6061 A Alloy

Alloy name: 6061 A
Diagram No.: 827
Type of diagram: TTT
Chemical composition in weight %: 6061 A: 0.65% Si, 0.81% Mg, 0.32% Fe, 0.26% Cu, 0.01% Ni, 0.05% Zn, 0.09% Cr, 0.04% Ti, 0.06% Mn, balance is Al. 6061 B: 0.6% Si, 1.01% Mg, 0.2% Fe, 0.2% Cu, 0.09% Zn, 0.17% Cr, 0.01% Ti, 0.06% Mn, balance is Al.
Alloy group: Aluminium-based alloys
Note: Diagram of the alloy TTP 6061 B (solid line) compared to the alloy 6061 A.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 20.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT of Steels
Hardenability Diagrams of Steels
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Tempering Diagrams of Steels

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.








Copyright © 2024 by Steel Data. All Rights Reserved.