24CrMo5 Steel

Steel name: 24CrMo5
Diagram No.: 1150
DIN designation: 24CrMo5
Mat.No. (Wr.Nr.) designation: 1.7258
Old name: Atrix 203
Chemical composition in weight %: 0.24% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
Steel group: Alloy special structural steels
Applications: No data
Comment: The legend: Harte in HRC-Hardness in HRC, Abstand von der abgeschreckten Stirnseite
der Probe in mm-Distance from quenched end in mm, Austenitisierungstemperatur-Austenitizing
temperature
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 900-950oC/oil, air

Hardenability Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.