Mn, 2.63% Mg, 7.28% Zn, 0.01% Ni, 0.02% Cu, 0.05% Ti, 0.11% Zr, balance is Al
0.11% Si, 0.17% Fe, 0.04% Cu, 0.15% Mn, 1.10% Mg, 0.11% Cr, 4.37% Zn, 0.03% Ti, balance is Al
0.11% Ca, 0.57% Sn, balance is Pb
0.12% Si, max. 0.15% Fe, 1.4-2.1% Cu, max. 0.20% Mn, 1.8-2.7% Mg, 7.5-8.7% Zn, max. 0.25% Ti, balance is Al
0.128% Ca, balance is Pb
0.128% Ca, balance is Pb
0.13% C, 5.92% Cr, 2.05% Mo, 1.01% Ti, 5.27% Al, 7.46% Co, 0.38% Hf, 8.97% Ta, 5.92% W, 0.32% Re, 0.10% Zr, 0.020% B, 0.47% Nb, balance is Ni
0.13% C, 5.92% Cr, 2.05% Mo, 1.01% Ti, 5.27% Al, 7.46% Co, 0.38% Hf, 8.97% Ta, 5.92% W, 0.32% Re, 0.10% Zr, 0.020% B, 0.47% Nb, balance is Ni
0.13% Si, 0.20% Fe, 0.05% Cu, 0.24% Mn, 2.87% Mg, 0.19% Cr, 4.25% Zn, 0.02% Ti, 0.01% Zr, 0.24% Ni, Zn/Mg=1.48, balance is Al
0.13% Si, 0.20% Fe, 0.05% Cu, 0.24% Mn, 2.87% Mg, 0.19% Cr, 4.25% Zn, 0.02% Ti, 0.01% Zr, 0.24% Ni, Zn/Mg=1.48, balance is Al
0.13% Si, 0.20% Fe, 0.05% Cu, 0.24% Mn, 2.87% Mg, 0.19% Cr, 4.25% Zn, 0.02% Ti, 0.01% Zr, 0.24% Ni, balance is Al
0.14% C, 9.51% Cr, 10.3% Co, 2.06% Ti, 5.05% Al, 12.15% W, 0.010% B, 0.048% Zr, 0.99% Nb, balance is Ni
0.14% C, 9.51% Cr, 10.3% Co, 2.06% Ti, 5.05% Al, 12.15% W, 0.010% B, 0.048% Zr, 0.99% Nb, balance is Ni
0.14% Sc, 0.23% Sc, 0.35% Sc, 0.40% Sc, 0.55% Sc, balance is Al
0.15% C, 22.5% Cr, 19.0% Co, 2.0% W, 1.0% Nb, 1.4% Ta, 8.7% Ti, 1.9% Al, 0.1% Zr, 0.01% B, balance is Ni
0.15% C, 6.86% Cr, 4.82% Co, 2.04% Mo, 1.08% Ti, 5.25% Al, 5.36% W, 0.023% B, 0.039% Zr, 8.17% Ta, 0.89% Nb, 2.01% Hf, 0.90% Re, balance is Ni
0.15% V, balance is Ti
0.15% C, 19.11% Co, 22.46% Cr, 3.71% Ti, 1.99% Al, 1.97% W, 1.44% Ta, 0.99% Nb, 0.09% Zr, 0.01% B, 0.002% P, 0.001% S, balance is Ni
0.157% Fe, 0.058% Si, 0.022% Zn, 0.013% Cu, 0.006% V, 0.004% Ni, 0.002% Ti, 0.001% Mn, balance is Al
0.16% C, 6.03% Cr, 7.19% Co, 2.24% Mo, 0.98% Ti, 5.26% Al, 5.78% W, 0.018% B, 0.12% Zr, 8.82% Ta, 0.84% Nb, 0.46% Hf, 0.57% Re, balance is Ni
0.16% C, 9.00% Cr, 10.0% Co, 2.50% Mo, 1.50% Ti, 6.60% Al, 10.0% W, 0.010% B, 0.05% Zr, 1.5% Ta, balance is Ni
0.17% Al, 4.97% Zr, 0.49% Mo, 0.22% Si, 0.10% 0, 0.029% N, balance is Ti
0.17% Al, 4.97% Zr, 0.49% Mo, 0.22% Si, 0.10% 0, 0.029% N, balance is Ti
0.17% C, 10.30% Cr, 14.30% Co, 2.89% Mo, 4.73% Ti, 6.79% Al, 0.016% B, 0.076% Zr, 0.93% V, balance is Ni
0.17% C, 10.30% Cr, 15.00% Co, 2.93% Mo, 4.68% Ti, 6.53% Al, 0.016% B, 0.082% Zr, 0.94% V, balance is Ni
0.18% C, 14.26% Co, 10.26% Cr, 2.97% Mo, 5.35% Ti, 5.00% Al, 0.30% Fe, 0.92% V, 0.012% B, 0.05% Zr, balance is Ni
0.18% C, 14.26% Co, 10.26% Cr, 2.97% Mo, 5.35% Ti, 5.00% Al, 0.30% Fe, 0.92% V, 0.012% B, 0.05% Zr, balance is Ni
0.19% Si, 0.11% Fe, 1.50% Cu, 0.04% Mn, 2.64% Mg, 0.18% Zn, 0.04% Ti, balance is Al
0.2% Zn, 0.6---1.2% Mg, <0.10% Cu, 0.40---1.0% Mn, 0.25% Cr, <0.1% Ti, <0.50% Fe, 0.7-1.2% Si, balance is Al
0.2% Zn, 0.6---1.2% Mg, <0.10% Cu, 0.40---1.0% Mn, 0.25% Cr, <0.1% Ti, <0.50% Fe, 0.7-1.2% Si, balance is Al
0.20% Zn, 0.60-1.20% Mg, 0.10% Cu, 0.40-1.00% Mn, 0.25% Cr, 0.10% Ti, 0.50% Fe, 0.70-1.30% Si, balance is Al
0.20% Si, 1.10% Fe, 2.40% Cu, 0.01% Mn, 1.55% Mg, 0.004% Cr, 1.10% Ni, 0.10% Zn, 0.06% Ti, 0.001% Zr, balance is Al
0.20% Si, 1.10% Fe, 2.40% Cu, 0.01% Mn, 1.55% Mg, 0.004% Cr, 1.10% Ni, 0.10% Zn, 0.06% Ti, 0.001% Zr, balance is Al
0.20-0.30% C, max. 1.00% Si, 25.00-29.00 Cr, max. 1.00% Mn, max. 1.00% Si, max. 0.007% B, balance is Co
0.2% Sc, balance is Al
0.23% Cr, 1.60% Cu, 2.50% Mg, 5.60% Zn, 90.00% Al
0.25% C, 0.60% Mn, 0.60% Si, 27% Cr, 3% Ni, 5% Mo, 1% Fe, balance is Co
0.25 at.% Ti, balance is Pu
0.25% Si, 0.35% Fe, 1.90% Cu, 0.20% Mn, 2.90% Mg, 0.22% Cr, 8.2% Zn, 0.10% Ti, balance is Al
0.25% C, 0.003% S, 0.21% Mn, 0.61% Si, 0.0014% P, 28.00% Cr, 0.43% Ni, 5.82% Mo, 0.02% W, 0.38% Fe, balance is Co
0.25% C, 0.003% S, 0.21% Mn, 0.61% Si, 0.0014% P, 28.00% Cr, 0.43% Ni, 5.82% Mo, 0.02% W, 0.38% Fe, balance is Co
0.25% Si, 0.35% Fe, 1.90% Cu, 0.20% Mn, 2.90% Mg, 0.22% Cr, 8.20% Zn, 0.10% Ti, balance is Al
0.26 at.% Cr, 0.6 at.% Mo, balance is U
0.30-0.60% Si, 0.10-0.30% Fe, 0.10% Cu, 0.10% Mn, 0.35-0.60% Mg, 0.05% Cr, 0.15% Zn, 0.10% Ti, balance is Al
0.3 at.% Cr, balance is U
0.33% C, 11.93% Cr, 14.20% Co, 5.05% Mo, 3.04% Ti, 4.60% Al, 4.93% W, 0.014% B, 0.10% Zr, 1.48% Ta, balance is Ni
0.33% C, 11.93% Cr, 14.20% Co, 5.05% Mo, 3.04% Ti, 4.60% Al, 4.93% W, 0.014% B, 0.10% Zr, 1.48% Ta, balance is Ni
0.34% Si, 0.07% Cr,38.1% Ni, 0.05% Al, 0.0085% B, 14.30% Co, 4.68% Nb, 1.54% Ti, balance is Fe
0.35% C, 11.92% Cr, 14.05% Co, 4.94% Mo, 4.87% W, 3.02% Ti, 4.60% Al, 0.013% B, 0.10% Zr, 1.56% Ta, balance is Ni
0.38% Si, 0.209% Fe, 4.64% Cu, 0.58% Mn, 1.50% Mg, 0.007% Cr, 0.066% Zn, 0.050% Ti, balance is Al
0.39% Si, 0.22% Fe, 0.01% Cu, 0.02% Mn, 0.43% Mg, 0.001% Cr, 0.01% Zn, 0.009% Ti, balance is Al
0.4-1.0% Cr, 1.6-2.0% Fe, max. 0.01% C, max. 1.0% Mn, max. 0.08% Si, max. 0.5% Cu, 26.0-30.0% Mo, max. 1.0% Co, max. 0.02% P, max. 0.010% S, balance is Ni
0.40% Si, 0.50% Fe, 1.2-2.0% Cu, 0.30% Mn, 2.1-2.9% Mg, 0.18-0.28% Cr, 5.1-6.1% Zn, 0.20% Ti, balance is Al
0.40% Si, 0.50% Fe, 1.60% Cu, 0.30% Mn, 2.50% Mg, 0.23% Cr, 5.60% Zn, Zn/Mg=2.24, balance is Al
0.40% Si, 0.50% Fe, 1.60% Cu, 0.30% Mn, 2.50% Mg, 0.23% Cr, 5.60% Zn, Zn/Mg=2.24, balance is Al
0.40-0.80% Si, max. 0.70% Fe, max. 0.15% Mn, 0.80-1.20% Mg, 0.03-0.35% Cr, max. 0.25% Zn, max. 0.15% Ti, balance is Al
0.40-0.8% Si, max. 0.7% Fe, 0.15-0.40% Cu, max. 0.15% Mn, 0.8-1.2% Mg, 0.04-0.35% Cr, max. 0.25% Zn, max. 0.15% Ti, balance is Al
0.40% Si, max. 0.50% Fe, 1.2-2.0% Cu, max. 0.30% Mn, 2.1-2.9% Mg, 0.18-0.28% Cr, 5.1-6.1% Zn, max. 0.20% Ti, balance is Al
0.45 at.% Cr, balance is U
0.45% Mg, 0.25% Mn, 2.60% Cu, 96.70% Al
0.5% Fe, 0.15% Si, 1.0% Mn, balance is Al
0.5% Fe, 0.15% Si, 1.0% Mn, balance is Al
0.5% Fe, 0.15% Si, 1.0% Mn, balance is Al
0.5% Fe, 0.15% Si, 1.0% Mn, balance is Al
0.5% Fe, 0.15% Si, 1.0% Mn, balance is Al
0.5% Fe, 0.15% Si, 1.0% Mn, balance is Al
0.5% Cr, 0.5% Mo, balance is U
0.5% Nb, 0.5% Mo, balance is U
0.5% Nb, 0.5% Mo, balance is U
0.50% Si, 0.50% Fe, 3.80-4.90% Cu, 0.30-0.90% Mn, 1.20-1.80% Mg, 0.10% Cr, 0.25% Zn, 0.15% Ti, balance is Al
0.50% Si, 0.50% Fe, 3.80-4.90% Cu, 0.30-0.90% Mn, 1.20-1.80% Mg, 0.10% Cr, 0.25% Zn, 0.15% Ti, balance is Al
0.50% Si, 0.50% Fe, 3.80-4.90% Cu, 0.30-0.90% Mn, 1.20-1.80% Mg, 0.10% Cr, 0.25% Zn, 0.15% Ti, balance is Al
0.50% Si, 0.50% Fe, 3.80-4.90% Cu, 0.30-0.90% Mn, 1.20-1.80% Mg, 0.10% Cr, 0.25% Zn, 0.15% Ti, balance is Al
0.50% Si, 0.19% Fe, 0.02% Cu, 0.03% Mn, 0.005% Cr, 0.03% Zn, 0.013% Ti, balance is Al
0.50% Si, 0.19% Fe, 0.02% Cu, 0.03% Mn, 0.005% Cr, 0.03% Zn, 0.013% Ti, balance is Al
0.50% Si, 0.50% Fe, 3.80-4.90% Cu, 0.30-0.90% Mn, 1.20-1.80% Mg, 0.10% Cr, 0.25% Zn, 0.15% Ti, balance is Al
0.50% Si, 0.50% Fe, 3.80-4.90% Cu, 0.30-0.90% Mn, 1.20-1.80% Mg, 0.10% Cr, 0.25% Zn, 0.15% Ti, balance is Al
0.50% Si, 0.50% Fe, 3.80-4.90% Cu, 0.30-0.90% Mn, 1.20-1.80% Mg, 0.10% Cr, 0.25% Zn, 0.15% Ti, balance is Al
0.55% C, 11.92% Cr, 14.05% Co, 4.94% Mo, 4.87% W, 3.02% Ti, 4.60% Al, 0.013% B, 0.10% Zr, 1.56 Ta, balance is Ni
0.55% Mg, 0.08% Si, 0.01% Cr, 0.014% Mn, 0.11% Fe, 0.036% Cu, 0.01% Ti, 0.002% B, balance is Al
0.59% Si, 0.19% Fe, 0.02% Cu, 0.03% Mn, 0.47% Mg, 0.005% Cr, 0.03% Zn, 0.013% Ti, balance is Al
0.60 at.% Cr, balance is U
0.60% C, 0.83% Mg, 0.29% Mn, 0.71% Si, 0.21% Fe, 0.10% Zn, 0.03% Ti, 0.05% Cr, 0.0008% B, 0.05% Zr, balance is Al
0.60% C, 0.83% Mg, 0.29% Mn, 0.71% Si, 0.21% Fe, 0.10% Zn, 0.03% Ti, 0.05% Cr, 0.0008% B, 0.05% Zr, balance is Al
0.6% Cu, 0.83% Mg, 0.29% Mn, 0.71% Si, 0.21% Fe, 0.1% Zn, 0.03% Ti, 0.05% Cr, 0.0008% B, 0.05% Zr, balance is Al
0.6% Cu, 0.83% Mg, 0.29% Mn, 0.71% Si, 0.21% Fe, 0.1% Zn, 0.03% Ti, 0.05% Cr, 0.0008% B, 0.05% Zr, balance is Al
0.60% Mg, 0.30% Si, 0.02% Mn, 0.16% Fe, 0.01% Zn, 0.02% Ti, balance is Al
0.60% Mg, 0.60% Mn, 1.00% Si, 97.80% Al
0.63% Mg, 0.76% Si, 0.12% Cr, 0.109% Zr, 0.11% Mn, 0.138% Fe, 0.04% Zn, 0.01% Ti, balance is Al
0.65% Mg, 0.52% Si, 0.11% Fe, balance is Al
0.65% Si, 0.81% Mg, 0.32% Fe, 0.26% Cu, 0.01% Ni, 0.05% Zn, 0.09% Cr, 0.04% Ti, 0.06% Mn, balance is Al
0.65% Si, 0.81% Mg, 0.32% Fe, 0.26% Cu, 0.01% Ni, 0.05% Zn, 0.09% Cr, 0.04% Ti, 0.06% Mn, balance is Al. 6061 B: 0.6% Si, 1.01% Mg, 0.2% Fe, 0.2% Cu, 0.09% Zn, 0.17% Cr, 0.01% Ti, 0.06% Mn, balance is Al.
0.68% Si, 0.2% Fe, 0.01% Cu, 0.11% Mn, 0.57% Mg, 0.04% Cr, 0.01% Zn, 0.018% Ti, balance is Al
0.68% Si, 0.2% Fe, 0.01% Cu, 0.11% Mn, 0.57% Mg, 0.04% Cr, 0.01% Zn, 0.018% Ti, balance is Al
0.68% Si, 0.20% Fe, 0.01% Cu, 0.11% Mn, 0.57% Mg, 0.04% Cr, 0.01% Zn, 0.018% Ti, balance is Al
0.68% Si, 0.20% Fe, 0.01% Cu, 0.11% Mn, 0.57% Mg, 0.040% Cr, 0.01% Zn, 0.018% Ti, balance is Al
0.68% Si, 0.20% Fe, 0.01% Cu, 0.11% Mn, 0.57% Mg, 0.040% Cr, 0.01% Zn, 0.018% Ti, balance is Al
0.68% Si, 0.20% Fe, 0.01% Cu, 0.11% Mn, 0.57% Mg, 0.040% Cr, 0.01% Zn, 0.018% Ti, balance is Al
0.69% Si, 0.196% Fe, 0.046% Cu, 0.45% Mn, 0.62% Mg, <0.003% Cr, <0.008% Zn, 0.002% Ti, balance is Al
0.72% Si, <5 ppm Fe, <4 ppm Cu, <3 ppm Mn, <1 ppm Mg, <3 ppm Cr, <14 ppm Zn, <20 ppm Ti, balance is Al
0.73% Si, 0.22% Fe, 0.05% Cu, 0.48% Mn, 0.61% Mg, 0.003% Cr, 0.009% Zn, balance is Al
0.79% Si, 0.001% Fe, 0.0005% Cu, 0.0005% Mn, 0.59% Mg, 0.0005% Cr, 0.001% Zn, balance is Al
0.8-1.8% Al, 7.6-8.6% V, 4.0-6.0% Fe, max 0.06% C, balance is Ti
0.81% Mg, 1.18% Si, 0.14% Cr, 0.09% Zr, 0.14% Mn, 0.39% Fe, 0.02% Cu, 0.01% Zn, 0.03% Ti, balance is Al
0.82 at.% Ti, balance is Pu
0.89% Si, 0.13% Zn, 0.065% P, 0.009% Sn, 2.08% Ni, 0.001% Sb, 0.001% Bi, 0.001% As, 0.001% Cd, 97.02% Cu
0.9% Mn, 0.35% Fe, 0.04% Si, balance is Al
0.9% Mn, 0.35% Fe, 0.04% Si, balance is Al
0.9% Mn, 0.85% Fe, 0.04% Si, balance is Al
0.9% Mg, 0.62% Si, 0.33% Fe, 0.17% Cr, 0.06% Mn, 0.02% Zn, 0.02% Ti, balance is Al
0.92% H, 0.0875% 0, 0.0038% N, 0.0909% Fe, 0.0048% Si, 0.0052% Al, 0.0025% Mn, balance is Zr
0.96% Cr, balance is U
0.96% Cr, balance is U
0.98-1.10% Mg, 1.00-1.12% Si, 0.52-0.61% Mn, 0.10% Cu, 0.50% Fe, 0.20% Zn, 0.25% Cr, balance is Al
0.98% Mg, 0.66% Si, 0.12% Cr, 0.12% Mn, 0.38% Fe, 0.23% Cu, 0.07% Zn, 0.014% Ti, 0.001% B, balance is Al
1.00% Co, max. 1.00% Cr, 26.00%-30.00% Mo, max. 2.00% Fe, max. 0.10% Si, max. 1.00% Mn, max. 0.02% C, max. 0.040% P, max. 0.030% S, balance is Ni
1.0% Mo, balance is Ti
1.00% Si, 0.80% Mg, 0.50% Mn, 0.35% Cu, 97.30% Al
1.00% Co, max. 1.00% Cr, 26.00%-30.00% Mo, max. 2.00% Fe, max. 0.10% Si, max. 1.00% Mn, max. 0.02% C, max. 0.040% P, max. 0.080% S, balance is Ni
1.022% Si, 0.149% Fe, <0.001% Cu, 0.547% Mn, 0.645% Mg, <0.002% Cr, 0.012% Zn, balance is Al
1.05 at.% Ti, balance is Pu
1.1036% Mg, 0.676% Si, 0.078% Mn, 0.1495% Cu, 0.1495% Fe, 0.1495% Cr, 0.1495% Ni, 0.21% Zn, 0.0273% Ti, balance is Al
1.20-1.70% Sn, 0.18-0.24% Fe, 0.07-0.13% Cr, 0.28-0.37% Fe+Cr, balance is Zr
1.23% Si, 0.20% Fe, 0.009% Cu, 0.65% Mn, 1.05% Mg, 0.2% Cr, 0.05% Zn, 0.03% Ti, balance is Al
1.3% Mo, balance is Zr
1.4-2.1% Cu, max. 0.15% Fe, 1.8-2.7% Mg, max. 0.20% Mn, max. 0.12% Si, 7.5-8.7% Zn, max. 0.25% Zr+Ti, max. 0.15% Others, balance is Al
1.42% Sn, 0.11% Fe, 0.09% Cr, 0.04% Ni, 0.165-0.170% O, 0.007% N, 0.018-0.066% C, 0.070-0.080% H, <0.07% (Al, Cu, Hf, Mo), 0.0025% (Cd, Co, Pb, Mg, Mn, Si, W, V), balance is Zr
1.42% Sn, 0.11% Fe, 0.09% Cr, 0.04% Ni, 0.165-0.170% O, 0.007% N, 0.018-0.066% C, 0.070-0.080% H, <0.07% (Al, Cu, Hf, Mo), 0.0025% (Cd, Co, Pb, Mg, Mn, Si, W, V), balance is Zr
1.5% Be, balance is Cu. b.) 2% Be, balance is Cu. c.) 1.8% Be, 0.2% Co, balance is Cu.
1.5% Be, balance is Cu. b.) 2% Be, balance is Cu. c.) 1.8% Be, 0.2% Co, balance is Cu.
1.50% Li, 3.80% Cu, 0.50% Zn, 0.40% Mn, 0.10% Zr, 0.05% Fe, 0.03% Si, balance is Al
1.58% Mn, balance is Mg
1.6 at.% Ga, balance is U
1.77% Be, 0.24% Co, balance is Cu
1.80 at.% Cr, balance is U
1.87% Be, 0.14% Co, balance is Cu
1.9 at.% Ga, balance is Pu
1.93% Sn, 1.95% Mo, 3.97% Zr, <0.01% C, 0.07% Fe, 0.11% Si, 6.13% Al, balance is Ti
1.93% Sn, 1.95% Mo, 3.97% Zr, <0.01% C, 0.07% Fe, 0.11% Si, 6.13% Al, balance is Ti
2.0% CaO, 35.0% SiO2, 4.6% Al2O3, 1.5% MgO, 0.83% Cu, 0.59% S, 0.96% Zn, 0.14% As, 0.05% Cr, 0.15% Pb, 7.5% Magnetite
2% Cr, 3% Co, 0.4% Mo, 5% W, 6% Re, 0.1% Nb, 5.7% Al, 0.2% Ti, 0.03% Hf, balance is Ni
2% Ni, 1% Si, 97% Cu
2% Zr, balance is U
2MgO x 2Al2O3 x 5SiO2
2.0% CaO, 35.0% SiO2, 4.6% Al2O3, 1.5% MgO, 37.9% TFe, 0.83% Cu, 0.59% S, 0.96% Zn, 0.14% As, 0.05% Cr, 0.15% Pb, 7.6% magnetite
2% Co, 16% Cr, 16% Mo, max. 3% Fe, max. 1% Mn, max. 0.7% Ti, max. 0.08% Si, max. 0.01% C, max. 0.5% Cu, balance is Ni
2.25% Al, 11.0% Sn, 5.0% Zr, 1.0% Mo, 0.25% Si, balance is Ti
2.28% Li, 0.86% Cu, 0.90% Mg, 0.13% Zr, 0.13% Fe, 0.06% Si, balance is Al
2.28% Li, 0.86% Cu, 0.90% Mg, 0.13% Zr, 0.13% Fe, 0.06% Si, balance is Al
2.28% Li, 0.86% Cu, 0.90% Mg, 0.13% Zr, 0.13% Fe, 0.06% Si, balance is Al
2.28% Li, 0.86% Cu, 0.90% Mg, 0.13% Zr, 0.13% Fe, 0.06% Si, balance is Al
2.35% Cr, balance is Ti
2.5% Zr, 7.5% Nb, balance is U
2.55% Mg, 5.44% Zn, 1.37% Cu, 0.15% Si, 0.39% Fe, 0.22% Mn, 0.21% Cr, 0.05% Ti, 0.02% Ni, balance is Al
2.6% Al, 7.5% Mo, balance is Ti
2.6% Al, 7.6% Mo, balance is Ti
2.60% MgO, 5.90% Al2O3, 16.5% R2O (R=Na,K,Li), 8.60% F, basicity=0.8
2.60% MgO, 5.90% Al2O3, 16.50% sum R2O (R=Na, K, Li), 8.60% F, basicity=8.0
2.6-3.4% Al, 0.05% C, 1.6-2.2% Fe, 0.015% H, 0.05% N, 0.13% O, 9-11% V, balance is Ti
2.6-3.4% Al, 0.05% C, 1.6-2.2% Fe, 0.015% H, 0.05% N, 0.13% O, 9-11% V, balance is Ti
2.68% Li, 1.36% Cu, 0.89% Mg, 0.13% Zr, 0.17% Fe, 0.04% Si, balance is Al
2.68% Li, 1.36% Cu, 0.89% Mg, 0.13% Zr, 0.17% Fe, 0.04% Si, balance is Al
2.68% Li, 1.36% Cu, 0.89% Mg, 0.13% Zr, 0.17% Fe, 0.04% Si, balance is Al
2.68% Li, 1.36% Cu, 0.89% Mg, 0.13% Zr, 0.17% Fe, 0.04% Si, balance is Al
2.7% Cu, 1.6% Li, 0.09% Zr, 0.05% Fe, 0.005% Si, 0.1% Ti, balance is Al
2.7% Cu, 1.6% Li, 0.09% Zr, 0.05% Fe, 0.005% Si, 0.1% Ti, balance is Al
2.7% Cu, 1.6% Li, 0.09% Zr, 0.05% Fe, 0.005% Si, 0.1% Ti, balance is Al
2.7% Cu, 1.6% Li, 0.09% Zr, 0.05% Fe, 0.005% Si, 0.1% Ti, balance is Al
2.7% Cu, 1.6% Li, 0.09% Zr, 0.05% Fe, 0.005% Si, 0.1% Ti, balance is Al
2.7% Cu, 1.6% Li, 0.09% Zr, 0.05% Fe, 0.05% Si, 0.10% Ti, balance is Al
2.7% Cu, 1.6% Li, 0.09% Zr, 0.05% Fe, 0.05% Si, 0.10% Ti, balance is Al
2.7% Cu, 1.6% Li, 0.09% Zr, 0.06% Fe, 0.005% Si, 0.1% Ti, balance is Al
2.91% Mn, balance is Ti. b.) 7.72% Mn, balance is Ti. c.) 12.3% Mn, balance is Ti.
3% Ti, balance is Cu
3Al8V6Cr4Mo4Zr
3.0% Cr, balance is Ti
3.0% Cr, balance is Ti
3.0% Cr, balance is Ti
3.0% Cr, balance is Ti
3.0% Cr, balance is Ti
3.0% Cr, balance is Ti
3.0% Mo, balance is Ti
3.0% Mo, balance is Ti
3.0% Mo, balance is Ti
3.03% Ni, balance is Ti
3.1% Al, 2.4% V, 0.006% C, 0.064% Fe, 0.0035% H, 0.0070% N, 0.0795% O, balance is Ti
3.1% Al, 2.4% V, 0.006% C, 0.064% Fe, 0.0035% H, 0.0070% N, 0.0795% O, balance is Ti
3.1% Al, 2.4% V, 0.006% C, 0.064% Fe, balance is Ti
3.1% Al, 2.4% V, 0.006% C, 0.064% Fe, balance is Ti
3.1% Al, 2.4% V, 0.006% C, 0.064% Fe, balance is Ti
3.1% Th, balance is Mg
3.30% Al, 4.70% Mo, 5.10% V, 4.00% Cr, 1.92% Zr, 0.01% C, 0.08% N, 0.01% H, 0.01% O, 0.08% Fe, <0.04% Si, balance is Ti
3.30% Al, 4.70% Mo, 5.10% V, 4.00% Cr, 1.92% Zr, 0.01% C, 0.08% N, 0.01% H, 0.01% O, 0.08% Fe, <0.04% Si, balance is Ti
3.30% Al, 4.70% Mo, 5.10% V, 4.00% Cr, 1.92% Zr, 0.01% C, 0.08% N, 0.01% H, 0.01% O, 0.08% Fe, <0.04% Si, balance is Ti
3.3% Mo, balance is Zr
3.39% Al, 3.18% Sn, 3.97% Mo, 0.50% Si, 0.22% 0, 0.022% N, balance is Ti
3.39% Al, 3.18% Sn, 3.97% Mo, 0.50% Si, 0.22% 0, 0.022% N, balance is Ti
3.4% Al, 8.3% V, 6.8% Cr, 4.2% Mo, 3.9% Zr, balance is Ti
3.90% Y, 2.20% Nd, 0.61% HR, 0.45% Zr, 0.01% Mn, 0.01% Zn, 0.01% Fe, 2.80% TR, <0.01% TO
3.92% Fe, 6.58% Al, 0.099% O, 0.013% Ni, 0.008% Cr, 0.003% C, 0.005% N, 0.0073% H, balance is Ti
3.93% Al, 3.18% Sn, 3.97% Mo, 0.50% Si, 0.22% 0, 0.022% N, balance is Ti
3.93% Al, 3.18% Sn, 3.97% Mo, 0.50% Si, 0.22% 0, 0.022% N, balance is Ti
3.93% Al, 3.18% Sn, 3.97% Mo, 0.50% Si, 0.22% 0, 0.022% N, balance is Ti
3.93% Al, 3.18% Sn, 3.97% Mo, 0.50% Si, 0.22% 0, 0.022% N, balance is Ti
3.93% Al, 3.18% Sn, 3.97% Mo, 0.50% Si, 0.22% 0, 0.022% N, balance is Ti
3.93% Al, 3.18% Sn, 3.97% Mo, 0.50% Si, 0.22% 0, 0.022% N, balance is Ti
3.93% Al, 3.18% Sn, 3.97% Mo, 0.50% Si, 0.22% 0, 0.022% N, balance is Ti
4.00 at.% Cr, balance is U
4% Cu, 1% Li, 0.3% Ag, 0.3% Mg, 0.1% Zr, balance is Al
4% Cu, 1% Li, 0.3% Ag, 0.3% Mg, 0.1% Zr, balance is Al
4% Cu, balance is Al
4% Cu, balance is Al
4% SrO, 96% GeO2
4% Ti, balance is Cu
4.0% Cr, 2.0% Mo, balance is Ti
4.0% Cr, 2.0% Mo, balance is Ti
4.0% Cr, 2.0% Mo, balance is Ti
4% Li, balance is Al
4.08% Al, 5.06% Cr, 5.05% Mo, 0.96% Nb, 4.90% V, 0.006% N, 0.011% C, 0.10% O, <0.001% H, balance is Ti
4.08% Cu, 0.72% Mg, 0.62% Mn, 0.60% Si, 0.27% Fe, O.O3% Ti, balance is Al
4.08% Cu, 0.72% Mg, 0.62% Mn, 0.60% Si, 0.27% Fe, O.O3% Ti, balance is Al
4.08% Cu, 0.72% Mg, 0.62% Mn, 0.60% Si, 0.27% Fe, O.O3% Ti, balance is Al
4.1% Al, 2.9% Mo, 1.0% V, balance is Ti
4.1% Al, 2.9% Mo, 1.0% V, balance is Ti
4.15% Al, max. 0.030% C, 14-16% Cr, 16-18% Co, 3.5-5.5% Mo, max. 3.65% Ti, 52.67-65.5% Ni
4.19% Cu, 0.46% Mg, 0.78% Mn, 0.82% Si, 0.33% Fe, 0.05% Ti, balance is Al
4.19% Cu, 0.46% Mg, 0.78% Mn, 0.82% Si, 0.33% Fe, 0.05% Ti, balance is Al
4.19% Cu, 0.46% Mg, 0.78% Mn, 0.82% Si, 0.33% Fe, 0.05% Ti, balance is Al
4.19% Cu, 0.46% Mg, 0.78% Mn, 0.82% Si, 0.33% Fe, 0.06% Ti, balance is Al
4.3% Al, 0.03% B, 0.07% C, 15.09% Cr, 18.5% Co, max. 1.0% Fe, 5.0% Mo, 2.4% Ti, balance is Ni
4.4% Cu, 0.8% Si, 0.5% Mg, max. 0.1% Cr, balance is Al
4.5%Zr, 2.25% Mg, balance is Al
4.5-5.5% Al, 3.5-4.5% Cr, max. 0.3% Fe, max. 0.0125% H, 3.5-4.5% Mo, max. 0.04% N, 1.5-2.5% Sn, 1.5-2.5% Zr, balance is Ti
4.5-5.5% Al, 3.5-4.5% Cr, max. 0.3% Fe, max. 0.0125% H, 3.5-4.5% Mo, max. 0.04% N, 1.5-2.5% Sn, 1.5-2.5% Zr, balance is Ti
4.52% Al, 2.41% Sn, 2.11% Zr, 3.78% Mo, 3.99% Cr, 0.063% 0, 0.031% C, 0.102% Fe, 0.0010% N, balance is Ti
4.52% Al, 2.41% Sn, 2.11% Zr, 3.78% Mo, 3.99% Cr, 0.063% 0, 0.031% C, 0.102% Fe, 0.0010% N, balance is Ti
4.52% Al, 2.41% Sn, 2.11% Zr, 3.78% Mo, 3.99% Cr, 0.063% 0, 0.031% C, 0.102% Fe, 0.0010% N, balance is Ti
4.52% Al, 2.41% Sn, 2.11% Zr, 3.78% Mo, 3.99% Cr, 0.063% 0, 0.031% C, 0.102% Fe, 0.0010% N, balance is Ti
4.52% Al, 2.41% Sn, 2.11% Zr, 3.78% Mo, 3.99% Cr, 0.063% 0, 0.031% C, 0.102% Fe, 0.0010% N, balance is Ti
4.52% Al, 2.41% Sn, 2.11% Zr, 3.78% Mo, 3.99% Cr, 0.063% 0, 0.031% C, 0.102% Fe, 0.0010% N, balance is Ti
4.52% Al, 2.41% Sn, 2.11% Zr, 3.78% Mo, 3.99% Cr, 0.063% 0, 0.031% C, 0.102% Fe, 0.0010% N, balance is Ti
4.57% Mo, balance is Ti
4.6-6.6% Al, 1.6-2.6% Sn, 1.6-2.6% Zr, 3.6-4.6% Mo, 3.6-4.6% Cr, 0.08-0.13% 0, max 0.30% Fe, balance is Ti
4.64% Cr, balance is Ti
4.64% Cu, 1.48% Mg, 0.82% Mn, 0.49% Fe, 0.02% Si, balance is Al
4.69% W, 0.23% C, balance is Co
4.75% Al, 2.5% Sn, balance is Ti
4.8 at.% Co, balance is Au
5% Al, 1% Sn, 1% V, 1% Zr, 0.8% Mg, 0.1% Fe, 0.1% Si, balance is Ti
5.0% Cr, balance is Ti
5.0% Cu, 3.0% Al, 2.0% Sn, balance is Ti
5.0% Mo, balance is Ti
5.10-6.10% Zn, 0.18-0.28% Cr, 1.20-2.00% Cu, 2.10-2.90% Mg, max. 0.50% Fe, max. 0.30% Mn, max.0.40% Si, max. 0.20% Ti, 87.10-91.40% Al
5.10-6.10% Zn, 0.18-0.28% Cr, 1.20-2.00% Cu, 2.10-2.90% Mg, max. 0.50% Fe, max. 0.30% Mn, max.0.40% Si, max. 0.20% Ti, 87.10-91.40% Al
5.10-6.10% Zn, 0.18-0.28% Cr, 1.20-2.00% Cu, 2.10-2.90% Mg, max. 0.50% Fe, max. 0.30% Mn, max.0.40% Si, max. 0.20% Ti, 87.10-91.40% Al
5.10-6.10% Zn, 0.18-0.28% Cr, 1.20-2.00% Cu, 2.10-2.90% Mg, max. 0.50% Fe, max. 0.30% Mn, max.0.40% Si, max. 0.20% Ti, balance is Al
5.10-6.10% Zn, 0.18-0.28% Cr, 1.20-2.00% Cu, 2.10-2.90% Mg, max. 0.50% Fe, max. 0.30% Mn, max.0.40% Si, max. 0.20% Ti, balance is Al
5.16% Mo, balance is Ti
5.2-6.2% Zn, 1.9 - 2.6% Mg, 1.2-1.9% Cu, 0.18-0.25% Cr, max 0.12% Fe, max 0.06% Mn, max. 0.1% Si, max. 0.06% Ti, balance is Al. 7A04 alloy: 6.7% Zn, 2.3% Mg, 1.68% Cu, 0.15% Cr, 0.50% Fe, 0.50% Si, 0.40% Mn, 0.1% Ti, balance is Al.
5.2% In, balance is Ni
5.21% Mo, 0.46% C, balance is Ti
5.4 to 12% Mo, balance is U
5.4 to 12% Mo, balance is U
5.4% Mo, 8% Mo, 10% Mo, 12% Mo, balance is U
5.4% Mo, 8% Mo, 10% Mo, 12% Mo, balance is U
5.4% Mo, balance is U
5.4% Mo, balance is U
5.4% Mo, balance is U
5.4% Mo, balance is Zr
5.42% Al, 2.05% V, 0.126% Cr, 0.003% H, 0.04% Fe, balance is Ti
5.44% Zn, 2.55% Mg, 1.37% Cu, balance is Al
5.5% Al, 5% V, 5% Mo, 2.4% Cr, 0.75% Fe, 0.15% O, balance is Ti
5.5% Mg, balance is Al
5.50-6.50% Al, 3.60-4.40% Zr, 1.80-2.20% Mo, 1.80-2.20% Sn, max. 0.15% O, max. 0.10% Si, max. 0.10% Fe, max. 0.10% Cu, max. 0.04% C
5.50-6.75% Al, 3.50-4.50% V, max. 0.40% Fe, max. 0.20% O, max. 0.05% N, max. 0.08% C, max. 0.015% H, max. 0.10% O
5.6% Zn, 2.5% Mg, 1.6% Cu, 0.23 Cr, balance is Al
5.67% Al, 2.13% V, 1.92% Nb, 0.109% O, 0.004% H, 0.11% Fe, balance is Ti
5.69% Al, 1.92% V, 1.70% Nb, 0.103% O, 0.006% H, 0.06% Fe, balance is Ti
5.70-6.70% Zn, 2.10-2.60% Mg, 1.50-2.0% Cu, 0.15% Fe, 0.10-0.16% Zr, 0.12% Si, 0.10% Mn, 0.060% Ti, 0.050% Cr, 0.050% Ni, 0.15% Others, balance is Al
5.7% Al, 0.68% Mo, 1.0% Ta, 2.1% Nb, 0.068% O, 0.010% H, 0.004% N, 0.04% Fe, balance is Ti
5.76% Al, 5.93% V, 0.116% O, 0.003% H, 0.05% Fe, balance is Ti
5.8% Al, 5.3% Mo, 5.1% V, 0.9% Cr, 0.8% Fe, 0.05% C, 0.15% Si, balance is Ti
5.8% Al, 5.3% Mo, 5.1% V, 0.9% Cr, 0.8% Fe, 0.05% C, 0.15% Si, balance is Ti
5.80% Al, 5.30% Mo, 5.10% V, 0.90% Cr, 0.80% Fe, 0.05% C, 0.15% Si, balance is Ti
5.86% Al, 2.05% Sn, 1.69% Zr, 1.01% Mo, 0.315% Bi, 0.102% Si, 0.067% Fe, 0.097% 0, 0.006% N, 0.0160% H, balance is Ti
5.86% Al, 2.05% Sn, 1.69% Zr, 1.01% Mo, 0.315% Bi, 0.102% Si, 0.067% Fe, O.O97% 0, 0.006% N, 0.0160% H, balance is Ti
5.86% Al, 2.05% Sn, 1.69% Zr, 1.01% Mo, 0.315% Bi, 0.102% Si, 0.067% Fe, O.O97% 0, 0.006% N, 0.0160% H, balance is Ti
5.9% Al, 0.60% Mo, 0.9% Ta, 2.0% Nb, 0.056% O, 0.011% H, 0.006% N, 0.04% Fe, balance is Ti
5.9% Al, 1.93% Sn, 3.90% Zr, 7.96% Mo, 0.076% Fe, 0.004% H, 0.124% 0, balance is Ti
5.9% Al, 1.93% Sn, 3.90% Zr, 7.96% Mo, 0.076% Fe, 0.004% H, 0.124% 0, balance is Ti
5.9% Al, 1.93% Sn, 3.90% Zr, 7.96% Mo, 0.076% Fe, 0.004% H, 0.124% 0, balance is Ti
5.9% Al, 1.93% Sn, 3.90% Zr, 7.96% Mo, 0.076% Fe, 0.004% H, 0.124% 0, balance is Ti
5.9% Al, 1.93% Sn, 3.90% Zr, 7.96% Mo, 0.076% Fe, 0.004% H, 0.124% 0, balance is Ti
5.9% Al, 1.99% Sn, 3.90% Zr, 7.96% Mo, 0.076% Fe, 0.004% H, 0.124% 0, balance is Ti
5.90% Al, 8.60% Co, 8.50% Cr, 0.90% Mo, 6.00% Re, 6.40% Ta, 5.90% W, balance is Ni
5.91% Al, 6.09% V, 0.095% O, 0.002% H, 0.06% Fe, balance is Ti
5.965% Be, trace Fe, balance is Cu
5.98% AL, 4.02% V, 0.04% Fe, balance is Ti
6.00% Al, 3.99% V, 0.25% Fe, 0.20% O, 0.02% C, 0.01% N, balance is Ti
6.0% Al, 3.99% V, 0.25% Fe, 0.2035% O, 0.021% C, 0.013% N, balance is Ti
6.0% Al, 3.99% V, 0.25% Fe, 0.2035% O, 0.021% C, 0.013% N, balance is Ti
6.0% Al, 3.99% V, 0.25% Fe, 0.2035% O, 0.021% C, 0.013% N, balance is Ti
6.0% Al, 3.99% V, 0.25% Fe, 0.2035% O, 0.021% C, 0.013% N, balance is Ti
6.0% Al, 3.99% V, 0.25% Fe, 0.2035% O, 0.021% C, 0.013% N, balance is Ti
6.0% Al, 3.99% V, 0.25% Fe, 0.2035% O, 0.021% C, 0.013% N, balance is Ti
6.0% Al, 3.99% V, 0.25% Fe, 0.2035% O, 0.021% C, 0.013% N, balance is Ti
6.00% Al, 3.99% V, 0.25% Fe, 0.20% O, 0.02% C, 0.01% N, balance is Ti
6.00% Al, 3.99% V, 0.25% Fe, 0.20% O, 0.02% C, 0.01% N, balance is Ti
6.00% Al, 3.99% V, 0.25% Fe, 0.20% O, 0.02% C, 0.01% N, balance is Ti
6.00% Al, 3.99% V, 0.25% Fe, 0.20% O, 0.02% C, 0.01% N, balance is Ti
6.0% Al, 0.81% Mo, 0.9% Ta, 1.9% Nb, 0.071% O, 0.009% H, 0.005% N, 0.09% Fe, balance is Ti
6.0% Al, 3.99% V, 0.25% Fe, 0.2035% O, 0.021% C, 0.013% N, balance is Ti
6.0% Al, 4.0% V, balance is Ti
6.0% Al, 4.10% V, 0.20% O, 0.007% H, 0.02% N, 0.18% Fe, balance is Ti
6 at.% (2.5 wt.%) Mo, balance is U
6 at.% (2.5 wt.%) Mo, balance is U
6% Al, 2% Sn, 4% Zr, 2% Mo, balance is Ti
6% Al, 2% Sn, 4% Zr, 2% Mo, balance is Ti
6% Al, 2% Sn, 4% Zr, 2% Mo, balance is Ti
6% Al, 2% Sn, 4% Zr, 2% Mo, balance is Ti
6% Al, 2% Sn, 4% Zr, 2% Mo, balance is Ti
6% Al, 2% Sn, 4% Zr, 2% Mo, balance is Ti
6% Al, 2% Zr, 1% Mo, 1% V, balance is Ti
6.0% Cu, 3.0% Al, balance is Ti
6.0% Cu, balance is Ti
6.0% Mn, balance is Ti
6.01% Al, 3.87% V, 0.18% Fe, 0.009% C, 0.14% O, 0.006% N, <50 ppm Y, balance is Ti
6.01% Al, 3.87% V, 0.18% Fe, 0.009% C, 0.14% O, 0.006% N, <50 ppm Y, balance is Ti
6.03% Al, 2.08% Sn, 3.91% Zr, 1.99% Mo, 0.066% 02, balance is Ti
6.05% Al, 4.06% V, 0.17% O, 0.025% N, 0.0045% H, balance is Ti
6.05% Al, 2.03% V, 0.107% O, 0.001% H, balance is Ti
6.1% Zn, 2.15% Mg, 2.37% Cu, balance is Al
6.1% Al, 2.1% Sn, 4.0% Zr, 6.3% Mo, 0.10% 02, balance is Ti
6.1% Al, 2.1% Sn, 4.0% Zr, 6.3% Mo, 0.10% 02, balance is Ti
6.1% Al, 2.1% Sn, 4.0% Zr, 6.3% Mo, 0.10% 02, balance is Ti
6.1% Al, 2.1% Sn, 4.0% Zr, 6.3% Mo, 0.10% 02, balance is Ti
6.1% Al, 4.3% V, 0.16% Fe, 0.01% C, balance is Ti
6.1% Al, 4.3% V, 0.16% Fe, 0.01% C, balance is Ti
6.10% Al, 4.30% V, 0.16% Fe, 0.01% C, balance is Ti
6.17% Al, 4.97% Zr, 0.49% Mo, 0.22% Si, 0.10% 0, 0.029% N, balance is Ti
6.17% Al, 4.97% Zr, 0.49% Mo, 0.22% Si, 0.10% 0, 0.029% N, balance is Ti
6.17% Al, 4.97% Zr, 0.49% Mo, 0.22% Si, 0.10% 0, 0.029% N, balance is Ti
6.17% Al, 4.97% Zr, 0.49% Mo, 0.22% Si, 0.10% 0, 0.029% N, balance is Ti
6.17% Al, 4.97% Zr, 0.49% Mo, 0.22% Si, 0.10% 0, 0.029% N, balance is Ti
6.17% Al, 4.97% Zr, 0.49% Mo, 0.22% Si, 0.10% 0, 0.029% N, balance is Ti
6.17% Al, 4.97% Zr, 0.49% Mo, 0.22% Si, 0.10% 0, 0.029% N, balance is Ti
6.17% Al, 4.97% Zr, 0.49% Mo, 0.22% Si, 0.10% 0, 0.029% N, balance is Ti
6.17% Al, 4.97% Zr, 0.49% Mo, 0.22% Si, 0.10% 0, 0.02996 N, balance is Ti
6.20% Al, 5.50% V, balance is Ti, Fe and other heavy impurities <0.1% each, 1350 ppm O
6.2% Zn, 2.3% Cu, 2.35% Mg, 0.13% Zr, balance is Al
6.2% Zn, 2.3% Cu, 2.35% Mg, 0.13% Zr, balance is Al
6.25% Al, 3.93% Nb, 0.040% O, 0.003% H, 0.04% Fe, balance is Ti
6.29% Mo, 26.53% Cr, 0.234% C, 0.423% Ni, 0.124% Fe, 0.822% Mn, 0.763% Si, 0.007% P, 0.53% W, <0.002% S, balance is Co
6.3% Al, 2.6% Mo, 2.1% Cr, 0.40% Fe, 0.05% C, 0.2% Si, balance is Ti
6.3% Al, 2.6% Mo, 2.1% Cr, 0.40% Fe, 0.05% C, 0.2% Si, balance is Ti
6.30% Al, 2.60% Mo, 2.10% Cr, 0.40% Fe, 0.05% C, 0.20% Si, balance is Ti
6.30% Cu, 0.30% Mn, 0.18% Zr, 0.10% V, 0.06% Ti, 93.00% Al
6.36% Al, 4.06% Nb, 0.093% O, 0.001% H, 0.04% Fe, balance is Ti
6.39% Be, balance is Cu
6.5-7.5% Si, max. 0.6% Fe, max. 0.25% Cu, 0.2-0.45% Mg, max. 0.25% Ti, max. 0.35% Zn, max. 0.35% Mn, balance is Al
6.5% Al, 4.4% V, 0.15% Fe, 0.023% C 0.013% O2, 0.017% N2, balance is Ti
6.5% Al, 4.4% V, 0.15% Fe, 0.023% C, 0.130% O2, 0.017% N2, 0.0024% H2, balance is Ti.
6.50% Al, 4.40% V, 0.15% Fe, 0.023% C, 0.13% O2, 0.017% N2, 0.0024% H2, balance is Ti
6.50% Al, 4.40% V, 0.15% Fe, 0.023% C, 0.13% O2, 0.017% N2, 0.0024% H2, balance is Ti
6.52% Si, 0.435% Fe, 3.88% Cu, 0.459% Mn, 0.01% Cr, 0.01% Ni, 0.465% Zn, 0.031% Pb, 0.003% Sn, 0.163% Ti, balance is Al
6.59% Al, 4.1% V, 0.18% Fe, 0.01% C, 20 ppm H, 50 ppm N, and 1900 ppm O, balance is Ti
6.63% Al, 2.08% Sn, 2.08% Zr, 1.99% Mo, 0.066% 02, balance is Ti
6.63% Al, 2.08% Sn, 3.91% Zr, 1.99% Mo, 0.066% 02, balance is Ti
6.63% Al, 2.08% Sn, 3.91% Zr, 1.99% Mo, 0.066% 02, balance is Ti
6.63% Al, 2.08% Sn, 3.91% Zr, 1.99% Mo, 0.066% 02, balance is Ti
6.63% Si, 3.23% Cu, 0.3% Mg, balance is Al
6.8% Al, 14.4% Mo, 6.1% W, 0.04% C, balance is Ni
7% Ni, balance is Ti
7% Si, 0.4% Mg, balance is Al
7.0% Cr, balance is Ti
7.0% Mo, balance is Ti
7.0% Mo, balance is Ti
7.0% Mo, balance is Ti
7.22% Cr, balance is Ti
7.3% Fe, balance is Ti
7.31% Si, 0.092% Fe, 0.005% Cu, 0.005% Mn, 0.31% Mg, 0.13% Ti, balance is Al.
7.31% Si, 0.092% Fe, 0.005% Cu, 0.005% Mn, 0.13% Ti, balance is Al
7.31% Si, 0.092% Fe, 0.005% Cu, 0.005% Mn, 0.31% Mg, 0.13% Ti, balance is Al
7.31% Si, 0.092% Fe, 0.005% Cu, 0.005% Mn, 0.31% Mg, 0.13% Ti, balance is Al
7.4% Si, 0.17% Fe, <0.01% Cu, 0.49% Mn, 0.20% Mg, <0.01% Zn, 0.08% Ti, 0.018% Sr, balance is Al
7.40% Si, 0.17% Fe, 0.49% Mn, 0.20% Mg, 0.08% Ti, 0.018% Sr, balance is Al
7.40% Si, 0.17% Fe, 0.49% Mn, 0.20% Mg, 0.08% Ti, 0.018% Sr, balance is Al
7.5% Zn, 1.6% Mg, 0.13% Zr, balance is Al. Ge-containing alloy: 7.5% Zn, 1.6% Mg, 0.13% Zr, 0.1% Ge, balance is Al.
7.5% Zn, 1.6% Mg, 0.13% Zr, balance is Al. Ge-containing alloy: 7.5% Zn, 1.6% Mg, 0.13% Zr, 0.1% Ge, balance is Al.
7.5% Cr, balance is Ti
7.5% Cr, balance is Ti
7.5% Cr, balance is Ti
7.5% Cr, balance is Ti
7.5% Cr, balance is Ti
7.5% Mo, balance is Zr
7.54% Cr, balance is Ti
7.6% Na2O, 6.5% Al2O3
7.6% Al, 1.0% V, 1.0% Mo, balance is Ti
7.6% Al, 1.0% V, 1.0% Mo, balance is Ti
7.6% Al, 1.0% V, 1.0% Mo, balance is Ti
7.6% Al, 1.0% V, 1.0% Mo, balance is Ti
7.89% Cr, 5.08% Cr, 2.11% Mo, 7.99% W, 5.05% Al, 1.49% Ti, 5.96% Ta, balance is Ni
7.9% Cr, balance is Ti
7.92% Fe, 0.15% Cu, 0.06% C, 0.17% Mn, 0.007% S, 0.22% Si, 15.40% Cr, balance is Ni
7.99% Zn, 1.98% Mg, 0.98% Cu, 0.11% Zr, 0.035% Ti, 0.003% Si, 0.034% Fe, balance is Al
7.99% Zn, 1.98% Mg, 0.98% Cu, 0.11% Zr, 0.035% Ti, 0.003% Si, 0.034% Fe, balance is Al
7.99% Zn, 1.98% Mg, 0.98% Cu, 0.11% Zr, 0.035% Ti, 0.003% Si, 0.034% Fe, balance is Al
7.99% Zn, 1.98% Mg, 0.98% Cu, 0.11% Zr, 0.035% Ti, 0.003% Si, 0.034% Fe, balance is Al
8% Al, 1% Be, 0.6% Co, balance is Cu
8% Al, 14% Ni, 3% Cu, 18-32% Co, balance is Fe
8% Al, 6% Mn, 3% Fe, 2% Ni, balance is Cu
8% Al, balance is Ti
8% Cr, balance is Ti
8% Mo, 0.5% Ti, balance is U
8% Mo, 1% Pt, balance is U
8% Mo, 1% Ti, balance is U
8% Mo, 1.5% Nb, balance is U
8% Mo, 10.8% Mo, balance is U
8% Mo, 3% Nb, balance is U
8% Mo, balance is U
8% Mo, balance is U
8% Mo, balance is U
8% Mo, balance is U
8% Mo, balance is U
8% Mo, balance is U
8% Mo, balance is U
8% Mo, balance is U
8.0% Cr, balance is Ti
8.0% Cu, 3.0% Al, 2.0% Sn, balance is Ti
8.0% Cu, 3.0% Al, balance is Ti
8.35% Si, balance is Cu
8.6% Mn, balance is Ti
8.65% Mg, 0.18% Fe, 0.24% Cu, 0.12% Si, 0.12% Zn, 0.003% Mn, 0.014% Pb, 0.012% Sn, 0.005% Ti, 0.006% Ni, 0.001% Be, 0.001% Cr, 0.001% V, balance is Al
8.65% Mg, 0.18% Fe, 0.24% Cu, 0.12% Si, 0.12% Zn, 0.003% Mn, 0.014% Pb, 0.012% Sn, 0.005% Ti, 0.006% Ni, 0.001% Be, 0.001% Cr, 0.001% V, balance is Al
8.8% Al, 5.4% Fe, 5% Ni, 0.9% Mn, balance is Cu
8.8% Al, 5.4% Fe, 5% Ni, 0.9% Mn, balance is Cu
8.85% U, balance is Zr
9.00-11.0% V, 1.6-2.2% Fe, 2.6-3.4% Al, max. 0.13% O, max. 0.05% C, max. 0.05% N, max. 0.015% H, balance is Ti
9Nb-1Zr-U
9.0% Cr, balance is Ti
9.0% Mo, balance is Ti
9.1% Al, 2.4% V, 0.006% C, 0.064% Fe, balance is Ti
9.37% W, 0.75% C, balance is Co
9.38% W, 0.49% C, balance is Co
9.46% Si, 0.16% Fe, 0.009% Cu, 0.003% Mn, 0.296% Mg, 0.018% Zn, 0.008% Ti, balance is Al
9.46% Si, 0.16% Fe, 0.009% Cu, 0.003% Mn, 0.296% Mg, 0.0182% Zn, 0.001% Ti, balance is Al
9.70% V, 2.08% Fe, 2.98% Al, balance is Ti
9.9% Al, 5.3% Fe, 5.1% Ni, 0.9% Mn, balance is Cu
9.9% Al, 5.8% Fe, 6.1% Ni, 0.9% Mn, balance is Cu
10.0% Mn, balance is Ti
10% Co, 8% Cr, 6% Mo, 6% Al, 4% Ta, 1% Ti+C+Zr+B, balance is Ni
10% Co, 8% Cr, 6% Mo, 6% Al, 4% Ta, 1% Ti+C+Zr+B, balance is Ni
10% Co, 8% Cr, 6% Mo, 6% Al, 4% Ta, 1% Ti+C+Zr+B, balance is Ni
10% Mo, balance is U
10% Mo, balance is U
10% Nb, balance is U. 20% Nb, balance is U.
10% Ni, balance is Ti
10% V, 2% Fe, 3% Al, balance is Al
10% V, 2% Fe, 3% Al, balance is Ti
10% V, 2% Fe, 3% Al, balance is Ti
10Nb-1Zr-U
10Nb-1Zr-U
10Nb-4Zr-U
10% Co, 1.5% Fe, 20% Cr, 8.5% Mo, 0.3% Mn, 0.15% Si, 1.5% Al, 2.1% Ti, 0.06% C, 0.005% B, balance is Ni
10% Co, 1.5% Fe, 20% Cr, 8.5% Mo, 0.3% Mn, 0.15% Si, 1.5% Al, 2.1% Ti, 0.06% C, 0.005% B, balance is Ni
10 % Mo, balance is U
10% Mo, balance is U
10% Mo, balance is U
10% SrO, 90% GeO2
10% V, 2% Fe, 3% Al, balance is Ti
10.05% Cr, 0.11% Fe, 10.03% Co, 0.01% Mo, 0.10% Ti, 1.48% Al, 0.06% Si, 0.00% Mn, 0.004% B, 0.11% O, 0.006% S, balance is Ni
10.1% Fe, 0.017% Si, 0.217% O2, balance is Ti
10.1% Si, 0.18% Fe, <0.01% Cu, 0.49% Mn, 0.55% Mg, <0.01% Zn, 0.06% Ti, 0.012% Sr, balance is Al
10.1% Si, 0.18% Fe, <0.01% Cu, 0.49% Mn, 0.55% Mg, <0.01% Zn, 0.06% Ti, 0.012% Sr, balance is Al
10.10% Si, 0.55% Mn, 0.55% Mg, 0.08% Ti, 0.011% Sr, 0.18% Fe, balance is Al
10.10% Si, 0.55% Mn, 0.59% Mg, 0.08% Ti, 0.012% Sr, 0.20% Fe, balance is Al
10.30% Al, 3.66% Fe, 1.61% Mn, 0.17% Nb, 0.025% Zn, 0.01% Pb, 0.008% P, 0.01% Si, 0.002% As, balance is Cu
10.3% Cr, balance is Ti
10.5% Al, 4.6% Fe, 5.0% Ni, balance is Cu
10.5% Al, 5% Ni, balance is Cu
10.5% Al, balance is Cu
10.5% Al, balance is Cu
10.5% Al, balance is Cu
10.5% Al, balance is Cu
10.50% Al, 4.1% Fe, balance is Cu
10.50-11.50% Sn, 4.00-6.00% Zr, 2.00-2.50% Al, 0.80-1.20 Mo, O.l5-0.27% Si, max 0.12% Fe, max 0.04% C, balance is Ti
10.54% Al, trace Fe, 3.03% Ni, balance is Cu
10.57% Al, 0.02% Fe, 1.02% Ni, trace Si, balance is Cu
10.6% Al, 3.0% Zn, balance is Cu
10.6% Al, 4.8% Fe, balance is Cu
10.8 % Mo, balance is U
10.8% Cr, balance is Ti
10.8% Mo, balance is U
10.92% Si, 0.16% Fe, 0.016% Cu, 0.386% Mn, 0.232% Mg, 0.015% Zn, 0.036% Ti, balance is Al
10.92% Si, 0.16% Fe, 0.016% Cu, 0.386% Mn, 0.232% Mg, 0.015% Zn, 0.326% Ti, balance is Al
10.92% Si, 0.35% Mg, 0.02% Ni, 0.11% Fe, 0.021% Zn, balance is Al
11.0% Al, 3.1% Zn, balance is Cu
11.0% Mo vs O, balance is Ti
11.0% Mo vs O, balance is Ti
11.0% Mo, balance is Ti
11.0% Mo, balance is Ti
11.0% Mo, balance is Ti
11.05% Al, trace Fe, 0.59% Zn, balance is Cu. b.) 11.68% Al, trace Fe, 1.05% Zn, balance is Cu. c.) 11.44% Al, trace Fe, 2.42% Zn, balance is Cu.
11.06% Al, balance is Cu
11.1% U, balance is Zr
11.2% Al, balance is Cu
11.3% Al, balance is Cu
11.3% Al, balance is Cu
11.40% Al, 0.01% Fe, balance is Cu
11.5% Al, 0.5% Be, balance is Cu
11.5% Al, 3.1% Zn, balance is Cu
11.5% Mo, 6% Zr, 4.5% Sn, 0.17% 0, balance is Ti
11.54% Al, 0.08% Fe, 0.59% Ag, balance is Cu. b) 11.55% Al, 0.08% Fe, 1.08% Ag, balance is Cu. c) 11.58% Al, 0.08% Fe, 2.63% Ag, balance is Cu.
11.60% Al, balance is Cu
11.6% Al, 5.3% Fe, 5.1% Ni, 0.9% Mn, balance is Cu
11.6% Mo, 6.0% Zr, 4.5% Sn, balance is Ti
11.6% Mo, 6.0% Zr, 4.5% Sn, balance is Ti
11.6% Mo, 6.0% Zr, 4.6% Sn, 0.17% 02, balance is Ti
11.6% Mo, 6.0% Zr, 4.6% Sn, 0.28% 02, balance is Ti
11.7% Al, 0.50% Mn, balance is Cu. b.) 11.6% Al, 0.96% Mn, balance is Cu.
11.7% Al, 0.62% Co, balance is Cu. b.) 11.8% Al, 1.1% Co, balance is Cu.
11.7% Al, balance is Cu
11.7% Al, 0.41% Fe, balance is Cu. b.) 11.6% Al, 0.93% Fe, balance is Cu.
11.73% Al, traces Fe, 0.63% In, balance is Cu. b.) 11.79% Al, traces Fe, 0.97% In, balance is Cu. c.) 11.84% Al, traces Fe, 2.44% In, balance is Cu.
11.74% Al, 0.01% Fe, 0.52% Sn, balance is Cu. b.) 11.84% Al, 0.01% Fe, 1.18% Sn, balance is Cu. c.) 11.56% Al, 0.01% Fe, 2.53% Sn, balance is Cu.
11.75% Al, traces Fe, 0.48% Be, balance is Cu. b.) 11.71% Al, traces Fe, 0.88% Be, balance is Cu. c.) 11.42% Al, traces Fe, 2.14% Be, balance is Cu.
11.8% Al, balance is Cu
11.8% Al, balance is Cu
11.8% Al, balance is Cu
11.8% Al, 0.19% Fe, 0.07% Si, balance is Cu
11.83% Al, 0.06% Fe, 0.025% Cd, balance is Cu. b.) 11.68% Al, 0.05% Fe, 0.43% Cd, balance is Cu. c.) 11.21% Al, 0.05% Fe, 0.64% Cd, balance is Cu.
11.87% Al, 0.06% Fe, 0.0256% Si, 0.01% Sn, balance is Cu
11.87% Al, balance is Cu
11.87% Al, balance is Cu
11.89% Al, 0.02% Fe, 0.01% Mn, balance is Cu
11.9% Al, 0.5% Be, balance is Cu
11.9% Al, balance is Cu
11.9% Mn, balance is Ti
11.9% Mo, balance is Ti
11.9% Al, balance is Cu
12.0% Al, balance is Cu
12.0% Cr, balance is Ti
12.0% Cr, balance is Ti
12.0% Al, balance is Cu
12% Mn, 8% Al, 8% Fe, 2% Ni, balance is Cu
12% Mo, balance is Ti
12.07% Al, 3.O8% Ni, trace Fe, balance is Cu
12.08% Al, 0.05% Fe, 0.1% Sb, balance is Cu. b.) 11.95% Al, 0.05% Fe, 0.45% Sb, balance is Cu. c.) 11.95% Al, 0.05% Fe, 0.73% Sb, balance is Cu.
12.16% Al, balance is Cu
12.2 at.% Ti, <0.02 at.% Al, <10 ppm B, 0.02 wt.% Si, 0.03 wt.% Fe, 0.01-0.02 wt.% C, <0.01 wt.% Co, <0.005 wt.% Mn, <0.001 wt.% Mg, <0.00l wt.% Cu, balance is Ni
12.2% Ti, <0.02% Al, 10 ppm B, 0.02% Si, 0.03% Fe, 0.01-0.02% C, <0.Ol% Co, <0.005% Mn, 0.001% Mg, <0.001% Cu, balance is Ni
12.20% Al, 0.04% Fe, trace Si, balance is Cu
12.31% Al, 3.68% Fe, 0.28% Ni, 0.03% Mn, balance is Cu
12.4% Al, balance is Cu
12.4% Al, balance is Cu
12.4% Al, balance is Cu
12.46% Al, 0.87% Ni, trace Fe, balance is Cu
12.5% Al, 4.9% Fe, 5.1% Ni, balance is Cu
12.5% V, balance is Ti
12.5 (at.%) Mg, balance is Al
12.7% Al, balance is Cu
12.78% Al, balance is Cu
12.8% Al, 7.7% Ni, balance is Cu
12.8% V, 11.1% Cr, 4.1% Al, balance is Ti
12.8% V, 11.1% Cr, 4.1% Al, balance is Ti
12.85% Al, balance is Cu
13.0% Al, balance is Cu
13% Mo, balance is Ti
13% Mo, balance is Ti
13% Co, 16% Cr, 4% Mo, 4% W, 2.1% Al, 3.7% Ti, 0.7% Nb, 0.03% C, 0.015% B, balance is Ni
13.25% Al, 29.00% Nb, 810 ppm O, 90 ppm N, 18 ppm H, balance is Ti
13.31% Al, balance is Cu
13.50% Al, balance is Cu
13.5% Al, balance is Cu
13.6% V, 10.5% Cr, 2.9% Al, balance is Ti
13.6% V, 10.5% Cr, 2.9% Al, balance is Ti
13.9% Fe, balance is Ti
14% Cr, 9.5% Co, 4% Mo, 4% W, 5% Ti, 3% Al, balance is Ni
14% SrO, 86% GeO2
14.10% W, 0.71% C, balance is Co
14.3% Mo, balance is U
14.3% U, balance is Zr
14.35-15.15% Cr, 14.0-19.0% Co, 4.25-5.25% Mo, 2.85-3.15% Al, 3.45-4.15% Ti, 1.35-2.15% Ta, 0.0-1.0% Hf, 0.05-0.07% Zr, 0.012-0.033% C, 0.01-0.025% B, balance is Ni
14.5% Cr, 17.5% Co, 5.1% Mo, 3.7% Ti, 4.1% A1, 0.015% B, 0.080% C, balance is Ni
14.5% Cr, 17.5% Co, 5.1% Mo, 3.7% Ti, 4.1% Al, 0.015% B, 0.06% C, balance is Ni
14.50-17.50% Cr, 14.0-17.0% Mo, max. 3.0% Fe, max. 0.009% C, max. 0.010% S, max. 1.0% Mn, max. 0.050% Si, max. 0.70% Ti, max. 0.20% P, max. 2.00% Co, balance is Ni
14.80% Al, 21.30% Nb, 0.065% Fe, 0.055% O, 0.006% N, balance is Ti
14.80% Al, 21.30% Nb, 0.065% Fe, 0.058% O, 0.006% N, balance is Ti
14.94-16.46% Cr, 15.47-16.47% Mo, 3.38-4.02% W, 5.05-6.77% Fe, 0.74-1.86% Co, 0.42-0.73% Mn, 0.42-0.73% Si, 0.22-0.32% V, 0.04-0.08% C, 0.004-0.012% P, 0.005-0.011% S, balance is Ni
15.0% Cr, 0.15% Fe, 19.0% Co, 5.15% Mo, 3.4% Ti, 4.45% Al, 0.10% Si, O.l% Mn, 0.O28% B, 0.06% C, balance is Ni
15.0% Cr, 0.15% Fe, 19.0% Co, 5.15% Mo, 3.49% Ti, 4.45% Al, 0.10% Si, 0.10% Mn, 0.028% B, 0.06% C
15.0% Cr, 0.15% Fe, 19.0% Co, 5.15% Mo, 3.49% Ti, 4.45% Al, 0.10% Si, 0.10% Mn, 0.028% B, 0.06% C, balance is Ni
15.0% Cr, 0.15% Fe, 19.0% Co, 5.15% Mo, 3.49% Ti, 4.45% Al, 0.10% Si, 0.10% Mn, 0.028% B, 0.06% C, balance is Ni
15.0% V, balance is Ti
15.0% V, balance is Ti
15% Co, 10% Cr, 5.5% Al, 4.7% Ti, 3% Mo, 0.95% V, balance is Ni
15% Co, 10% Cr, 5.5% Al, 4.7% Ti, 3% Mo, 0.96% V, balance is Ni
15% Mo, 0.2% Pd, balance is Ti
15% Mo, 5% Zr, balance is Ti
15% Mo, balance is Ti
15% V, 3% Al, 3% Sn, 3% Cr, balance is Ti
15.6% Cr, 8.1% Fe, 0.2% Ti, 0.03% Mo, 0.03% N, 0.03% Cu, 0.16% Al, 0.040% C, 0.27% Si, 0.13% Mn, balance is Ni
15.6% Cr, 8.1% Fe, 0.2% Ti, 0.03% Mo, 0.03% N, 0.03% Cu, 0.16% Al, 0.040% C, 0.27% Si, 0.13% Mn, balance is Ni
15.6% Cr, 8.1% Fe, 0.2% Ti, O.O3% Mo, 0.03% N, 0.03% Cu, 0.16% Al, 0.040% C, 0.27% Si, 0.13% Mn, balance is Ni
15.7% Co, 11.5% Cr, 6.5% Mo, 4.35% Al, 4.35% Ti, 0.50% Hf, 0.015% C, 0.015% B, 0.03% Zr, balance is Ni
16.0% Cr, 15.0% Co, 3.0% Mo, 1.25% W, 5.0% Ti, 2.5% Al, 0.010-0.025% C, 0.010-0.020% B, 0.03% Zr, balance is Ni
16.0% V, 2.5% Al, balance is Ti
16.0% V, 2.5% Al, balance is Ti
16.0% V, 2.5% Al, balance is Ti
16.0% V, 2.5% Al, balance is Ti
16.0% V, 2.5% Al, balance is Ti
16.0% V, 2.5% Al, balance is Ti
16% Co, 10% Cr, 5.5% Al, 4.7% Ti, 9% Mo, 0.96% V, balance is Ni
16% Cr, 0.15% W, 0.3% Fe, <0.01% C, 0.03% Si, 0.1% Co, 0.05% Mn, 0.03% V, 15% Mo, 0.45% Ti, balance is Ni
16% Cr, 3.4% W, 6% Fe, 0.01% C, 0.02% Si, 1% Co, 0.45% Mn, 0.2% V, 16% Mo, balance is Ni
16% Cr, 10% Co, 4.9% Nb, 2.7% Ti, 1.4% Ta, 1.0% Al, 5.0% Mo, 0.004% B, 0.06% C, 2.0% W, balance is Ni
16.0% Cr, 5.0% Ti, 3.0% Mo, 0.005% C, balance is Co
16.0% Cr, 5.0% Ti, 3.0% Mo, 0.005% C, balance is Co
16.08% Cr, 13.05% Co, 4.08% Mo, 4.05% W, 3.66% Ti, 2.33% Al, 0.69% Nb, 0.05% Zr, 0.040% C, 0.015% B, 0.01% P, 0.006% O, 0.006% N, balance is N. VAR bar.
16.1% Mo, balance is U
16.2% Mo, 0.002% Si, 0.234% O2, balance is Ti
16.5% Sn, balance is Cu
16.5% Sn, balance is Cu
17-21% Cr, 2.8-3.3% Mo, max. 1.0% Co, 4.7-55% Nb(+Ta), 0.65-1.15% Ti, max. 0.3% Cu, max. 0.08% C, max. 0.35% Mn, max. 0.35% P, max. 0.015% S, 0.2-0.8% Al, 50-55% Ni, balance is Fe
17-21% Cr, 50-55% Ni, 2.8-3.3% Mo, <1% Co, 4.7-5.5% Nb, 0.65-1.15% Ti, <0.3% Cu, <0.08% C, <0.35% Mn, <0.015% S, 0.2-0.8% Al, Fe is balance.
17-21% Cr, max. 0.08% C, max. 0.35% Mn, max. 0.35% Si, 2.80-3.30% Mo, 4.75-5.5% Ni+Ta, 0.65-1.50% Ti, 0.20-0.80% Al, max. 0.006% B, balance is Ni
17.0% Cr, balance is Ti
17.1% Cr, 42.5% Ni, 3.1% Mo, 1.2% Ti, 1.3% Al, 0.03% Zr, 0.05% Mn, 0.0003% B, 0.06% C, balance is Ni
17.4% Cr, 18.7% Fe, 6.16% Nb, 2.96% Mo, 0.99% Ti, 0.48% Al, 0.06% C, 0.07% Mn, 0.10% Si, <0.01% B, 0.003% S, balance is Ni
17.42% Cr, balance is Ti
17.68% Fe, 18.83% Cr, 0.98% Ti, 2.97% Mo, 6.13% Nb, 0.63% Al, 0.06% Ta, 0.30% Co, 0.09% Mn, 0.04% C, 0.004% S, 0.01% P, 0.17% Si, 0.09% Cu, balance is Ni
17.8-19.1% Fe, 0.03-0.06% C, 0.21- 1.12% Si, 17.9-18.3% Cr, 3.0-3.06% Mo, 5.11-6.17% Nb+Ta, 0.96-1.0% Ti, 0.42-0.47% Al, balance is Ni
17.8-19.1% Fe, 0.03-0.06% C, 0.21- 1.12% Si, 17.9-18.3% Cr, 3.0-3.06% Mo, 5.11-6.17% Nb+Ta, 0.96-1.0% Ti, 0.42-0.47% Al, balance is Ni
17.87% Cr, 2.68% Mo, 1.12% W, 9.2% Co, 9.59% Fe, 5.55% Nb, 0.83% Ti, 1.39% Al, balance is Ni
17.87% Cr, 2.68% Mo, 1.12% W, 9.2% Co, 9.59% Fe, 5.55% Nb, 0.83% Ti, 1.39% Al, balance is Ni
17.87% Cr, 2.68% Mo, 1.12% W, 9.2% Co, 9.59% Fe, 5.55% Nb, 0.83% Ti, 1.39% Al, balance is Ni
17.87% Cr, 2.68% Mo, 1.12% W, 9.2% Co, 9.59% Fe, 5.55% Nb, 0.83% Ti, 1.39% Al, balance is Ni
17.87% Cr, 2.68% Mo, 1.12% W, 9.2% Co, 9.59% Fe, 5.55% Nb, 0.83% Ti, 1.39% Al, balance is Ni
17.87% Cr, 2.68% Mo, 1.12% W, 9.2% Co, 9.59% Fe, 5.55% Nb, 0.83% Ti, 1.39% Al, balance is Ni
17.97% Cr, 9.09% Co, 9.64% Fe, 2.69% Mo, 1.02% W, 5.49% Nb, 1.6% Al, 0.75% Ti, 0.009% P, 0.005% B, 0.022% C, balance is Ni
18.0% Cr, 18.1% Fe, 0.47% Co, 5.1% Nb, 3.0% Mo, 0.4% Al, 0.9% Ti, 0.03% C, 0.25% Others, balance is Ni
18% Al, 0.87% Cu, 0.037% Mg, 0.02% Ca, balance is Zn
18% Al, 0.87% Cu, 0.037% Mg, 0.024% Ca, balance is Zn
18% Mo, balance is Ti
18.49% Cr, 16.79% Fe, 5.07% Nb+Ta, 3.11% Mo, 0.95% Ti, 0.51% Al, 0.30% Si, 0.28% Mn, 0.05% Cu, 0.04% C, 0.011% P, 0.007% S, 0.0023% B, balance is Ni
18.60% Cr, 3.10% Al, 5.00% Nb, 0.90% Ti, 18.50% Fe, 0.04% C, 0.20% Mn, 0.30% Si, balance is Ni
18.64% Cr, 0.20% Fe, 0.075% C, 0.05% Si, 10.76% Co, 0.05% Mn, 9.76% Mo, 1.62% Al, 3.13% Ti, 0.009% B, 0.008% P, 0.007% S, balance is Ni
19.00% Cr, 52.5O% Ni, 3.00% Mo, 0.90% Ti, 0.50% Al, 18.50% Fe, max. 0.08% C, max. 0.15 Cu
19.00-23.00% Cr, 8.00-10.00% Mo, 3.15-4.15% Nb, max. 5.00% Fe, max. 0.10% C, max. 1.00% Si, max. 0.40% Al, max. 0.50% Mn, max. 0.015% S, balance is Ni
19% Cr, 18% Fe, 5% Nb, 3% Mo, 0.15% Si, 0.10% Cu, 0.20% Mn, 1.0% Ti, 0.4% Al, 0.04% C, 0.007% S, balance is Ni
19% Cr, 18% Fe, 5% Nb, 3% Mo, 0.15% Si, 0.10% Cu, 0.20% Mn, 1.0% Ti, 0.4% Al, 0.04% C, 0.007% S, balance is Ni
19% Cr, 18% Fe, 6% Nb, 3% Mo, 0.16% Si, 0.10% Cu, 0.20% Mn, 1.0% Ti, 0.4% Al, 0.04% C, 0.007% S, balance is Ni
19% Cr, 18% Fe, 6% Nb, 3% Mo, 0.16% Si, 0.10% Cu, 0.20% Mn, 1.0% Ti, 0.4% Al, 0.04% C, 0.007% S, balance is Ni
19% Cr, 18% Fe, 6% Nb, 3% Mo, 0.16% Si, 0.10% Cu, 0.20% Mn, 1.0% Ti, 0.4% Al, 0.04% C, 0.007% S, balance is Ni
19% Cr, 18% Fe, 5% Nb, 3% Mo, 0.15% Si, 0.10% Cu, 0.20% Mn, 1.0% Ti, 0.4% Al, 0.04% C, 0.007% S, balance is Ni
19% Cr, 18% Fe, 5% Nb,0 3% Mo, 0.15% Si, 0.10% Cu, 0.20% Mn, 1.0% Ti, 0.4% Al, 0.04% C, 0.007% S, balance is Fe
19.02% Cr, 0.30% Fe, 0.07% C, 0.06% Si, 10.64% Co, 0.04% Mn, 9.84% Mo, 1.46% Al, 3.18% Ti, 0.0056% B, 0.005% P, 0.005% S, balance is Ni
19.02% Cr, 0.30% Fe, 0.07% C, 0.06% Si, 10.84% Co, 0.04% Mn, 9.84% Mo, 1.45% Al, 3.18% Ti, 0.0056% B, 0.005% P, 0.005% S, balance is Ni
19.05% Cr, 0.71% Fe, 10.93% Co, 9.91% Mo, 3.10% Ti, 1.48% Al, 0.06% Si, 0.06% Mn, 0.004% B, 0.11% C, 0.008% S, balance is Ni
19.22% Fe, 17.94% Cr, 5.11% Nb+Ta, 2.95% Mo, 0.03% Ti, 0.53% Al, 0.14% Co, 0.04% Si, 0.04% Mn, <0.10% Cu, <0.002% Ca, <0.003% Mg, <0.001% Pb, 0.034% C, <0.005% B, <0.002% S, 0.009% P, balance is Ni
19.73% Cr, 2.03% Fe, 0.067% C, 0.18% Si, 11.12% Co, 0.05% Mn, 10.09% Mo, 1.60% Al, 3.10% Ti, 0.0045% B, 0.020% S, balance is Ni. Low Fe-Si-Mn-S composition: Composition: 18.64% Cr, 0.20% Fe, 0.075% C, 0.05% Si, 10.76% Co, 0.05% Mn, balance is Ni.
19.90% Cr, 11.90% Co, 6.00% Mo, 3.21% Ti, 2.22% Al, 1.05% W, 0.06% C, 0.006% B, 0.02% S, balance is Ni
19.9% Fe, 18.2% Cr, 6.1% Nb, 2.9% Mo, 1.16% Ti, 0.2% Mn, balance is Ni
19.9% Fe, 18.2% Cr, 6.1% Nb, 2.9% Mo, 1.16% Ti, 0.2% Mn, balance is Ni
20-23% Cr, 8-10% Mo, 3.15-4.15% Nb+Ta, max. 5.0% Fe, max. 0.40% Ti, max. 0.10% C, max. 0.50% Mn, max. 0.50% Si, max. 0.015% P, max. 0.015% S, max. 0.40% Al, max. 1.0% Co, balance is Ni
20-23% Cr, 8-10% Mo, 3.15-4.15% Nb+Ta, max. 5.0% Fe, max. 0.40% Ti, max. 0.10% C, max. 0.50% Mn, max. 0.50% Si, max. 0.015% P, max. 0.015% S, max. 0.40% Al, max. 1.0% Co, balance is Ni
20-23% Cr, 8-10% Mo, 3.15-4.15% Nb+Ta, max. 5.0% Fe, max. 0.40% Ti, max. 0.10% C, max. 0.50% Mn, max. 0.50% Si, max. 0.015% P, max. 0.015% S, max. 0.40% Al, max. 1.0% Co, balance is Ni
20-23% Cr, 8-10% Mo, 3.15-4.15% Nb+Ta, max. 5.0% Fe, max. 0.40% Ti, max. 0.10% C, max. 0.50% Mn, max. 0.50% Si, max. 0.015% P, max. 0.015% S, max. 0.40% Al, max. 1.0% Co, balance is Ni
20.0-24.0% Cr, 10.0-15.0% Co, 8.0-10.0% Mo, 0.8-1.5% Al, 0.05-0.15% C, max. 3.0% Fe, max. 1.0% Mn, max. 1.0% Si, max. 0.015% S, max. 0.6% Ti, max. 0.5% Cu, max. 0.006% B, balance is Ni
20.0-24.0% Cr, 10.0-15.0% Co, 8.0-10.0% Mo, max. 3.0% Fe, max. 1.0% Mn, 0.8-1.5% Al, 0.05-0.15% C, max. 0.5% Cu, max. 1.0% Si, max. 0.015% S, max. 0.006% B, balance is Ni
20-24% Cr, 20-24% Ni, 13-16% W, 0.06-0.16% C, 0.03-0.16% La, 0.20-0.60% Si, up to 3% Fe, up to 1.26% Mn, balance is Co
20% Cr, 14% Co, 4% Mo, 3% Ti, l% Al, balance is Ni
20% Cr, balance is Co
20% Nb, balance is U
20% Nb, balance is U
20-23% Cr, 8-10% Mo, 3.15-4.15% Nb+Ta, max. 5.0% Fe, max. 0.40% Ti, max. 0.10% C, max. 0.50% Mn, max. 0.50% Si, max. 0.015% P, max. 0.015% S, max. 0.40% Al, max. 1.0% Co, balance is Ni
20% Cr, 10% Co, 8.5% Mo, 2.1% Ti, 1.5% Al, max. 1.5% Fe, max. 0.3% Mn, max. 0.15% Si, 0.06% C, 0.005% B, balance is Ni
20% Cr, 10% Co, 8.5% Mo, 2.1% Ti, 1.5% Al, max. 1.5% Fe, max. 0.3% Mn, max. 0.15% Si, 0.06% C, 0.005, balance is Ni
20.0% Cr, 14.84% W, 10.02% Ni, 3.12% Fe, 1.39% Mn, 0.47% Si, 0.003% P, trace Zr, balance is Co.
20.0% Cr, 14.84% W, 10.02% Ni, 3.12% Fe, 1.39% Mn, 0.47% Si, 0.003% P, trace Zr, balance is Co
20.1% Co, 19.6% Cr, 5.7% Mo, 2.1% Ti, 0.4% Al, 0.5% Fe, 0.06% C, balance is Ni
20.10% Cr, 2.03% Fe, 0.89% C, 0.25% Si, 11.55% Co, 0.05% Mn, 10.17% Mo, 1.60% A1, 3.17% Ti, 0.0056% B, 0.016% S, balance is Ni
20.10% Cr, 2.03% Fe, 0.089% C, 0.25% Si, 11.55% Co, 0.05% Mn, 10.17% Mo, 1.60% Al, 3.17% Ti, 0.0056% B, 0.016% S, balance is Ni
20.10% Cr, 2.03% Fe, 0.089% C, 0.25% Si, 11.55% Co, 0.05% Mn, 10.17% Mo, 1.60% Al, 3.17% Ti, 0.0056% B, 0.016% S, balance is Ni
20.10% Cr, 2.03% Fe, 0.089% C, 0.25% Si, 11.65% Co, 0.05% Mn, 10.17% Mo, 1.60% Al, 3.17% Ti, 0.0056% B, 0.016% S, balance is Ni
20.18% Cr, 15.11% W, 9.93% Ni, 0.07% C, 0.034% N, 2.01% Fe, 0.01% Si, 1.51% Mn, balance is Co
20.2% Cr, 15.8% Ni, 14.8% W, 1.2% Ti, 0.53% Al, 0.07% Mn, 0.05% Si, 0.25% Fe, 0.11% C, balance is Co
20.5% Cr, 6.2% Mo, 4.3% Fe, 3.6% Nb, 0.1% Co, 0.1% Al, 0.1% Ti, 0.1% Si, 0.1% Mn, 0.03% C, balance is Ni
20.5% Cr, 8.2% Mo, 4.3% Fe, 3.6% Nb, 0.1% Co, 0.1% Al, 0.1% Ti, 0.1% Mn, 0.03% C, balance is Ni
20.5-22.5% Cr, 4.0-5.0% Fe, 8.1-8.9% Mo, 3.4-3.7% Nb+Ta, 0.01-0.40% C, 0.02-0.10% Mn, 0.05-0.10% Si, 0.02-0.04% Al, 0.1-0.25% Ti, balance is Ni
20.5-22.5% Cr, 4.0-5.0% Fe, 8.1-8.9% Mo, 3.4-3.7% Nb+Ta, 0.01-0.40% C, 0.02-0.10% Mn, 0.05-0.10% Si, 0.02-0.04% Al, 0.1-0.25% Ti, balance is Ni
20.5-22.5% Cr, 4.0-5.0% Fe, 8.1-8.9% Mo, 3.4-3.7% Nb+Ta, 0.01-0.40% C, 0.02-0.10% Mn, 0.05-0.10% Si, 0.02-0.04% Al, 0.1-0.25% Ti, balance is Ni
20.5% Mo, balance is Ti
20.5-22.5% Cr, 4.0-4.5% Fe, 8.1-8.9% Mo, 3.4-3.7% Nb+Ta, 0.01-0.04% C, 0.02-0.10% Mn, 0.05-0.10% Si, 0.02-0.03% Al, 0.1-0.25% Ti, balance is Ni
20.6% Cr, 8.2% Mo, 4.3% Fe, 3.6% Nb, 0.1% Co, 0.1% Al, 0.1% Ti, 0.1% Si, 0.1% Mn, 0.03% C, balance is Ni
20.7% U, balance is Zr
20.78% Cr, 12.78% Mo, balance is Ni
21.0% Al, 1.0% Cu, balance is Zn
21.1% Cr, 13.5% Mo, balance is Ni
21.1% Cr, 13.5% Mo, balance is Ni
21.1% Cr, 13.5% Mo, balance is Ni
21.1% Cr, 7.5% Mo, balance is Ni
21.28% Cr, 8.7% Mo, 3.83% Fe, 3.58% Nb, 0.27% Mn, 0.30% Si, 0.28% Ti, 0.029% C, 0.007% Ta, <0.005% P, <0.002% S, balance is Ni
21.28% Cr, 8.7% Mo, 3.83% Fe, 3.58% Nb, 0.27% Mn, 0.26% Al, 0.30% Si, 0.28% Ti, 0.029% C, 0.007% Ta, balance is Ni
21.3% Cr, 13.4% Mo, 2.5% Fe, 3.1% W, 0.008% C, balance is Ni
21.6 at.% Zn, balance is Al
21.74% Cr, 2.87% Fe, 8.58% Mo, 3.80% Nb, 0.021% C, 0.20% Mn, 0.23% Si, 0.01% P, 0.003% S, 0.12% Al, 0.16% Ti, balance is Ni
21.9% Cr, 8.94% Mo, 1.4% Fe, 0.03% Mn, 0.04% Si, 0.18% Ti, 3.74% Nb+Ta, 0.16% Al, 0.03% C, balance is Ni
21.9% Al, 0.1% Cu, balance is Zn
21.9% Cr, 8.94% Mo, 1.4% Fe, 0.03% Mn, 0.04% Si, 0.18% Ti, 3.74% Nb+Ta, 0.16% Al, 0.03% C, balance is Ni
22.00% Cr, 12.50% Co, 9.00% Mo, 1.20% Al, 1.00% Fe, 0.40% Ti, 0.10% Si, 0.10% C, 0.50% Cu, 0.006% B, 0.015% S, balance is Ni
22 wt% Cr, 9 wt% Mo, <5 wt% Fe, 3.5 wt% Nb, balance is Ni
22 wt% Cr, 9 wt% Mo, <5 wt% Fe, 3.5 wt% Nb, balance is Ni
22% Al, 0.16% Mg, 0.6% Cu, balance is Zn
22% Al, balance is Zn
22% Al, balance is Zn
22% Al, balance is Zn
22 at.% Zn, 0.1 at.% Sn, balance is Al
22.25% Cr, 9.27% Mo, 2.05% Fe, 0.1% Mn, 0.04% Si, 0.3% Ti, 3.42% Nb+Ta, 0.14% A1, 0.011% C
22.25% Cr, 9.27% Mo, 2.05% Fe, 0.1% Mn, 0.04% Si, 0.3% Ti, 3.42% Nb+Ta, 0.14% Al, 0.011% C, balance is Ni
22.26% Cr, 9.27% Mo, 2.06% Fe, 0.1% Mn, 0.04% Si, 0.3% Ti, 3.42% Nb+Ta, 0.14% Al, 0.011% C, balance is Ni
22.5% Al, balance is Zn
22.5% Al, balance is Zn
22.6 at.% Zn, 0.1 at.% Mg, balance is Al
22.8% Cr, 9.0% Mo, 11.9% Co, 1.15% Al, 0.48% Ti, 0.35% Fe, 0.06% C, 0.05% Si, 0.02% W, 0.02% Mn, 0.013% Cu, 0.005% Zr, 0.005% P, 0.005% V, 0.004% N, 0.003% Nb, 0.001% S, 0.0002% B, balance is Ni
22.8% Cr, 9.0% Mo, 11.9% Co, 1.15% Al, 0.48% Ti, 0.35% Fe, 0.06% C, 0.05% Si, 0.02% W, 0.02% Mn, 0.013% Cu, 0.005% Zr, 0.005% P, 0.005% V, 0.004% N, 0.003% Nb, 0.001% S, 0.0002% B, balance is Ni
23% Al, 0.92% Cu, 0.034% Mg, 0.026% Ca, balance is Zn
23% Al, 0.92% Cu, 0.034% Mg, 0.026% Ca, balance is Zn
23% Al, 0.92% Cu, 0.034% Mg, 0.026% Ca, balance is Zn
23% Al, 0.92% Cu, 0.034% Mg, 0.026% Ca, balance is Zn
23.1 at.% Ga, balance is Cu
23.4% Fe, 0.41% Al, 0.031% Ca, balance is Si. Unrefined: 23.4% Al, 1.11% Al, 0.13 Ca, 0.04% C, balance is Si.
24% Co, 12-16% Ni, 8% Al, 3% Cu, balance is Fe; nickel content modified at the expense of iron in 1%
24.7% Ni, 14.4% Cr, 2.2% Ti, 1.1% Mo, 0.20% Al, balance is Fe
25% W, 1.0% Ti, 0.5% Zr, 3.0% Cr, 0.5% C, balance is Co
25% W, balance is Co
25.1% Ni, 14.5% Cr, 1.20% Mo, 2.00% Ti, 0.30% V, 0.26% sol. Al, 0.052% C, 0.11% Mn, 0.20% Si, 0.009% S, 0.007% P, 0.0023% N, balance is Ni
25.6% Sn, 0.02% Pb, 0.01% Fe, 0.01% Ni, 0.02% Zn, <O.Ol% P, balance is Cu
26.0% Sb, balance is Ag
26% Ni, 15% Cr, 1.3% Mo, 1.8% Ti, 0.03% Ca, 0.3% V, balance is Fe (similar to A-286)
27.00-30.00% Cr, 5.00-7.00% Mo, max. 1.00% Mn, max. 1.00% Si, max. 0.75% Fe, max. 0.50% Ni, max. 0.35% C, max. 0.10% Al, max. 0.01% B, max. 0.25% N, max. 0.02% P, max. 0.01% S, max. 0.20% W, max. 0.10% Ti, balance is Co
27% Ni, 14.8% Cr, 3% Mo, 5.1% Nb, 0.5% Al, 18.5% Fe, 0.18% Si, 0.04% C, 0.002% B
27% Ni, 14.80% Cr, 3% Mo, 5.10% Nb, 0.50% Al, 18.50% Fe, 0.18% Si, 0.04% C, 0.002% B
27.27% Zn, 3.37% Al, balance is Cu
28.2 at.% Cu, balance is Ag
28.5% Mo, 1.5% Cr, 1.5% Fe, max. 3% Co, max. 3% W, max. 3% Mn, max. 0.5% Al, max. 0.2% Ti, max. 0.1% Si, max. 0.01% C, balance is Ni
28.5% Mo, 1.5% Cr, 1.5% Fe, max. 3% W, max. 3% Co, max. 0.5% Al, max. 0.2% Ti, max. 0.1% Si, max. 0.01% C, max. 0.2% Nb, max. 0.2% V, max. 0.2% Cu, max. 0.2% Ta, max. 0.01% Zr, balance is Ni
30.0-35.0% Ni, 19.0-23.0% Cr, min. 39.5% Fe, max. 0.10% C, max. 1.50% Mn, max. 0.015% P, max. 1.0% Si, max. 0.75% Cu, 0.15-0.60% Al, 0.15-0.60% Ti
30.0-35.0% Ni, 19.0-23.0% Cr, min. 39.5% Fe, max. 0.10% C, max. 1.50% Mn, max. 0.015% S, max. 1.0% Si, max. 0.75% Cu, 0.15-0.60% Al, 0.15-0.60% Ti
30.0-35.0% Ni, 19.0-23.0% Cr, min. 39.5% Fe, max. 0.10% C, max. 1.50% Mn, max. 0.015% S, max. 1.0% Si, max. 0.75% Cu, 0.15-0.60% Al, 0.15-0.60% Ti
30.0-35.0% Ni, 19.0-23.0% Cr, min. 39.5% Fe, max. 0.10% Cr, 0.15-0.60% Al, 0.15-0.60% Ti, Al+Ti=0.30-1.20%
30(33)% CaO, 57(62)% Al2O3, 5% MgO, 0(8)% Li2O
30.5% Sb, balance is Cu
31.l% Ni, 21.4% Cr, 0.90% Mn, 0.28% Si, 0.037% C, 0.02% N, 0.01% P, 0.007% S, 0.5% Al, 0.3% Ti, balance is Fe
31.l% Ni, 21.4% Cr, 0.9O% Mn, 0.28% Si, 0.037% C, 0.02% N, 0.01% P, 0.007% S, 0.5% Al, 0.3% Ti, balance is Fe
31.l% Ni, 21.4% Cr, 0.9O% Mn, 0.28% Si, 0.037% C, 0.02% N, 0.01% P, 0.007% S, 0.5% Al, 0.3% Ti, balance is Fe
31.l% Ni, 21.4% Cr, 0.9O% Mn, 0.28% Si, 0.037% C, 0.02% N, 0.01% P, 0.007% S, 0.5% Al, 0.3% Ti, balance is Fe
31.1% Ni, 21.4% Cr, 0.90% Mn, 0.28% Si, 0.037% C, 0.02% N, 0.01% P, 0.007% S, 0.5% Al, 0.3% Ti, balance is Fe
31.1% Ni, 21.4% Cr, 0.90% Mn, 0.28% Si, 0.037% C, 0.02% N, 0.01% P, 0.007% S, 0.5% A, 0.3% Ti, balance is Fe
31.1% Ni, 21.4% Cr, 0.90% Mn, 0.28% Si, 0.037% C, 0.02% N, 0.01% P, 0.007% S, 0.5% Al, 0.3% Ti, balance is Fe
31.1% Ni, 21.4% Cr, 0.90% Mn, 0.28% Si, 0.037% C, 0.02% N, 0.01% P, 0.007% S, 0.5% Al, 03% Ti, balance is Fe
31.36% In, balance is Cu
31.85% Ni, 0.28% Cu, 0.08% C, 0.81% Mn, 0.007% S, 0.3296 Si, 21.81% Cr, balance is Fe
32.0-37.0% Ni, 25.0-29.0% Cr, 0.06-0.10% C, 0.15-0.60% Al, 0.15-0.60% Ti, max. 0.75% Cu, max. 0.015% S, max. 1.5% Mn, max. 1.0% Si, balance is Fe
32.3% In, balance is Cu
32.3% Sn, balance is Cu
33 at.% Zr, balance is Nb
33 at.% Zr, balance is Nb
33 at.% Zr, balance is Nb
33 at.% Zr, balance is Nb
33 at.% Zr, balance is Nb
33.4% CaO, 39.5% SiO2, 19.5% Al2O3, 7.3% MgO
33.4% CaO, 39.5% SiO2, 19.5% Al2O3, 7.3% MgO
34.5% CaO, 37.5% SiO2, 3.0% Al2O3, 2.5% MgO, 12.5% Na2O, 0.5% Li2O, 8.5% F, 1% others
34.5% CaO, 37.5% SiO2, 3.0% Al2O3, 2.5% MgO, 12.5% Na2O, 0.5% Li2O, 8.5% F, 1% others
35.4% CaO, 25.2% Al2O3, 39.4% SiO2, CaO/SiO2=0.90
35.4% CaO, 25.2% Al2O3, 39.4% SiO2, CaO/SiO2=0.90
35.58% CaO, 40.94% SiO2, 6.94% Al2O3, 9.57% Na2O, 1.0% CaF2
36.9% Fe, 16.0% Cr, 3.02% Nb, 1.65% Ti, 0.19% Al, 0.01% C, 0.05% Si, 0.003% N, 0.001% S, balance is Ni.
36.9% Fe, 16.0% Cr, 3.02% Nb, 1.65% Ti, 0.19% Al, 0.01% C, 0.05% Si, 0.003% N, 0.001% S, balance is Ni.
37% Fe, 16% Cr, 2.9% Nb, 1.8% Ti, balance is Ni
37% Fe, 16% Cr, 2.9% Nb, 1.8% Ti, balance is Ni
37% Fe, 16% Cr, 2.9% Nb, 1.8% Ti, balance is Ni
37% Fe, 16% Cr, 2.9% Nb, 1.8% Ti, balance is Ni
37.26% SiO2, 28.11% Al2O3, 7.73% CaO, 26.89% CaF2, 4.50% K2O
37.26SiO2-28.11Al2O3-7.73CaO-26.89CaF2-4.5K2O
37.4% SiO2, 30.6% CaO, 23.0% Al2O3, 9.0% MgO
37.4% SiO2, 30.6% CaO, 23.0% Al2O3, 9.0% MgO
37.4% SiO2, 30.6% CaO, 23.0% Al2O3, 9.0% MgO
37.7% Ni, 16.0% Co, 3.0% Nb, 1.75% Ti, 1.0% Al, 0.008% B, 0.03% C, balance is Fe
37.8% CaO, 33.3% SiO2, 7.9% Al2O3, 8.2% Na2O, 8.4% T.F., 0.6% MgO, 0.6% K2O, 1.7% Fe2O3
37.8% CaO, 33.3% SiO2, 7.9% CaO, 8.2% Na2O, 0.6% MgO, 0.6% K2O, 1.7% Fe2O3
38.0-46.0% Ni, min. 22.0% Fe, 19.5-23.5% Cr, 2.5-3.5% Mo, 1.5-3.0% Cu, 0.6-1.2% Ti, max. 0.05% C, max. 1.0% Mn, max. 0.03% C, max. 0.5% Si, max. 0.2% Al
38.0-46.0% Ni, min. 22.0% Fe, 19.5-23.5% Cr, 2.5-3.5% Mo, 1.5-3.0% Cu, 0.6-1.2% Ti, max. 0.05% C, max. 1.0% Mn, max. 0.03% C, max. 0.5% Si, max. 0.2% Al
38.3% Cu, balance is Ag
38.3% Cu, balance is Ag
38.3% N, 12.9% Co, 4.70% Nb, 1.58% Ti, 0.36% Si, 0.04% Al, 0.01% C, 0.01% Cr, balance is Fe
39.0-44.0% Ni+Co, 14.5-17.5% Cr, 2.5-3.3% Nb+Ta, 1.5-2.0% Ti, max. 0.40% Al, max. 0.06% C, max. 0.30% Cu, max. 0.35% Mn, max. 0.35% Si, max. 0.015% S, max. 0.020% P, max. 0.006% B, max. 1.0% Co, balance is Fe
39.0-44.0% Fe, 14.5-17.5% Cr, 2.5-3.3% Nb+Ta, 1.5-2.0% Ti, max. 0.40% Al, max. 0.06% C, max. 0.30% Cu, max. 0.35% Si, max. 0.35% Mn, max. 0.015% P, max. 0.020% P, max. 0.006% B, max. 1.0% Co, balance is Fe
39.0-44.0% Ni+Co, 14.5-17.5% Cr, 2.5-3.3% Nb+Ta, 1.5-2.0% Ti, max. 0.40% Al, max. 0.06% C, max. 0.30% Cu, max. 0.35% Mn, max. 0.35% Si, max. 0.015% S, max. 0.020% P, max. 0.006% B, max. 1.0% Co, balance is Fe
39.0-44.0% Ni+Co, 14.5-17.5% Cr, 2.5-3.3% Nb+Ta, 1.5-2.0% Ti, max. 0.40% Al, max. 0.06% C, max. 0.30% Cu, max. 0.35% Mn, max. 0.35% Si, max. 0.015% S, max. 0.020% P, max. 0.006% B, max. 1.0% Co, balance is Fe
39.5% Zn, balance is Cu
39.58% CaO, 40.94% SiO2, 6.94% Al2O3, 9.57% Na2O, 1.00% CaF2
39.58% CaO, 40.94% SiO2, 6.94% Al2O3, 9.57% Na2O, 1.00% CaF2
39.58% CaO, 40.94% SiO2, 6.94% Al2O3, 9.57% Na2O, 1.00% CaF2
39.58% CaO, 40.94% SiO2, 6.94% Al2O3, 9.57% Na2O, 1.00% CaF2
39.58% CaO, 40.94% SiO2, 6.94% Al2O3, 9.57% Na2O, 1.00% CaF2
39.58% CaO, 40.94% SiO2, 6.94% Al2O3, 9.57% Na2O, 1.00% CaF2
39.66% CaO, 32.10% SiO2, 17.62% Al2O3, 8.48% MgO, <0.10% MnO, <0.45% TFe, <0.10% P, 1.17% S, 0.44% K, CaO/SiO2=1.24
39.8% Zn, balance is Cu
39.9% Zn, 4.2% Au, balance is Cu
39.9% Zn, 4.2% Au, balance is Cu
40.5% Zn, balance is Cu
41.3% SiO2, 33.7% CaO, 24.5% Al2O3
41.5% SiO2, 33.9% CaO, 24.6% Al2O3
41.5% SiO2, 33.9% Ca0, 24.6% Al2O3
41.5% SiO2, 33.9% CaO, 24.6% Al2O3
41.6% Zn, balance is Cu
41.7% Si02, 37.9% Ca0, 20.4% Al203
41.8% Ni, 36.9% Fe, 16.0% Cr, 3.02% Nb, 1.65% Ti, 0.19% Al, 0.01% C, 0.05% Si, 0.003% N, 0.001% S
41.8% Ni, 36.9% Fe, 16.0% Cr, 3.02% Nb, 1.65% Ti, 0.19% Al, 0.01% C, 0.05% Si, 0.003% N, 0.001% S
42.0-46.0% Ni, 19.5-22.5% Cr, min 22% Fe, 2.5-3.5% Mo, 1.5-3.0% Cu, 1.9-2.4% Ti, 0.1-0.5% Al, max. 1.0% Mn, max. 0.5% Si, max. 0.5% Nb, max. 0.03% C, max. 0.03% P
42.0-46.0% Ni, 19.5-22.5% Cr, min. 22.0% Fe, 2.5-3.5% Mo, 1.9-2.4% Ti, 0.1-0.5% Al, max. 1.0% Mn, ma. 0.5% Si, max. 0.5% Nb, max. 0.03% C, max. 0.03% S
42.0-46.0% Ni, 19.5-22.5% Cr, min. 22.0% Fe, 2.5-3.5% Mo, 1.9-2.4% Ti, 0.1-0.5% Al, max. 1.0% Mn, ma. 0.5% Si, max. 0.5% Nb, max. 0.03% C, max. 0.03% S
42.0-46.0% Ni, 19.5-22.5% Cr, min. 22.0% Fe, 2.5-3.5% Mo, 1.9-2.4% Ti, 0.1-0.5% Al, max. 1.0% Mn, ma. 0.5% Si, max. 0.5% Nb, max. 0.03% C, max. 0.03% S
42.1% Fe, 38.3% Ni, 12.9% Co, 4.70% Nb, 1.58% Ti, 0.35% Si, 0.04% Al, 0.01% C, 0.01% Cr
42.5% Ni, 25.0% Cr, max. 0.10% C, 0.10% Al, max. 0.4% Nb, max. 1.0% Ti, max. 1.0% Mn, max. 1.8% Si, max. 0.03% P, max. 0.015% S, max. 0.75% Cu, max. 1.5% Mo, max. 0.2% Ta, balance is Fe
42.99% CaO, 33.52% SiO2, 13.77% Al2O3, 6.28% MgO, <0.37% Fe2O3, 0.27% MnO, C/S=1.28
42.99% CaO, 33.52% SiO2, 13.77% Al2O3, 6.28% MgO, <0.37% Fe2O3, 0.27% MnO
42.99% CaO, 33.52% SiO2, 13.77% Al2O3, 6.28% MgO, 0.37% FeO, <0.02% P2O5.
43.0% Zn, balance is Cu
43.67% Al, 4.08% Nb, 1.02% Mo, 0.1% B, balance is Ti
43.7% Ni, balance is Zn
44.0% Ni, 16.0% Cr, 0.1% C, 3.0% Mo, 29.6% Co, 2.5% Ti, 3.0% Al
44.1% Zn, balance is Cu
44.5% CaO, 20.6% Fe (total iron in the oxides), 10.2% Fe2+, 10.4% Fe3+, 10.14% SiO2, 4.78% MnO, 2.18% MgO, 2.05% Al2O3, 2.43% P2O5, 0.89% TiO2, 0.37% V2O5
44.5% CaO, 20.6% Fe (total iron in the oxides), 10.2% Fe2+, 10.4% Fe3+, 10.14% SiO2, 4.78% MnO, 2.18% MgO, 2.05% Al2O3, 2.43% P2O5, 0.89% TiO2, 0.37% V2O5
45% W, balance is Ni. 45% W, 10% Co, balance is Ni.
45.9% Al, 8% Nb, balance is Ti
46.5-48.0% Ni, 19.5-23.0% Cr, 3.00-4.00% Mo, 2.80-3.50% Nb, 1.50-3.00% Cu, 0.50-2.50% Ti, 0.01-0.70% Al, max. 1.00% Mn, max. 0.50% Si, max. 0.010% S, max. 0.020% P, 0.005-0.040% C, balance is Fe
46.5-48.0% Ni, 19.5-23.0% Cr, 3.00-4.00% Mo, 2.80-3.50% Nb, 1.50-3.00% Cu, 0.50-2.50% Ti, 0.01-0.70% Al, max. 1.00% Mn, max. 0.50% Si, max. 0.010% S, max. 0.020% P, 0.005-0.040% C, balance is Fe
47.1% Ni, 22.4% Fe, 20.5% Cr, 3.2% Mo, 3.1% Nb, 2.0% Cu, 1.49% Ti, 0.20% Al, 0.011% Cu, 0.07% Mn, 0.0004% S
47.1% Ni, 22.4% Fe, 20.5% Cr, 3.2% Mo, 3.1% Nb, 2.0% Cu, 1.49% Ti, 0.20% Al, 0.011% Cu, 0.07% Mn, 0.0004% S
47.34% Fe, 2.00% V, 0.007% C, 0.105% Si, 0.22% Ni, balance is Co
48 at.% Ti, balance is Ni
48% Fe, 15% Cr, 14% Mo, 2% Y, 6% B, 15% C
48% Fe, 3.6% Ni, 1.6% V, balance is Co
48.2SiO2-9.8Al2O3-19.2MgO-7.4MgF-6.7K2O-8.7B2O3
49.2% Cd, balance is Ag
50% CaO, 43% Al2O3, 7% SiO2, 0% B2O3. CS-2: 47% CaO, 41% Al2O3, 7% SiO2, 5% B2O3.
50.00-55.00% Ni, 17.00-21.00% Cr, 4.75-5.50% Cb, 2.80-3.30% Mo, 0.20-0.80% Al, 0.65-1.15% Ti, max. 0.35% Mn, max. 0.35% Si, max. 0.006% B, max. 0.08% C, max. 0.15% S, Mg residual, balance is Fe
50.00-55.00% Ni, 17.00-21.00% Cr, 4.75-5.50% Nb+Ta, 2.80-3.30% Mo, 0.65-1.15% Ti, 0.20-0.80% Al, max. 1.00% Co, max. 0.08% C, max. 0.35% Mn, max. 0.35% Si, max. 0.015% P, max. 0.015% S, max. 0.006% B, max. 0.30% Cu, balance is Fe
50.00-55.00% Ni, 17.00-21.00% Cr, 4.75-5.50% Nb+Ta, 2.80-3.30% Mo, 0.65-1.15% Ti, 0.20-0.80% Al, max. 1.00% Co, max. 0.08% C, max. 0.35% Mn, max. 0.35% Si, max. 0.015% P, max. 0.015% S, max. 0.006% B, max. 0.30% Cu, balance is Fe
50.52 at% S - 0.6 at% Fe
50.59% Ni, 0.10% O, 0.12% C, 0.012% Fe, balance is Ti
50.8 at% Ni - 49.2 at% Ti
50.8 % Ni, balance is Ti
50.8% Ni, balance is Ti
51-63% Ni, 15-15.50% Cr, 4-7% Fe, max. 0.01% C, max. 1% Mn, max. 0.08% Si, 3-4.50% W, 15-17% Mo, max. 2.50% Co, max. 0.30% V, max. 0.02% P, max. 0.01% S
51-63% Ni, 15-16.50% Cr, 4-7% Fe, max. 0.01% C, max. 1.00 % Mn, max. 0.08% Si, 3-4.50% W, 1.50-1.70% Mo, max. 2.50% Co, max. 0.30% V, max. 0.02% P, max. 0.01% S
51% Co, 10% Ni, 20% Cr, 15% W, 3% Fe, 1.50% Mn, 0.40% Si, 0.10% C
51.5% Ni, 19.9% Fe, 18.2% Cr, 5.1% Nb, 2.9% Mo, 1.15% Ti, 0.57% Al, 0.035% C
51.5% Ni, 19.9% Fe, 18.2% Cr, 5.1% Nb, 2.9% Mo, 1.15% Ti, 0.57% Al, 0.035% C
51.5% Ni, 19.9% Fe, 18.2% Cr, 5.1% Nb, 2.9% Mo, 1.15% Ti, 0.57% Al, 0.035% C
51.5% Ni, 18.2% Cr, 5.1% Nb, 2.9% Mo, 1.15% Ti, 0.57% Al, 0.035% Cr
51.5% Ni, 18.2% Cr, 5.1% Nb, 2.9% Mo, 1.15% Ti, 0.57% Al, 0.035% Cr
51.5% Ni, 18.2% Cr, 5.1% Nb, 2.9% Mo, 1.15% Ti, 0.57% Al, 0.035% Cr
52% Ni, 19% Fe, 19% Cr, 5.3% Nb, 3.1% Mo, 0.95% Ti, 0.55% Al
52%, 54%, 56% Ni, balance is Ti
52% Ni, 19% Cr, 8% Mo, 5% Nb+Ta, 0.8% Ti, 0.6% Al, 0.05% C, balance is Ni
52% Ni, 19% Fe, 19% Cr, 5.3% Nb, 3.1% Mo, 0.95% Ti, 0.55% Al
52% Zn, balance is Mg and 55% Zn, balance is Mg
52.3% Fe, 15% Cr, 2% Mn, 2.5% Mo, 1.7% W, 16% B, 4% C, 2.5% Si
52.5% Ni, 0.04% C, 19.0% Cr, 0.90% Ti, 0.50% Al, 0.005% B, 3.05% Mo, 5.30% Nb, balance is Fe
52.5% Ni, 0.04% C, 19.0% Cr, 0.90% Ti, 0.50% Al, 0.005% B, 3.05% Mo, 5.30% Nb, balance is Fe
52.5 at.% Ni, balance is Ti
52.52% Ni, 18.67% Fe, 18.29% Cr, 3.07% Mo, 0.97% Ti, 0.59% Al, 5.37% Nb, 0.09% Mn, 0.10% Si
52.7% Ni, 17.5% Cr, 5.0% Nb, 3.17% Mo, 1.07% Ti, 0.68% Al, balance is Fe
52.8% Ni, 18.6% Cr, 5.5% Nb, 3.1% Mo, 1.l% Ti, 0.5% Al, 0.2% Co, 0.04% C, balance is Fe
52.81% Ni, 18.28% Fe, 18.38% Cr, 3.08% Mo, 0.99% Ti, 0.61% Al, 5.31% Nb, 0.12% Mn, 0.16% Si. Ingot: 52.52% Ni, 18.67% Fe, 18.29% Cr, 3.07% Mo, 0.97% Ti, 0.59% Al, 5.37% Nb, 0.09% Mn, 0.10% Si.
52.9% Ni, 10.1% Fe, 8.6% Co, 8.10% Mo, 5.05% Nb+Ta, 0.90% Ti, 0.48% Al, 0.04% Mn, 0.06% Si, 0.03% C, 0.003% B, 0.006% S, 0.005% P, 0.01% Cu
53% Ni, 0.05% C, 1.0% Ti, 0.7% Al, 19.0% Cr, 3.0% Mo, 5.3% Nb+Ta, 0.008% B, 0.03% Zr, 0.2% Mn, 0.3% Si, balance is Fe
53.1-53.2% Ni, 17.8-19.1% Fe, 0.03-0.05% C, 0.21-1.12% Si, 17.9-18.3% Cr, 3.0-3.06% Mo, 5.11-5.17% Nb+Ta, 0.96-1.O% Ti, 0.42-0.47% Al
53.30% Ni, 17.66% Fe, 19.21% Cr, 1.03% Ti, 0.4% Al, 5.06% Nb, 2.92% Mo, 0.01% Co, 0.04% C, <0.10% Mn
53.30% Ni, 17.66% Fe, 19.21% Cr, 1.03% Ti, 0.4% Al, 5.06% Nb, 2.92% Mo, 0.01% Co, 0.04% C, <0.10% Mn
53.46% Ni, 18.65% Cr, 3.06% Mo, 5.08% Nb, 0.99% Ti, 0.72% Al, 0.035% C
53.8% Ni, 18.0% Cr, 3.0% Mo, 5.24% Cb+Ta, 1.0% Ti, 0.59% Al, 0.05% C, 0.003% , 0.004% B, balance is Fe
53.8% Ni, 18.0% Cr, 3.00% Mo, 5.24% Nb+Ta, 1.00% Ti, 0.59% Al, 0.05% C, 0.003% S, 0.004% B, balance is Fe
53.8% Ni, 18.0% Cr, 3.00% Mo, 5.24% Nb+Ta, 1.00% Ti, 0.59% Al, 0.059% C, 0.003% S, 0.004% B, balance is Fe
53.8% Ni, 18.0% Cr, 3.00% Mo, 5.24% Nb+Ta, 1.00% Ti, 0.59% Al, 0.05% C, 0.003% S, 0.004% B, balance is Fe
53.8% Ni, 18.0% Cr, 3.00% Mo, 5.24% Nb+Ta, 1.00% Ti, 0.59% Al, 0.05% C, 0.003% S, 0.004% B, balance is Fe
54.02% Ni, 20.64% Cr, 14.41% Fe, 3.19% Mo, 3.91% Nb, 1.93% Cu, 1.44% Ti, 0.18% Al, 0.06% Mn, 0.05% Si, 0.0008% S, 0.007% P, 0.007% C, 0.002% B, 0.02% W, 0.12% Co
54.02% Ni, 20.64% Cr, 14.41% Fe, 3.19% Mo, 3.91% Nb, 1.93% Cu, 1.44% Ti, 0.18% Al, 0.06% Mn, 0.05% Si, 0.0008% S, 0.007% P, 0.007% C, 0.002% B, 0.02% W, 0.12% Co
54.02% Ni, 20.64% Cr, 14.41% Fe, 3.19% Mo, 3.91% Nb, 1.93% Cu, 1.44% Ti, 0.18% Al, 0.06% Mn, 0.05% Si, 0.0008% S, 0.007% P, 0.007% C, 0.002% B, 0.02% W, 0.12% Co
54.02% Ni, 20.64% Cr, 14.41% Fe, 3.19% Mo, 3.91% Nb, 1.93% Cu, 1.44% Ti, 0.18% Al, 0.06% Mn, 0.05% Si, 0.0008% S, 0.007% P, 0.007% C, 0.002% B, 0.02% W, 0.12% Co
54.5-57.0% Ni, max. 0.050% C, max. 0.010% Cu, max. 0.010% Cr, max. 0.005% H, max. 0.050% Fe, max. 0.025% Nb, 0.050% N+O, balance is Ti
54.5-57.0% Ni, max. 0.050% C, max. 0.010% Cu, max. 0.010% Cr, max. 0.005% H, max. 0.050% Fe, max. 0.025% Nb, 0.050% N+O, balance is Ti
55.0-59.0% Ni, 19.0-22.5% Cr, 7.0-9.5% Mo, 2.75-4.00% Nb, 1.0-1.7% Ti, max. 0.35% Al, max. 0.03% C, max. 0.35% Mn, max. 0.20% Si, max. 0.015% P, max. 0.010% S, balance is Fe.
57% FeO, 26% SiO2, 6% ZnO, 3% Al2O3, 2% CaO, Pb, Cr and Cu oxides are bellow 0.7%
58.0% Ni, 20.0-23.0% Cr, max. 5.0% Fe, 8.0-10.0% Mo, Nb+Ta=3.15-4.15%, max. 0.10% C, max. 0.50% Mn, max. 0.50% Si, max. 0.015% P, max. 0.015% S, max. 0.40% Al, max. 0.40% Ti, max. 1.0% Co
58.3% Ni, 20.8% Cr, 8.0% Mo, 7.4% Fe, 3.5% Nb, 1.52% Ti, 0.21% Al, 0.006% C, 0.008% N, 0.07% Mn, 0.0004% S
58.3% Ni, 20.8% Cr, 8.0% Mo, 7.4% Fe, 3.5% Nb, 1.52% Ti, 0.21% Al, 0.006% C, 0.008% N, 0.07% Mn, 0.0004% S
59% Ni, 22% Cr, 13% Mo, 3% W, 3% Fe
60% Cu, 40% Zn
60-40 Alpha-Beta Brass
60NiTi
60.2% Ni, 22.2% Cr, 9.2% Mo, 4.1% Fe, 0.06% Cu, 0.06% W, 0.12% Mn, 0.08% Si, 0.17% Ti, 0.16% Al, 3.5% Cb, 0.04% N, 0.02% C, 0.007% P, 0.002% S
60.6% Ni, balance is Ti
60.64% Ni, 0.02% C, 0.09% Mn, 0.19% Si, 22.14% Cr, 4.06% Fe, 9.0% Mo, 3.39% Nb+Ta, 0.22% Al, 0.24% Ti, 0.001% B, 0.05% Co
60.64% Ni, 0.02% C, 0.09% Mn, 0.19% Si, 22.14% Cr, 4.06% Fe, 9.0% Mo, 3.39% Nb+Ta, 0.22% Al, 0.24% Ti, 0.001% B, 0.05% Co
60.64% Ni, 0.02% C, 0.09% Mn, 0.19% Si, 22.14% Cr, 4.06% Fe, 9.0% Mo, 3.39% Nb+Ta, 0.22% Al, 0.24% Ti, 0.001% B, 0.05% Co
60.64% Ni, 0.02% C, 0.09% Mn, 0.19% Si, 22.14% Cr, 4.06% Fe, 9.0% Mo, 3.394% Nb+Ta, 0.22% Al, 0.24% Ti, 0.001% B, 0.05% Co
60.96% Ni, 0.02% C, 0.12% Mn, 0.31% Si, 21.94% Cr, 8.82% Fe, 8.94% Mo, 8.47% Nb+Ta, 0.21% Al, 0.20% Ti, 0.06% Co, 0.001% B
60.96% Ni, 0.02% C, 0.12% Mn, 0.31% Si, 21.94% Cr, 8.82% Fe, 8.94% Mo, 8.47% Nb+Ta, 0.21% Al, 0.20% Ti, 0.06% Co, 0.001% B
60.96% Ni, 22.21% Cr, 3.61% Fe, 8.97% Mo, 8.60% Nb+Ta, 0.19% Al, 0.27% Ti, 0.26% Si, 0.06% Mn, 0.006% P, 0.004% S, 0.08% Cu, 0.03% C, balance is Ni
61.0% Ni+Co, 21.6% Cr, 9.0% Mo, 3.66% Nb+Ta, 2.6% Fe, 0.06% C, 0.26% Mn, 0.008% S 0.26% Si, 0.2% Al, 0.2% Ti, balance is Ni
61.0% Ni+Co, 21.6% Cr, 9.0% Mo, 3.66% Nb+Ta, 2.6% Fe, 0.06% C, 0.26% Mn, 0.008% S, 0.26% Si, 0.2% Al, 0.2% Ti, balance is Ni
61.0% Ni+Co, 21.6% Cr, 9.0% Mo, 3.66% Nb+Ta, 2.6% Fe, 0.06% C, 0.26% Mn, 0.008% S, 0.26% Si, 0.2% Al, 0.2% Ti, balance is Ni
61.0% Ni+Co, 21.6% Cr, 9.0% Mo, 3.66% Nb+Ta, 2.6% Fe, 0.06% C, 0.26% Mn, 0.008% S, 0.26% Si, 0.2% Al, 0.2% Ti, balance is Ni
61% Ni, 0.01% C, 21% Cr, 6% Mo, 3.4% Nb, 1.3% Ti, 0.2% Al, 5% Fe
61.6% Ni, 19.9% Fe, 18.2% Cr, 6.1% Nb, 2.9% Mo, 1.16% Ti, 0.67% Al, 0.036% Cr
61.6% Ni, 20.2% Fe, <0.06% Co, 3.20% Mo, 5.28% Nb+Ta, 0.94% Ti, 0.46% Al, 0.04% Mn, 0.06% Si, 0.03% C, 0.008% B, 0.007% S, 0.004% P, <0.01% Cu
61.6% Ni, 9.8% Fe, <0.05% Co, 8.20% Mo, 5.18% Nb+Ta, 0.96% Ti, 0.58% Al, 0.04% Mn, 0.06% Si, 0.02% C, 0.001% B, 0.006% S, 0.002% P, <0.01% Cu
62.0% Ni, 9.50% Co, 6.60% Cr, 4.50% Mo, 0.00% W, 2.80% Re, 5.60% Al, 1.30% Ti, 7.30% Ta, 0.30% Nb, 0.10% Hf
62.0% Ni, 9.50% Co, 6.60% Cr, 4.50% Mo, 0.00% W, 2.80% Re, 5.60% Al, 1.30% Ti, 7.30% Ta, 0.30% Nb, 0.10% Hf
62.0% Ni, 9.50% Co, 6.60% Cr, 4.50% Mo, 0.00% W, 2.80% Re, 5.60% Al, 1.30% Ti, 7.30% Ta, 0.30% Nb, 0.10% Hf
62.6% Ni, 0.04% C, 19.0% Cr, 0.90% Ti, 0.60% Al, 0.006% B, 3.06% Mo, 6.30% Nb, balance is Fe
62.7% Ni, 15.0% Cr, 0.07% C, 6.3% Mo, 18.5% Co, 3.5% Ti, 4.3% Al, 0.03% B
62.8% Ni, <0.05% Fe, 8.8% Co, 3.0% Mo, 5.09% Nb+Ta, 0.86% Ti, 0.47% Al, 0.04% Mn, 0.05% Si, 0.03% C, 0.002% B, 0.006% S, 0.004% P, 0.01% Cu
63.1-63.2% Ni, 17.8-19.1% Fe, 0.03-0.06% C, 0.21-1.12% Si, 17.9-18.3% Cr, 3.0-3.06% Mo, 5.11-6.17% Nb+Ta, 0.96-1.0% Ti, 0.42-0.47% Al
63.6% Ni, 8.0% Cr, 7.5% Co, 1.5% Mo, 4.0% W, 5.0% Ta, 1.5% Ti, 5.8% Al, 3.0% Re
64.2% Ni, 0.26% Fe, 17.6% Co, 3.19% Mo, 6.31% Nb+Ta, 0.92% Ti, 0.48% Al, 0.03% Mn, 0.04% Si, 0.04% C, 0.003% C, 0.006% S, 0.006% P, 0.01% Cu
70.0% Ni+Co, 14.0-17.0% Cr, 5.0-9.0% Fe, 2.25-2.75% Ti, 0.70-1.20% Nb+Ta, max. 1.0% Mn, max. 0.50% Si, max. 0.01% S, max. 0.50% Cu, max. 0.08% C, max. 1.0% Co, balance is Ni
70% (CaO and SiO2), 0-6% MgO, 2-6% Al2O3, 2-10% Na2O (+ K2O), 0-10% F with varying additions of TiO2, ZrO2, B2O3
72.0% Ni, 7.6% Fe, 15.4% Cr, 0.9% Al, 2.5% Ti, 0.9% Nb, 0.1% Si, 0.004% C
72.02% Ni, 0.06% C, 0.19% Mn, 7.82% Fe, 0.001% S, 0.40% Si, 0.37% Cu, 14.82% Cr, 0.85% Al, 2.49% Ti, 0.98% Nb+Ta
72.02% Ni, 0.06% C, 0.19% Mn, 7.82% Fe, 0.001% S, 0.40% Si, 037% Cu, 14.82% Cr, 0.85% Al, 2.49% Ti, 0.98% Nb+Ta
73.19% Ni, 0.03% C, 0.56% Mn, 6.51% Fe, 0.00796 S, 0.27% Si, 0.06% Cu, 15.24% Cr, 0.76% Al, 2.50% Ti, 0.85% Nb+Ta
73.5% Fe, 16.5% Si, 6.00% B, 3.00% Nb, 1.00% Cu
74.5% Ni, 0.029% C, 0.211% Mn, 8.05% Fe, 0.003% S, 0.180% Si, 0.219% Cu, 14.09% Cr, 0.464% A1, 0.259% Ti, 0.034% Co, 0.007% P, 0.002% B, 0.026% Mg
75% FeSi
78.19% Ni, O.O3% C, 0.56% Mn, 6.51% Fe, 0.007% S, 0.27% Si, 0.06% Cu, 15.24% Cr, 0.76% Al, 2.50% Ti, 0.85% Nb+Ta
95.83% Cu, 3.95% Ti, 0.13% Zn, 0.01% Ni
97.7% Cu, 2.1-2.6% Fe, 0.015-0.15% P, max.0.03% Pb, 0.05-0.20% Zr
99.03% Cu, 0.7% Cr, 0.13% Zn, 0.003% Pb
299 ppm Fe, 2 ppm Si, 1 ppm Cu, 1 ppm Mn, 0 ppm Cr, 1 ppm Ni, 1 ppm Zn, 1 ppm Ga, 0.3 ppm Ti, balance is Al
300 ppm total impurities
Al-59 at.% Zn
Al-59 at.% Zn
Al-59 at.% Zn
Al-6.5 at.% Mn
Al2O3 and SiO2
Al2O3, TiO2, Ti3O5
Al2O3
Al2O3
Al2O3
Au49 Ag5.5 Pd2.3 Cu26.9 Si16.3
Al-0.9Mg-0.5Si
Al-5.2Mg-2.0Li-0.1Zr
Al-5.2Mg-2.0Li-0.1Zr
Al-5.4Zn-1.23Mg-0.16Zr-0.15Fe-0.08Si
Al-6.3Cu-0.25Mn-0.13Zr-0.06V-0.08Si-0.14Fe-0.07Ti
Al-6.3Cu-0.25Mn-0.13Zr-0.06V-0.08Si-0.14Fe-0.07Ti
Al88Mn12
Au78Ge14Si8, Pd82Si18, Pd78Cu6Si16
Bi1.7-Pb0.4-Sr1.6-Ca2.4-Cu3.6-Ox
Bi 1.7Pb 0.4 Sr1.6 Ca2.4 Cu3.6 Ox.
Base alloy: 16.0% Cr, 5.0% Ti, 3.0% Mo, 0.005% C, balance is Co. Low Ti: 17.6% Cr, 4.4% Ti, 8.0% Mo, 0.015% C, balance is Co.
Base alloy: 16.0% Cr, 5.0% Ti, 3.0% Mo, 0.005% C, balance is Co. Ni-Modified: 17.3% Cr, 4.4% Ti, 3.0% Mo, 11.6% Ni, 0.017% C, balance is Co.
Co-27Cr-5Mo-0.05C
Co-27Cr-5Mo-0.05C
Co-27Cr-5Mo-0.05C
Co-27Cr-5Mo-0.05C
Co-27Cr-5Mo-0.05C
Cu-11.87% Al
Cu-11.8% Al
Cu-10.5% Al
Cu-9.90% Al-5.30% Fe-5.10% Ni-0.90% Mn
Cu-8.8% Al-5.4% Fe-5% Ni-0.9% Mn
Cu60Cd40
Cu60Zr40
Ce0.5Zr0.5O2(22.25)
Ce0.8Gd0.2O(1.9-x)
Co77.4Fe1.4B14Si2Nb4Mn1.4
Cu(100-x)Zr(x) (x=35-38.2 at.%
CeO(2-x)
CaO-SiO2-13% Al2O3-8% MgO-25% FeO
Cu50Zr43Al7 and (Cu50Zr43Al7)99Si1 BMGs
Cu50Zr50 and Cu20Zr80
CaO - SiO2 - 13% Al2O3 - 8% MgO - 25% FeO
CaO-SiO2-Al2O3-CaF2
CaO-SiO2-Al2O3-Na2O-CaF2-NaF
CaO-SiO2-CaF2-Na2O
CaO-SiO2-CaF2
CaO-SiO2-Na2O-Al2O3-CaF2
CaO-SiO2-Na2O-CaF2
CaO-SiO2
Co77.4Fe1.4B14Si2Nb4Mn1.4
CoFe: 60% Fe, balance is Co. CoFeV: 48.8% Fe, 2.5% V, balance is Co. CoFeCr: 49.8% Fe, 0.4% Cr, balance is Co.
Cu-15Ni-8Sn
Cu6Sn5, (Cu,Ni)6Sn5
69% SiO2, 25% B2O3, 6% Na2O
69.8% Ni, <0.05% Fe, <0.05% Co, 3.02% Mo, 5.14% Nb+Ta, 0.93% Ti, 0.53% Al, 0.04% Mn, 0.05% Si, 0.03% C, 0.003% B, 0.008% S, 0.004% P, <0.01% Cu
Fe80B20
Fe80B20
Fe90Ca10
Fe40Ni38B18Mo4
Fe80P13C7
Fe81Zr9B10
Fe73.5Si16.5B6Nb3Cu1
Fe-Si, Si
FeO, Fe3O4
Ge2Sb2Te5
Li2Si2O5
Mg-2Sn, Mg-10Gd-2Y-0.5Zr, Mg-6Zn-0.7Zr
MgO x Al203
Nb-30% Zr, Nb-40% Zr, Nb-50% Zr, Nb-60% Zr
Ni-18.26Fe-18.87Cr-4.97Nb-2.97Mo-0.94Ti-0.46Al-0.03C-0.06Mn-0.23Co-0.05Cu-0.06Si. AM alloy: Ni-18.5Fe-18.3Cr-4.99Nb-3.04Mo-1.02Ti-0.55Al-0.051C-0.23Mn-0.39Co-0.07Cu-0.08Si.
Ni-18.26Fe-18.87Cr-4.97Nb-2.97Mo-0.94Ti-0.46Al-0.03C-0.06Mn-0.23Co-0.05Cu-0.06Si. AM alloy: Ni-18.5Fe-18.3Cr-4.99Nb-3.04Mo-1.02Ti-0.55Al-0.051C-0.23Mn-0.39Co-0.07Cu-0.08Si.
Ni-18.26Fe-18.87Cr-4.97Nb-2.97Mo-0.94Ti-0.46Al-0.03C-0.06Mn-0.23Co-0.05Cu-0.06Si. AM alloy: Ni-18.5Fe-18.3Cr-4.99Nb-3.04Mo-1.02Ti-0.55Al-0.051C-0.23Mn-0.39Co-0.07Cu-0.08Si.
Ni-18.26Fe-18.87Cr-4.97Nb-2.97Mo-0.94Ti-0.46Al-0.03C-0.06Mn-0.23Co-0.05Cu-0.06Si. AM alloy: Ni-18.5Fe-18.3Cr-4.99Nb-3.04Mo-1.02Ti-0.55Al-0.051C-0.23Mn-0.39Co-0.07Cu-0.08Si.
Ni-18.26Fe-18.87Cr-4.97Nb-2.97Mo-0.94Ti-0.46Al-0.03C-0.06Mn-0.23Co-0.05Cu-0.06Si. AM alloy: Ni-18.5Fe-18.3Cr-4.99Nb-3.04Mo-1.02Ti-0.55Al-0.051C-0.23Mn-0.39Co-0.07Cu-0.08Si.
Ni-15Cr-4Al-6Nb
Ni-14% Al
Ni 0-20% Mo (Ni4Mo)
Nb80Si20
Ni52Ti48
Ni85Ti15
Ni-12Co-2.5Cr-9W-6.4Re-6Al-5.5Ta-0.15Hf
Ni4Mo
NiS
NiS
NiS
Pb-80.00% Sn
Pb-61.90% Sn
Pu-1.9 at% Ga
Pu-1.9 at.% Ga
Pu-1.4 at.% Ga, Pu-1.9 at.% Ga
Pu-0.56 wt.% Ga
Pd40Cu30Ni10P20
Pd40Cu30Ni10P20
Pd70Ni10Si20
Pd60Ni20Si20
Pd50Ni30Si20
Pd80Si20
Pd0.82Si0.18, Pd0.775Si0.165Cu0.06
Pd43-Ni40-Cu27-P20
Pd43Ni10Cu27P20
Pd43Ni10Cu27P20
Pd43Ni10Cu27P20
Pd55Ni30Si15
Pd31Ni42S27
Pd31Ni42S27
Pd40Cu30Ni10P20
Pd40Cu30Ni10P20
Pt42:5Cu27Ni9:5P21
Pd42.5Ni7.5Cu30P20, Zr46Cu30.14Ag8.14Al8Be7.5, Zr41.2Ti13.8Cu12.5Ni10Be22.5, (Ti36.1Zr33.2Ni5.8Ni10Be24.9)91Cu9
Pd43Ni10Cu27P20
POS and SOS (purity at least 99%) were purchased
POS and SOS (purity at least 99%) were purchased
PZT-sol-gel
Pt57.3Cu14.6Ni5.3P22.8
Pu-1.9 at.% Ga
Ti-51Ni
Ti-13% Mo
Ti-6Al-2Sn-4Zr-2Mo, Ti-10V-2Fe-3Al
Ti-6Al-4V (TIMETAL 6-4)
Ti-6Al-4V
Ti-3Al-5Mo-5V-4Cr-2Zr
TiO2
Ti-6Cr-5Mo-5V-4Al alloy (Ti-6554): 5.7% Cr, 4.7% Mo, 4.81% V, 3.93% Al, 0.08% Fe, 0.028% Si, 0.025% V, balance is Ti
Ti-8.0% Co, T-14.0% Cr, Ti-5.5% Cu, Ti-13.0% Fe, Ti-5.1% Ni
Ti-10V-2Fe-3Al: 10V2Fe3Al
Ti-10V-xFe-3A
Ti13V11Cr3Al
Ti13V11Cr4Al
Ti16V0.5Al
Ti-48Al
Ti-25Al-16Nb
Ti-44Al-8Nb, Ti-44Al-4Ta-4Zr-0.2Si
Ti-45Al-2Cr-2Nb
Ti-46.5Al-2Cr-2Nb-0.9Mo-0.2B
Ti-48Al. b.) a.) Ti-48Al. c) Ti-46.5Al-2Cr-2Nb-0.9Mo-0.2B. d.) Ti-45Al-2Cr-2Nb.
Ti-48Al
Ti-48Al
Ti-5Al-2.5Fe, Ti-6.4Al-1.2Fe, Ti-8Al-2Fe
Ti-5Al-2Sn-2Zr-4Mo-4Cr
Ti-62.5 at.% Al
Ti-6Al-2.5Cu (IM 230)
Ti-6Al-2Sn-4Zr-2Mo
Ti-6Al-4V
Ti70Ta30
U-2.5Zr-7.5Nb
U-5 Mo with 1, 3% Zr, 5% Mo
U-5Nb, U-5Nb-5Mo, U-5Mo
U-6 wt% Nb
U-7 Mo with 1, 2, 3% Zr, 7% Mo
U-10 Mo with 1, 2, 6, 10% Zr
U-520 composition: 0.03% C, 18.8% Cr, 11.8 Co, 6.0% Mo, 0.9% W, 2.9% Ti, 2.1% Al, 0.02% B, balance is Ni. U-710 composition: 0.08% C, 17.7% Cr, 15.1% Co, 3.0% Mo, 1.4% W, 4.8% Ti, 2.4% Al, 0.02% B, balance is Ni.
U-8 wt% Mo
Zr-1.3% Mo
Zr41.2Ti13.8Cu12.5Ni10.0Be22.5
Zr41.2Ti13.8Cu12.5Ni10Be22.5 (Vit1), Zr57Cu15.4Ni12.6Al10Nb5 (Vit106)
Zr41.2Ti13.8Cu12.5Ni10Be22.5, Zr57Cu15.4Ni12.6Al10Nb5, Zr55Al22.5Co22.5
Zr41.2Ti13.8Cu12.5Ni10Be22.5
Zr52.5Ti5Al10Ni14Cu17.9
Zr55Al22.5Co22.5, Zr57Cu15.4Ni12.6Al10Nb5, Zr41.2Ti13.8Cu12.5Ni10Be22.5
Zr55Co26Al19, Zr46Cu30.14Al8Ag8.36Be7.5
Zr55Co26Al19, Zr46Cu30.14Al8Ag8.36Be7.5
Zr57Cu15.4Ni12.6Al10Nb5, Zr52.5Cu17.9Ni14.6Al10Ti5
Zr58.5Nb2.8Cu15.6Ni12.8Al10.3
Zr41:2Ti13:8Cu12:5Ni10Be22:5
Zr41.2Ti13.8Cu12.5Ni10.0Be22.5
Zr41.2Ti13.8Cu12.5Ni10.0Be22.5
Zr41.2Ti13.8Cu12.5Ni10.0Be22.5
Zr44Ti11Cu10Ni10Be25
Zr-12% Nb, Zr-17.5% Nb
Zr52.5Cu17.9Ni14.6Al10Ti5
Zr58.5Cu15.6Ni12.8Al10.3Nb2.8
Zr75.91Ni24.1