Chemical Composition of Steels in Weight %

0.04-0.12% C, 0.10-0.40% Si, max. 0.025% P, 0.010-0.035% S, 3.70-4.30% Cr, 0.40-0.60% Mo, max. 0.25% Cu
0.05-0.15% C, 0.35-0.70% Mn, 0.10-0.40% Si, 1.25-1.75% Cr, 3.25-3.75% Ni
0.07-0.12% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 1.20-1.50% Ni
0.07-0.12% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 1.20-1.50% Ni
0.07-0.12% C, mwx. 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 1.20-1.50% Ni
0.07-0.13% C, 0.15-0.35% Si, 0.40-0.70% Mn, 1.00-1.45% Cr, 2.95-3.55% Ni, 0.08-0.15% Mo
0.07-0.13% C, 0.15-0.35% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.025% S, 1.00-1.45% Cr, 2.95-3.55% Ni, 0.35% Cu, 0.08-0.15% Mo
0.07-0.13% C, 0.20-0.35% Si, 0.30-0.70% Mn, 1.30-1.80% Cr, 3.20-3.80% Ni
0.07-0.13% C, 0.20-0.35% Si, 0.40-0.70% Mn, 1.00-1.45% Cr, 2.95-3.55% Ni, 0.08-0.15% Mo
0.07-0.13% C, max. 0.35% Si, 0.20-0.50% Mn, max. 0.040% P, max. 0.035% S, 1.80-2.30% Cr
0.08% C, 0.21% Si, 0.49% Mn, 0.005% P, 0.012% S, 0.53% Cr, 1.85% Ni, 0.01% Mo, 0.26% V, 0.003% Ti, 0.05% Cu, 0.042% Al, 0.006% N
0.08% C, 0.25% Si, 0.54% Mn, 0.012% P, O.012% S, 1.56% Cr, 3.42% Ni, 0.05% Mo, 0.10% Cu, 0.032% Al
0.08% C, 0.31% Mn, 0.08% Si, 0.029% P, 0.05% S, 0.07% Ni, 0.045% Cr, 0.02% Mo
0.08% C, 0.49% Mn, 8.94% Ni
0.08-0.13% C, 0.15-0.35% Si, 0.40-0.60% Mn, max. 0.025% P max. 0.040% S, 1.40-1.75% Cr, 3.25-3.75% Ni, max. 0.35% Cu, 0.06%% Mo
0.08-0.13% C, 0.15-0.35% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.040% S, 1.40-1.75% Cr, 3.25-3.75% Ni, 0.35% Cu, 0.06% Mo
0.08-0.13% C, 0.15-0.35% Si, 0.45-0.65% Mn, max. 0.025% P, max. 0.040% S, 1.00-1.40% Cr, 0.35% Cu, 0.08-0.15% Mo, 3.00-3.50% Ni
0.08-0.13% C, 0.15-1.35% Si, 0.45-0.65% Mn, max. 0.035% P, max. 0.040% S, 1.00-1.40% Cr, 3.00-3.50% Ni, 0.35% Cu, 0.08-0.15% Mo
0.08-0.14% C, max. 0.50% Si, 0.40-0.80% Mn, max. 0.020% P, max. 0.010% S, 2.00-2.50% Cr, max. 0.30% Ni, max. 0.030% Cu, 0.90-1.10% Mo
0.08-0.14% C, max. 0.50% Si, 0.40-0.80% Mn, max. 0.020% P, max. 0.010% S, 2.00-2.50% Cr, max. 0.30% Ni, max. 0.030% Cu, 0.90-1.10% Mo
0.08-0.18% C, max. 0.35% Si, 0.40-1.00% Mn, max. 0.025% P, max. 0.010% S, 0.70-1.15% Cr, 0.40-0.60% Mo, max. 0.30% Cu
0.09-0.12% C, 0.20-0.40% Si, 1.20-1.40% Mn, max. 0.020% P, max. 0.020% S, 0.70-0.90% Cr, 0.020-0.050% Ti, 0.0015-0.0040% B
0.09-0.15% C, 0.17-0.37% Si, 0.30-0.60% Mn, 1.25-1.65% Cr, 3.25-3.65% Ni
0.09-0.15% C, 0.17-0.37% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.25-1.65% Cr, 3.25-3.65% Ni, max. 0.30% Cu
0.09-0.15% C, 0.20-0.35% Si, 0.30-0.70% Mn, 3.20-3.80% Ni, 0.20-0.30% Mo
0.09-0.15% C, 0.30% Si, 0.30-0.60% Mn, max. 0.025% P, max. 0.025% S, 0.40-0.70% Cr, max. 0.50-0.80% Ni, max. 0.25% Cu
0.09-0.15% C, 0.30% Si, 0.30-0.60% Mn, max. 0.025% P, max. 0.025% S, 0.40-0.70% Cr, max. 0.50-0.80% Ni, max. 0.25% Cu
0.09-0.16% C, 0.17-0.31% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.60-0.90% Cr, 2.75-3.15% Ni, max. 0.30% Cu
0.09-0.16% C, 0.17-0.37% Si, 0.30-0.60% Mn, 0.60-0.90% Cr, 2.75-3.15% Ni
0.10% C, 0.25% Si, 0.50% Mn, 1.20% Cr, 3.25% Ni, 0.12% Mo
0.10% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 1.45% Ni, +Pb
0.10% C, 0.30% Si, 0.50% Mn, 1.50% Cr, 3.50% Ni
0.10% C, 0.30% Si, 0.50% Mn, 1.50% Cr, 3.50% Ni
0.10% C, 0.30% Si, 0.58% Mn, 0.012% P, O.015% S, 1.26% Cr, 3.26% Ni, 0.11% Mo, 0.11% Cu, 0.044% Al
0.10% C, 0.52% Mn, 5.00% Ni
0.10% C, 1.50% Mn, 0.03% S, + B, Ti
0.10% C, 1.63% Mn, 0.41% Mo
0.10% V, 0.002% B
0.10% V, 0.045% Ti
0.10-0.15% C, 0.10-0.35% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.035% S, 0.60-1.00% Cr, 3.00-3.50% Ni, 0.020-0.050% Al
0.10-0.15% C, 0.15-0.35% Si, 0.40-0.60% Mn, max. 0.020% P, 0.005-0.010% S, 1.35-1.60% Cr, 3.25-3.75% Ni, max. 0.15% Mo
0.10-0.15% C, 0.15-0.35% Si, 0.40-0.60% Mn, max. 0.020% P, max. 0.010% S, 1.35-1.60% Cr, 3.25-3.75% Ni, max. 0.15% Mo
0.10-0.15% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, max. 0.25% Cu, 0.15-0.25% Mo
0.10-0.15% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, max. 0.25% Cu, 0.15-0.25% Mo
0.10-0.16% C, 0.10-0.35% Si, 0.35-0.60% Mn, max. 0.040% P, max. 0.040% S, 0.70-1.00% Cr, 3.00-3.75% Ni
0.10-0.16% C, 0.10-0.35% Si, 0.35-0.60% Mn, max. 0.040% P, max. 0.040% S, 0.70-1.00% Cr, 3.00-3.75% Ni
0.10-0.17% C, 0.17-0.37% Si, 0.30-0.65% Mn, max. 0.035% P, max. 0.035% S, 1.20-1.75% Cr, 3.20-4.65% Ni, max. 0.30% Cu
0.10-0.19% C, 0.40% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.60-1.00% Cr, 0.80-1.10% Ni
0.10-0.22% C, <0.40% Si, 1.10-1.40% Mn, <0.035% P, <0.035% S, 1.00-1.30% Cr
0.11% C, 0.38% Mn, 0.44% Si, 5.46% Cr, 0.42% Mo
0.11% C, 0.44% Mn, 0.37% Si, 0.16% Ni, 12.18% Cr
0.11% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
0.11% C, 0.45% Si, 0.49% Mn, 0.005% S, 0.012% P, 0.13% Ni, 12.0% Cr, 0.020% Mo
0.11% C, 0.67% Mn, 0.29% Si, 3.09% Ni, 1.19% Cr, 0.08% Mo
0.11-0.17% C, 0.15-0.40% Si, 0.35-0.65% Mn, max. 0.035% P, max. 0.035% S, 1.40-1.70% Cr, 1.40%-1.70 Ni
0.11-0.17% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 0.10-0.25% Mo, 3.0-3.50% Ni
0.11-0.17% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 0.10-0.25% Mo, 3.0-3.50% Ni
0.11-0.18% C, 0.15-0.35% Si, 0.30-0.70% Mn, max. 0.030% P, max. 0.030% S, 0.20-0.55% Cr, 0.35% Cu, 1.95-2.50% Ni
0.11-0.18% C, 0.15-0.35% Si, 0.30-0.70% Mn, max. 0.030% P, max. 0.030% S, 0.55-1.05% Cr, 0.30% Cu, 2.95-3.50% Ni
0.12% C, 0.05% Si, 0.86% Mn, 0.29% S, 0.020% P
0.12% C, 0.17% Si, 1.17% Mn, 0.11% S, 0.019% P
0.12% C, 0.22% Si, 0.36% Mn, 0.008% P, 0.013% S, 0.52% Cr, 1.84% Ni, 0.10% Mo, 0.15% V, 0.06% Cu, 0.032% Al, 0.008% N
0.12% C, 0.25% Si, 0.50% Mn, 2.15% Cr, 1.00% Mo
0.12% C, 0.25% Si, 0.50% Mn, 2.15% Cr, 1.00% Mo
0.12% C, 0.28% Si, 0.51% Mn, 0.83% Cr, 1.07% Ni, 0.95% Mo
0.12% C, 0.29% Si, 0.57% Mn, 0.47% Cr, 1.86% Ni, 0.07% V, 0.001% B
0.12-0.17% C, 0.10-0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.85-1.15% Cr, 1.20-1.60% Ni
0.12-0.17% C, 0.15-0.40% Si, 0.40-0.60% Mn, <0.035% P, <0.035% S, 1.40-1.70% Cr, 1.40-1.70% Ni
0.12-0.18% C, <0.40% Si, 0.30-0.60% Mn, <0.035% P, <0.035% S
0.12-0.18% C, <0.40% Si, 0.30-0.60% Mn, <0.035% P, <0.035% S
0.12-0.18% C, 0.10-0.35% Si, 0.25-0.50% Mn, max. 0.040% P, max. 0.040% S, 1.00-1.40% Cr, 0.15-0.30% Mo, 3.90-4.30% Ni
0.12-0.18% C, 0.10-0.35% Si, 0.25-0.50% Mn, max. 0.040% P, max. 0.040% S, 1.00-1.40% Cr, 0.15-0.30% Mo, 3.90-4.30% Ni
0.12-0.18% C, 0.10-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.040% S, 0.30-0.35% Cr, 0.08-0.15% Mo, 0.20-0.40% Ni
0.12-0.18% C, 0.10-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.040% S, 0.30-0.35% Cr, 0.08-0.15% Mo, 0.20-0.40% Ni
0.12-0.18% C, 0.10-0.35% Si, 0.60-1.00% Mn, max. 0.035% P, max. 0.035% S, 0.75-1.25% Cr, 1.50-1.25% Ni, 0.10-0.20% Mo, 0.020-0.050% Al
0.12-0.18% C, 0.15-0.35% Si, 0.30-0.70% Mn, 3.20-3.80% Ni, 0.20-0.30% Mo
0.12-0.18% C, 0.15-0.35% Si, 0.30-0.70% Mn, max. 0.040% P, max. 0.030% S, 0.20% Cr, 3.20-3.80% Ni, max. 0.35% Cu, 0.20-0.30% Mo
0.12-0.18% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.30% Mo
0.12-0.18% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu
0.12-0.18% C, 0.15-0.35% Si, 0.70-1.05% Mn, 0.25-0.55% Cr, 0.25-0.65% Ni, 0.08-0.15% Mo
0.12-0.18% C, 0.15-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.25-0.55% Cr, 0.35% Cu, 0.08-0.15% Mo, 0.0005-0.0030% B
0.12-0.18% C, 0.15-0.40% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.60-0.90% Cr, 2.50-3.00% Ni, max. 0.10% Mo
0.12-0.18% C, 0.15-0.40% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.69-0.90% Cr, 2.50-3.00% Ni
0.12-0.18% C, 0.15-0.40% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.70% Cr
0.12-0.18% C, 0.15-0.40% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.70% Cr
0.12-0.18% C, 0.15-0.40% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.70% Cr
0.12-0.18% C, 0.17-0.37% Si, 0.40-0.70% Mn, 0.70-1.00% Cr
0.12-0.18% C, 0.17-0.37% Si, 0.55-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.85-1.25% Cr, max. 0.30% Ni, max. 0.30% Cu, 0.15-0.25% Mo
0.12-0.18% C, 0.17-0.37% Si, 0.55-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.85-1.25% Cr, max. 0.30% Ni, max. 0.30% Cu
0.12-0.18% C, 0.20-0.35% Si, 0.30-0.70% Mn, 3.20-3.80% Ni, 0.20-0.30% Mo
0.12-0.18% C, 0.20-0.35% Si, 0.30-0.70% Mn
0.12-0.18% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.25-0.55% Cr, 0.25-0.65% Ni, 0.08-0.15% Mo, +B
0.12-0.18% C, 0.40% Si, 0.60-0.80% Mn, max. 0.025% P, max. 0.015% S, 0.90-1.20% Cr, max. 0.050% Al, max. 0.30% Cu, 0.15-9.25% Mo
0.12-0.18% C, 0.40% Si, 0.60-0.80% Mn, max. 0.025% P, max. 0.015% S, 0.90-1.20% Cr, max. 0.050% Al, max. 0.30% Cu, 0.15-9.25% Mo
0.12-0.18% C, max. 0.35% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 2.50-3.00% Ni, 0.60-0.90% Cr
0.12-0.18% C, max. 0.35% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S. 2.50-3.00% Ni, 0.60-0.90% Cr
0.12-0.18% C, max. 0.40% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S
0.12-0.18% C, max. 0.40% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S
0.13% C, 0.24% Si, 0.47% Mn, 3.06% Ni, 0.19% Cr, 0.05% Mo
0.13% C, 0.25% Si, 0.84% Mn, 0.058% Si, 0.028% Mn, 0.09% Ni, 0.04% Cr, 0.05% Mo
0.13% C, 0.31% Si, 0.51% Mn, 0.023% P, 0.009% S, 0.010% Al, 1.50% Cr, 0.06% Mo, 1.55% Ni, <0.01% V
0.13% C, 0.31% Si, 0.51% Mn, 0.023% P, 0.009% S, 1.50% Cr, 0.06% Mo, 1.55% Ni, 0.010% V, 0.010% Al
0.13% C, 0.46% Si, 1.03% Mn, 0.79% Cr, 0.79% Ni, 0.40% Mo, 0.19% V
0.13% C, 0.54% Mn 0.20% Si, 3.52% Ni, 1.56% Cr
0.13-0.18% C, <0.40% Si, 0.40-0.70% Mn, <0.035% P, <0.020-0.040% S, 0.60-1.00% Cr, 0.80-1.10% Ni
0.13-0.18% C, <0.40% Si, 0.40-0.70% Mn, <0.035% P, <0.020-0.040% S, 0.60-1.00% Cr, 0.80-1.10% Ni
0.13-0.18% C, 0.15-0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40-0.60% Cr, 0.15-0.25% Mo, 0.35-0.65% Ni
0.13-0.18% C, 0.15-0.40% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 0.80-1.10% Ni
0.13-0.18% C, 0.15-0.40% Si, 0.70-1.00% Mn, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr, 0.80-1.00% Ni
0.13-0.18% C, 0.17-0.37% Si, 1.00-1.30% Mn, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr, max. 0.30% Ni, max. 0.30% Cu, 0.0005-0.0030% B
0.13-0.19% C, 0.10-0.25% Si, 0.70-1.00% Mn, max. 0.035% P, 0.010-0.040% S, 0.60-1.00% Cr, 0.80-1.10% Ni
0.13-0.19% C, 0.15-0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 0.80-1.1% Cr, 0.30-0.40% Mo, 2.70-3.20% Ni
0.13-0.19% C, 0.15-0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr, 2.70-3.20% Ni, 0.30-0.40% Mo
0.13-0.19% C, 0.15-0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.035% S, 2.70-3.20% Ni, 0.80-1.10% Ct, 0.30-0.40% Mo
0.13-0.19% C, 0.15-0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.035% S, 2.70-32.0% Ni, 0.80-1.10% Cr, 0.30-0.40% Mo
0.13-0.19% C, 0.15-0.40% Si, 1.00-1.30% Mn, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr
0.13-0.19% C, 0.20-0.35% Si, 0.30-0.70% Mn, 1.30-1.80% Cr, 3.20-3.80% Ni
0.13-0.19% C, 0.40% Si, 0.70-1.00% Mn, 0.035% P, 0.020-0.040% S, 0.60-1.00% Cr, 0.80-1.10% Ni
0.13-0.19% C, 0.40% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.60-1.00% Cr, 0.80-1.10% Ni
0.13-0.19% C, max. 0.40% Si, 0.70-1.00% Mn, 0.60-1.00% Cr, 0.80-1.10% Ni
0.13-0.19% C, max. 0.40% Si, 0.70-1.00% Mn, 0.60-1.00% Cr, 0.80-1.10% Ni
0.13-0.19% C, max. 0.40% Si, 0.70-1.00% Mn, 0.60-1.00% Cr, 0.80-1.10% Ni
0.13-0.20% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.20-0.30% Mo, max. 0.40% Ni
0.13-0.20% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.20-0.30% Mo, max. 0.40% Ni
0.13-0.22% C, 0.05-0.15% Si, 0.70-1.10% Mn, max. 0.035% P, 0.035-0.050% S, 0.60-1.20% Cr, 0.80-1.40% Ni, 0.05-0.20% Mo
0.13-0.25% C, 0.01-0.15% Si, 0.70-1.10% Mn, max. 0.020% P, 0.035-0.050% S, 0.60-1.20% Cr, 0.80-1.40% Ni, max. 0.20% Mo, max. 0.35% Cu, 0.010-0.015% N
0.14% C, 0.19% Si, 0.46% Mn, 0.009% S, 0.006% P, 3.55% Ni, 1.11% Cr, 0.12% Mo
0.14% C, 0.20% Si, 0.40% Mn, 0.015% P, 0.009% S, 1.12% Cr, 4.43% Ni
0.14% C, 0.20% Si, 0.40% Mn, 0.015% P, 0.009% S, 1.12% Cr, 4.43% Ni
0.14% C, 0.25% Si, 0.55% Mn, 0.75% Cr, 3.50% Ni
0.14% C, 0.25% Si, 0.55% Mn, 0.75% Cr, 3.50% Ni
0.14% C, 0.25% Si, 0.55% Mn, 1.10% Cr, 4.50% Ni
0.14% C, 0.25% Si, 0.60% Mn, 0.80% Cr, 2.70% Ni
0.14% C, 0.30% Si, 0.45% Mn, 0.70% Cr, 3.50% Ni
0.14% C, 0.81% Mn, 1.81% Ni, 0.49% Cr, 0.27% Mo, 0.0030% B. Blue lines: 0.17% C, 0.57% Mn, 1.87% Ni, 0.45% Cr, 0.24% Mo, B-none
0.14-0.17% C, 0.15% Si, 1.20-1.40% Mn, 0.020% P, 0.020-0.030% S, 2.10-2.30% Cr, 0.45-0.55% Mo, 0.45-0.55% Ni, 0.15-0.25% V
0.14-0.17% C, 0.15-0.30% Si, 1.20-1.40% Mn, max. 0.020% P, max. 0.015% S, 2.10-2.30% Cr, 0.45-0.55% Ni, 0.45-0.55% Mo, 0.15-0.25% V
0.14-0.17% C, 0.30% Si, 1.20-1.40% Mn, 0.020% P, 0.002% S, 2.10-2.30% Cr, 0.45-0.55% Mo, 0.45-0.55% Ni, 0.15-0.25% V
0.14-0.17% C, 0.30% Si, 1.20-1.40% Mn, 0.020% P, 0.002% S, 2.10-2.30% Cr, 0.45-0.55% Mo, 0.45-0.55% Ni
0.14-0.17% C, 0.30% Si, 1.20-1.40% Mn, 0.020% P, 0.002% S, 2.10-2.30% Cr, 0.45-0.55% Mo, 0.45-0.55% Ni
0.14-0.18% C, 0.10-0.40% Si, 1.00-1.35% Mn, max. 0.025% P, 0.020-0.040% S, 0.80-1.10% Cr, max. 0.35% Cu, 0.005-0.050% Al
0.14-0.18% C, 0.40% Si, 0.25-0.55% Mn, max. 0.025% P, max. 0.015% S, 1.00-1.40% Cr, max. 0.050% Al, max. 0.30% Cu, 0.20-0.30% Mo
0.14-0.18% C, max. 0.40% Si, 0.25-0.55% Mn, max. 0.025% P, max. 0.015% S, 1.00-1.40% Cr, 0.20-0.30% Mo, 3.80-4.30% Ni, max. 0.30% Cu, max. 0.050% Al
0.14-0.19% C, <0.40% Si, 1.00-1.30% Mn, <0.035% P, <0.035% S, 0.80-1.10% Cr
0.14-0.19% C, 0.10-0.35% Si, 1.00-1.30% Mn, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr, 0.020-9.050% Al
0.14-0.19% C, 0.37% Si, 1.00-1.30% Mn, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr, max. 0.30% Ni, max. 0.30% Cu
0.14-0.19% C, 0.40% Si, 1.00-1.30% Mn, 0.020-0.035% S, 0.80-1.10% Cr
0.14-0.19% C, 0.40% Si, 1.00-1.30% Mn, 0.045% P, 0.045% S, 0.80-1.10% Cr
0.14-0.19% C, 0.40% Si, 1.00-1.30% Mn, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, 0.80-1.10% Cr
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, 0.80-1.10% Cr
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, 0.80-1.10% Cr
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, 0.020-0.040% S, 0.80-1.10% Cr
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, max. 0.015% S, 0.80-1.10% Cr, max. 0.30% Cu, max. 0.050% Al
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, max. 0.015% S, 0.80-1.10% Cr, max. 0.30% Cu, max. 0.050% Al
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, max. 0.035% S, 0.80-1.10% Cr, 0.0008-0.0050% B
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, 0.020-0.040% S, 0.80-1.10% Cr
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, max. 0.015% S, 0.80-1.10% Cr, max. 0.30% Cu, max. 0.050% Al
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, max. 0.015% S, 0.80-1.10% Cr, max. 0.30% Cu, max. 0.050% Al
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, max. 0.035% S, 0.80-1.10% Cr, 0.0008-0.0050% B
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, max. 0.035% S, 0.80-1.10% Cr
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr
0.14-0.20% C, <0.40% Si, 0.40-0.60% Mn, <0.035% P, <0.035% S, 1.40-1.70% Cr, 1.40-1.70% Ni
0.14-0.20% C, <0.40% Si, 0.40-0.60% Mn, <0.035% P, <0.035% S, 1.40-1.70% Cr, 1.40-1.70% Ni
0.14-0.20% C, <0.40% Si, 0.40-0.70% Mn, <0.035% P, <0.035% S, 0.60-0.90% Cr, 3.50-.360% Ni
0.14-0.20% C, <0.40% Si, 0.40-0.70% Mn, <0.035% P, <0.035% S, 0.60-0.90% Cr, 3.50-3.60% Ni
0.14-0.20% C, <0.40% Si, 0.50-0.90% Mn, <0.035% P, <0.035% S, 1.40-1.70% Cr, 1.40-1.70% Ni
0.14-0.20% C, <0.40% Si, 0.50-0.90% Mn, <0.035% P, <0.035% S, 1.40-1.70% Cr, 1.40-1.70% Ni
0.14-0.20% C, <0.40% Si, 0.50-0.90% Mn, <0.035% P, <0.035% S, 1.40-1.70% Cr, 1.40-1.70% Ni
0.14-0.20% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.70-1.00% Cr
0.14-0.20% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.14-0.20% C, 0.10-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.040% S, 0.35-0.65% Cr, 0.15-0.25% Mo, 0.35-0.75% Ni
0.14-0.20% C, 0.10-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.040% S, 0.35-0.65% Cr, 0.15-0.25% Mo, 0.35-0.75% Ni
0.14-0.20% C, 0.15-0.35% Si, 0.30-0.70% Mn, 3.20-3.80% Ni, 0.20-0.30% Mo
0.14-0.20% C, 0.15-0.35% Si, 0.30-0.70% Mn, max. 0.040% P, max. 0.030% S, 0.20% Cr, 3.20-3.80% Ni, max. 0.35% Cu, 0.20-0.30% Mo
0.14-0.20% C, 0.15-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.14-0.20% C, 0.15-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.14-0.20% C, 0.15-0.35% Si, 0.70-1.05% Mn, 0.25-0.55% Cr, 0.25-0.65% Ni, 0.08-0.15% Mo, +B
0.14-0.20% C, 0.15-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.25-0.55% Cr, 0.35% Cu, 0.08-0.15% Mo, 0.0005-0.0030% B
0.14-0.20% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.60% Ni
0.14-0.20% C, 0.20-0.35% Si, 0.30-0.70% Mn, 3.20-3.80% Ni, 0.20-0.30% Mo
0.14-0.20% C, 0.20-0.35% Si, 0.30-0.70% Mn, 4.70-5.30% Ni
0.14-0.20% C, 0.20-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.14-0.20% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.25-0.55% Cr, 0.25-0.65% Ni, 0.08-0.15% Mo, +B
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.70-1.00% Cr
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.70-1.00% Cr
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr, + Pb
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr, + Pb
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.14-0.20% C, max. 0.40% Si, 0.60-0.90% Mn, 0.80-1.10% Cr, 1.20-1.50% Ni, 0.15-0.25% Mo
0.14-0.20% C, max. 0.40% Si, 0.60-0.90% Mn, 0.80-1.10% Cr, 1.20-1.50% Ni, 0.15-0.25% Mo
0.14-0.20% C, max. 0.40% Si, 0.60-0.90% Mn, 0.80-1.10% Cr, 1.20-1.50% Ni, 0.15-0.25% Mo
0.14-0.20% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.035% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.14-0.20% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.035% Si, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.14-0.20% C, max. 0.40% Si, max. 0.60% Si, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.15% C, <0.40% Si, 0.45% Mn
0.15% C, 0.15% Si, 0.90% Mn, 1.35% Cr, 0.25% V, 0.90% Mo
0.15% C, 0.15-0.50% Si, max. 1.70% Mn, max. 0.035% P, max. 0.035% S, max. 0.009% N
0.15% C, 0.23% Si, 0.42% Mn, 0.15% Cr, 5.05% Ni, 0.23% Mo. Heat B: 0.17% C, 0.29% Si, 0.51% Mn, 0.17% Cr, 4.85% Ni, 0.24% Mo
0.15% C, 0.23% Si, 1.47% Mn, 0.006% P, 0.020% S, 0.04% V, 0.020% Ti, 0.002% B, 0.030% Al
0.15% C, 0.25% Si, 0.40% Mn, max. 0.030% S, +Pb. Cm15: 0.15% C, 0.25% Si, 0.40% Mn, 0.020-0.035% S, +Pb
0.15% C, 0.25% Si, 0.50% Mn, 0.60% Cr, + Pb
0.15% C, 0.25% Si, 0.50% Mn, 0.60% Cr, +Pb
0.15% C, 0.25% Si, 0.50% Mn, 0.60% Cr
0.15% C, 0.25% Si, 0.50% Mn, 1.55% Cr, 1.55% Mo
0.15% C, 0.25% Si, 0.50% Mn, 1.55% Cr, 1.55% Mo
0.15% C, 0.25% Si, 0.50% Mn, 1.55% Cr, 1.55% Ni, + Pb
0.15% C, 0.25% Si, 0.50% Mn, 1.55% Cr, 1.55% Ni
0.15% C, 0.25% Si, 0.60% Mn, 0.90% Cr, 0.50% Mo
0.15% C, 0.25% Si, 0.60% Mn, 0.90% Cr, 0.50% Mo
0.15% C, 0.25% Si, 0.90% Mn, 0.80% Cr, 0.10% Mo, 1.20% Ni
0.15% C, 0.26% Si, 0.92% Mn, 0.50% Cr, 0.88% Ni, 0.46% Mo, 0.06% V, 0.32% Cu, 0.003% B
0.15% C, 0.35% Si, 0.30-0.80% Mn, max. 0.020% P, max. 0.010% S, 4.75-5.25% Ni, max. 0.05% V
0.15% C, 0.50% Mn, 0.59% Si, 0.97% Ni, 0.75% Mo
0.15% C, 0.51% Mn, 0.58% Si, 1.00% Ni, 0.99% Mo
0.15% C, 0.63% Mn, 1.90% Ni, 0.24% Mo
0.15% C, 1.00-2.00% Si, 2.00% Mn, max. 0.045% P, max. 0.015% S, 15.00-17.00% Cr, 33.00-37.00% Ni, 0.110% N
0.15-0.18% C, 0.15-0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.005% S, 1.30-1.60% Cr, 3.25-3.75% Ni, 0.15-0.25% Mo. Steel 255Q: 0.15-0.18% C, 0.15-0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.005% S, 1.30-1.60% Cr, 3.25-3.75% Ni, 0.15-0.25% Mo
0.15-0.20% C, <0.40% Si, 0.40-0.60% Mn, <0.035% P, <0.035% S, 1.50-1.80% Cr, 1.40-1.70% Ni, 0.25-0.35% Mo
0.15-0.20% C, 0.10-0.35% Si, 0.40-0.60% Mn, max. 0.040% P, max. 0.040% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.15-0.20% C, 0.10-0.35% Si, 0.40-0.60% Mn, max. 0.040% P, max. 0.040% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.15-0.20% C, 0.10-0.35% Si, 0.40-0.60% Mn, max. 0.040% P, max. 0.040% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.15-0.20% C, 0.10-0.40% Si, 0.40-0.70% Mn, max. 0.030% P, max. 0.030% S, 1.40-1.70% Cr, 1.40-1.70% Ni, 0.15-0.35% Mo
0.15-0.20% C, 0.15-0.40% Si, 0.40-0.60% Mn, <0.035% P, <0.035% S, 1.80-2.10% Cr, 1.80-2.10% Ni
0.15-0.20% C, 0.15-0.40% Si, 0.40-0.60% Mn, <0.035% P, <0.035% S, 1.80-2.10% Cr, 1.80-2.10% Ni
0.15-0.20% C, 0.17-0.37% Si, 1.00-1.30% Mn, max. 0.035% P, max. 0.035% S, 1.00-1.30% Cr, max. 0.30% Ni, max. 0.30% Cu, 0.0005-0.0030% B
0.15-0.20% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, 0.25% Cu, 0.0008-0.0050% B
0.15-0.20% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, 0.25% Cu, 0.0008-0.0050% B
0.15-0.20% C, 0.30% Si, 0.90-1.20% Mn, max. 0.025% P, max. 0.025% S, max. 0.30% Cr, max. 0.25% Cu, 0.0008-0.0050% B
0.15-0.20% C, 0.30% Si, 0.90-1.20% Mn, max. 0.025% P, max. 0.025% S, max. 0.30% Cr, max. 0.25% Cu, 0.0008-0.0050% B
0.15-0.20% C, 0.40% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.50-1.80% Cr, 1.40-1.70% Ni, 0.030% Cu
0.15-0.20% C, max. 0.40% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni, max. 0.30% Cu
0.15-0.21% C, <0.40% Si, 0.50-0.90% Mn, <0.035% P, <0.035% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.15-0.21% C, <0.40% Si, 0.50-0.90% Mn, <0.035% P, <0.035% S, 1.50-1.80% Cr, 1.40-1.70% Ni, 0.25-0.35% Mo
0.15-0.21% C, <0.40% Si, 0.50-0.90% Mn, <0.035% P, <0.035% S, 1.50-1.80% Cr, 1.40-1.70% Ni, 0.25-0.35% Mo
0.15-0.21% C, <0.40% Si, 0.50-0.90% Mn, <0.035% P, <0.035% S, 1.50-1.80% Cr, 1.40-1.70% Ni, 0.25-0.35% Mo
0.15-0.21% C, 0.15-0.35% Si, 0.40-0.80% Mn, 0.40-0.80% Cr, 0.10-0.15% V
0.15-0.21% C, 0.15-0.35% Si, 0.40-0.80% Mn, max. 0.040% P, max. 0.030% S, 0.40-0.80% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.15-0.21% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.30% Mo
0.15-0.21% C, 0.15-0.35% Si, 0.60-0.95% Mn, 0.30-0.60% Cr, 0.85-1.25% Ni, 0.30-0.40% Mo
0.15-0.21% C, 0.15-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.030% S, 0.30-0.60% Cr, 0.85-1.25% Ni, max. 0.35% Cu, 0.30-0.40% Mo
0.15-0.21% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.70-1.00% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni, (0.15-0.30% Pb)
0.15-0.21% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.70-1.00% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.15-0.21% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.70-1.00% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.15-0.21% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.70-1.00% Cr, 1.20-1.50% Ni, 0.15-0.25% Mo
0.15-0.21% C, 0.20-0.35% Si, 0.60-0.95% Mn, 0.30-0.60% Cr, 0.85-1.20% Ni, 0.30-0.40% Mo
0.15-0.21% C, 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.015% S, 1.30-1.60% Cr, 3.25-3.75% Ni, max. 0.30% Cu, max. 0.0020% O, 0.15-0.25% Mo
0.15-0.21% C, 0.40% Si, 0.50-0.90% Mn, 0.035% P, 0.035% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.15-0.21% C, 0.40% Si, 0.50-0.90% Mn, 0.035% P, 0.035% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.15-0.21% C, 0.40% Si, 0.50-0.90% Mn, 0.035% P, 0.035% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.15-0.21% C, 0.40% Si, 0.50-0.90% Mn, 0.035% P, 0.035% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.15-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.25% Mo
0.15-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.25% Mo
0.15-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.25% Mo
0.15-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.25% Mo
0.15-0.21% C, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.15-0.21% C, max. 0.35% Si, 0.50-0.90% Mn, max. 0.025% P, max. 0.025% S, 1.50-1.80% Cr, 1.40-1.47% Ni, 0.25-0.35% Mo
0.15-0.21% C, max. 0.40% Si, 0.50-0.90% Mn, max. 0.025% P, max. 0.035% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.15-0.21% C, max. 0.40% Si, 0.50-0.90% Mn, max. 0.025% P, max. 0.035% S, 1.50-1.80% Cr, 0.25-0.35% Ni, 1.40-1.70% Ni
0.15-0.21% C, max. 0.40% Si, 0.50-0.90% Mn, max. 0.040% P, max. 0.035% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.16% C, 0.18% Si, 0.53% Mn, 0.011% S, 0.022% P, 1.56% Ni, 0.26% Cr, 0.25% Mo
0.16% C, 0.22% Si, 1.12% Mn, 0.030% P, 0.008% S, 0.99% Cr, 0.02% Mo, 0.12% Ni, 0.010% V, 0.015% Al
0.16% C, 0.25% Si, 0.50% Mn, 0.018% P, 0.018% S, 1.62% Cr, 0.27% Mo, 1.48% Ni
0.16% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni, + Pb
0.16% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni
0.16% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni
0.16% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr, + B, Pb
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr, max. 0.035% S, +Pb. 16MnCrS5: 0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr, 0.020-0.035% S, +Pb
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr
0.16% C, 0.25% Si, 1.35% Mn, 0.006% P, 0.012% S, 0.04% V, 0.020% Ti, 0.002% B, 0.025% Al
0.16% C, 0.25% Si, 1.35% Mn, 0.006% P, 0.012% S, 0.04% V, 0.020% Ti, 0.002% B, 0.025% Al
0.16% C, 0.27% Si, 0.47% Mn, 0.012% P, 0.007% S, 1.34% Cr, 0.18% Mo, 3.54% Ni, 0.15% Cu
0.16% C, 0.28% Si, 0.50% Mn, 1.55% Cr, 1.55% Ni
0.16% C, 0.32% Si, 0.48% Mn, 0.015% P, 0.010% S, 1.65% Cr, 0.29% Mo, 1.50% Ni
0.16% C, 0.34% Si, 0.46% Mn, 0.029% P, 0.022% S, 0.69% Cr, 0.15% Mo, 3.50% Ni, 0.035% Al
0.16% C, 0.50% Mn, 0.31% Si, 0.013% P, 0.014% S, 0.03% Al, 1.95% Cr, 0.03% Mo, 2.02% Ni, 0.01% V
0.16% C, 0.50% Mn, 0.31% Si, 0.013% P, 0.014% S, 0.03% Al, 1.95% Cr, 0.03% Mo, 2.02% Ni, 0.01% V
0.16% C, 0.51% Mn, 0.15% Si, 0.12% Ni, 0.15% Cr, 0.51% Mo
0.16% C, 0.52% Mn, 3.36% Si, 0.19% Mo
0.16% C, 0.60% Mn, 1.92% Ni, 0.27% Mo, 0.0017% B. Blue lines: 0.15% C, 0.63% Mn, 1.90% Ni, 0.24% Mo, B-none
0.16% C, 0.78% Mn, 0.50% Cr, 0.18% Mo
0.16% C, 1.11% Mn, 0.21% Si, 0.10% Ni, 1.00% Cr, 0.03% Mo
0.16-0.19% C, <0.40% Si, 1.00-1.30% Mn, <0.035% P, <0.035% S, 0.80-1.10% Cr
0.16-0.19% C, <0.40% Si, 1.00-1.30% Mn, <0.035% P, <0.035% S, 0.80-1.10% Cr
0.16-0.19% C, 0.20-0.40% Si, 0.75-1.00% Mn, max. 0.020% P, 0.020-0.030% S, 1.75-2.00% Cr, max. 0.30% Ni, 0.50-0.60% Mo, max. 0.10% V
0.16-0.20% C, max. 0.30% Si, 0.90-1.20% Mn, max. 0.025% P, max. 0.025% S, 0.0008-0.0050% B, max. 0.25% Cu
0.16-0.20% C, max. 0.30% Si, 0.90-1.20% Mn, max. 0.025% P, max. 0.025% S, 0.0008-0.0050% B, max. 0.25% Cu
0.16-0.21% C, 0.24-0.26% Si, 0.58-0.61% Mn, 0.011-0.015% P, 0.57-0.66% Cr, 0.017-0.027% Al, 1.65-1.68% Ni, 0.21-0.22% Mo, 0.15-0.22% Cu
0.16-0.21% C, 0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 1.20-1.50% Ni
0.16-0.21% C, 0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 1.20-1.50% Ni
0.16-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.50% Cr, 1.20-1.50% Ni
0.16-0.23% C, 0.15-0.35% Si, 1.15-1.55% Mn, max. 0.030% P, max. 0.030% S, 0.35% Cr, 0.25% Ni, 0.30% Cu
0.16-0.23% C, 0.15-0.35% Si, 1.15-1.55% Mn, max. 0.030% P, max. 0.030% S, 0.35-0.70% Cr, 0.25% Ni, 0.30% Cu
0.16-0.23% C, 0.40% Si, 0.50-0.90% Mn, max. 0.035% P, 0.020-0.040% S, 0.60-0.90% Cr, 1.40-1.70% Ni, 0.25-0.35% Mo
0.16-0.23% C, 0.40% Si, 0.50-0.90% Mn, max. 0.035% P, 0.020-0.040% S, 0.60-0.90% Cr, 1.40-1.70% Ni, 0.25-0.35% Mo
0.17% C, <0.40% Si, 0.55% Mn, 0.75% Cr, 3.25% Ni
0.17% C, 0.18% Si, 0.63% Mn, 1.85% Ni, 0.51% Mo
0.17% C, 0.21% Si, 0.50% Mn, 0.54% Cr, 1.06% Ni, 0.55% Mo
0.17% C, 0.22% Si, 0.88% Mn, 0.016% S, 0.019% P, 0.86% Ni, 0.59% Cr, 0.05% Mo
0.17% C, 0.25% Si, 0.50% Mn, 1.65% Cr, 0.30% Mo, 1.55% Ni, + Pb
0.17% C, 0.25% Si, 0.50% Mn, 1.65% Cr, 1.55% Ni, 0.30% Mo
0.17% C, 0.25% Si, 0.50%Mn, 1.65% Cr, 1.55% Ni, 0.30% Mo
0.17% C, 0.27% Si, 0.43% Mn, 1.48% Cr, 0.25% Mo, 3.45% Ni, 0.13% Cu, 0.026% Al
0.17% C, 0.30% Si, 0.59% Mn, 1.12% Cr, 3.18% Ni, 0.13% Mo
0.17% C, 0.47% Mn, 0.27% Si, 0.09% Cr, 0.54% Mo
0.17% C, 0.50% Si, 0.60% Mn, 0.019% P, 0.011% S, 0.62% Cr, 0.11% Ni, 0.39% Mo, 0.003% Ti, 0.14% Al, 0.003% V, 0.004% Nb. Steel L20G: 0.25% C, 0.56% Si, 1.16% Mn, 0.014% P, 0.029% S, 0.07% Cr, 0.08% Ni, 0.05% Mo, 0.03% Ti, 0.05% Al.
0.17% C, 0.51% Mn, 0.31% Si, 1.12% Ni, 0.11% Cr, 1.00% Mo
0.17% C, 0.57% Mn, 1.87% Ni, 0.45% Cr, 0.24% Mo
0.17% C, 0.57% Mn, 1.87% Ni, 0.45% Cr, 0.24% Mo
0.17% C, 0.63% Mn, 0.25% Si, 0.013% S, 0.013% P 2.02% Ni, 0.38% Cr, 0.13% Mo, 0.07% Cu
0.17% C, 0.63% Mn, 0.25% Si, 0.013% S, 0.013% P 2.02% Ni, 0.38% Cr, 0.13% Mo, 0.07% Cu
0.17% C, 0.72% Mn, 0.01% Si, 0.01% Cr, 0.007% Mo
0.17% C, 0.74% Mn, 0.34% Si, 1.40% Ni, 1.06% Cr, 0.01% Mo
0.17% C, 0.81% Mn, 0.29% Si, 0.18% Ni, 0.72% Cr, 0.05% Mo
0.17% C, 0.85% Mn, 1.85% Cr, 0.55% Mo
0.17% C, 0.85% Mn, 1.85% Cr, 0.55% Mo
0.17% C, 0.92% Mn
0.17-0.19% C, 0.20-0.30% Si, 1.15-1.30% Mn, max. 0.015% P, max. 0.010% S, 1.70-1.90% Cr, 1.15-1.30% Ni, 0.42-0.48% Mo
0.17-0.19% C, 0.30-0.40% Si, 1.45-1.60% Mn, <0.030% P, 0.020-0.035% S, 0.20-0.30 Cr, 0.30% Ni, 0.08-0.12% V
0.17-0.20% C, 0.30-0.45% Si, 1.45-1.60% Mn, max. 0.030% P, 0.020-0.035% S, 0.20-0.30% Cr, max. 0.30% Ni, 0.08-0.12% V
0.17-0.21% C, 0.10-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.040% S, 0.35-0.65% Cr, 0.15-0.25% Mo, 0.35-0.75% Ni
0.17-0.22% C, 0.10-0.25% Si, 1.10-1.30% Mn, max. 0.025% P, max. 0.002% S, 1.00-1.20% Cr, 0.10-0.25% Ni, max. 0.08% Mo, 0.050-0.200% Al
0.17-0.22% C, 0.10-0.35% Si, 1.00-1.40% Mn, 1.00-1.30% Cr
0.17-0.22% C, 0.15-0.35% Si, 0.45-0.65% Mn, 0.20-0.30% Mo, 1.65-2.00% Ni. Steel 4640: 0.38-0.43% C, 0.20-0.35% Si, 0.60-0.80% Mn, 0.20-0.30% Mo, 1.65-2.00% Ni
0.17-0.22% C, 0.15-0.35% Si, 0.45-0.65% Mn, max. 0.025% P, max. 0.040% S, 0.20% Cr, 1.65-2.00% Ni, 0.35% Cu, 0.20-0.30% Mo
0.17-0.22% C, 0.15-0.35% Si, 0.45-0.65% Mn, max. 0.025% P, max. 0.040% S, 0.40-0.60% Cr, 1.65-2.00% Ni, 0.35% Cu, 0.20-0.30% Mo
0.17-0.22% C, 0.15-0.35% Si, 0.45-0.65% Mn, max. 0.03% P, max. 0.040% S, 1.65-2.00% Ni, 0.20-0.30% Mo
0.17-0.22% C, 0.15-0.35% Si, 0.45-0.65% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.60% Cr, 1.00-2.00% Ni, 0.20-0.40% Mo
0.17-0.22% C, 0.15-0.35% Si, 0.80-1.10% Mn, max. 0.025% P, max. 0.040% S, 0.20% Cr, max 0.06% Mo
0.17-0.22% C, 0.15-0.35% Si, 0.80-1.10% Mn, max. 0.035% P, max. 0.040% S, 0.20% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo, 0.0005-0.0030% B
0.17-0.22% C, 0.15-0.38% Si, 0.45-0.65% Mn, max. 0.035% P, max. 0.040% S, 0.20-0.30% Mo, 1.65-2.00% Ni
0.17-0.22% C, 0.15-0.40% Si, 1.10-1.40% Mn, max. 0.035% P, max. 0.035% S, 1.00-1.30% Cr
0.17-0.22% C, 0.15-1.35% Si, 0.45-0.65% Mn, max. 0.035% P, max. 0.040% S, 0.40-0.60% Cr, 1.65-2.00% Ni, 0.35% Cu, 0.20-0.30% Mo
0.17-0.22% C, 0.15-1.35% Si, 0.45-0.65% Mn, max. 0.035% P, max. 0.040% S, 0.40-0.60% Cr, 1.65-2.00% Ni, 0.35% Cu, 0.20-0.30% Mo
0.17-0.22% C, 0.20-0.30% Si, 0.55-0.65% Mn, max. 0.015% P, 0.002-0.005% S, 0.50-0.60% Cr, 0.23-0.28% Mo, 1.65-2.00% Ni max. 0.014% V
0.17-0.22% C, 0.20-0.30% Si, 0.55-0.65% Mn, <0.015% P, 0.005% S, 0.50-0.60 Cr, 1.65-2.00% Ni, 0.23-0.28% Mo
0.17-0.22% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 0.80-1.20% Cr, 0.30-0.50% Mo, 3.00-3.50% Ni
0.17-0.22% C, 0.40% Si, 1.00-1.40% Mn, max. 0.035% P, max. 0.020-0.035% S, 1.00-1.30% Cr
0.17-0.22% C, 0.40% Si, 1.10-1.40% Mn, 0.035% P, 0.020-0.040% S, 1.00-1.30% Cr
0.17-0.22% C, 0.40% Si, 1.10-1.40% Mn, 0.035% P, 0.020-0.040% S, 1.00-1.30% Cr
0.17-0.22% C, max. 0.37% Si, 1.00-1.40% Mn, max. 0.035% P, max. 0.035% S, 1.00-1.30% Cr, max. 0.30% Ni, max. 0.30% Cu
0.17-0.22% C, max. 0.40% Si, 1.10-1.40% Mn, 1.00-1.30% Cr
0.17-0.22% C, max. 0.40% Si, 1.10-1.40% Mn, 1.00-1.30% Cr
0.17-0.22% C, max. 0.40% Si, 1.10-1.40% Mn, 1.00-1.30% Cr
0.17-0.22% C, max. 0.40% Si, 1.10-1.40% Mn, max. 0.025% P, max. 0.015% S, 1.00-1.20% Cr, max. 0.30% Cu, 0.050% Al
0.17-0.22% C, max. 0.40% Si, 1.10-1.40% Mn, max. 0.025% P, max. 0.015% S, 1.00-1.20% Cr, max. 0.30% Cu, 0.050% Al
0.17-0.22% C, max. 0.40% Si, 1.10-1.40% Mn, max. 0.025% P, max. 0.035% S, 1.00-1.30% Cr
0.17-0.22% C, max. 0.40% Si, 1.10-1.40% Mn, max. 0.025% P, max. 0.035% S, 1.00-1.30% Cr
0.17-0.23% C, <0.40% Si, 0.65-0.95% Mn, <0.035% P, <0.035% S, 0.35-0.70% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.17-0.23% C, <0.40% Si, 0.65-0.95% Mn, <0.035% P, 0.020-0.040% S, 0.35-0.70% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.17-0.23% C, 0.10-0.35% Si, 0.35-0.75% Mn, max. 0.040% P, max. 0.040% S, 0.20-0.30% Mo, 1.55-2.00% Ni
0.17-0.23% C, 0.10-0.35% Si, 0.35-0.75% Mn, max. 0.040% P, max. 0.040% S, 0.20-0.30% Mo, 1.55-2.00% Ni
0.17-0.23% C, 0.10-0.35% Si, 0.35-0.75% Mn, max. 0.040% P, max. 0.040% S, 0.20-0.30% Mo, 1.55-2.00% Ni
0.17-0.23% C, 0.10-0.35% Si, 0.35-0.75% Mn, max. 0.040% P, max. 0.040% S, 0.60-1.00% Cr
0.17-0.23% C, 0.10-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.040% S, 0.35-0.65% Cr, 0.15-0.25% Mo, 0.35-0.75% Ni
0.17-0.23% C, 0.10-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.040% S, 0.60-1.00% Cr
0.17-0.23% C, 0.10-0.35% Si, 0.70-1.00% Mn, max. 0.030% P, max. 0.030% S, 0.0008% B
0.17-0.23% C, 0.10-0.35% Si, 0.80-1.10% Mn, max. 0.030% P, max. 0.030% S, 0.0008% B
0.17-0.23% C, 0.10-0.35% Si, 1.10-1.40% Mn, max. 0.030% P, max. 0.030% S, 0.0008B
0.17-0.23% C, 0.15-0.35% Si, 0.30-0.50% Mn, max. 0.025% P, max. 0.020% S, 3.00-3.30% Cr, 0.50-0.60% Mo, max. 0.30% Ni, 0.45-0.55% V, max. 0.30% Cu, max. 0.040% Al
0.17-0.23% C, 0.15-0.35% Si, 0.30-0.50% Mn, max. 0.025% P, max. 0.020% S, 3.00-3.30% Cr, 0.50-0.60% Mo, max. 0.30% Ni, 0.45-0.55% V, max. 0.30% Cu, max. 0.040% Al
0.17-0.23% C, 0.15-0.35% Si, 0.35-0.75% Mn, 0.45-0.60% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.35-0.75% Mn, 1.55-2.00% Ni, 0.20-0.30% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.35-0.75% Mn, max. 0.040% P, max. 0.030% S, 0.20% Cr, 1.55-2.00% Ni, 0.35% Cu, 0.20-0.30% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.40-0.70% Mn, 0.35-0.65% Cr, 1.55-2.00% Ni, 0.20-0.30% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.40-0.70% Mn, max. 0.030% P, max. 0.030% S, 0.35-0.65% Cr, 0.30% Cu, 1.55-2.00% Ni, 0.15-0.30% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.40-0.70% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 1.55-2.00% Ni, 0.35% Cu, 0.20-0.30% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.40-0.80% Mn, 3.20-3.80% Ni, 0.20-0.30% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.40-0.80% Mn, max. 0.040% P, max. 0.030% S, 0.20% Cr, 3.20-3.80% Ni, max. 0.35% Cu, 0.20-0.30% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.45-0.75% Mn, 0.30-0.60% Cr, 0.85-1.25% Ni, 0.15-0.25% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.45-0.75% Mn, max. 0.040% P, max. 0.030% S, 0.30-0.60% Cr, 0.85-1.25% Ni, max. 0.35% Cu, 0.30-0.40% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.30% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu
0.17-0.23% C, 0.15-0.35% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.030% S, 0.40-0.70% Ni, 0.40-0.65% Cr, 0.15-0.30% Mo, max. 0.30% Cu
0.17-0.23% C, 0.15-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.20-0.30% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.60-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.35-0.65% Cr, 0.30% Cu, 0.35-0.75% Ni, 0.15-0.30% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35% Cu, 0.20-0.30% Mo, 0.35-0.75% Ni
0.17-0.23% C, 0.15-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.30-0.70% Cr, 0.08-0.15% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.60-1.00% Cr
0.17-0.23% C, 0.15-0.35% Si, 0.60-1.00% Mn, 1.55-2.00% Ni, 0.20-0.30% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.30-0.70% Cr, 0.25% Ni, 0.35% Cu, 0.08-0.15% Mo
0.17-0.23% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.60-1.00% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.17-0.23% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.35-0.65% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.17-0.23% C, 0.17-0.37% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.035% S, 0.35-0.65% Cr, 1.55-2.00% Ni, max. 0.30% Cu, 0.20-0.30% Mo
0.17-0.23% C, 0.17-0.37% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.035% S, 0.60-0.95% Cr, 2.70-3.25% Ni, max. 0.30% Cu
0.17-0.23% C, 0.17-0.37% Si, 0.50-0.80% Mn, 0.70-1.00% Cr
0.17-0.23% C, 0.17-0.37% Si, 0.55-0.85% Mn, max. 0.035% P, max. 0.035% S, 0.70-1.10% Cr, max. 0.30% Ni, max. 0.30% Cu
0.17-0.23% C, 0.17-0.37% Si, 0.55-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.85-1.25% Cr, max. 0.30% Ni, max. 0.30% Cu, 0.15-0.25% Mo
0.17-0.23% C, 0.17-0.37% Si, 0.55-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.85-1.25% Cr, max. 0.30% Ni, max. 0.30% Cu
0.17-0.23% C, 0.17-0.37% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.35-0.65% Cr, 0.35-0.75% Ni, max. 0.20% Cu, 0.15-0.25% Mo
0.17-0.23% C, 0.17-0.37% Si, 0.80-1.10% Mn, 1.00-1.30% Cr, 0.03-0.09% Ti
0.17-0.23% C, 0.17-0.37% Si, 0.80-1.10% Mn, max. 0.035% P, max. 0.035% S, 1.00-1.30% Cr, max. 0.30% Ni, max. 0.30% Cu, 0.030-0.090% Ti
0.17-0.23% C, 0.17-0.37% Si, 0.80-1.20% Mn, max. 0.035% P, max. 0.035% S, 1.00-1.35% Cr, max. 0.30% Ni, max. 0.30% Cu, 0.04-0.10% Ti
0.17-0.23% C, 0.17-0.37% Si, 0.80-1.20% Mn, max. 0.035% P, max. 0.035% S, 1.05-1.40% Cr, max. 0.30% Ni, max. 0.30% Cu, 0.20-0.30% Mo
0.17-0.23% C, 0.17-0.37% Si, 1.05-1.45% Mn, max. 0.035% P, max. 0.035% S, 0.30% Cr, max. 0.30% Ni, max. 0.30% Cu, 0.0005-0.0035% B
0.17-0.23% C, 0.17-0.37% Si, 1.20-1.55% Mn, max. 0.035% P, max. 0.035% S, 0.30% Cr, max. 0.30% Ni, max. 0.30% Cu, 0.0005-0.0035% B
0.17-0.23% C, 0.20-0.35% Si, 0.35-0.75% Mn, 1.55-2.00% Ni, 0.20-0.30% Mo
0.17-0.23% C, 0.20-0.35% Si, 0.40-0.70% Mn, 0.35-0.65% Cr, 1.55-2.00% Ni, 0.20-0.30% Mo
0.17-0.23% C, 0.20-0.35% Si, 0.40-0.80% Mn, 1.55-2.00% Ni, 0.20-0.30% Mo
0.17-0.23% C, 0.20-0.35% Si, 0.40-0.80% Mn, 3.20-3.80% Ni, 0.20-0.30% Mo
0.17-0.23% C, 0.20-0.35% Si, 0.50-0.90% Mn, 0.45-0.85% Cr, 1.00-1.45% Ni
0.17-0.23% C, 0.20-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.20-0.30% Mo
0.17-0.23% C, 0.20-0.35% Si, 0.60-1.00% Mn, 1.55-2.00% Ni, 0.20-0.30% Mo
0.17-0.23% C, 0.20-35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.17-0.23% C, 0.30-0.60% Si, 1.30-1.60% Mn, max. 0.035% P, max. 0.035% S
0.17-0.23% C, 0.30-0.70% Cr, 0.60-1.00% Mn, 0.08-0.15% Mo, 0.15-0.30% Si
0.17-0.23% C, 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, 0.90-1.00% Cr, max. 0.30% Cu, max. 0.050% Al, max. 0.002% O
0.17-0.23% C, 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, 0.90-1.00% Cr, max. 0.30% Cu, max. 0.050% Al, max. 0.002% O
0.17-0.23% C, 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, 0.025-0.040% S, 0.40-0.70% Cr, 0.30-0.40% Mo
0.17-0.23% C, 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, 0.025-0.040% S, 0.40-0.70% Cr, 0.30-0.40% Mo
0.17-0.23% C, 0.40% Si, 0.60-0.95% Mn, max. 0.025% P, max. 0.015% S, 0.35-0.65% Cr, max. 0.40-0.70% Ni, 0.15-0.25% Mo, 0.30% Cu, 0.050% Al, 0.002% O
0.17-0.23% C, 0.40% Si, 0.60-0.95% Mn, max. 0.025% P, max. 0.015% S, 0.35-0.65% Cr, max. 0.40-0.70% Ni, 0.15-0.25% Mo, 0.30% Cu, 0.050% Al, 0.002% O
0.17-0.23% C, 0.40% Si, 0.65-1.10% Mn, max. 0.025% P, max. 0.015% S, 0.40-0.75% Cr, max. 0.30% Cu, 0.050% Al, 0.10-0.20% Mo
0.17-0.23% C, 0.40% Si, 0.65-1.10% Mn, max. 0.025% P, max. 0.015% S, 0.40-0.75% Cr, max. 0.30% Cu, 0.050% Al, 0.002% O
0.17-0.23% C, 0.40% Si, 0.65-1.10% Mn, max. 0.025% P, max. 0.015% S, 0.40-0.75% Cr, max. 0.30% Cu, 0.050% Al, 0.10-0.20% Mo
0.17-0.23% C, 0.40% Si, 1.10-1.40% Mn, max. 0.025% P, max. 0.035% S, 0.0008-0.0050% B
0.17-0.23% C, 0.40% Si, 1.10-1.40% Mn, max. 0.025% P, max. 0.035% S, 0.0008-0.0050% B
0.17-0.23% C, max. 0.25% Si, 0.60-0.90% Mn, max. 0.020% P, max. 0.020% S, 0.35-0.65% Cr, 0.15-0.25% Mo, 0.70-0.90% Ni, max. 0.25% Cu, 0.020-0.050% Al
0.17-0.23% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, 0.90-1.20% Cr, max. 0.30% Cu, max. 0.050% Al, 0.15-0.25% Mo
0.17-0.23% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.035% S, 0.40-0.70% Cr, 0.30-0.40% Mo
0.17-0.23% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, 0.90-1.20% Cr, max. 0.050% Al, max. 0.30% Cu, max. 0.002% O
0.17-0.23% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, 0.90-1.20% Cr, max. 0.30% Cu, max. 0.050% Al, 0.15-0.25% Mo
0.17-0.23% C, max. 0.40% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.040% S, 0.35-0.65% Cr%, 0.35-0.75% Ni, 0.15-0.25% Mo
0.17-0.23% C, max. 0.40% Si, 0.60-1.00% Mn, max. 0.025% P, max. 0.015% S, 0.60-1.00% Cr, max. 0.050% Al, max. 0.30% Cu, max. 0.002% O
0.17-0.23% C, max. 0.40% Si, 0.60-1.60% Mn, max. 0.025% P, max. 0.015% S, 0.60-1.00% Cr, max. 0.30% Cu, 0.050% Al
0.17-0.23% C, max. 0.40% Si, 0.65-0.95% Mn, 0.35-0.70% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.17-0.23% C, max. 0.40% Si, 0.65-0.95% Mn, 0.35-0.70% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.17-0.23% C, max. 0.40% Si, 0.65-0.95% Mn, 0.35-0.70% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.17-0.23% C, max. 0.40% Si, 0.65-0.95% Mn, max. 0.025% P, max. 0.035% S, 0.35-0.75% Cr, 0.15-0.25% Mo, 0.40-0.0% Ni
0.17-0.23% C, max. 0.40% Si, 0.65-0.95% Mn, max. 0.025% P, max. 0.035% Si, 0.35-0.70% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni
0.17-0.23% C, max. 0.40% Si, 0.65-0.95% Mn, max. 0.035% P, max. 0.035% S, 0.35-0.70% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.17-0.23% C, max. 0.40% Si, 0.65-1.10% Mn, max. 0.025% P, max. 0.015% S, 0.40-0.75% Cr, max. 0.30% Cu, max. 0.050% Al
0.17-0.23% C, max. 0.40% Si, 0.70-1.00% Mn, max. 0.025% P, 0.020-0.040% S, 0.30-0.60% Cr, 0.40-0.50% Mo
0.17-0.23% C, max. 0.40% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.035% S, 0.30-0.60% Cr, 0.40-0.50% Mo
0.17-0.23% C, max. 0.40% Si, 1.10-1.40% Mn, max. 0.025% P, max. 0.035% S, 0.0008-0.0050% B
0.17-0.24% C, <0.40% Si, 0.40-0.70% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63%
0.17-0.24% C, <0.40% Si, 0.40-0.70% Mn, <0.045% P, <0.040% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=<0.63
0.17-0.24% C, 0.10-0.35% Si, 1.30-1.80% Mn, max. 0.040% P, max. 0.040% S
0.17-0.24% C, 0.15-0.35% Si, 0.70-1.20% Mn, +B
0.17-0.24% C, 0.15-0.35% Si, 0.70-1.20% Mn, max. 0.030% P, max. 0.050% S, 0.0005-0.0030% B
0.17-0.24% C, 0.17-0.37% Si, 0.30-0.60% Mn, 0.60-0.90% Cr, 2.75-3.15% Ni
0.17-0.24% C, 0.17-0.37% Si, 0.30-0.60% Mn, 0.60-0.90% Cr, 2.75-3.15% Ni
0.17-0.24% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.17-0.24% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.17-0.24% C, max. 0.40% Si, 0.80-1.15% Mn, max. 0.030% P, max. 0.035% S, min. 0.020% Al, 0.0008-0.0050% B
0.17-0.25% C, 0.15-0.35% Si, 1.00-1.50% Cr, max. 0.030% P, max. 0.050% S
0.17-0.25% C, 0.15-0.35% Si, 1.00-1.50% Mn
0.17-0.25% C, 0.30-0.60% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.20-1.50% Cr, 1.00-1.20% Mo, max. 0.60% Ni, 0.25-0.35% V
0.17-0.25% C, 0.30-0.60% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.20-1.50% Cr, 1.00-1.20% Mo, max. 0.60% Ni, 0.25-0.35% V
0.17-0.27% C, 0.20-0.35% Si, 0.45-0.75% Mn, 0.30-0.60% Cr, 0.85-1.25% Ni, 0.15-0.25% Mo
0.17-0.27% C, 0.40% Si, 0.70-1.00% Mn, max. 0.035% P, 0.020-0.035% S, 0.30-0.60% Cr, 0.40-0.50% Mo
0.17-0.33% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.75-1.20% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.17-0.33% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.040% P, max. 0.030% S, 0.80-1.10% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.17-0.35% C, 0.15-0.35% Si, 0.70-1.20% Mn, max. 0.030% P, max. 0.050% S, 0.0005-0.0030% B
0.17-0.38% C, 0.15-0.35% Si, 0.30-0.70% Mn, max. 0.040% P, max. 0.030% S, 0.75-1.20% Cr, 0.25% Ni, 0.35% Cu, 0.15-0.25% Mo
0.17-0.57% C, 0.35% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 0.30% Cu
0.18% C, <0.40% Si, 0.70% Mn, 1.65% Cr, 0.30% Mo, 1.55% Ni
0.18% C, 0.17% Si, 0.76% Mn, 0.54% Cr, 0.75% Mo, 1.76% Ni
0.18% C, 0.24% Si, 0.80% Mn, 0.53% Cr, 0.65% Ni, 0.42% Mo
0.18% C, 0.24% Si, 0.80% Mn, 0.53% Cr, 0.65% Ni, 0.42% Mo
0.18% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni
0.18% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni
0.18% C, 0.25% Si, 0.62% Mn, 0.011% P, 0.017% S, 0.80% Cr, 0.40% Mo
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo, + Pb
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo, +Pb
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo
0.18% C, 0.26% Si, 0.93% Mn, 0.008% S, 0.016% P, 1.34% Ni, 1.11% Cr, 0.11% Mo
0.18% C, 0.28% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni
0.18% C, 0.28% Si, 0.53% Mn, 0.18% Cr, 3.54% Ni, 0.23% Mo
0.18% C, 0.28% Si, 0.83% Mn, 0.42% Cr, 1.09% Ni, 0.37% Mo
0.18% C, 0.29% Si, 0.51% Mn, 3.47% Ni, 0.25% Mo
0.18% C, 0.29% Si, 0.61% Mn, 0.010% P, 0.014% S, 0.50% Cr, 1.79% Ni, 0.23% Mo, 0.09% Cu, 0.021% Al
0.18% C, 0.46% Mn, 0.28% Si, 1.68% Ni, 0.03% Cr, 0.21% Mo
0.18% C, 0.55% Mn, 0.29% Si, 1.02% Mo
0.18% C, 0.79% Mn, 0.52% Ni, 0.56% Cr, 0.19% Mo
0.18% C, 0.80% Mn, 0.21% Si, 0.99% Ni, 0.77% Mo
0.18% C, 0.81% Mn, 0.24% Si, 0.54% Cr, 0.43% Mo
0.18% C, 0.83% Mn, 0.49% Ni, 0.49% Cr, 0.19% Mo, 0.0013% B. Blue lines: 0.18% C, 0.79% Mn, 0.52% Ni, 0.56% Cr, 0.19% Mo, B-none
0.18% C, 0.88% Mn, 0.27% Si, 0.98% Mo, 0.004% B
0.18-0.21% C, max. 0.10% Si, 0.22-0.30% Mn, max. 0.025% P, max. 0.002% S, 0.35-0.40% Cr, 0.67-0.70% Mo, 2.25-2.35% Ni, max. 0.10% V
0.18-0.22% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.035% P, 0.020-0.035% S, 0.40-0.50% Cr, 0.40-0.50% Mo, max. 0.20% Ni max. 0.10% V
0.18-0.22% C, 0.15-1.35% Si, 0.50-0.70% Mn, max. 0.035% P, max. 0.040% S, 0.30% Cr, 3.25-3.75% Ni, 0.35% Cu, 0.20-0.30% Mo
0.18-0.22% C, max. 0.30% Si, 0.30-0.60% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Cu
0.18-0.23% C, 0.15-0.35% Si, 0.50-0.70% Mn, max. 0.025% P, max. 0.040% S, 0.20% Cr, 3.25-3.75% Ni, max. 0.35% Cu, 0.20-0.30% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.70-0.90% Mn, 0.40-0.60% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni, 0.35% Cu. Steel 8630: 0.28-0.23% C, 0.15-0.35% Si, 0.70-0.90% Mn, 0.40-0.60% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni, 0.35% Cu. Steel 8640: 0.38-0.43% C, 0.15-0.35% Si, 0.75-1.00% Mn, 0.40-0.60% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni, 0.35% Cu.
0.18-0.23% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.025% P, max. 0.030% S, 0.40-0.60% Cr, 0.35% Cu, 0.20-0.30% Mo, 0.40-0.70% Ni
0.18-0.23% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.025% P, max. 0.040% S, 0.40-0.60% Cr, 0.25% Ni, 0.35% Cu, 0.08-0.15% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.025% P, max. 0.040% S, 0.40-0.60% Cr, 0.40-0.70% Ni, 0.35% Cu, 0.15-0.25% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.40-0.60% Cr, 0.25% Ni, 0.35% Cu, 0.08-0.15% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.60% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.40-0.60% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.40-0.60% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.90-1.10% Mn, max. 0.035% P, max. 0.035% S, 0.10-0.30% Cr, 0.0010-0.0060% B
0.18-0.23% C, 0.15-0.35% Si, 0.90-1.20% Mn, max. 0.025% P, max. 0.040% S, 0.40-0.60% Cr, 0.25% Ni, 0.35% Cu, 0.13-0.20% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.90-1.20% Mn, max. 0.035% P, max. 0.040% S, 0.40-0.60% Cr, 0.25% Ni, 0.35% Cu, 0.13-0.20% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.90-1.20% Mn, max. 0.035% P, max. 0.035% S, 1.10-1.40% Cr, 0.20-0.30% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.90-1.20% Mn, max. 0.040% P, max. 0.030% S, 0.40-0.60% Cr, 0.25% Ni, 0.35% Cu, 0.13-0.25% Mo
0.18-0.23% C, 0.15-0.38% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.40-0.60% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni
0.18-0.23% C, 0.15-0.40% Si, 0.80-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10% Mo, 0.90-1.20% Ni
0.18-0.23% C, 0.15-0.40% Si, 0.80-1.10% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.90-1.20% Ni
0.18-0.23% C, 0.15-1.35% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.40-0.60% Cr, 0.40-0.70% Ni, 0.35% Cu, 0.15-0.25% Mo
0.18-0.23% C, 0.15-1.35% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.40-0.60% Cr, 0.40-0.70% Ni, 0.35% Cu, 0.20-0.30% Mo
0.18-0.23% C, 0.30-0.60% Mn. Steel 1040: 0.37-0.44% C, 0.60-0.90% Mn
0.18-0.23% C, 0.40% Si, 0.90-1.20% Mn, max. 0.035% P, 0.020-0.035% S, 1.10-1.40% Cr, 0.20-0.30% Mo
0.18-0.23% C, 0.90-1.20% Mn, 0.15-0.35% Si, 0.40-0.60% Cr, 0.13-0.20% Mo
0.18-0.24% C, 0.15-0.35% Si, 1.10-1.40% Mn, max. 0.030% P, max. 0.030% S, 1.00-1.30% Cr
0.18-0.24% C, 0.15-0.35% Si, 1.10-1.40% Mn, max. 0.030% P, max. 0.030% S, 1.00-1.30% Cr
0.18-0.24% C, 0.17-0.37% Si, 0.70-1.00% Mn, 0.75-1.05% Cr
0.18-0.24% C, 0.17-0.37% Si, 0.70-1.00% Mn, 0.75-1.05% Cr
0.18-0.26% C, 0.15-0.35% Si, 1.25-1.75% Mn, max. 0.030% P, max. 0.030% S
0.18-0.26% C, 0.15-0.35% Si, 1.25-1.75% Mn
0.18-0.28% C, <0.40% Si, 0.50-0.70% Mn, <0.035% P, 0.020-0.040% S, 0.65-0.85% Cr, 1.50-1.90% Ni, 0.25-0.40% Mo
0.19% C, 0.14% Si, 1.37% Mn, 0.012% S, 0.026% P, 0.56% Ni, 0.20% Cr, 0.31% Mo
0.19% C, 0.17% Si, 0.54% Mn, 0.99% Cr, 0.17% V
0.19% C, 0.21% Si, 0.90% Mn, 0.015% S, 0.017% P, 1.87% Ni, 1.08% Cr, 0.18% Mo
0.19% C, 0.24% Si, 0.85% Mn, 0.88% Cr, 0.11% V
0.19% C, 0.27% Si, 0.56% Mn, 0.21% Cr, 1.72% Ni, 0.23% Mo
0.19% C, 0.28% Si, 0.75% Mn, 0.56% Cr, 0.60% Ni, 0.21% Mo
0.19% C, 0.29% Si, 0.58% Mn, 0.48% Cr, 1.82% Ni, 0.25% Mo
0.19% C, 0.32% Si, 0.60% Mn, 0.013% P, 0.019% S, 0.20% Cr, 1.75% Ni, 0.22% Mo, 0.05% Cu
0.19% C, 0.41% Si, 0.80% Mn, 0.021% P, 0.005% S, 0.57% Cr, 0.81% Ni, 0.50% Mo, 0.06% V, 0.11% Ti, 0.0011% Nb, 0.002% B, 0.30% Cu, 0.014% Al, 0.014% N
0.19% C, 0.48% Mn, 0.28% Si, 0.97% Mo
0.19% C, 0.48% Mn, 0.97% Mo
0.19% C, 0.50% Mn, 0.26% Si, 0.17% Ni, 0.10% Cr, 0.40% Mo
0.19% C, 0.52% Mn, 0.23% Si, 0.12% Ni, 0.20% Cr, 0.51% Mo
0.19% C, 0.52% Mn, 0.23% Si, 0.12% Ni, 0.20% Cr, 0.51% Mo
0.19% C, 0.52% Mn, 0.23% Si, 0.12% Ni, 0.20% Cr, 0.51% Mo
0.19% C, 0.52% Mn, 0.26% Si, 1.06% Ni, 0.76% Mo
0.19% C, 0.87% Mn, 0.30% Si, 0.55% Mo, 0.004% B
0.19-0.23% C, 0.20-0.35% Si, 0.70-0.90% Mn, max. 0.015% P, 0.008-0.015% S, 0.40-0.60% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.19-0.24% C, <0.40% Si, 0.70-1.00% Mn, <0.035% P, 0.020-0.040% S, 0.70-1.00% Cr, 0.40-0.50% Mo
0.19-0.24% C, <0.40% Si, 0.70-1.00% Mn, 0.70-1.00% Cr, 0.40-0.50% Mo, <0.035% P, 0.020-0.040% S
0.19-0.24% C, 0.40% Si, 0.70-1.00% Mn, max. 0.035% P, 0.020-0.040% S, 0.70-1.00% Cr, 0.40-0.50% Mo
0.19-0.24% C, 0.40% Si, 0.70-1.00% Mn, max. 0.035% P, 0.020-0.040% S, 0.70-1.00% Cr, 0.40-0.50% Mo
0.19-0.25% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu, 0.35-0.45% Mo
0.19-0.25% C, 0.15-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.19-0.25% C, 0.15-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.19-0.25% C, 0.15-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.30-0.40% Mo
0.19-0.25% C, 0.15-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35% Cu, 0.30-0.40% Mo, 0.35-0.75% Ni
0.19-0.25% C, 0.17-0.37% Si, 0.55-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.85-1.25% Cr, max. 0.30% Ni, max. 0.30% Cu, 0.35-0.45% Mo
0.19-0.25% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.30-0.40% Mo
0.19-0.25% C, 0.20-35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.19-0.26% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, max. 0.60% Ni, 0.40-0.50% Mo
0.20% C, <0.40% Si, 0.85% Mn, 0.45% Cr, 0.45% Mo
0.20% C, 0.10% Si, 0.30% Mn, 3 ppm S, 5.10% Cr, 0.70% Mo, 6.10% Ni, 0.50% V, 2.4 ppm Al, 3 ppm O, 28 ppm N
0.20% C, 0.15% Si, 0.71% Mn, 0.018% S, 0.032% P, 1.13% Ni, 0.80% Cr, 0.05% Mo
0.20% C, 0.20% Si, 0.50% Mn, 0.00% Cr, <0.025% P, <0.025% S, <0.25% Cu
0.20% C, 0.20% Si, 0.90% Mn
0.20% C, 0.23% Si, 0.61% Mn, 0.011% S, 0.015% P, 2.0% Ni, 1.65% Cr, 0.19% Mo
0.20% C, 0.23% Si, 1.14% Mn, 0.013% P, 0.009% S, 0.030% Al, 0.0021% O.0047% N, 0.0030% B
0.20% C, 0.25% Si, 0.40% Mn, 3.15% Cr, 0.50% V, 0.55% Mo
0.20% C, 0.25% Si, 0.40% Mn, 3.15% Cr, 0.50% V, 0.55% Mo
0.20% C, 0.25% Si, 0.50% Mn, max. 0.03% S, +Pb. Steel Cm22: 0.20% C, 0.25% Si, 0.50% Mn, 0.020-0.025% S, +Pb
0.20% C, 0.25% Si, 0.50% Mn
0.20% C, 0.25% Si, 0.50% Mn
0.20% C, 0.25% Si, 0.70% Mn, 0.60% Cr, 0.35% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo, 0.020-0.035% S, + Pb
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo, max. 0.035% S, +Pb. 20MoCrS4: 0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo, 0.020-0.035% S, +Pb
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.80% Mn, 0.50% Cr, 1.70% Ni, 0.45% Mo
0.20% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni
0.20% C, 0.25% Si, 0.83% Mn, 0.70% Cr, 0.08% Ni, 0.03% Mo, 0.13% V
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr, max. 0.035% S, +Pb. 20MnCrS5: 0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr, 0.020-0.035% S, +Pb
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
0.20% C, 0.25% Si, 1.33% Mn, 0.005% P, 0.018% S, 0.07% V, 0.020% Ti, 0.002% B, 0.030% Al
0.20% C, 0.29% Si, 0.60% Mn, 0.009% P, 0.021% S, 0.52% Cr, 0.26% Mo, 1.67% Ni, 0.09% Cu
0.20% C, 0.29% Si, 0.60% Mn, 0.009% P, 0.021% S, 0.52% Cr, 0.26% Mo, 1.67% Ni, 0.09% Cu
0.20% C, 0.29% Si, 0.60% Mn, 0.009% P, 0.021% S, 0.52% Cr, 0.26% Mo, 1.67% Ni, 0.09% Cu
0.20% C, 0.29% Si, 0.64% Mn, 0.21% Cr, 1.93% Ni, 0.31% Mo
0.20% C, 0.29% Si, 0.82% Mn, 0.58% Cr, 0.43% Ni, 0.18% Mo
0.20% C, 0.30% Si, 0.72% Mn, 0.010% P, 0.010% S, 0.79% Cr, 0.02% Mo, 0.27% Ni, 0.02% Cu
0.20% C, 0.30% Si, 0.72% Mn, 0.010% P, 0.010% S, 0.79% Cr, 0.02% Mo, 0.27% Ni, 0.02% Cu
0.20% C, 0.30% Si, 0.72% Mn, 0.010% S, 0.010% P, 0.27% Ni, 0.59% Cr, 0.02% Mo
0.20% C, 0.30% Si, 0.85% Mn, 0.010% P, 0.014% S, 0.50% Cr, 0.51% Ni, 0.19% Mo, 0.09% Cu, 0.031% Al
0.20% C, 0.55% Mn, 0.051% S*, 0.37% Si, 0.035% Ni, 0.07% Cr, 0.59% Mo, *-off-analysis
0.20% C, 0.59% Mn, 0.25% Si, 0.01% Ni, 0.05% Cr, 0.50% Mo
0.20% C, 0.72% Mn, 0.33% Si, 0.15% Ni, 0.12% Cr, 0.48% Mo
0.20% C, 0.80% Mn, 0.25% Si, 0.76% Mo
0.20% C, 0.83% Mn, 0.25% Si, 0.08% Ni, 0.70% Cr, 0.03% Mo, 0.13% V
0.20% C, 0.83% Mn, 0.56% Cr, 0.15% Mo
0.20% C, 0.86% Mn, 0.24% Si, 0.07% Ni, 1.11% Cr, 0.23% Mo
0.20% C, 0.90-1.25% Mn, 0.85-1.20% Si, 1.50-1.80% Cu
0.20% C, 1.50-2.50% Si, 2.00% Mn, max. 0.045% P, max. 0.015% S, 24.00-26.00% Cr, 19.00-22.00% Ni, 0.110% N
0.20% C, 1.88% Mn
0.20-0.24% C, 0.30% Si, 0.90-1.20% Mn, max. 0.025% P, max. 0.025% S, 0.00-0.00% Cr, 0.25% Cu, 0.0008-0.0050% B
0.20-0.24% C, 0.30% Si, 0.90-1.20% Mn, max. 0.025% P, max. 0.025% S, 0.00-0.00% Cr, 0.25% Cu, 0.0008-0.0050% B
0.20-0.25% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.10-0.20% Mo, 0.0008-0.0050% B
0.20-0.25% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.025% P, max. 0.040% S, 0.40-0.60% Cr, 0.40-0.70% Ni, 0.35% Cu, 0.15-0.25% Mo
0.20-0.25% C, 0.15-0.35% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.040% S, 0.40-0.60% Cr, 0.35% Cu, 0.30-0.40% Mo, 0.40-0.70% Ni
0.20-0.25% C, 0.15-1.35% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.40-0.60% Cr, 0.40-0.70% Ni, 0.35% Cu, 0.15-0.25% Mo
0.20-0.25% C, 0.15-1.35% Si, 0.75-1.00% Mn, max. 0.035% P, max. 0.040% S, 0.40-0.60% Cr, 0.40-0.70% Ni, 0.35% Cu, 0.30-0.40% Mo
0.20-0.25% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, max. 0.25% Cu, 0.0008-0.0050% B
0.20-0.25% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, max. 0.25% Cu, 0.0008-0.0050% B
0.20-0.25% C, 0.30% Si, 0.90-1.20% Mn, 0.025% P, 0.025% S, 0.30% Cr, 0.0008-0.0050% B, 0.25% Cu
0.20-0.25% C, 0.30% Si, 0.90-1.20% Mn, 0.025% P, 0.025% S, 0.30% Cr, 0.0008-0.0050% B, 0.25% Cu
0.20-0.25% C, max. 0.30% Si, max. 0.025% P, max. 0.025% S, max. 0.30% Cr, max. 0.25% Cu, 0.0008-0.005% B
0.20-0.26% C, <0.25% Si, 1.00-1.40% Mn, <0.020% P, <0.020% S, <0.012% N, 0.40-0.60% Cr, <0.25% Cu, 0.20-0.30% Mo, 0.40-0.70% Ni
0.20-0.26% C, <0.25% Si, 1.00-1.40% Mn, <0.020% P, <0.020% S, <0.012% N, 0.40-0.60% Cr, <0.25% Cu, 0.20-0.30% Mo, 0.40-0.70% Ni
0.20-0.26% C, 0.10-0.35% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.030% S, 0.0008% B
0.20-0.26% C, 0.10-0.35% Si, 0.70-1.00% Mn, max. 0.030% P, max. 0.030% S, 0.0008% B
0.20-0.26% C, 0.10-0.35% Si, 1.10-1.40% Mn, max. 0.030% P, max. 0.030% S, 0.0008% B
0.20-0.26% C, max. 0.25% Si, 1.10-1.40% Mn, max. 0.020% P, max. 0.020% S, 0.40-0.60% Cr, 0.20-0.30% Mo, 0.70-0.90% Ni, max. 0.25% Cu, 0.020-0.050% Al
0.20-0.26% C, max. 0.25% Si, 1.10-1.40% Mn, max. 0.020% P, max. 0.020% S, 0.40-0.60% Cr, 0.50-0.60% Mo, 0.90-1.10% Ni, max. 0.25% Cu, 0.020-0.050% Al
0.20-0.28% C, 0.15-0.35% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.20-1.50% Cr, 0.50-0.60% Mo, max. 0.60% Ni, 0.15-0.25% V
0.20-0.28% C, 0.15-0.35% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.20-1.50% Cr, 0.50-0.60% Mo, max. 0.60% Ni, 0.15-0.25% V
0.20-0.28% C, max. 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.20-0.30% Mo, max. 0.60% Ni
0.20-0.35% C, 0.15-0.35% Si, 0.50-0.80% Mn, 0.030% P, 0.035% S, 0.90-1.20% Cr, 0.20-0.35% Mo
0.20-0.60% C, 1.50-2.00% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.30% Cr, 0.25% Ni, 0.20% Cu
0.21% C, <0.40% Si, 1.05% Mn, 1.25% Cr, 0.25% Mo
0.21% C, 0.21% Si, 0.76% Mn, 0.010% P, 0.030% S, 0.45% Cr, 0.56% Ni, 0.08% Mo, 0.08% V
0.21% C, 0.24% Si, 0.70% Mn, 0.001% P, 0.010% S, 0.63% Cr, 0.03% Ni, 0.03% Mo, 0.01% V, 0.058% Ti, 0.001% B, 0.03% Cu, 0.051% Al, 0.007% N
0.21% C, 0.25% Si, 0.75% Mn, 0.50% Cr, 0.20% Mo, 0.55% Ni, + Pb
0.21% C, 0.25% Si, 0.75% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.21% C, 0.25% Si, 0.75% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.21% C, 0.25% Si, 0.80% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.21% C, 0.25% Si, 1.05% Mn, 1.25% Cr, 0.25% Mo
0.21% C, 0.26% Si, 0.81% Mn, 0.026% P, 0.018% S, 0.59% Cr, 0.17% Mo, 0.53% Ni
0.21% C, 0.26% Si, 0.81% Mn, 0.026% P, 0.018% S, 0.59% Cr, 0.17% Mo, 0.53% Ni
0.21% C, 0.26% Si, 0.81% Mn, 0.026% P, 0.018% S, 0.59% Cr, 0.17% Mo, 0.53% Ni
0.21% C, 0.26% Si, 0.81% Mn, 0.026% P, 0.018% S, 0.59% Cr, 0.17% Mo, 0.53% Ni
0.21% C, 0.31% Si, 0.55% Mn, 0.22% Cr, 1.64% Ni, 0.25% Mo
0.21% C, 0.33% Si, 0.58% Mn, 0.21% Cr, 1.66% Ni, 0.22% Mo
0.21% C, 0.35% Si, 0.40% Mn, 1.35% Cr, 1.10% Mo, 0.30% V
0.21% C, 0.35% Si, 0.40% Mn, 1.35% Cr, 0.30% V, 1.10% Mo
0.21% C, 0.35% Si, 0.40% Mn, 1.35% Cr, 1.10% Mo, 0.30% V
0.21% C, 0.35% Si, 0.83% Mn, 0.97% Cr, 0.24% Mo
0.21% C, 0.47% Si, 0.63% Mn, 0.52%Cr, 0.55% Mo, 1.62% Ni, 0.18% V, 0.10% Nb, 0.04% Al
0.21% C, 0.62% Mn, 0.31% Si, 0.08% Ni, 0.17% Cr, 0.53% Mo
0.21% C, 0.93% Mn, 0.26% Si, 0.08% Cr, 0.88% Mo
0.21% C, 2.04% Mn, 0.0015% B. Blue lines: 0.20% C, 1.88% Mn, B-none
0.21-0.23% C, 0.20-0.35% Si, 0.65-0.75% Mn, max. 0.020% P, 0.015-0.025% S, 1.25-1.35% Cr, 2.85-3.05% Ni, 0.22-0.26% Mo
0.21-0.30% C, 0.15-0.35% Si, 1.00-1.50% Mn, max. 0.030% P, max. 0.030% S
0.21-0.30% C, 0.15-0.35% Si, 1.00-1.50% Mn
0.22% C, 0.21% Si, 0.77% Mn, 0.010% P, 0.030% S, 0.46% Cr, 0.57% Ni, 0.08% Mo, 0.11% V
0.22% C, 0.22% Si, 1.24% Mn, 0.001% P, 0.013% S, 0.12% V, 0.02% Mo
0.22% C, 0.23% Si, 0.84% Mn, 0.009% P, 0.021% S, 0.51% Cr, 0.57% Ni, 0.19% Mo, 0.20% Cu
0.22% C, 0.24% Si, 0.40% Mn, 0.03% S, 0.02% P, 0.11% Ni, 0.73% Cr, 0.40% Mo, 0.13% Cu, 0.02% W, 0.02% Co, 0.01% Nb
0.22% C, 0.25% Si, 0.40% Mn, 1.45% Cr, 3.65% Ni, 0.40% Mo
0.22% C, 0.25% Si, 0.40% Mn, 1.45% Cr, 3.65% Ni, 0.40% Mo
0.22% C, 0.25% Si, 1.33% Mn, 0.18% Cr, 0.02% Mo, 0.12% Ni, 0.033% Ti, 0.11% Cu, 0.034% Al, 0.090% N
0.22% C, 0.25% Si, 1.33% Mn, 0.18% Cr, 0.02% Mo, 0.12% Ni, 0.033% Ti, 0.11% Cu, 0.034% Al, 0.090% N
0.22% C, 0.26% Si, 0.83% Mn, 0.53% Cr, 0.61% Ni, 0.55% Mo
0.22% C, 0.28% Si, 0.65% Mn, 1.05% Cr, 0.45% Mo, <0.60% Ni
0.22% C, 0.28% Si, 0.70% Mn, 0.07% Cr, 0.25% Mo, 1.97% Ni, 0.010% V, 0.11% Cu
0.22% C, 0.30% Si, 0.80% Mn, 0.53% Cr, 0.59% Ni, 0.76% Mo
0.22% C, 0.36% Si, 0.56% Mn, 1.45 Ni
0.22% C, 0.79% Mn, 0.50% Mo. Blue lines: 0.22% C, 0.79% Mn, 0.50% Mo
0.22% C, 0.79% Mn, 0.50% Mo
0.22% C, 0.80% Mn, 0.22% Si, 0.54% Cr, 0.76% Mo
0.22% C, 0.82% Mn, 0.26% Si, 0.54% Cr, 0.57% Mo
0.22% C, 0.88% Mn, 0.25% Si, 0.04% Ni, 0.48% Cr, 0.12% Mo
0.22% C, 11.50% Cr, 0.60% Ni, 1.00% Mo, 0.30% V
0.22% Co, 0.79% Mn, 0.24% Si, 0.57% Mo
0.22-0.28% C, 0.15-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.22-0.28% C, 0.15-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.22-0.28% C, 0.15-0.35% Si, 1.20-1.40% Mn, max. 0.035% P, max. 0.035% S, 0.10-0.30% Cr, 0.0010-0.0060% B
0.22-0.28% C, 0.20-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.22-0.29% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.22-0.29% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.15-0.30% Mo
0.22-0.29% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.15-0.30% Mo
0.22-0.29% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.15-0.30% Mo
0.22-0.29% C, 0.35% Si, 0.50-0.80% Mn, 0.025% P, 0.020% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.30% Cu
0.22-0.29% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.22-0.29% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.35-0.40% Cr, 0.15-0.30% Mo
0.22-0.31% C, 0.10-0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.85-1.15% Cr, 1.20-1.60% Ni
0.22-0.50% C, <0.40% Si, 0.50-0.80% Mn, <0.045% P, <0.040% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=<0.63
0.23% C, 0.25% Si, 0.80% Mn, 0.80% Cr, 0.35% Mo + B
0.23% C, 0.26% Si, 0.42% Mn, 0.52% Cr, 5.40% Ni, 0.23% Mo, 2.34% Al
0.23% C, 0.27% Si, 0.63% Mn, 0.52% Cr, 1.81% Ni, 0.23% Mo
0.23% C, 0.28% Si, 0.92% Mn, 0.53% Cr, 0.49% Ni, 0.35% Mo
0.23% C, 0.54% Mn, 0.36% Si, 0.046% Ni, 0.08% Cr, 0.50% Mo
0.23% C, 0.55% Mn, 0.23% Si, 0.18% Ni, 0.09% Cr, 0.51% Mo
0.23% C, 0.56% Mn, 0.32% Si, 0.16% Ni, 0.08% Cr, 0.60% Mo
0.23% C, 0.60% Si, 1.15-1.60% Mn, 0.045% P, 0.045% S
0.23-0.26% C, 1.40-1.70% Si, 1.30-1.50% Mn, max. 0.025% P, max. 0.010% S, 0.25-0.40% Cr, 1.65-2.00% Ni, 0.39-0.45% Mo
0.23-0.27% C, 0.80-1.05% Si, 1.00-1.20% Cr, max. 0.025% P, max. 0.015% S, 1.65-1.95% Cr, 0.20-0.35% Ni, 0.15-0.20% Ni
0.23-0.28% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.30% Mo
0.23-0.28% C, 1.30-1.70% Si, 1.20-1.50% Mn, 0.20-0.40% Cr, 0.35-0.40% Mo
0.23-0.29% C, 0.10-0.35% Si, 0.90-1.20% Mn, max. 0.030% P, max. 0.030% S, 0.0008% B
0.23-0.29% C, 0.10-0.35% Si, 1.20-1.50% Mn, max. 0.030% P, max. 0.030% S, 0.0008% B
0.23-0.29% C, 0.15-0.35% Si, 0.40-0.70% Mn, 0.65-1.05% Ni, 0.15-0.35% Mo
0.23-0.29% C, 0.17-0.37% Si, 0.90-1.20% Mn, 0.90-1.20% Cr, 0.20-0.30% Mo
0.23-0.29% C, 0.17-0.37% Si, 0.90-1.20% Mn, 0.90-1.20% Cr, 0.20-0.30% Mo
0.24% C, 0.20% Si, 1.58% Mn, 0.016% P, 0.014% S, 0.24% Cr, 0.02% Mo, 0.20% Ni, 0.12% Cu
0.24% C, 0.20% Si, 1.58% Mn, 0.016% P, 0.014% S, 0.24% Cr, 0.02% Mo, 0.20% Ni, 0.12% Cu
0.24% C, 0.24% Si, 0.57% Mn, 0.012% P, 0.010% S, 1.10% Cr, 0.25% Mo
0.24% C, 0.24% Si, 0.57% Mn, 0.012% P, 0.010% S, 1.10% Cr, 0.25% Mo
0.24% C, 0.25% Si, 0.45% Mn, 1.35% Cr, 0.20% V, 0.55% Mo
0.24% C, 0.25% Si, 0.45% Mn, 1.35% Cr, 0.20% V, 0.55% Mo
0.24% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.24% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.24% C, 0.28% Si, 0.95% Mn, 0.44% Cr, 0.56% Ni, 0.31% Mo
0.24% C, 0.50% Mn, 0.39% Si*, 0.08% Ni, 0.13% Cr, 0.52% Mo, *-off-anlysis
0.24% C, 0.61% Mn, 0.31% Si, 0.06% Ni, 0.12% Cr, 0.51% Mo
0.24% C, 0.94% Mn, 0.47% Si, 0.30% Ni, 0.34% Cr, 0.14% Mo
0.24% C, 1.15% Mn, 0.86% Si, 0.11% Mo
0.24-0.29% C, 0.20-0.35% Si, 0.45-0.65% Mn, 0.70-1.00% Ni, 0.15-0.25% Mo
0.24-0.30% C, 0.15-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.24-0.30% C, 0.15-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.24-0.30% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.20-0.30% Mo
0.24-0.30% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.050% S, 0.20% Cr, 0.25% Ni, 0.35% Cu, 0.20-0.30% Mo
0.24-0.30% C, 0.20-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.24-0.30% C,< 0.40% Si, 1.10-1.40% Mn, <0.035% P, <0.040% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.24-0.30% C,< 0.40% Si, 1.10-1.40% Mn, <0.035% P, <0.040% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.24-0.31% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.025% S, 0.90-1.20% Cr
0.24-0.31% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.025% S, 0.90-1.20% Cr
0.24-0.31% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.025% S, 0.90-1.20% Cr
0.24-0.31% C, 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.24-0.32% C, 0.17-0.37% Si, 0.50-0.80% Mn, 0.80-1.10% Cr
0.24-0.32% C, 0.17-0.37% Si, 0.50-0.80% Mn, 0.80-1.10% Cr
0.24-0.32% C, 0.17-0.37% Si, 0.80-1.10% Mn, 1.00-1.30% Cr, 0.03-0.09% Ti
0.24-0.32% C, 0.17-0.37% Si, 0.80-1.10% Mn, 1.00-1.30% Cr, 0.03-0.09% Ti
0.25% C, 0.15% Si, 0.52% Mn, 0.024% S, 0.010% P, 3.33% Ni, 1.14% Cr, 0.65% Mo, 0.16% V
0.25% C, 0.25% Si, 0.58% Mn, 1.13% Cr, 3.57% Ni, 0.24% Mo, 1.42% Al
0.25% C, 0.25% Si, 0.59% Mn, 1.19% Cr, 3.63% Ni, 0.24% Mo, 0.93% Al
0.25% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.00% Cr, 1.45% Ni, +Pb
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo, +Pb
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.75% Mn, 0.50% Cr, 0.45% Mo
0.25% C, 0.30% Si, 0.70% Mn, 0.50% Cr, 0.50% Mo
0.25% C, 0.78% Mn, 0.24% Si, 0.047% S, 0.14% Ni, 0.14% Cr, 0.22% Mo
0.25% C, 1.50% Si, 1.35% Mn, 0.30% Cr, 0.40% Mo, 1.80% Ni
0.25-0.30% C, 0.15-0.30% Si, 0.20-0.50% Mn, max. 0.020% P, max. 0.010% S, 1.20-1.70% Cr, 0.35-0.55% Mo, 3.30-3.80% Ni, max. 0.080% V, 0.020-0.050% Al
0.25-0.30% C, 0.15-0.30% Si, 0.90-1.20% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, max. 0.25% Cu, 0.0008-0.0050% B
0.25-0.30% C, 0.15-0.30% Si, 0.90-1.20% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, max. 0.25% Cu, 0.0008-0.0050% B
0.25-0.30% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.025% P, max. 0.040% S, 0.20% Cr, 0.25% Ni, 0.35% Cu, 0.20-0.30% Mo
0.25-0.30% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.20% Cr, 0.25% Ni, 0.35% Cu, 0.20-0.30% Mo
0.25-0.30% C, 0.15-0.35% Si, 1.00-1.40% Mn, max. 0.035% P, max. 0.035% S, 0.30-0.60% Cr, max. 0.040% Al, 0.0010-0.0060% B
0.25-0.30% C, 0.15-0.35% Si, 1.10-1.30% Mn, max. 0.025% P, max. 0.015% S, 0.15-0.25% Cr, 0.010-0.040% Al, 0.0010-0.0050% B
0.25-0.30% C, 0.15-0.35% Si, 1.10-1.30% Mn, max. 0.035% P, 0.015-0.035% S, 0.10-0.30% Cr, 0.0010-0.0060% B
0.25-0.31% C, 0.17-0.37% Si, 0.70-1.00% Mn, 0.70-1.0% Cr
0.25-0.31% C, 0.17-0.37% Si, 0.70-1.00% Mn, 0.70-1.00% Cr
0.25-0.32% C, <0.40% Si, 1.30-1.60% Mn, 0.035% S, <0.035% P, < 0.40% Ni, <0.40% Cr, <0.10% Mo, Cr+Mn+Ni=<0.63
0.25-0.32% C, <0.40% Si, 1.30-1.65% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=<0.63
0.25-0.32% C, <0.40% Si, 1.30-1.65% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=<0.63
0.25-0.32% C, <0.40% Si, 1.30-1.65% Mn, <0.035% P, <0.035% S, <0.40%Cr, <0.40% Ni, <0.10% Mo, <0.05% V, Cr+Mo+Ni=<0.63
0.25-0.32% C, max. 0.60% Si, 1.20-1.80% Mn, max. 0.035% P, max. 0.030% S
0.25-0.34% C, 0.15-0.35% Si, 1.00-1.50% Mn, max. 0.030% P, max. 0.050% S, 0.0005-0.0030% B
0.25-0.34% C, 0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.030% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.25-0.34% C, 1.00-1.50% Mn, 0.15-0.35% Si, 0.0005-0.003% B
0.25-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.80-2.20% Cr, 0.30-9.50% Mo, 1.80-2.20% Ni
0.26% C, 0.10% Si, 1.40% Mn, 0.002% S, 1.40% Cr, 0.30% Ni, 0.45% Mo, +B
0.26% C, 0.10-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.020-0.050% Al
0.26% C, 0.15% Si, 0.46% Mn, 0.009% P, 0.014% S, 0.54% Cr, 1.92% Ni, 0.01% Mo, 0.10% V, 0.002% Ti, 0.03% Cu, 0.069% Al, 0.007% N
0.26% C, 0.21% Si, 0.55% Mn, 0.022% S, 0.010% P, 0.25% Ni, 3.34% Cr, 0.54% Mo
0.26% C, 0.22% Si, 0.54% Mn, 0.002% P, 0.018% S, 0.54% Cr, 1.80% Ni, 0.10% Mo, 0.16% V, 0.045% Ti, 0.064% Al, 0.006% N
0.26% C, 0.24% Si, 0.53% Mn, 0.002% P, 0.017% S, 0.56% Cr, 1.87% Ni, 0.01% Mo, 0.27% V, 0.044% Ti, 0.048% Al, 0.014% N
0.26% C, 0.24% Si, 0.60% Mn, 0.007% P, 0.008% S, 1.13% Cr, 0.15% Ni, 0.21% Mo, 0.041% V, 0.16% Cu. Steel 2#: 0.26% C, 0.32% Si, 0.80% Mn, 0.007% P, 0.009% S, 1.07% Cr, 0.16% Ni, 0.22% Mo, 0.040% V, 0.16% Cu
0.26% C, 0.29% Si, 0.86% Mn, 0.011% P, 0.027% S, 0.05% Cr, 0.09% Ni, 0.22% Mo, 0.07% Cu, 0.032% Al
0.26% C, 0.37% Si, 0.61% Mn, 0.70% Cr, 0.08% Ni, 0.02% Mo, 0.12% V
0.26% C, 0.60% Mn, 0.33% Mo, 0.020% Ti, 0.007% N, +B. Steel B: 0.29% C, 1.00% Mn, 0.45% Mo, 0.010% Ti, 0.012% N
0.26% C, 0.61% Mn, 0.37% Si, 0.08% Ni, 0.70% Cr, 0.02% Mo, 0.12% V
0.26% C, 0.87% Mn, 0.26% Mo
0.26% C, 0.87% Mn, 0.26% Mo
0.26-0.33% C, 0.15-0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.33% C, 0.17-0.37% Si, 0.40-0.70% Mn, 0.80-1.10% Cr, 0.15-0.25% Mo
0.26-0.33% C, 0.17-0.37% Si, 0.40-0.70% Mn, 0.80-1.10% Cr, 0.15-0.25% Mo
0.26-0.33% C, 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 1.20-1.50% Cr, 3.30-4.30% Ni, 0.30-0.60% Mo
0.26-0.33% C, 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 1.20-1.50% Cr, 3.30-4.30% Ni, 0.40-0.60% Mo
0.26-0.33% C, 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 1.20-1.50% Cr, 3.30-4.30% Ni, 0.40-0.60% Mo
0.26-0.34% C, <0.40% Si, 0.30-0.60% Mn, <0.035% P, <0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, <0.40% Si, 0.30-0.60% Mn, <0.035% P, <0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo
0.26-0.34% C, <0.40% Si, 0.30-0.60% Mn, <0.035% P, <0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, <0.40% Si, 0.40-0.70% Mn, <0.035% P, <0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, <0.60% Ni, 0.10-0.20% V
0.26-0.34% C, <0.40% Si, 0.40-0.70% Mn, <0.035% P, <0.030% S, 2.30-2.70%Cr, 0.15-0.25% Mo, <0.60% Ni, 0.10-0.20% V
0.26-0.34% C, <0.40% Si, 0.40-0.70% Mn, <0.035% P, <0.030% S, 2.30-2.70%Cr, 0.15-0.25% Mo, <0.60% Ni, 0.10-0.20% V
0.26-0.34% C, 0.15-0.35% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.80-2.10% Cr, 1.80-2.10% Ni, 0.25-0.35% Mo
0.26-0.34% C, 0.15-0.40% Si, 0.30-0.60% Mn, max. 0.025% P, max. 0.025% S, 1.80-2.30% Cr, 0.30-0.65% Mo, 1.80-2.30% Ni
0.26-0.34% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.80-2.20% Cr, 1.80-2.20% Ni, 0.15-0.30% Mo
0.26-0.34% C, 0.40% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.030% S, 1.80-2.20% Cr, 1.80-2.20% Ni, 0.30-0.50% Mo
0.26-0.34% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, max. 0.60% Ni, 0.10-0.20% V
0.26-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.80-1.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.35% C, 0.15-0.35% Si, 0.30-0.70% Mn, max. 0.030% P, max. 0.030% S, 0.55-1.05% Cr, 0.30% Cu, 2.45-3.00% Ni
0.27% C, 0.10% Si, 0.76% Mn, 0.013% P, 0.008% S, 0.23% Cr, 0.05% Mo, 0.18% Ni, 0.16% Cu, 0.040% Al
0.27% C, 0.10% Si, 0.76% Mn, 0.013% P, 0.008% S, 0.23% Cr, 0.05% Mo, 0.18% Ni, 0.16% Cu, 0.040% Al
0.27% C, 0.10% Si, 0.76% Mn, 0.013% P, 0.008% S, 0.23% Cr, 0.05% Mo, 0.18% Ni, 0.16% Cu, 0.040% Al
0.27% C, 0.13% Si, 0.50% Mn, 0.022% S, 0.030% P, 0.19% Ni, 0.74% Cr, 0.55% Mo
0.27% C, 0.26% Si, 1.0% Mn, 0.018% P, 0.026% S, 0.57% Cr, 0.12% Ni, 0.15% Mo, 0.22% Cu
0.27% C, 0.93% Mn, 0.31% Si, 0.05% Ni, 0.05% Cr, 0.40% Mo
0.27-0.30% C, max. 0.40% Si, 1.15-1.45% Mn, max. 0.025% P, max. 0.035% S, 0.0008-0.0050% B
0.27-0.32% C, 0.15-0.35% Si, 1.20-1.40% Mn, max. 0.035% P, max. 0.035% S, 0.10-0.25% Cr, 0.025-0.050% Ti, 0.0010-0.0050% B
0.27-0.32% C, 0.40% Si, 0.80-1.10% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, 0.25% Cu, 0.0008-0.0050% B
0.27-0.32% C, 0.40% Si, 0.80-1.10% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, 0.25% Cu, 0.0008-0.0050% B
0.27-0.33% C, 0.10-0.35% Si, 0.30-0.70% Mn, max. 0.040% P, max. 0.040% S, 0.75-1.20% Cr, 0.15-0.25% Mo
0.27-0.33% C, 0.10-0.35% Si, 0.30-0.70% Mn, max. 0.040% P, max. 0.040% S, 0.75-1.20% Cr, 0.15-0.25% Mo
0.27-0.33% C, 0.10-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.040% S, 0.35-0.65% Cr, 0.15-0.25% Mo, 0.35-0.75% Ni. Can be expected to have 0.0005% minimum boron content.
0.27-0.33% C, 0.10-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.040% S, 0.35-0.65% Cr, 0.15-0.25% Mo, 0.35-0.75% Ni
0.27-0.33% C, 0.15-0.35% Si, 0.30-0.70% Mn, 0.75-1.20% Cr, 0.15-0.25% Mo
0.27-0.33% C, 0.15-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo, +B
0.27-0.33% C, 0.15-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.27-0.33% C, 0.15-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35% Cu, 0.15-0.25% Mo, 0.0005-0.0030% B
0.27-0.33% C, 0.15-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.27-0.33% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.75-1.20% Cr
0.27-0.33% C, 0.15-0.35% Si, 0.70-1.05% Mn, 0.25-0.55% Cr, 0.25-0.65% Ni, 0.08-0.15% Mo, +B
0.27-0.33% C, 0.15-0.35% Si, 1.45-2.05% Mn
0.27-0.33% C, 0.15-0.35% Si, 1.45-2.05% Mn
0.27-0.33% C, 0.20-0.35% Si, 0.50-0.90% Mn, 0.45-0.85% Cr, 1.00-1.45% Ni
0.27-0.33% C, 0.20-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.27-0.33% C, 0.20-0.35% Si, 0.60-0.95% Mn, 0.35-0.75% Ni, 0.35-0.65% Cr, 0.15-0.25% Mo
0.27-0.33% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.25-0.55% Cr, 0.25-0.65% Ni, 0.08-0.15% Mo, +B
0.27-0.33% C, 0.30-0.70% Mn, 0.15-0.30% Si, 0.75-1.20% Cr, 0.15-0.25% Mo
0.27-0.33% C, 0.30-0.70% Mn, 0.15-0.30% Si, 0.75-1.20% Cr, 0.15-0.25% Mo
0.27-0.33% C, max. 0.30% Si, 1.15-1.45% Cr, max. 0.025% P, max. 0.035% S, 0.0008-0.005% B
0.27-0.33% C, max. 0.40% Si, 1.15-1.45% Mn, max. 0.025% P, max. 0.035% S, 0.0008-0.0050% B
0.27-0.34% C, <0.60% Si, 1.20-1.50% Mn, <0.015% P, <0.035% S, <0.40%Cr, <0.40% Ni, <0.10% Mo, <0.05% V, Cr+Mo+Ni=<0.63
0.27-0.34% C, 0.10-0.40% Si, 0.35-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.60-0.90% Cr, 2.50-3.00% Ni
0.27-0.34% C, 0.15-0.25% Si, 0.35-0.60% Mn, 0.035% P, 0.035% S, 0.80-1.15% Cr, 0.15-0.25% Mo
0.27-0.34% C, 0.15-0.25% Si, 0.35-0.60% Mn, 0.035% P, 0.035% S, 0.80-1.15% Cr, 0.15-0.25% Mo
0.27-0.34% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu
0.27-0.34% C, 0.20-0.35% Si, 0.55-0.85% Mn, 3.20-3.80% Ni
0.27-0.34% C, 0.60-0.90% Mn. Steel 1070: 0.65-0.75% C, 0.60-0.90% Mn
0.27-0.34% C, max. 0.30% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.27-0.34% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.27-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo max. 0.40% Ni
0.27-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.27-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.27-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.28% C, <0.40% Si, 1.48% Mn, <0.40% Cr, <0.10% Mo, <0.40% Ni, (Cr+Mo+Ni)=max. 0.63
0.28% C, 0.20% Si, 0.79% Mn, 0.036% S, 0.030% P, 0.14% Ni, 0.10% Cr
0.28% C, 0.25% Si, 1.45% Mn
0.28-0.30% C, 0.33% Si, 0.90-1.20% Mn, max. 0.025% P, max. 0.025% S, 0.40-0.55% Cr, max. 0.15% Mo, max. 0.25% Cu
0.28-0.30% C, max. 0.33% Si, 0.90-1.20% Mn, max. 0.025% P, max. 0.025% S, 0.40-0.55% Cr, max. 0.15% Mo, max. 0.25% Cu
0.28-0.32% C, 0.20-0.35% Si, 0.40-0.60% Mn, max. 0.015% P, max. 0.005% S, 1.25-1.40% Cr, 3.90-4.25% Ni, 0.20-0.25% Mo, max. 0.10% V
0.28-0.32% C, max. 0.30% Si, 0.80-1.00% Mn, max. 0.025% P, max. 0.025% S, max. 0.30% Cr, 0.08-0.12% Mo, max. 0.25% Cu, 0.0008-0.0050% B
0.28-0.32% C, max. 0.30% Si, 0.80-1.00% Mn, max. 0.025% P, max. 0.025% S, max. 0.30% Cr, 0.08-0.12% Mo, max. 0.25% Cu, 0.0008-0.0050% B
0.28-0.33% C, 0.15-0.35% Si, 0.40-0.60% Mn, max. 0.025% P, max. 0.040% S, 0.80-1.10% Cr, 0.25% Ni, 0.35% Cu, 0.15-0.25% Mo
0.28-0.33% C, 0.15-0.35% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.040% S, 0.80-1.10% Cr, 0.25% Ni, 0.35% Cu, 0.13-0.20% Mo
0.28-0.33% C, 0.15-0.35% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo
0.28-0.33% C, 0.15-0.35% Si, 0.70-0.90% Mn, 0.40-0.60% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni, 0.35% Cu. Steel 86B30: 0.27-0.34% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.35-0.60% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni, 0.35% Cu, 0.0005-0.0030% B
0.28-0.33% C, 0.15-0.35% Si, max. 0.035% P, max. 0.040% S, 0.40-0.60% Mn, 0.80-1.10% Cr, 01.5-0.25% Mo
0.28-0.33% C, 0.15-0.40% Si, 1.10-1.50% Mn, max. 0.030% P, max. 0.030% S, 0.25-0.60% Cr, 0.0020-0.0050% B
0.28-0.33% C, 0.15-1.35% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.80-1.00% Cr, 0.25% Ni, 0.35% Cu
0.28-0.33% C, 0.20-0.35% Si, 0.60-0.80% Mn, 0.55-0.75% Cr, 1.10-1.40% Ni
0.28-0.33% C, 0.25-0.35% Si, 0.60-0.80% Mn, 3.25-3.75% Ni
0.28-0.33% C, 1.60-1.90% Mn, 0.15-0.35% Si
0.28-0.34% C, 0.10-0.35% Si, 0.70-1.00% Mn, max. 0.030% P, max. 0.030% S, 0.0008% B
0.28-0.34% C, 0.90-1.20% Si, 0.80-1.10% Mn, 0.80-1.10% Cr
0.28-0.34% C, 0.90-1.20% Si, 0.80-1.10% Mn, 0.80-1.10% Cr
0.28-0.35% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.60-1.00% Cr, 2.60-3.20% Ni, 0.30-0.60% Mo
0.28-0.35% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.035% S, 2.80-3.30% Cr, 0.30-0.50% Mo, max. 0.60% Ni
0.28-0.35% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, 0.020-0.040% S, 0.40-0.60% Cr
0.28-0.35% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.60% Cr
0.28-0.36% C, 0.50-0.90% Si, 0.65-1.00% Cr, 0.30-0.45% Mo, 2.00% Ni, 0.35% Cu
0.28-0.40% C, 0.60-1.00% Mn, 0.20-0.80% Si, 1.40-2.00% Cr, 0.30-0.35% Mo
0.29% C, 0.20% Si, 0.54% Mn, 0.017% P, 0.012% S, 0.53% Cr, 1.74% Ni, 0.01% Mo, 0.15% V, 0.002% Ti, 0.04% Cu, 0.052% Al, 0.005% N
0.29% C, 0.22% Si, 0.45% Mn, 0.015% S, 0.022% P, 4.15% Ni, 1.17% Cr, 0.12% Mo
0.29% C, 0.23% Si, 0.77% Mn, 2.72% Ni, 0.05% Mo
0.29% C, 0.26% Si, 1.67% Mn, 0.030% S, 0.033% P, 0.21% Ni, 0.12% Cr, 0.04% Mo
0.29% C, 0.27% Si, 0.75% Mn, 0.043% P, 0.040% S, 0.85% Cr, 0.02% Ni, 0.11% Mo, 0.09% V, 0.05% Ti, 0.029% Al, 0.013% N
0.29% C, 0.67% Si, 0.61% Mn, 1.30% Cr, 0.18% Ni, 0.47% Mo, 0.26% V
0.29-0.35% C, 0.10-0.35% Si, 0.50-0.90% Mn, max. 0.040% P, max. 0.040% S, 0.65-1.10% Cr
0.29-0.35% C, 0.10-0.35% Si, 0.50-0.90% Mn, max. 0.040% P, max. 0.040% S, 0.64-1.10% Cr
0.29-0.35% C, 0.10-0.35% Si, 0.50-0.90% Mn, max. 0.040% P, max. 0.040% S, 0.65-1.10% Cr
0.29-0.35% C, 0.15-0.35% Si, 0.50-0.90% Mn, 0.65-1.10% Cr
0.29-0.35% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.20-0.30% Mo
0.29-0.35% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.20% Cr, 0.25% Ni, 0.35% Cu, 0.20-0.30% Mo
0.29-0.36% C, 0.15-0.35% Si, 1.15-1.55% Mn, max. 0.030% P, max. 0.030% S, 0.35% Cr, 0.25% Ni, 0.30% Cu
0.30% C, 0.10% Si, 0.30% Mn, 1.00% Cr, 1.00% Mo, 0.10% V, 4.50% Co, 7.50% Ni
0.30% C, 0.13% Si, 0.40% Mn, 0.011% P, 0.014% S, 0.46% Cr, 1.77% Ni, 0.01% Mo, 0.23% V, 0.003% Ti, 0.04% Cu, 0.043% Al, 0.009% N
0.30% C, 0.18% Si, 0.94% Mn, 0.012% P, 0.028% S, 0.10% Cr
0.30% C, 0.19% Si, 0.52% Mn, 0.017% P, 0.012% S, 0.53% Cr, 1.75% Ni, 0.05% Mo, 0.15% V, 0.002% Ti, 0.03% Cu, 0.043% Al, 0.007% N
0.30% C, 0.25% Si, 0.45% Mn, 2.00% Cr, 1.00% Ni, 0.40% Mo
0.30% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni, 0.45% Mo
0.30% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni, 0.45% Mo
0.30% C, 0.25% Si, 0.52% Mn, 0.010% P, 0.002% S, 1.93% Cr, 0.32% Mo, 1.92% Ni, 0.010% V, 0.07% Cu, 0.009% Al
0.30% C, 0.25% Si, 0.55% Mn, 2.50% Cr, 0.15% V, 0.20% Mo
0.30% C, 0.25% Si, 0.55% Mn, 2.50% Cr, 0.15% V, 0.20% Mo
0.30% C, 0.25% Si, 0.55% Mn, 2.50% Cr, 0.20% Mo, 0.15% V
0.30% C, 0.25% Si, 0.65% Mn, <0.03% S, + Pb, Cm30: 0.30% C, 0.25% Si, 0.65% Mn, 0.020-0.035% S, + Pb
0.30% C, 0.25% Si, 1.35% Mn
0.30% C, 0.25% Si, 1.35% Mn
0.30% C, 0.25% Si, 1.40% Mn
0.30% C, 0.26% Si, 0.79% Mn, 0.022% P, 0.026% S, 0.98% Cr, 0.09% Ni, 0.02% Mo, 0.14% Cu, 0.019% Al
0.30% C, 0.29% Si, 1.24% Mn, 0.012% P, 0.010% S, 0.41% Cr, 0.07% Mo, 0.21% Ni, 0.0030% B
0.30% C, 0.30% Si, 0.50% Mn, 2.00% Cr, 0.35% Mo, 2.00% Ni
0.30% C, 0.30% Si, 0.80% Mn, 0.50% Cr, 0.20% Mo, 0.55% Ni
0.30% C, 0.30% Si, 0.80% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.30% C, 0.30% Si, 0.80% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.30% C, 0.30% Si, 0.85% Mn, 0.85% Cr, 0.40% Mo, 0.07% V, 1.80% Ni
0.30% C, 0.40% Mn, 0.30% Si, 0.016% S, 0.015% P 3.20% Ni, 0.86% Cr, 0.40% Mo, 0.17% Cu
0.30% C, 0.77% Mn, 0.043% S, 0.26% Si, 0.12% Ni, 0.06% Cr, 0.27% Mo
0.30% C, 0.80% Mn, 0.54% Ni, 0.55% Cr, 0.21% Mo
0.30% C, 2.50-3.50% Cr, 0.40-0.60% Mo
0.30-0.34% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, 0.0008-0.0050% B
0.30-0.34% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, 0.0008-0.0050% B
0.30-0.34% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, 0.0008-0.0050% B
0.30-0.35% C, 0.15-0.50% Si, 0.40-0.60% Mn, 0.80-1.10% Cr, 0.15-0.25% Mo, 0.25% Ni, 0.35% Cu. Steel 4140: 0.38-0.43% C, 0.15-0.35% Si, 0.75-1.00% Mn, 0.80-1.10% Cr, 0.15-0.25% Mo, 0.25% Ni, 0.35% Cu
0.30-0.35% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, 0.25% Cu, 0.0008-0.050% B
0.30-0.35% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, 0.25% Cu, 0.0008-0.050% B
0.30-0.35% C, max. 0.35% Si, max. 0.60% Mn, max. 0.025% P, max. 0.010% S, 2.80-3.20% Cr, 0.80-1.20% Mo, 0.25-0.35% V
0.30-0.36% C, <0.40% Si, 1.20-1.50% Mn, <0.035% P, <0.040% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.30-0.36% C, <0.40% Si, 1.20-1.50% Mn, <0.035% P, <0.040% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.30-0.36% C, 0.40% Si, 1.20-1.50% Mn, max. 0.025% P, max. 0.035% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.30-0.37% C, <0.40% Si, 0.30-0.60% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr
0.30-0.37% C, <0.40% Si, 0.30-0.60% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr
0.30-0.37% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.30-0.37% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr
0.30-0.37% C, 0.15-0.35% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 1.20-1.50% Cr, 0.80-1.10% Al
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.020-0.040% S, 0.90-1.20% Cr
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, 0.020-0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, 0.020-0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.030% S, 0.90-1.20% Cr
0.30-0.37% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 1.00-1.30% Cr, 0.15-0.25% Mo, 0.80-1.20% Al
0.30-0.37% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 0.15-0.25% Cr, 0.80-1.20% Al
0.30-0.37% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 1.50-1.80% Cr, 0.15-0.25% Mn, 0.85-1.15% Ni, 0.80-1.20% Al
0.30-0.37% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.035% S, 1.50-1.80% Cr, 0.85-1.15% Ni, 0.15-0.25% Mo, 0.80-1.20% Al
0.30-0.37% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.035% S, 0.90-1.20% Cr
0.30-0.37% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.80-1.10% Cr, 1.20-1.60% Ni
0.30-0.37% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.035% S, 0.90-1.20% Cr
0.30-0.37% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.80-1.10% Cr, 1.20-1.60% Ni
0.30-0.37% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.38% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 1.30-1.70% Cr, 1.30-1.70% Ni, 0.15-0.30% Mo
0.30-0.38% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, 0.15-0.35% Si, 0.30-0.60% Mn, max. 0.025% P, max. 0.020% S, 1.60-1.90% Cr, 0.25-0.45% Mo, 3.80-4.00% Ni
0.30-0.38% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.026% P, max. 0.035% S, 1.30-1.70% Cr, 1.30-1.70% Ni, 0.15-0.30% Mo
0.30-0.38% C, 0.20-0.40% Si, 0.20-0.50% Mn, <0.035% P, <0.035% S, 1.50-1.90% Cr, 3.50-4.00% Ni
0.30-0.38% C, 0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.030% S, 1.40-1.70% Cr, 1.40-1.70% Ni, 0.15-0.30% Mo
0.30-0.38% C, max. 0.0% Si, 1.30-1.70% Cr, 1.30-1.70% Ni, 0.15-0.30% Mo
0.30-0.38% C, max. 0.0% Si, 1.30-1.70% Cr, 1.30-1.70% Ni, 0.15-0.30% Mo
0.30-0.38% C, max. 0.0% Si, 1.30-1.70% Cr, 1.30-1.70% Ni, 0.15-0.30% Mo
0.30-0.38% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.39% C, 0.15-0.35% Si, 1.00-1.50% Mn, +B
0.30-0.39% C, 0.15-0.35% Si, 1.00-1.50% Mn, max. 0.030% P, max. 0.050% S, 0.0005-0.0030% B
0.30-0.40% C, 0.15-0.35% Si, 0.40-0.90% Mn, 0.80-2.00% Cr, 0.35-0.90% Mo, 2.50-4.00% Ni, 0.05-0.25% V
0.31% C, 0.20% Si, 0.62% Mn, 0.012% S, 0.018% P, 2.63% Ni, 0.64% Cr, 0.58% Mo
0.31% C, 0.23% Si, 0.71% Mn, 0.007% P, 0.011% S, 0.82% Cr, 1.86% Ni, 0.01% Mo, 0.26% V, 0.004% Ti, 0.05% Cu, 0.043% Al, 0.009% N
0.31% C, 0.23% Si, 0.77% Mn, 0.037% S, 0.014% P, 0.16% Ni, 0.07% Cr, 0.02% Mo
0.31% C, 0.25% Si, 0.60% Mn, 2.55% Cr, 0.15% V, 0.20% Mo
0.31% C, 0.25% Si, 0.70% Mn, 0.033% S, 0.018% P, 0.05% Ni, 0.05% Cr
0.31% C, 0.27% Si, 0.64% Mn, 0.020% P, 0.022% S, 0.79% Cr, 2.89% Ni
0.31% C, 0.27% Si, 1.07% Mn, 11.35% Cr, 2.85% Mo, 0.24% V, 0.43% Ni
0.31% C, 0.28% Si, 1.35% Mn, <0.30% Cr
0.31% C, 0.30% Si, 0.51% Mn, 0.013% P, 0.020% S, 0.96% Cr, 0.20% Ni, 0.21% Mo, 0.12% Cu
0.31% C, 0.53% Si, 0.54% Mn, 1.25% Cr, 0.52% Mo, 0.27% V, 1.05% Co
0.31% C, 0.58% Mn, 0.32% Si, 1.07% Cr, 0.15% Ni, 0.21% Mo, 0.025% V, 0.028% Nb. 4130 steel: 0.31% C, 0.57% Mn, 0.28% Si, 0.93% Cr, 0.12% Ni, 0.19% Mo, 0.006% V, 0.002% Nb
0.31-0.37% C, 0.10-0.35% Si, 0.70-1.00% Mn, max. 0.030% P, max. 0.030% S, 0.0008% B
0.31-0.37% C, 0.10-0.35% Si, 1.20-1.50% Mn, max. 0.030% P, max. 0.030% S, 0.0008% B
0.31-0.38% C, 0.150.40% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.60-1.20% Cr, 3.70-4.20% Ni, 0.25-0.45% Mo
0.31-0.39% C, 0.15-0.35% Si, 0.70-1.20% Mn, +B
0.31-0.39% C, 0.15-0.35% Si, 0.70-1.20% Mn, max. 0.030% P, max. 0.050% S, 0.0005-0.0030% B
0.31-0.39% C, 0.17-0.37% Si, 0.50-0.80% Mn, 0.80-1.10% Cr
0.32% C, 0.10% Si, 0.75% Mn, 0.010% P, 0.008% S, 1.11% Cr, 0.002% Cu, 0.0030% B
0.32% C, 0.10% Si, 0.75% Mn, 0.010% P, 0.008% S, 1.11% Cr, 0.02% Cu, 0.0030% B
0.32% C, 0.17% Si, 0.45% Mn, 0.010% P, 0.015% S, 0.47% Cr, 1.73% Ni, 0.12% Mo, 0.15% V, 0.003% Ti, 0.05% Cu, 0.048% Al, 0.012% N
0.32% C, 0.19% Si, 0.72% Mn, 0.82% Cr, 1.70% Ni, 0.31% Mo, 0.17% V
0.32% C, 0.24% Si, 1.40% Mn, 0.004% P, 0.010% S, 0.03% Cr, 0.01% Mo, 0.11% V, 0.040% Al, 0.010% N
0.32% C, 0.25% Si, 0.40% Mn, 3.10% Cr, 0.30% V, 1.00% Mo
0.32% C, 0.25% Si, 0.50% Mn, 0.80% Cr, 2.80% Ni, +Pb
0.32% C, 0.25% Si, 0.55% Mn, 3.00% Cr, 0.40% Mo
0.32% C, 0.25% Si, 0.55% Mn, 3.05% Cr, 0.40% Mo
0.32% C, 0.28% Si, 0.61% Mn, 0.013% S, 0.018% P, 3.22% Ni, 0.63% Cr, 0.22% Mo
0.32% C, 0.31% Si, 0.74% Mn, 1.70% Ni, 0.23% Mo
0.32-0.37% C, 0.20-0.40% Si, 0.60-0.80% Mn, 0.90-1.10% Cr, 0.20-0.25% Mo
0.32-0.38% C, 0.15-0.35% Si, 0.50-0.90% Mn, 0.70-1.15% Cr
0.32-0.38% C, 0.15-0.35% Si, 0.50-0.90% Mn, max. 0.040% P, max. 0.030% S, 0.70-1.15% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.32-0.38% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.75-1.20% Cr, 0.15-0.25% Mo
0.32-0.38% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.75-1.20% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.25% Mo
0.32-0.38% C, 0.15-0.35% Si, 1.45-2.05% Mn
0.32-0.38% C, 0.15-0.35% Si, 1.45-2.05% Mn
0.32-0.38% C, 0.20-0.35% Si, 0.79-0.80% Mn, max. 0.025% P, 0.020-0.030% S, 1.35-1.60% Cr, 0.20-0.30% Mo, max. 0.10% V
0.32-0.38% C, 0.60-1.20% Mn, 0.15-0.35% Si, 0.75-1.20% Cr, 0.15-0.25% Mo
0.32-0.39% C, <0.40% Si, 0.30-0.60% Mn, <0.030% P, <0.025% S, 1.60-2.00% Cr, 0.25-0.45% Mo, 3.60-4.10% Ni
0.32-0.39% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63
0.32-0.39% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63
0.32-0.39% C, <0.40% Si, 0.70-1.10% Mn, <0.060% P, 0.15-0.25% S
0.32-0.39% C, 0.10-0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S
0.32-0.39% C, 0.10-0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 1.30-1.70% Cr, 1.30-1.70% Ni, 0.15-0.30% Mo
0.32-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S
0.32-0.39% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.30% Mo
0.32-0.39% C, 0.17-0.37% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.25% Cr, 0.25% Ni, 0.30% Cu
0.32-0.39% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.020-0.035% S, 0.25% Cu
0.32-0.39% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.025% Cu
0.32-0.39% C, 0.40% Si, 0.30-0.60% Mn, 0.030% P, 0.025% S, 1.60-2.50% Cr, 0.25-0.45% Mo, 3.60-4.10% Ni
0.32-0.39% C, 0.40% Si, 0.30-0.60% Mn, 0.030% P, 0.025% S, 1.60-2.50% Cr, 0.25-0.45% Mo, 3.60-4.10% Ni
0.32-0.39% C, max. 0.30% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Cu
0.32-0.39% C, max. 0.40% Si, 0.30-0.60% Mn, 1.60-2.00% Cr, 3.60-4.10% Ni, 0.25-0.45% Mo
0.32-0.39% C, max. 0.40% Si, 0.30-0.60% Mn, 1.60-2.00% Cr, 3.60-4.10% Ni, 0.25-0.45% Mo
0.32-0.39% C, max. 0.40% Si, 0.30-0.60% Mn, 1.60-2.00% Cr, 3.60-4.10% Ni, 0.25-0.45% Mo
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, 0.020-0.035% S, max. 0.25% Cu
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 1.60-2.00% Cr, 0.25-0.45% Mo, 3.60-4.10% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 1.60-2.00% Cr, 0.25-0.45% Mo, 3.60-4.10% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=<0.63
0.32-0.40% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.030% S, 0.90-1.20% Cr, 0.90-1.20% Ni, 0.15-0.30% Mo
0.32-0.40% C, 0.50-0.80% Mn, <0.40% Si, 0.60-1.00% Cr, 0.15-0.25% Mo, 0.70-1.00% Ni
0.32-0.40% C, 0.50-0.80% Mn, <0.40% Si, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.15-0.30% Ni
0.32-0.40% C, 0.50-0.80% Mn, <0.40% Si, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.15-0.30% Ni
0.32-0.40% C, max. 0.40% Si, 0.50-0.80% Mn, 0.90-1.20% Cr, 0.90-1.20% Ni, 0.15-0.30% Mo
0.32-0.40% C, max. 0.40% Si, 0.50-0.80% Mn, 0.90-1.20% Cr, 0.90-1.20% Ni, 0.15-0.30% Mo
0.32-0.40% C, max. 0.40% Si, 0.50-0.80% Mn, 0.90-1.20% Cr, 0.90-1.20% Ni, 0.15-0.30% Mo
0.32-0.40% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, max. 0.40% Si, 1.20-1.50% Mn, max. 0.035% P, max. 0.035% S
0.32-0.40% C, max. 0.40% Si, 1.20-1.50% Mn, max. 0.035% P, max. 0.035% S
0.32-0.43% C, 0.235-0.290% Si, 0.595-0.690% Mn, 0.013-0.021% P, 0.960-1.530% Cr, 0.012-0.015% Al, 1.485-1.720% Ni, 0.165-0.230% Mo, 0.110-0.210% Cu
0.33% C, 0.17% Si, 0.51% Mn, 1.44% Cr, 4.16% Ni, 0.31% Mo
0.33% C, 0.18% Si, 1.48% Mn, 0.028% S, 0.028% P, 0.26% Ni, 0.16% Cr, 0.27% Mo
0.33% C, 0.21% Si, 0.62% Mn, 0.025% S, 0.022% P, 0.89% Ni, 0.10% Cr, 0.05% Mo
0.33% C, 0.23% Si, 0.57% Mn, 0.007% S, 0.005% P, 3.26% Ni, 0.85% Cr, 0.09% Mo
0.33% C, 0.23% Si, 0.57% Mn, 0.85% Cr, 3.26% Ni, 0.09% Mo
0.33% C, 0.23% Si, 0.74% Mn, 0.027% S, 0.031% P, 3.47% Ni, 0.07% Cr, 0.11% Mo
0.33% C, 0.23% Si, 1.54% Mn, 0.024% S, 0.021% P, 0.18% Ni, 0.15% Cr, 0.05% Mo
0.33% C, 0.28% Si, 0.84% Mn, 0.004% P, 0.009% S, 0.03% Cr, 0.03% Ni, 0.01% Mo, 0.10% V, 0.005% Ti, 0.003% B, 0.02% Cu, 0.032% Al, 0.011% N
0.33% C, 0.41% Mn, 1.96% Mo
0.33% C, 0.41% Si, 0.69% Mn, 0.72% Cr, 1.41% Ni, 0.28% Mo
0.33% C, 0.45% Mn, 1.97% Cr
0.33% C, 0.53% Mn, 0.90% Cr, 0.18% Mo
0.33-0.38% C, 0.15-0.35% Si, 0.80-1.10% Mn, max. 0.025% P, max. 0.040% S, max. 0.20% Cr, max. 0.35% Cu, max. 0.06% Mo, 0.0005-0.0030% B
0.33-0.38% C, 0.15-0.35% Si, 0.80-1.10% Mn, max. 0.035% P, max. 0.040% S, 0.20% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo, 0.0005-0.0030% B
0.33-0.38% C, 0.30% Si, 0.80-1.10% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, 0.25% Cu, 0.0008-0.0050% B
0.33-0.38% C, 0.30% Si, 0.80-1.10% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, 0.25% Cu, 0.0008-0.0050% B
0.33-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, <0.025% P, <0.035% S
0.33-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, <0.025% P, <0.035% S
0.33-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S
0.33-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S
0.33-0.39% C, 0.15-0.40% Si, 0.80-1.10% Mn, 0.030% P, 0.030% S, 0.90-1.20% Cr
0.33-0.39% C, 0.15-0.40% Si, 0.80-1.10% Mn, max. 0.030% P, max. 0.030% S, 0.90-1.20% Cr
0.33-0.40% C, 0.15-0.35% Si, 0.80-1.10% Mn, 0.035% P, 0.035% S, 1.00-1.30% Cr
0.33-0.40% C, 0.15-0.35% Si, 0.80-1.10% Mn, 0.035% P, 0.035% S, 1.00-1.30% Cr
0.33-0.40% C, 0.15-0.40% Si, 0.80-1.20% Mn, max. 0.035% P, max. 0.035% S, 1.00-1.30% Cr
0.33-0.41% C, 1.10-1.40% Si, 1.10-1.40% Mn, max. 0.035% P, max. 0.035% S
0.34% C, <0.40% Si, 0.65% Mn, 1.50% Cr, 0.23% Mo, 1.50% Ni
0.34% C, 0.18% Si, 1.53% Mn, 0.028% P, 0.026% S, 0.08% Cr, 0.02% Mo, 0.17% Ti
0.34% C, 0.18% Si, 1.53% Mn, 0.028% P, 0.026% S, 0.08% Cr, 0.02% Mo, 0.17% Ti
0.34% C, 0.22% Si, 0.71% Mn, 2.52% Ni, 0.42% Mo, 0.02% V
0.34% C, 0.23% Si, 0.55% Mn, 0.011% P, 0.022% S, 1.39% Cr, 4.59% Ni
0.34% C, 0.25% Si, 0.50% Mn, 1.50% Cr, 0.25% Mo, 1.55% Ni, + Pb
0.34% C, 0.25% Si, 0.50% Mn, 1.50% Cr, 1.55% Ni, 0.25% Mo
0.34% C, 0.25% Si, 0.50% Mn, 1.50% Cr, 1.55% Ni, 0.25% Mo
0.34% C, 0.25% Si, 0.50% Mn, 1.70% Cr, 1.00% Ni, 0.20% Mo, 0.90% Al
0.34% C, 0.25% Si, 0.55% Mn, 1.55% Cr, 1.55% Ni, 0.20% Mo
0.34% C, 0.25% Si, 0.55% Mn, 1.65% Cr, 1.00% Al, 1.00% Ni, 0.20% Mo
0.34% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.75% Mn, 1.05% Cr
0.34% C, 0.25% Si, 0.75% Mn, 1.50% Cr, 1.00% Al
0.34% C, 0.25% Si, 0.75% Mn, 1.50% Cr, 1.00% Al
0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr, <0.035% S, (Pb). 34CrS4: 0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr, 0.020-0.035% S, (Pb)
0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr, <0.035% S, +Pb. 34CrS4: 0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr, 0.020-0.035% S, +Pb
0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr, max. 0.035% S
0.34% C, 0.27% Si, 1.46% Mn, 0.003% P, 0.010% S, 0.03% Cr, 0.01% Mo, 0.11% V, 0.001% B, 0.037% Al, 0.010% N
0.34% C, 0.29% Si, 0.59% Mn, 0.012% P, 0.007% S, 1.54% Cr, 0.24% Mo, 1.52% Ni
0.34% C, 0.30% Si, 0.50% Mn, 1.50% Cr, 0.20% Mo, 1.50% Ni
0.34% C, 0.35% Si, 0.65% Mn, 1.15% Cr, 1.00% Al, 0.20% Mo
0.34-0.38% C, 0.30% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, max. 0.25% Cu, 0.0008-0.0050% B
0.34-0.38% C, 0.30% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, max. 0.25% Cu, 0.0008-0.0050% B
0.34-0.39% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu
0.34-0.40% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr
0.34-0.40% C, 0.10-0.35% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.030% S, 0.0008% B
0.34-0.40% C, 0.15-0.40% Si, 0.60-0.90% Mn, <0.025% P, <0.035% S, 0.90-1.20% Cr
0.34-0.40% C, 0.15-0.40% Si, 0.60-0.90% Mn, <0.025% P, <0.035% S, 0.90-1.20% Cr
0.34-0.40% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr
0.34-0.41% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.34-0.41% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.20-0.30% Mo
0.34-0.41% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.75-1.20% Cr, 0.15-0.25% Mo
0.34-0.41% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.75-1.20% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.25% Mo
0.34-0.41% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.20% Cr, 0.25% Ni, 0.35% Cu, 0.20-0.30% Mo
0.34-0.41% C, 0.15-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.34-0.41% C, 0.15-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.34-0.41% C, 0.15-0.35% Si, 1.30-1.70% Mn, max. 0.030% P, max. 0.030% S, 0.35% Cr, 0.25% Ni, 0.30% Cu
0.34-0.41% C, 0.15-0.80% Si, 1.20-1.60% Mn, <0.025% P, 0.020-0.060% S, <0.30% Cr, <0.08% Mo, 0.08-0.20% V, 0.01-0.02% N
0.34-0.41% C, 0.20-0.35% Si, 0.55-0.90% Mn, 0.65-0.95% Cr, 1.55-2.00% Ni, 0.20-0.30% Mo
0.34-0.41% C, 0.20-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.34-0.41% C, 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr
0.34-0.41% C, 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, 0.020-0.035% S, 0.90-1.20% Cr
0.34-0.41% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.035% S, 0.90-1.20% Cr
0.34-0.41% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.035% S, 0.90-1.20% Cr
0.34-0.42% C, 0.15-0.35% Si, 1.40-1.65% Mn, max. 0.035% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.34-0.42% C, 1.00-1.40% Si, 0.30-0.60% Mn, 1.30-1.60% Cr
0.34-0.42% C, 1.00-1.40% Si, 0.30-0.60% Mn, 1.30-1.60% Cr
0.34-0.43% C, 0.15-0.30% Si, 0.50-1.00% Mn
0.34-0.43% C, 0.15-0.35% Si, 0.50-1.00% Mn, max. 0.030% P, max. 0.050% S
0.34-0.44% C, 0.15-0.35% Si, 0.50-1.00% Mn
0.35% C, <0.40% Si, 0.45% Mn, 1.80% Cr, 0.35% Mo, 3.85% Ni
0.35% C, 0.10% Si, 0.76% Mn, 0.009% P, 0.008% S, 1.10% Cr, 0.02% Cu, 0.0030% B
0.35% C, 0.10% Si, 0.76% Mn, 0.009% P, 0.008% s, 1.10% Cr, 0.02% Cu, 0.0030% B
0.35% C, 0.13% Si, 0.65% Mn, 0.032% S, 0.035% P, 1.27% Ni, 0.55% Cr
0.35% C, 0.14% Si, 0.44% Mn, 1.43% Cr, 4.23% Ni, 0.13% Mo
0.35% C, 0.20% Si, 0.70% Mn, <0.025% P, <0.025% S, <0.25% Cu
0.35% C, 0.20% Si, 0.70% Mn, <0.025% S, <0.025% P, <0.25% Cu
0.35% C, 0.24% Si, 0.75% Mn, 0.009% P, 0.013% S, 0.81% Cr, 1.85% Ni, 0.11% Mo, 0.17% V, 0.004% Ti, 0.06% Cu, 0.053% Al, 0.012% N
0.35% C, 0.25% Si, 0.00% Mn, 0.65% Cr, 0.020-0.035% S, + Pb
0.35% C, 0.25% Si, 0.35% Mn, 1.70% Cr, 3.75% Ni
0.35% C, 0.25% Si, 0.40% Mn, 1.35% Cr, 3.55% Ni, 0.25% Mo
0.35% C, 0.25% Si, 0.65% Mn, <0.03% S, + Pb. Cm35: 0.35% C, 0.25% Si, 0.65% Mn, 0.020-0.035% S, + Pb
0.35% C, 0.25% Si, 0.65% Mn
0.35% C, 0.25% Si, 0.65% Mn
0.35% C, 0.25% Si, 0.65% Mn
0.35% C, 0.25% Si, 1.08% Mn, 0.004% P, 0.009% S, 0.03% Cr, 0.03% Ni, 0.01% Mo, 0.10% V, 0.004% Ti, 0.003% B, 0.02% Cu, 0.022% Al, 0.010% N
0.35% C, 0.25% Si, 1.35% Mn, +Pb
0.35% C, 0.26% Si, 0.50% Mn, 0.010% P, 0.020% S, 0.49% Cr, 1.54% Ni
0.35% C, 0.30% Si, 0.75% Mn, 1.05% Cr, 1.45% Ni, +Pb
0.35% C, 0.37% Mn
0.35% C, 0.50% Si, 0.75% Mn, 0.80% Cr, 1.85% Ni, 0.35% Mo, 0.20% V
0.35% C, 0.50% Si, 1.20% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.08% Mo, 0.30% Ni, 0.020% Al, 0.012% N
0.35% C, 0.80% Mn, 0.25% Mo
0.35% C, 0.92% Si, 4.76% Cr, 1.42% W, 1.45% Mo. Steel 2: 0.96% C, 0.29% Si, 2.93% Cr
0.35% C, 1.00% Si, 10.00% Cr, 0.20% Mo, 1.00% Ni
0.35% C, 1.85% Mn
0.35-0.39% C, 0.65-1.0% Mn, max. 0.13% Ni, max. 0.05% Cr, max. 0.03% Mo. 4130H steel: 0.27-0.33% C, 0.30-0.70% Mn, 0.15-0.30% Si, 0.75-1.20% Cr, 0.15-0.25% Mo
0.35-0.40% C, 0.15-0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, 0.30% Cu, 0.0008-0.0050% B
0.35-0.40% C, 0.15-0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.30% Cr, 0.30% Cu, 0.0008-0.0050% B
0.35-0.40% C, 0.30% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.20-0.30% Mo, 0.25% Cu
0.35-0.40% C, 0.30% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.20-0.30% Mo, 0.25% Cu
0.35-0.40% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, 0.25% Cu, 0.15-0.30% Cu
0.35-0.40% C, 0.30% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, 0.25% Cu, 0.15-0.30% Cu
0.35-0.40% C, 0.30% Si, 1.15-1.45% Mn, 0.025% P, 0.025% S, 0.30% Cr, 0.0008-0.0050% B, 0.25% Cu
0.35-0.40% C, 0.30% Si, 1.15-1.45% Mn, 0.025% P, 0.025% S, 0.30% Cr, 0.0008-0.0050% B, 0.25% Cu
0.35-0.40% C, 0.70-0.90% Mn, 0.15-0.30% Si, 0.80-1.10% Cr, 0.15-0.25% Mo
0.35-0.42% C, 1.50-1.80% Si, 0.50-0.80% Mn, 0.030% P, 0.030% S
0.35-0.42% C, 1.50-1.80% Si, 0.50-0.80% Mn, 0.030% P, 0.030% S
0.35-0.42% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.40-0.60% Cr
0.35-0.42% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.40-0.60% Cr
0.35-0.42% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, 0.020-0.040% S, 0.40-0.60% Cr
0.35-0.43% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.60-1.00% Cr, 0.70-1.00% Ni, 0.15-0.25% Mo
0.35-0.43% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.60-1.00% Cr, 0.15-0.25% Mo, 0.70-1.00% Ni
0.35-0.43% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.60-1.00% Cr, 0.15-0.25% Mo, 0.70-1.00% Ni
0.35-0.45% C, 0.10-0.40% Si, 0.20-0.55% Mn, max. 0.030% P, max. 0.025% S, 1.40-1.70% Cr, 0.35-0.60% Mo, 4.30-4.90% Ni
0.35-0.45% C, 0.15-0.35% Si, 1.25-1.75% Mn, +B
0.35-0.45% C, 0.15-0.35% Si, 1.25-1.75% Mn, max. 0.030% P, max. 0.050% S, 0.0005-0.0030% B
0.35-0.45% C, 0.15-0.35% Si, 1.25-1.75% Mn, max. 0.030% P, max. 0.050% S
0.35-0.45% C, 0.15-0.35% Si, 1.25-1.75% Mn
0.36% C, 0.17% Mn, 0.82% Mo
0.36% C, 0.22% Si, 1.59% Mn, 0.001% P, 0.012% S, 0.02% Mo, 0.12% V, 0.002% Ti, 0.048% Al, 0.018% N
0.36% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.20% Mo, 1.05% Ni, + Pb
0.36% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 1.05% Ni, 0.20% Mo
0.36% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 1.05% Ni, 0.20% Mo
0.36% C, 0.25% Si, 0.70% Mn, 1.40% Cr, 1.40% Ni, 0.20% Mo
0.36% C, 0.25% Si, 1.25% Mn, + Pb
0.36% C, 0.25% Si, 1.35% Mn, +Pb
0.36% C, 0.28% Si, 0.67% Mn, 0.037% P, 0.029% S, 0.86% Cr, 0.02% Ni, 0.02% Mo, 0.28% V, 0.02% Ti, 0.034% Al, 0.013% N
0.36% C, 0.63% Mn, 1.84% Ni, 0.23% Mo
0.36-0.40% C, 0.10-0.30% Si, 0.50-0.70% Mn, max. 0.020% P, max. 0.025% S, max. 0.10% Cr, max. 0.03% Mo, max. 0.10% Ni, max. 0.15% Cu, max. 0.010% Al
0.36-0.42% C, <0.40% Si, 1.40-1.70% Mn, <0.035% P, <0.040% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.36-0.42% C, <0.40% Si, 1.40-1.70% Mn, <0.035% P, <0.040% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.36-0.42% C, 0.15-0.35% Si, 1.30-1.70% Mn, max. 0.035% P, max. 0.035% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.36-0.42% C, 0.40% Si, 1.40-1.70% Mn, max. 0.025% P, max. 0.035% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.36-0.42% C, max. 0.40% Si, 1.15-1.45% Mn, max. 0.025% P, max. 0.035% S, 0.0008-0.0050% B
0.36-0.42% C, max. 0.40% Si, 1.15-1.45% Mn, max. 0.025% P, max. 0.035% S, 0.0008-0.0050% B
0.36-0.44% C, 0.17-0.37% Si, 0.50-0.80% Mn, 0.80-1.10% Cr
0.36-0.44% C, 0.17-0.37% Si, 0.50-0.80% Mn, 0.80-1.10% Cr
0.36-0.44% C, 0.25-0.50% Si, 0.80-1.10% Mn, max. 0.035% P, max. 0.035% S
0.37% C, 0.25% Si, 0.75% Mn, 1.05% Cr
0.37% C, 0.28% Si, 0.79% Mn, 0.006% P, 0.029% S, 0.95% Cr, 0.15% Ni, 0.07% Mo, 0.006% V, 0.037% Ti, 0.19% Cu, 0.012% Al, 0.010% N
0.37% C, 0.29% Si, 0.76% Mn, 0.005% P, 0.029% S, 0.90% Cr, 0.15% Ni, 0.08% Mo, 0.003% V, 0.042% Ti, 0.19% Cu, 0.025% Al, 0.010% N
0.37% C, 0.29% Si, 0.76% Mn, 0.006% P, 0.029% S, 0.90% Cr, 0.15% Ni, 0.08% Mo, 0.003% V, 0.042% Ti, 0.19% Cu, 0.025% Al, 0.010% N
0.37% C, 0.29% Si, 0.76% Mn, 0.006% P, 0.029% S, 0.90% Cr, 0.15% Ni, 0.08% Mo, 0.003% V, 0.042% Ti, 0.19% Cu, 0.025% Al, 0.010% N
0.37% C, 0.30% Si, 0.60% Mn, 0.71% Cr, 0.22% Mo, 1.43% Ni
0.37% C, 0.32% Si, 0.76% Mn, 0.009% P, 0.033% S, 0.97% Cr, 0.14% Ni, 0.03% Mo, 0.11% V, 0.22% Cu, 0.012% Al, 0.010% N
0.37% C, 0.32% Si, 0.76% Mn, 0.009% P, 0.033% S, 0.97% Cr, 0.14% Ni, 0.03% Mo, 0.11% V, 0.22% Cu, 0.012% Al, 0.010% N
0.37% C, 0.59% Si, 1.38% Mn, 0.22% Cr, 0.01% Mo, 0.09% V, 0.027% Ti, 0.20% Cu, 0.027% Al
0.37% C, 0.68% Mn, 3.41% Ni
0.37% C, 0.77% Mn, 0.98% Cr, 0.21% Mo. Blue lines: 0.37% C, 0.77% Mn, 0.98% Cr, 0.21% Mo
0.37% C, 0.77% Mn, 0.98% Cr, 0.21% Mo
0.37% C, 1.25% Si, 1.25% Mn, +Pb
0.37% C, 1.25% Si, 1.25% Mn
0.37% C, 1.25% Si, 1.25% Mn
0.37% C, 1.25% Si, 1.25% Mn
0.37% C, 1.30% Si, 1.30% Mn
0.37-0.40% C, 0.17-0.37% Si, 1.00-1.40% Mn, max. 0.035% P, max. 0.035% S, 0.30% Cr, 0.30% Ni, 0.30% Cu, 0.0005-0.0035% B
0.37-0.43% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.030% S, 0.60-1.00% Cr, 0.15-0.25% Mo, 0.70-1.00% Ni
0.37-0.43% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.030% S, 0.60-1.00% Cr, 0.15-0.25% Mo, 0.70-1.00% Ni
0.37-0.44% C, 0.10-0.35% Si, 0.55-0.90% Mn, max. 0.040% P, max. 0.040% S, 0.65-0.95% Cr, 0.20-0.35% Mo, 1.55-2.00% Ni
0.37-0.44% C, 0.10-0.35% Si, 0.55-0.90% Mn, max. 0.040% P, max. 0.040% S, 0.65-0.95% Cr, 0.20-0.30% Mo, 1.55-2.00% Ni
0.37-0.44% C, 0.10-0.35% Si, 0.65-1.10% Cr, max. 0.040% P, max. 0.040% S, 0.75-1.20% Cr, 0.15-0.25% Mo
0.37-0.44% C, 0.10-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.040% S, 0.75-1.20% Cr, 0.15-0.30% Mo
0.37-0.44% C, 0.10-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.040% S, 0.75-1.20% Cr, 0.15-0.25% Mo
0.37-0.44% C, 0.10-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.040% S, 0.35-0.65% Cr, 0.20-0.30% Mo, 0.35-0.75% Ni
0.37-0.44% C, 0.10-0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S
0.37-0.44% C, 0.15-0.30% Si, 0.65-1.10% Mn, 0.75-1.2% Cr, 0.15-0.30% Mo
0.37-0.44% C, 0.15-0.35% Si, 0.55-0.90% Mn, max. 0.040% P, max. 0.030% S, 0.65-0.95% Cr, 1.55-2.00% Ni, 0.35% Cu, 0.20-0.30% Mo
0.37-0.44% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.30% Mo
0.37-0.44% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu
0.37-0.44% C, 0.15-0.35% Si, 0.60-0.95% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.20-0.30% Mo
0.37-0.44% C, 0.15-0.35% Si, 0.60-0.95% Mn, 0.65-0.95% Cr, 1.55-2.00% Ni, 0.20-0.30% Mo
0.37-0.44% C, 0.15-0.35% Si, 0.60-0.95% Mn, 0.65-0.95% Cr, 1.55-2.00% Ni, 0.20-0.30% Mo
0.37-0.44% C, 0.15-0.35% Si, 0.60-0.95% Mn, max. 0.025% P, max. 0.025% S, 0.65-0.95% Cr, 1.55-2.00% Ni, 0.35% Cu, 0.20-0.30% Mo
0.37-0.44% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.60-1.00% Cr
0.37-0.44% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.60-1.00% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.37-0.44% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.30-0.70% Cr, +B
0.37-0.44% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.75-1.20% Cr, 0.15-0.25% Mo
0.37-0.44% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.30-0.70% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo, 0.0005-0.0030% B
0.37-0.44% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.75-1.20% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.25% Mo
0.37-0.44% C, 0.15-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.37-0.44% C, 0.15-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35% Cu, 0.20-0.30% Mo, 0.35-0.75% Ni
0.37-0.44% C, 0.15-0.35% Si, 1.45-2.05% Mn
0.37-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.60-0.90% Cr, 0.20-0.30% Mo, 1.60-1.90% Ni
0.37-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.60-0.90% Cr, 0.20-0.30% Mo, 1.60-1.90% Ni
0.37-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.60-0.90% Cr, 1.60-1.90% Ni, 0.20-0.30% Mo
0.37-0.44% C, 0.17-0.37% Si, 0.50-0.80% Mn, 0.80-1.10% Cr, 0.10-0.18% V
0.37-0.44% C, 0.17-0.37% Si, 0.50-0.80% Mn, 0.80-1.10% Cr, 0.10-0.18% V
0.37-0.44% C, 0.17-0.37% Si, 0.50-0.85% Mn, max. 0.035% P, max. 0.035% S, 0.70-1.10% Cr, 0.30% Ni, 0.30% Cu
0.37-0.44% C, 0.17-0.37% Si, 0.55-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.85-1.25% Cr, 0.30% Ni, 0.30% Cu, 0.15-0.25% Mo
0.37-0.44% C, 0.20-0.35% Si, 0.50-0.90% Mn, 1.55-2.00% Ni, 0.20-0.30% Mo
0.37-0.44% C, 0.20-0.35% Si, 0.55-0.90% Mn, 0.65-0.95% Cr, 1.55-2.00% Ni, 0.20-0.30% Mo
0.37-0.44% C, 0.20-0.35% Si, 0.56-1.00% Mn, 0.45-0.85% Cr, 1.00-1.45% Ni
0.37-0.44% C, 0.20-0.35% Si, 0.60-0.95% Mn, 0.65-0.95% Cr, 0.80-1.20% Ni, 0.20-0.30% Mo
0.37-0.44% C, 0.20-0.35% Si, 0.60-0.95% Mn, 0.65-0.95% Cr, 1.55-2.00% Ni, 0.20-0.30% Mo
0.37-0.44% C, 0.20-0.35% Si, 0.70-0.90% Mn, max. 0.020% P, max. 0.015% S, 0.70-0.95% Cr, 0.30-0.40% Mo, 1.65-2.00% Ni, 0.005-0.050% Al
0.37-0.44% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.25-0.55% Cr, 0.25-0.65% Ni, 0.08-0.15% Mo, +B
0.37-0.44% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.37-0.44% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.20-0.30% Mo
0.37-0.44% C, 0.25-0.35% Si, 0.70-0.90% Mn, max. 0.020% P, max. 0.015% S, 0.70-0.95% Cr, 0.30-0.40% Mo, 1.65-2.00% Ni, 0.005-0.050% Al
0.37-0.44% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.37-0.44% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.37-0.44% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.37-0.44% C, 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, 0.40% Cr, 0.40% Ni, 0.10% Mo
0.37-0.44% C, 0.65-1.10% Mn, 0.15-0.0.30% Si, 0.75-1.20% Cr, 0.15-0.25% Mo. Steel 4140 RH: 0.38-0.43% C, 0.75-1.10% Mn, 0.15-0.35% Si, 0.80-1.10% Cr, 0.15-0.25% Mo
0.37-0.44% C, 0.65-1.10% Mn, 0.20-0.35% Si, 0.75-1.20% Cr, 0.15-0.25% Mo
0.37-0.44% C, 0.70-1.05% Mn, 0.15-0.30% Si, 0.35-0.75% Ni, 0.35-0.65% Cr, 0.15-0.20% Mo
0.37-0.44% C, 1.45-2.05% Mn, max. 0.035% P, max. 0.035% S, 0.15-0.30% Si
0.37-0.44% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.40% Ni
0.37-0.44% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.37-0.55% C, 0.40% Si, 0.70-1.10% Mn, max. 0.035% P, 0.030% S, 0.90-1.20% Cr, 0.10-0.20% V
0.38% C, 0.19% Si, 0.76% Mn, 0.035% P, 0.050% S, 0.89% Cr, 0.02% Ni, 0.02% Mo, 0.02% V, 0.02% Ti, 0.030% Al, 0.010% N
0.38% C, 0.20% Si, 0.69% Mn, 0.010% S, 0.017% P, 1.58% Ni, 0.95% Cr, 0.26% Mo
0.38% C, 0.23% Si, 0.64% Mn, 0.019% P, 0.013% S, 0.99% Cr, 0.16% Mo
0.38% C, 0.24% Si, 0.72% Mn, 0.013% S, 0.015% P, 0.13% Ni, 0.96% Cr, 0.035% Mo
0.38% C, 0.25% Si, 0.65% Mn, 0.50% Cr
0.38% C, 0.25% Si, 0.65% Mn, 0.80% Cr, 1.80% Ni, 0.35% Mo, 0.10% V
0.38% C, 0.25% Si, 1.49% Mn, 0.028% S, 0.036% P, 0.24% Ni, 0.14% Cr, 0.41% Mo
0.38% C, 0.27% Mn, 0.57% Cr. Blue line: 0.35% C, 0.37% Mn, 0.05% Cr
0.38% C, 0.29% Si, 0.78% Mn, 0.05% P, 0.030% S, 0.99% Cr, 0.14% Ni, 0.08% Mo, 0.06% V, 0.02% Ti, 0.20% Cu, 0.022% Al, 0.010% N
0.38% C, 0.30% Si, 0.76% Mn, 0.046% P, 0.041% S, 0.92% Cr, 0.07% Ni, 0.13% Mo, 0.10% V, 0.085% Al, 0.014% N
0.38% C, 0.72% Mn, 1.32% Ni, 0.49% Cr
0.38% C, 0.85% Si, 0.40% Mn, 4.87% Cr, 0.11% Ni, 1.34% Mo, 0.60% V
0.38% C, 1.08% Mn, 0.70% Si, 0.34% Ni, 0.40% Cr, 0.11% Mo, 0.030% Zr
0.38-0.42% C, 0.150-1.80% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, max. 0.35% Cu
0.38-0.43% C, 0.15-0.35% Si, 0.60-0.80% Mn, max. 0.035% P, max. 0.040% S, 0.70-0.90% Cr, 0.20-0.30% Mo
0.38-0.43% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.025% P, max. 0.030% S, 0.70-0.90% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.38-0.43% C, 0.15-0.35% Si, 0.70-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.38-0.43% C, 0.15-0.35% Si, 0.75-1.00% Mn, max. 0.025% P, max. 0.040% S, 0.40-0.60% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo, 0.0005-0.0030% B
0.38-0.43% C, 0.15-0.35% Si, 0.75-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.80-1.10% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.25% Mo
0.38-0.43% C, 0.15-0.38% Si, 0.60-0.80% Mn, max. 0.035% P, max. 0.040% S, 0.70-0.90% Cr, 0.20-0.30% Mo, 1.65-2.00% Ni
0.38-0.43% C, 0.15-1.35% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.70-0.90% Cr, 0.25% Ni, 0.35% Cu
0.38-0.43% C, 0.15-1.35% Si, 0.75-1.00% Mn, max. 0.035% P, max. 0.040% S, 0.40-0.60% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo, 0.0005-0.0030% B
0.38-0.43% C, 0.15-1.35% Si, 0.75-1.00% Mn, max. 0.035% P, max. 0.040% S, 0.80-1.10% Cr, 0.25% Ni, 0.35% Cu, 0.15-0.25% Mo
0.38-0.43% C, 0.20-0.35% Si, 0.70-0.90% Mn, 0.70-0.90% Cr, 1.10-1.40% Ni
0.38-0.43% C, 0.20-0.50% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 1.50-1.80% Cr, 0.25-0.40% Mo, 0.80-1.20% Al
0.38-0.43% C, 0.40% Si, 0.70-1.00% Mn, 0.015% P, 0.010% S, 0.90-1.10% Cr, 0.20-0.30% Mo, 0.30-0.60% Ni, 0.020-0.040% Al
0.38-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, <0.025% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, <0.025% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr
0.38-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.030% S, 0.90-1.20% Cr, 0.15-0.25% Mo
0.38-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.44% C, 0.15-040% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.030% S, 0.90-1.20% Cr, 0.15-0.25% Mo
0.38-0.44% C, 0.30% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.70-0.90% Cr, 0.15-0.30% Mo, 1.65-2.00% Ni, 0.25% Cu
0.38-0.44% C, 0.30% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.70-0.90% Cr, 0.15-0.30% Mo, 1.65-2.00% Ni, 0.25% Cu
0.38-0.44% C, 0.30% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.70-0.90% Cr, 0.15-0.30% Mo, 1.65-2.00% Ni, 0.25% Cu
0.38-0.45% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.38-0.45% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr
0.38-0.45% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.25% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, 0.020-0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, 0.020-0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, 0.020-0.035% S, 0.90-1.20% Cr
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% S, max. 0.035% S, 1.50-1.80% Cr, 0.20-0.35% Mo, 0.80-1.20% Al
0.38-0.45% C, max. 0.40% Si, 0.60-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, max. 0.40% Si, 0.60-0.90% Mn, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, max. 0.40% Si, 0.60-0.90% Mn, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, max. 0.40% Si, 0.60-0.90% Mn, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.020-0.035% S, 0.90-1.20% Cr
0.38-0.45% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr
0.38-0.45% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr
0.39% C, 0.23% Si, 0.62% Mn, 0.018% S, 0.021% P, 1.44% Ni, 1.11% Cr, 0.18% Mo
0.39% C, 0.23% Si, 0.79% Mn, 0.007% P, 0.033% S, 0.96% Cr, 0.13% Ni, 0.05% Mo, 0.12% V, 0.20% Cu, 0.012% Al, 0.009% N
0.39% C, 0.23% Si, 0.80% Mn, 0.043% P, 0.033% S, 0.93% Cr, 0.02% Ni, 0.31% Mo, 0.02% V, 0.02% Ti, 0.02% Cu
0.39% C, 0.23% Si, 1.61% Mn, 0.001% P, 0.012% S, 0.13% V, 0.060% Ti, 0.003% B, 0.043% Al, 0.010% N, 0.02% Mo
0.39% C, 0.24% Si, 0.75% Mn, 0.040% P, 0.042% S, 0.89% Cr, 0.02% Ni, 0.02% Mo, 0.07% V, 0.02% Ti, 0.034% Al, 0.012% N
0.39% C, 0.26% Si, 0.75% Mn, 0.008% P, 0.033% S, 0.94% Cr, 0.19% Ni, 0.03% Mo, 0.003% V, 0.007% Ti, 0.21% Cu, 0.011% Al, 0.010% N
0.39% C, 0.26% Si, 0.75% Mn, 0.008% P, 0.033% S, 0.94% Cr, 0.19% Ni, 0.03% Mo, 0.003% V, 0.007% Ti, 0.21% Cu, 0.011% Al, 0.010% N
0.39% C, 0.27% Si, 0.75% Mn, 0.006% P, 0.035% S, 0.94% Cr, 0.13% Ni, 0.08% Mo, 0.20% V, 0.20% Cu, 0.024% Al, 0.009% N
0.39% C, 0.28% Si, 0.76% Mn, 0.007% P, 0.033% S, 0.99% Cr, 0.14% Ni, 0.03% Mo, 0.20% V, 0.042% Ti, 0.21% Cu, 0.006% Al, 0.010% N
0.39% C, 0.29% Si, 0.75% Mn, 0.006% P, 0.037% S, 0.97% Cr, 0.13% Ni, 0.02% Mo, 0.19% V, 0.20% Cu, 0.032% Al, 0.010% N
0.39% C, 0.29% Si, 0.76% Mn, 0.006% P, 0.032% S, 0.97% Cr, 0.13% Ni, 0.07% Mo, 0.06% V, 0.066% Ti, 0.20% Cu, 0.020% Al, 0.010% N
0.39% C, 0.29% Si, 0.77% Mn, 0.006% P, 0.034% S, 0.95% Cr, 0.15% Ni, 0.001% V, 0.21% Cu, 0.011% Al, 0.010% N
0.39% C, 0.29% Si, 0.77% Mn, 0.006% P, 0.034% S, 0.95% Cr, 0.15% Ni, 0.20% Mo, 0.001% V, 0.21% Cu, 0.011% Al, 0.010% N
0.39% C, 0.29% Si, 0.77% Mn, 0.006% P, 0.034% S, 0.95% Cr, 0.15% Ni, 0.20% Mo, 0.001% V, 0.21% Cu, 0.011% Al, 0.010% N
0.39% C, 0.30% Si, 0.75% Mn, 0.008% P, 0.033% S, 1.00% Cr, 0.14% Ni, 0.03% Mo, 0.12% V, 0.060% Ti, 0.22% Cu, 0.017% Al, 0.010% N
0.39% C, 0.30% Si, 0.77% Mn, 0.006% P, 0.032% S, 0.96% Cr, 0.14% Ni, 0.08% Mo, 0.05% V, 0.21% Cu, 0.009% Al, 0.010% N
0.39% C, 0.31% Si, 0.82% Mn, 0.031% P, 0.021% S, 0.96% Cr, 0.13% Ni, 0.20% Mo, 0.08% Cu
0.39% C, 0.39% Si, 0.76% Mn, 0.007% P, 0.033% S, 0.99% Cr, 0.14% Ni, 0.03% Mo, 0.12% V, 0.047% Ti, 0.21% Cu, 0.009% Al, 0.010% N
0.39% C, 0.39% Si, 0.76% Mn, 0.007% P, 0.033% S, 1.00% Cr, 0.14% Ni, 0.03% Mo, 0.12% V, 0.047% Ti, 0.21% Cu, 0.009% Al, 0.010% N
0.39% C, 0.72% Si, 0.29% Mn, 0.005% P, 0.013% S, 0.41% Cr, 0.08% V, 0.02% Nb, 0.013 Al, 0.008% N
0.39% C, 0.86% Si, 0.52% Mn, 5.10% Cr, 0.68% V
0.39% C, 0.91% Mn, 0.93% Cr, 0.16% Mo
0.39% C, 1.00% Si, 0.40% Mn, max. 0.030% P, max. 0.010% S, 5.15% % Cr, 1.40% Mo, 0.80% V. Steel DM: 0.55% C, 0.25% Si, 0.85% Mn, max. 0.030% P, max. 0.010% S, 1.65% Ni, 1.20% Cr, 0.35% Mo, 0.15% V
0.39% C, 1.28% Si, 1.08% Mn, 0.001% P, 0.004% S, 0.05% Cr, 0.06% Ni, 0.01% Mo, 0.08% V, 0.060% Ti, 0.07% Nb, 0.002% B, 0.03% Cu, 0.035% Al, 0.018% N
0.39%C, 1.5% Cr, 0.5%Mo, 0.7% V, 0.55% W
0.39-0.44% C, 0.230-0.280% Si, 0.670-0.720% Mn, 0.018-0.029% P, 1.080-1.140% Cr, 0.015-0.030% Al, 0.090-0.130% Ni, 0.180-0.230% Mo, 0.200-0.230% Cu
0.39-0.46% C, 0.10-0.40% Si, 1.30-1.65% Mn, max. 0.035% P, max. 0.035% S
0.39-0.46% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.20-0.30% Mo
0.39-0.46% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.20% Cr, 0.25% Ni, 0.35% Cu, 0.20-0.30% Mo
0.39-0.46% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.75-1.20% Cr, 0.15-0.25% Mo
0.39-0.46% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.75-1.20% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.25% Mo
0.39-0.46% C, 0.15-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.39-0.46% C, 0.15-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.39-0.46% C, 0.15-0.35% Si, 1.30-1.70% Mn, max. 0.030% P, max. 0.030% S, 0.35% Cr, 0.25% Ni, 0.30% Cu
0.39-0.46% C, 0.15-0.35% Si, 1.30-1.70% Mn, max. 0.030% P, max. 0.030% S, 0.35-0.70% Cr, 0.25% Ni, 0.30% Cu
0.39-0.46% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.39-0.46% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.20-0.30% Mo
0.40% C, 0.21% Si, 1.34% Mn, 0.027% S, 0.028% P, 1.03% Ni, 0.53% Cr, 0.22% Mo
0.40% C, 0.24% Si, 1.87% Mn, 0.011% P, 0.013% S, 0.08% Cr, 0.09% Ni, 0.02% Mo, 0.11% Cu, 0.019% Al
0.40% C, 0.25% Si, 0.40% Mn, 1.55% Cr, 4.55% Ni, 0.50% Mo
0.40% C, 0.25% Si, 0.40% Mn, 1.65% Cr, 4.35% Ni
0.40% C, 0.25% Si, 0.65% Mn, <0.03% Cr, + Pb
0.40% C, 0.25% Si, 0.65% Mn, max. 0.030% S, +Pb. Cm40: 0.40% C, 0.25% Si, 0.65% Mn, 0.020-0.035% S, +Pb
0.40% C, 0.25% Si, 0.79% Mn, 0.041% P, 0.033% S, 0.92% Cr, 0.02% Ni, 0.21% Mo, 0.10% V, 0.02% Ti, 0.02% Cu
0.40% C, 0.26% Si, 0.62% Mn, 0.005% S, 0.007% P, 3.45% Ni, 0.28% Cr, 0.10% Mo
0.40% C, 0.26% Si, 0.75% Mn, 0.045% P, 0.040% S, 0.90% Cr, 0.02% Ni, 0.11% Mo, 0.10% V, 0.02% Ti, 0.032% Al, 0.012% N
0.40% C, 0.26% Si, 0.83% Mn, 0.041% P, 0.035% S, 0.91% Cr, 0.03% Ni, 0.22% Mo, 0.29% V, 0.02% Ti, 0.04% Cu
0.40% C, 0.27% Si, 0.75% Mn, 0.007% P, 0.034% S, 0.96% Cr, 0.13% Ni, 0.07% Mo, 0.06% V, 0.035% Ti, 0.20% Cu, 0.014% Al, 0.010% N
0.40% C, 0.29% Si, 0.62% Mn, 0.009% S, 0.012% P, 0.21% Ni, 3.49% Cr, 0.97% Mo, 0.26% V
0.40% C, 0.29% Si, 0.80% Mn, 0.007% P, 0.029% S, 1.00% Cr, 0.13% Ni, 0.13% Mo, 0.15% V, 0.20% Cu, 0.017% Al, 0.009% N
0.40% C, 0.30% Si, 0.60% Mn, 1.60% Cr, 0.35% Mo, 1.20% Al
0.40% C, 0.30% Si, 0.60% Mn, 1.60% Cr, 0.35% Mo, 1.20% Al
0.40% C, 0.30% Si, 0.76% Mn, 0.007% P, 0.029% S, 0.98% Cr, 0.13% Ni, 0.16% Mo, 0.05% V, 0.20% Cu, 0.009% Al, 0.008% N
0.40% C, 0.30% Si, 0.90% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.40% C, 0.30% Si, 0.90% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.40% C, 0.31% Si, 0.89% Mn, 0.11% Cr, 3.34% Ni
0.40% C, 0.34% Si, 1.64% Mn, 0.015% P, 0.032% S, 0.24% Cr, 0.17% Ni, 0.05% Mo, 0.11% V, 0.033% Ti, 0.20% Cu, 0.009% Al, 0.010% N
0.40% C, 0.34% Si, 1.69% Mn, 0.013% P, 0.035% S, 0.17% Cr, 0.13% Ni, 0.09% Mo, 0.07% V, 0.044% Ti, 0.21% Cu, 0.016% Al, 0.010% N
0.40% C, 0.35% Si, 1.00% Mn
0.40% C, 0.40% Si, 1.00% Mn, +Pb
0.40% C, 0.40% Si, 1.00% Mn, +Pb
0.40% C, 0.42% Mn, 0.53% Mo
0.40% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
0.40% C, 0.52% Mn, 5.00% Ni
0.40% C, 0.53% Si, 0.56% Mn, 0.012% P, 0.001% S, 1.65% Cr, 0.23% Mo, 0.21% Ni, 0.15% Cu, 1.10% Al
0.40% C, 1.34% Si, 1.21% Mn, 0.40% Cr
0.40% C, 1.61% Si, 0.74% Mn, 0.93% Cr, 1.92% Ni, 0.47% Mo, 0.70% V
0.40% C, 1.88% Mn
0.40% C, 2.04% Mn, 0.0015% B. Blue lines: 0.40% C, 1.88% Mn, B-none
0.40-0.45% C, 0.15-0.38% Si, 0.75-1.00% Mn, max. 0.035% P, max. 0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo
0.40-0.45% C, 0.15-0.38% Si, 0.75-1.00% Mn, max. 0.035% P, max. 0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo
0.40-0.46% C, 0.15-0.35% Si, 1.30-1.50% Mn, max. 0.035% P, max. 0.035% S, 0.10-0.30% Cr, 0.0010-0.0060% B
0.40-0.46% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, 0.90-1.20% Cr, 0.15-0.30% Mo, max. 0.30% Cu, max. 0.050% Al
0.40-0.46% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, 0.90-1.20% Cr, 0.15-0.30% Mo, max. 0.30% Cu, max. 0.050% Al
0.40-0.46% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, 0.90-1.20% Cr, 0.15-0.30% Mo, max. 0.30% Cu, max. 0.050% Al
0.40-0.50% C, 1.30-1.70% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.40-0.80% Cr, 0.10-0.20% V
0.40-0.50% C, 1.30-1.70% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.40-0.80% Cr, 0.10-0.20% V
0.41% C, <0.40% Si, 0.75% Mn, 1.05% Cr
0.41% C, 0.13% Si, 0.48% Mn, 0.043% S, 0.016% P, 1.75% Ni, 0.17% Cr, 0.22% Mo
0.41% C, 0.23% Si, 0.67% Mn, 0.016% S, 0.015% P, 0.20% Ni, 1.01% Cr, 0.23% Mo
0.41% C, 0.25% Si, 0.65% Mn, 1.05% Cr
0.41% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.41% C, 0.25% Si, 0.81% Mn, 0.043% P, 0.037% S, 0.90% Cr, 0.02% Ni, 0.21% Mo, 0.02% V, 0.02% Ti, 0.02% Cu
0.41% C, 0.26% Si, 0.76% Mn, 0.040% P, 0.041% S, 0.87% Cr, 0.02% Ni, 0.10% Mo, 0.26% V, 0.02% Ti, 0.035% Al, 0.016% N
0.41% C, 0.27% Si, 0.74% Mn, 0.052% P, 0.039% S, 0.91% Cr, 0.02% Ni, 0.11% Mo, 0.10% V, 0.042% Al, 0.014% N
0.41% C, 0.27% Si, 0.81% Mn, 0.044% P, 0.033% S, 0.93% Cr, 0.20% Ni, 0.12% Mo, 0.27% V, 0.02% Ti, 0.22% Cu
0.41% C, 0.28% Si, 0.77% Mn, 0.054% P, 0.038% S, 0.91% Cr, 0.02% Ni, 0.12% Mo, 0.10% V, 0.053% Al, 0.014% N
0.41% C, 0.29% Si, 0.76% Mn, 0.007% P, 0.028% S, 1.11% Cr, 0.13% Ni, 0.06% Mo, 0.10% V, 0.038% Ti, 0.20% Cu, 0.016% Al, 0.010% N
0.41% C, 0.30% Si, 0.70% Mn, 1.10% Cr, 0.20% Mo
0.41% C, 0.30% Si, 0.74% Mn, 0.014% P, 0.015% S, 0.72% Cr, 1.75% Ni, 0.26% Mo, 0.13% Cu
0.41% C, 0.30% Si, 0.74% Mn, 0.039% P, 0.039% S, 0.89% Cr, 0.02% Ni, 0.11% Mo, 0.10% V, 0.055% Ti, 0.033% Al, 0.014% N
0.41% C, 0.30% Si, 0.77% Mn, 0.047% P, 0.042% S, 0.88% Cr, 0.02% Ni, 0.02% Mo, 0.52% V, 0.002% Ti, 0.031% Al, 0.014% N
0.41% C, 0.31% Si, 0.79% Mn, 0.038% P, 0.039% S, 0.02% Cr, 0.02% Ni, 0.11% Mo, 0.30% V, 0.02% Ti, 0.040% Al, 0.012% N
0.41% C, 0.32% Si, 0.79% Mn, 0.045% P, 0.034% S, 0.88% Cr, 0.02% Ni, 0.30% Mo, 0.50% V, 0.02% Ti, 0.032% Al, 0.014% N
0.41% C, 0.32% Si, 0.98% Mn, 1.07% Cr, 0.22% Mo, 0.15% Ni. 4140 steel: 0.42% C, 0.27% Si, 0.97% Mn, 1.04% Cr, 0.18% Mo
0.41% C, 0.33% Si, 0.76% Mn, 0.005% P, 0.033% S, 1.06% Cr, 0.14% Ni, 0.02% Mo, 0.07% V, 0.19% Cu, 0.005% Al, 0.010% N
0.41% C, 0.33% Si, 0.76% Mn, 0.006% P, 0.033% S, 1.06% Cr, 0.14% Ni, 0.02% Mo, 0.07% V, 0.19% Cu, 0.005% Al, 0.010% N
0.41% C, 0.57% Mn, 1.57% Cr, 0.36% Mo, 1.26% Al
0.41% C, 1.60% Si, 0.55% Mn, 0.80% Cr, 1.50% Ni, 0.40% Mo, 0.08% V
0.41% C, max. 0.40% Si, 0.75% Mn, 1.05% Cr, 0.28% Mo
0.41% C, max. 0.40% Si, max. 0.75% Mn, 1.05% Cr
0.41-0.49% C, 0.17-0.37% Si, 0.50-0.80% Mn, 0.80-1.10% Cr
0.41-0.49% C, 0.17-0.37% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr, 0.30% Ni, 0.30% Cu
0.41-0.49% C, 0.17-0.37% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr, max. 0.30% Ni, max. 0.30% Cu
0.42% C, 0.16% Si, 0.68% Mn, 0.83% Cr
0.42% C, 0.20% Mn, 0.21% Mo
0.42% C, 0.22% Si, 0.79% Mn, 0.019% P, 0.023% S, 0.11% Cr, 0.18% Ni, 0.04% Mo, 0.04% Cu
0.42% C, 0.24% Si, 0.77% Mn, 0.040% P, 0.034% S, 0.91% Cr, 0.03% Ni, 0.11% Mo, 0.02% V, 0.02% Cu
0.42% C, 0.24% Si, 0.78% Mn, 0.037% P, 0.033% S, 0.92% Cr, 0.10% Ni, 0.22% Mo, 0.49% V, 0.02% Ti, 0.02% Cu
0.42% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.25% Mo
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr, <0.035% S, + Pb
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr, <0.035% S, +Pb. 41CrS4: 0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.020-0.035% S, +Pb
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.75% Mn, 1.05% Cr, 0.20% Mo
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo, <0.035% S, (Pb). 42CrMoS4: 0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo, 0.020-0.035% S, (Pb)
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.42% C, 0.25% Si, 0.76% Mn, 0.044% P, 0.040% S, 0.02% Cr, 0.02% Ni, 0.11% Mo, 0.10% V, 0.034% Al, 0.010% N
0.42% C, 0.25% Si, 1.80% Mn, 0.10% V
0.42% C, 0.26% Si, 0.79% Mn, 0.052% P, 0.042% S, 0.87% Cr, 0.02% Ni, 0.02% Mo, 0.10% V, 0.030% Al, 0.012% N
0.42% C, 0.29% Si, 0.77% Mn, 0.045% P, 0.040% S, 0.92% Cr, 0.02% Ni, 0.11% Mo, 0.48% V, 0.029% Al, 0.014% N
0.42% C, 0.30% Si, 0.80% Mn, 0.85% Cr, 0.30% Mo, 0.06% V, 1.90% Ni, 0.03% Al
0.42% C, 0.31% Si, 0.67% Mn, 0.022% S, 0.029% P, 2.53% Ni, 0.73% Cr, 0.48% Mo
0.42% C, 0.67% Mn. B14 steel: 0.41% C, 0.64% Mn, 0.0024% B
0.42% C, 0.68% Mn, 0.93% Cr
0.42% C, 0.78% Mn, 1.79% Ni, 0.80% Cr, 0.33% Mo
0.42% C, 0.85% Si, 1.00% Mn, 1.50% Cr, 0.35% V, 0.60% Mo
0.42% C, 1.65% Si, 0.75% Mn, 0.80% Cr, 0.40% Mo, 0.07% V, 1.80% Ni
0.42% C, 1.65% Si, 0.75% Mn, 0.80% Cr, 0.40% Mo, 0.07% V, 1.80% Ni
0.42-0.47% C, 0.50-0.80% Si, 1.30-1.60% Mn, max. 0.035% P, 0.020-0.035% S, 0.10-0.15% V
0.42-0.48% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.40-0.60% Cr
0.42-0.48% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.40-0.60% Cr
0.42-0.48% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.40-0.60% Cr, max. 0.30% Cu
0.42-0.49% C, 0.10-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.040% S, 0.60-1.00% Cr
0.42-0.49% C, 0.10-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.040% S, 0.60-1.00% Cr
0.42-0.49% C, 0.15-0.35% Si, 0.55-0.95% Mn, max. 0.030% P, max. 0.030% S, 0.85-1.25% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.30% Mo
0.42-0.49% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.60-1.00% Cr
0.42-0.49% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.30-0.70% Cr, +B
0.42-0.49% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.75-1.20% Cr, 0.15-0.25% Mo
0.42-0.49% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.75-1.20% Cr, 0.15-0.25% Mo
0.42-0.49% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.30-0.70% Cr, 0.35% Cu, 0.06% Mo, 0.0005-0.0030% B
0.42-0.49% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.75-1.20% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.25% Mo
0.42-0.49% C, 0.15-0.35% Si, 0.70-1.05% Mn, 0.30-0.60% Cr, 0.15-0.45% Ni, 0.08-0.15% Mo, +B
0.42-0.49% C, 0.15-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo, +B
0.42-0.49% C, 0.15-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.42-0.49% C, 0.15-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.30-0.60% Cr, 0.15-0.45% Ni, 0.35% Cu, 0.08-0.15% Mo, 0.0005-0.0030% B
0.42-0.49% C, 0.15-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35% Cu, 0.15-0.25% Mo, 0.0005-0.0030% B
0.42-0.49% C, 0.15-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.42-0.49% C, 0.15-0.35% Si, 1.45-2.05% Mn, max. 0.040% P, max. 0.030% S, 0.20% Cr, max. 0.35% Cu, max. 0.06% Mo, 0.25% Ni
0.42-0.49% C, 0.15-0.35% Si, 1.45-2.05% Mn
0.42-0.49% C, 0.15-0.80% Si, 1.20-1.60% Mn, <0.025% P, 0.020-0.060% S, <0.30% Cr, <0.08% Mo, 0.08-0.20% V, 0.01-0.02% N
0.42-0.49% C, 0.17-0.37% Si, 0.50-0.85% Mn, max. 0.035% P, max. 0.035% S, 0.70-1.10% Cr, 0.30% Ni, 0.30% Cu
0.42-0.49% C, 0.17-0.37% Si, 1.00-1.40% Mn, max. 0.035% P, max. 0.035% S, 0.30% Cr, 0.30% Ni, 0.30% Cu, 0.0005-0.0035% B
0.42-0.49% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.30-0.60% Cr, 0.15-0.45% Ni, 0.08-0.15% Mo, +B
0.42-0.49% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo, +B
0.42-0.49% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.42-0.50% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, 0.020-0.040% S, 0.40-0.60% Cr 0.42-0.50% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63
0.42-0.50% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63
0.42-0.50% C, 0.10-0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S
0.42-0.50% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S
0.42-0.50% C, 0.15-0.40% Si, 0.60-0.80% Mn, max. 0.030% P, max. 0.030% S
0.42-0.50% C, 0.17-0.37% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.25% Cr, 0.30% Ni, 0.25% Cu
0.42-0.50% C, 0.17-0.37% Si, 0.50-0.85% Mn, max. 0.035% P, max. 0.035% S, 0.25% Cr, 0.30% Ni, 0.30% Cu
0.42-0.50% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.25% Cu
0.42-0.50% C, 0.30% Si, 0.50-0.80% Mn, max. 0.025% P, 0.020-0.035% S, 0.25% Cu
0.42-0.50% C, 0.30% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 0.25% Cu
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.030% S, 0.40-0.60% Cr, 0.30% Cu
0.42-0.50% C, 1.30-1.70% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 0.50-0.80% Cr, 0.20-0.30% Mo
0.42-0.50% C, 1.30-1.70% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 0.50-0.80% Cr, 0.20-0.30% Mo
0.42-0.50% C, 1.30-1.70% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 0.50-0.80% Cr, 0.20-0.30% Mo
0.42-0.50% C, max. 0.30% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Cu
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, 0.020-0.035% S, max. 0.25% Cu
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.40-0.60% Cr
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.40-0.60% Cr
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.42-0.51% C, 0.15-0.35% Si, 0.50-1.00% Mn, max. 0.030% P, max. 0.050% S
0.42-0.51% C, 0.15-0.35% Si, 0.50-1.00% Mn
0.42-0.52% C, 1.50-2.00% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S
0.42-9.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.43% C, 0.27% Si, 0.75% Mn, 0.010% P, 0.033% S, 0.90% Cr, 0.21% Ni, 0.11% Mo, 0.26% V, 0.02% Ti, 0.22% Cu
0.43% C, 0.29% Si, 0.80% Mn, 0.007% P, 0.029% S, 1.16% Cr, 0.13% Ni, 0.10% Mo, 0.10% V, 0.039% Ti, 0.20% Cu, 0.023% Al, 0.009% N
0.43% C, 0.30% Si, 1.78% Mn, 0.019% P, 0.017% S, 0.10% V
0.43% C, 0.74% Mn, 0.92% Cr, 0.16% V
0.43% C, 0.90% Si, 0.32% Mn, 0.011% P, 0.046% S, 0.30% Cr, 0.10% V, 0.03% Nb, 0.015% Al, 0.015% N
0.43% C, 1.3% Cr, 0.7% Mo, 0.23% V
0.43% C, 1.55% Si, 0.63% Mn, 0.91% Cr, 0.40% Mo, 0.12% V, 0.063% Al
0.43% C, 1.58% Mn
0.43-0.48% C, 0.15-0.35% Si, 0.75-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.80-1.10% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.25% Mo
0.43-0.48% C, 0.15-1.35% Si, 0.75-1.00% Mn, max. 0.035% P, max. 0.040% S, 0.80-1.10% Cr, 0.25% Ni, 0.35% Cu, 0.15-0.25% Mo
0.43-0.49% C, 0.15-0.35% Si, 0.50-0.80% Mn, <0.025% P, <0.035% S
0.43-0.49% C, 0.15-0.35% Si, 0.50-0.80% Mn, <0.025% P, <0.035% S
0.43-0.49% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S
0.43-0.49% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S
0.43-0.50% C, 0.10-0.35% Si, 0.30-0.90% Mn, <0.040% P, <0.040% S
0.43-0.50% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.13-0.43% Cr, + B
0.43-0.50% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.13-0.43% Cr
0.43-0.50% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.13-0.40% Cr, 0.35% Cu, 0.06% Mo, 0.0005-0.0030% B
0.43-0.50% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.13-0.43% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.43-0.53% C, 0.15-0.35% Si, 1.00-1.50% Mn, max. 0.030% P, max. 0.050% S, 0.0005-0.0030% B
0.43-0.55% C, 0.15-0.35% Si, 1.00-1.50% Mn, +B
0.44% C, 0.26% Si, 0.75% Mn, 0.016% P, 0.019% S, 1.70% Cr, 0.08% Mo, 0.17% Ni, 0.090% V, 0.18% Cu
0.44% C, 0.29% Si, 1.30% Mn, 0.020% P, 0.025% S, 0.08% Cr, 0.02% Ni, 0.14% Cu
0.44% C, 0.31% Si, 0.78% Mn, 0.007% P, 0.029% S, 1.19% Cr, 0.13% Ni, 0.06% Mo, 0.06% V, 0.032% Ti, 0.20% Cu, 0.015% Al, 0.008% N
0.44% C, 0.51% Si, 0.42% Mn, 1.39% Cr, 1.48% Mo, 1.01% V, 1.70% W
0.44% C, 0.90% Mn, 0.45% Ni, 0.54% Cr, 0.22% Mo
0.44-0.51% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.20-0.30% Mo
0.44-0.51% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.20% Cr, 0.25% Ni, 0.35% Cu, 0.20-0.30% Mo
0.44-0.51% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.75-1.20% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.25% Mo
0.45% C, 0.19% Si, 0.65% Mn, 0.017% S, 0.016% P, 0.23% Ni, 0.31% Cr, 0.07% Mo, 0.20% V
0.45% C, 0.20% Si, 0.70% Mn, <0.025% P, <0.025% S, <0.25% Cu
0.45% C, 0.25% Si, 0.65% Mn, max. 0.030% S, +Pb. Cm45: 0.45% C, 0.25% Si, 0.65% Mn, 0.020-0.035% S, +Pb
0.45% C, 0.25% Si, 0.65% Mn
0.45% C, 0.25% Si, 0.65% Mn
0.45% C, 0.25% Si, 0.65% Mn
0.45% C, 0.35% Si, 1.04% Mn, 0.03% P, 0.012% S, 1.22% Cr, 0.55% Ni, 0.05% Mo, 0.13% V, 0.16% Cu
0.45% C, 0.50% Si, 1.20% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.08% Mo, 0.30% Ni, 0.020% Al, 0.012% N
0.45-0.52% C, 0.15-0.35% Si, 0.60-1.05% Mn, 0.80-1.25% Cr
0.45-0.52% C, 0.15-0.35% Si, 0.60-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.80-1.25% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.45-0.52% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.030% S
0.455% C, 0.275% Si, 0.875% Mn, 0.975% Cr, 0.20% Mo
0.46% C, 0.23% Si, 0.68% Mn, 0.003% P, 0.016% S, 0.82% Cr, 1.75% Ni, 0.11% Mo, 0.17% V, 0.003% Ti, 0.04% Cu, 0.066% Al, 0.012% N
0.46% C, 0.25% Si, 0.65% Mn, 0.50% Cr
0.46% C, 0.99% Mn
0.46% C, 1.80% Si, 0.70% Mn
0.46% C, 1.80% Si, 0.70% Mn
0.46% C, 1.80% Si, 0.70% Mn
0.46-0.50% C, 0.15-0.30% Si, 0.70-0.85% Mn, max. 0.015% P, 0.010-0.025% S, 1.00-1.20% Cr, 0.40-0.50% Ni, 0.90-1.00% Mo, 0.10-0.14% V
0.46-0.52% C, <0.40% Si, 0.50-0.80% Mn, <0.025% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.52% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.52% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.52% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, max. 0.30% Cu
0.46-0.54% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.030% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, 1.40-1.80% Si, 0.70-1.10% Mn, 0.025% P, 0.025% S, 0.80-1.10% Cr, 0.20-0.35% Mo
0.46-0.54% C, 1.40-1.80% Si, 0.70-1.10% Mn, 0.025% P, 0.025% S, 0.80-1.10% Cr, 0.20-0.35% Mo
0.46-0.54% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.47% C, 0.28% Si, 0.77% Mn, 0.01% P, 0.07% S, 0.03% Cr, 0.01% Ni, 0.02% Cu
0.47% C, 0.46% Mn
0.47-0.54% C, 0.10-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.040% S, 0.75-1.20% Cr, 0.15-0.25% V
0.47-0.54% C, 0.10-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.040% S, 0.75-1.20% Cr, 0.15-0.25% Mo
0.47-0.54% C, 0.10-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.040% S, 0.75-1.20% Cr, 0.15-0.25% Mo
0.47-0.54% C, 0.15-0.35% Si, 0.60-0.80% Mn, max. 0.040% P, max. 0.030% S, 0.75-1.20% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.47-0.54% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.60-1.00% Cr
0.47-0.54% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.75-1.20% Cr, min. 0.15% V
0.47-0.54% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.60-1.00% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.47-0.54% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.040% S, 0.75-1.20% Cr, 0.15-0.25% Mo
0.47-0.54% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.30-0.70% Cr, + B
0.47-0.54% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.75-1.20% Cr, 0.15-0.25% Mo
0.47-0.54% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.30-0.70% Cr, 0.35% Cu, 0.06% Mo, 0.0005-0.0030% B
0.47-0.54% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.75-1.20% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.25% Mo
0.47-0.54% C, 0.15-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.47-0.54% C, 0.15-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.47-0.54% C, 0.20-0.35% Si, 0.60-0.95% Mn, 0.65-0.95% Cr, 0.80-1.20% Ni, 0.20-0.30% Mo
0.47-0.54% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.47-0.55% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, <0.40% Si, 0.70-1.10% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S
0.47-0.55% C, 0.15-0.35% Si, 0.80-1.10% Mn, max. 0.030% P, max. 0.030% S, 0.90-1.20% Cr, 0.10-0.20% V
0.47-0.55% C, 0.15-0.40% Si, 0.70-1.10% Mn, 0.80-1.20% Cr, 0.07-0.12% V
0.47-0.55% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.47-0.55% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.47-0.55% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.47-0.55% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.47-0.55% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.47-0.55% C, max. 0.40% Si, 0.70-1.10% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, 0.10-0.25% V
0.48% C, 0.57% Mn, 0.46% Cu. Blue lines: 0.47% C, 0.57% Mn, 0.06% Cu
0.48% C, 0.94% Mn, 0.25% Mo
0.48-0.53% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.80-1.10% Cr, max. 0.15% V
0.48-0.53% C, 0.15-0.38% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.80-1.10% Cr, max. 0.15% V
0.48-0.54% C, max. 0.40% Si, 0.70-1.10% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.10-0.20% V
0.48-0.55% C, 0.15-0.35% Si, 1.60-1.90% Mn, max. 0.035% P, max. 0.035% S, 0.07-0.12% V
0.48-0.55% C, 0.17-0.37% Si, 0.80-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.95-1.10% Cr, 0.15-0.25% V
0.48-0.56% C, max. 0.40% Si, 0.70-1.10% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.10-0.20% V
0.49% C, 0.23% Si, 0.90% Mn, 0.016% P, 0.010% S, 1.03% Cr, 0.12% V
0.49% C, 0.24% Si, 0.68% Mn, 0.003% P, 0.015% S, 0.80% Cr, 1.74% Ni, 0.01% Mo, 0.25% V, 0.007% Ti, 0.04% Cu, 0.054% Al, 0.013% N
0.49% C, 0.25% Si, 0.65% Mn, 0.003% P, 0.018% S, 0.80% Cr, 1.71% Ni, 0.01% Mo, 0.25% V, 0.003% Ti, 0.04% Cu, 0.057% Al, 0.012% N
0.49% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.20% Mo
0.49% C, 0.54% Mn, 1.49% Cu
0.49% C, 1.98% Si, 0.90% Mn, 0.047% S, 0.044% P
0.49-0.56% C, 1.20-1.50% Si, 0.70-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr, 0.50-0.70% Ni
0.49-0.56% C, 1.20-1.50% Si, 0.70-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr, 0.50-0.70% Ni
0.49-0.56% C, 1.20-1.50% Si, 0.70-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr, 0.50-0.70% Ni
0.49-0.56% C, 1.20-1.50% Si, 0.70-0.90% Mn, 0.70-1.00% Cr, 0.50-0.70% Ni
0.49-0.56% C, 1.20-1.50% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.70-1.00% Cr, 0.50-0.70% Ni
0.50% C, <0.40% Si, 1.80% Mn
0.50% C, 0.23% Mn, 0.53% Si, 0.05% Cr
0.50% C, 0.25% Si, 0.65% Mn, 1.005% Cr, 0.25% Mo
0.50% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.20% Mo, + Pb
0.50% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.20% Mo, (Pb)
0.50% C, 0.25% Si, 0.75% Mn, <0.03% S, + Pb
0.50% C, 0.25% Si, 0.75% Mn, <0.03% S, +Pb. Cm50: 0.50% C, 0.25% Si, 0.75% Mn, 0.020-0.035% S, +Pb
0.50% C, 0.25% Si, 0.90% Mn, 1.05% Cr, 0.15% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V, + Pb
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V, +Pb
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.25% Mo, 0.10% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.25% Mo, 0.10% V
0.50% C, 0.80% Cr, 0.20% V
0.50% C, 0.80% Cr, and 0.20% V
0.50% C, 0.91% Mn
0.50% C, 1.00% Si, 0.40% Mn, 0.50% Mo
0.50-0.52% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, 0.030-0.050% S, 0.90-1.20% Cr, 0.18-0.25% Ni, 0.18-0.25% Mo
0.50-0.57% C, 0.15-0.35% Si, 0.40-0.70% Mn, <0.025% P, <0.035% S
0.50-0.57% C, 0.15-0.35% Si, 0.40-0.70% Mn, <0.025% P, <0.035% S
0.50-0.57% C, 0.15-0.35% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S
0.50-0.57% C, 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S
0.50-0.57% C, 0.80-1.00% Si, 0.80-1.20% Mn, max. 0.035% P, max. 0.035% S
0.50-0.57% C, 0.80-1.00% Si, 0.80-1.20% Mn, max. 0.035% P, max. 0.035% S
0.50-0.60% C, 0.15-0.25% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.50-0.60% C, 0.15-0.35% Si, 0.60-1.00% Mn, 0.60-1.00% Cr
0.50-0.60% C, 0.15-0.35% Si, 0.60-1.00% Mn, max. 0.040% P, max. 0.030% S, 0.60-1.00% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.50-0.60% C, 0.15-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.50-0.60% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.45-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.50-0.60% C, 0.20-0.60% Si, 1.00-1.25% Mn, <0.025% P, 0.08-0.025% S, <0.15% Cr, <0.02% Mo, <0.10% Ni, <0.030% V, <0.004% Al
0.50-0.60% C, 0.20-0.60% Si, 1.00-1.25% Mn, <0.025% P, 0.08-0.025% S, <0.15% Cr, <0.02% Mo, <0.10% Ni, <0.030% V, <0.004% Al
0.50-0.60% C, 1.20-1.60% Si, 0.50-0.90% Mn, max. 0.030% P, max. 0.025% S, 0.50-0.80% Cr, 0.12% Cu
0.505% C, 0.275% Si, 0.80% Mn, 0.975% Cr, 0.075% V
0.51% C, <0.40% Si, 0.90% Mn, 1.05% Cr, 0.18% V
0.51% C, 0.22% Si, 0.67% Mn, 0.005% P, 0.015% S, 0.81% Cr, 1.74% Ni, 0.11% Mo, 0.16% V, 0.085% Ti, 0.03% Cu, 0.098% Al, 0.011% N
0.51% C, 0.25% Mn, 3.80% Si, 0.32% Cr
0.51% C, 0.27% Si, 0.72% Mn, 0.020% S, 0.021% P, 0.15% Ni, 0.94% Cr, 0.05% Mo, 0.20% V
0.51% C, 1.75% Si, 0.70% Mn
0.51-0.56% C, 0.25-0.40% Si, 0.94-1.10% Mn, max. 0.015% P, max. 0.015% S, 1.02-1.12% Cr, max. 0.20% Ni, 0.15-0.20% Mo, 0.10-0.12% V, max. 0.040% Ti, max. 0.21% Cu
0.51-0.59% C, 1.20-1.60% Si, 0.50-0.80% Mn, 0.030% P, 0.030% S, 0.50-0.80% Cr
0.51-0.59% C, 1.20-1.60% Si, 0.50-0.80% Mn, 0.030% P, 0.030% S, 0.50-0.80% Cr
0.51-0.59% C, 1.20-1.60% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 0.50-0.80% Cr, 0.10-0.20% V
0.51-0.59% C, 1.20-1.60% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 0.50-0.80% Cr, 0.10-0.20% V
0.51-0.59% C, 1.20-1.60% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 0.50-0.80% Cr
0.52% C, 0.25% Si, 1.75% Mn, 0.10% V
0.52-0.50% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.59% C, max. 0.40% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.70-1.00% Cr
0.52-0.59% C, max. 0.40% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.70-1.00% Cr
0.52-0.59% C, max. 0.40% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.70-1.00% Cr
0.52-0.60% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63
0.52-0.60% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63
0.52-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S
0.52-0.60% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.60% C, 1.60-1.20% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S
0.52-0.60% C, 1.60-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.60% C, 1.60-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.60% C, 1.60-2.00% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S
0.52-0.60% C, 1.60-2.00% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.010-0.040% Al
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, max. 0.30% Cu, max. 0.050% Al
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.53% C, 0.03% Si, 0.43% Mn, 0.030% P, 0.035% S, 0.02% Al
0.53% C, 0.24% Mn, 2.32% Si, 0.32% Cr
0.53% C, 0.25% Si, 0.55% Mn
0.53% C, 0.25% Si, 0.55% Mn
0.53% C, 0.28% Si, 0.20% Mn, 2.00% W, 1.65% Cr, and 0.25% V
0.53% C, 0.67% Mn, 0.93% Cr, 0.18% V
0.53% C, 0.67% Mn, 0.93% Cr, 0.18% V
0.53-0.55% C, 1.60-1.80% Si, 0.70-0.80% Mn, max. 0.025% P, max. 0.015% S, 0.20-0.30% Cr
0.53-0.56% C, 0.15-0.30% Si, 0.75-0.85% Mn, max. 0.015% P, max. 0.015% S, 0.70-0.80% Cr, 0.010-0.030% Ti, 0.015-0.035% Al, 0.025-0.035% Nb
0.53-0.59% C, 1.60-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr
0.53-0.59% C, 1.60-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr
0.53-0.59% C, 1.60-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr
0.54% C, 0.23% Mn, 1.27% Si, 0.05% Cr
0.54-0.67% C, 0.40-0.60% Si, 1.00-1.50% Mn, +B
0.55% C, 0.22% Si, 0.98% Mn, 0.017% P, 0.013% S, 1.02% Cr, 0.01% Ni, 0.07% Cu, 0.11% V
0.55% C, 0.25% Si, 0.75% Mn, <0.03% S, +Pb. Cm55: 0.55% C, 0.25% Si, 0.75% Mn, 0.020-0.035% S, +Pb
0.55% C, 0.25% Si, 0.75% Mn, 0.020-0.035% S, + Pb
0.55% C, 0.28% Si, 0.65% Mn, 0.038% S, 0.027% P, 0.08% Cr, 0.05% Mo
0.55% C, 0.60% Mn, 1.03% Cr, 0.19% Mo, 0.36% Ni
0.55% C, 1.00% Si, 1.00% Mn, 0.50% Cr, 2.70% Ni, 0.50% Mo, 0.10% V
0.55% C, 2.00% Si, 0.85% Mn, 0.25% Cr. Steel 2: 0.50% C, 1.50% Si, 0.70% Mn, 0.40% Mo, 0.12% V. Steel 3: 0.55% C, 2.00% Si, 0.90% Mn, 0.25% Cr, 1.20% Mo, 0.25% V.
0.55-0.62% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.55-0.62% C, 0.15-0.40% Si, 0.70-1.10% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.10-0.20% V
0.55-0.62% C, 0.15-0.40% Si, 0.70-1.10% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.10-0.20% V
0.55-0.63% C, 1.60-2.00% Si, 0.60-1.00% Mn, max. 0.030% P, max. 0.030% S
0.55-0.65% C, 0.10-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.040% S, 0.35-0.65% Cr, 0.15-0.25% Mo, 0.35-0.75% Ni
0.55-0.65% C, 0.10-0.35% Si, 0.60-0.95% Mn, max. 0.040% P, max. 0.040% S, 0.35-0.65% Cr, 0.15-0.25% Mo, 0.35-0.75% Ni
0.55-0.65% C, 0.10-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.040% S, 0.35-0.65% Cr, 0.15-0.25% Mo, 0.35-0.75% Ni
0.55-0.65% C, 0.10-0.40% Si, 0.70-1.00% Mn, 0.025% P, 0.025% S, 0.60-0.90% Cr
0.55-0.65% C, 0.10-0.40% Si, 0.70-1.00% Mn, 0.025% P, 0.025% S, 0.60-0.90% Cr
0.55-0.65% C, 0.15-0.25% Si, 0.70-1.05% Mn, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.55-0.65% C, 0.15-0.30% Si, 0.65-1.10% Mn, max. 0.035% P, max. 0.040% S, 0.60-1.00% Cr
0.55-0.65% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.30-0.70% Cr, +B
0.55-0.65% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.60-1.00% Cr, +B
0.55-0.65% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.60-1.00% Cr
0.55-0.65% C, 0.15-0.35% Si, 0.65-1.10% Mn, 0.65-0.95% Cr, 0.25-0.35% Mo
0.55-0.65% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.30-0.70% Cr, 0.35% Cu, 0.06% Mo, 0.0005-0.0030% B
0.55-0.65% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.60-1.00% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo, 0.0005-0.0030% B
0.55-0.65% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.60-1.00% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.55-0.65% C, 0.15-0.35% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.65-0.95% Cr, 0.25% Ni, 0.30% Cu, 0.15-0.25% Mo
0.55-0.65% C, 0.15-0.35% Si, 0.70-1.05% Mn, max. 0.040% P, max. 0.030% S, 0.35-0.65% Cr, 0.35-0.75% Ni, 0.35% Cu, 0.15-0.25% Mo
0.55-0.65% C, 0.20-0.35% Si, 0.70-1.05% Mn, 0.45-0.65% Cr, 0.35-0.75% Ni, 0.15-0.25% Mo
0.55-0.65% C, 1.70-2.20% Si, 0.65-1.00% Mn, max. 0.050% P, max. 0.050% S
0.55-0.65% C, 1.70-2.20% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.20% Cr, 0.35% Cu, 0.06% Mo, 0.25% Ni
0.55-0.65% C, 1.70-2.20% Si, 0.65-1.10% Mn, max. 0.050% P, max. 0.050% S, 0.05-0.35% Cr
0.55-0.65% C, 1.70-2.20% Si, 0.65-1.10% Mn, max. 0.050% P, max. 0.050% S
0.55-0.65% C, 1.70-2.20% Si, 0.65-1.10% Mn. max. 0.050% P, max. 0.050% S, 0.05-0.35% Cr
0.55-0.65% C, 1.70-2.20% Si, 0.65-1.10% Mn
0.55-0.65% C, 1.80-2.20% Si, 0.70-1.00% Mn, max. 0.035% P, max. 0.035% S, 0.30% Cr, 0.25% Ni, 0.20% Cu
0.56% C, <0.40% Si, 0.75% Mn, <0.40% Cr, <0.10% Mo, <0.40% Ni, (Cr+Mo+Ni) = max. 0.63
0.56% C, 0.26% Mn, 1.97% Ni
0.56% C, 2.02% Si, 0.94% Mn, 0.045% S, 0.036% P, 0.19% Ni, 0.10% Cr, 0.12% Mo
0.56-0.64% C, 0.15-0.35% Si, 0.75-1.00% Mn, max. 0.025% P, max. 0.040% S, 0.75-0.90% Cr, 0.25% Ni, 0.35% Cu, 0.25-0.35% Mo
0.56-0.64% C, 0.15-0.35% Si, 0.75-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.70-0.90% Cr, 0.25% Ni, 0.35% Cu, 0.06% Mo
0.56-0.64% C, 0.15-0.40% Si, 0.70-1.00% Mn, max. 0.030% P, max. 0.030% S, 0.60-0.90% Cr
0.56-0.64% C, 0.15-0.40% Si, 0.70-1.00% Mn, max. 0.030% P, max. 0.030% S, 0.70-1.00% Cr, 0.08-0.15% Mo
0.56-0.64% C, 0.15-1.35% Si, 0.71-1.00% Mn, max. 0.035% P, max. 0.040% S, 0.70-0.90% Cr, 0.25% Ni, 0.35% Cu
0.56-0.64% C, 0.40% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.70-1.00% Cr, 0.06-0.15% Mo
0.56-0.64% C, 0.40% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.70-1.00% Cr, 0.15-0.25% Mo
0.56-0.64% C, 0.40% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.70-1.00% Cr, 0.15-0.25% Mo
0.56-0.64% C, 0.40% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.70-1.00% Cr, 0.25-0.35% Mo
0.56-0.64% C, 0.40% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.70-1.00% Cr, 0.25-0.35% Mo
0.56-0.64% C, 0.40% Si, 0.70-1.00% Mn, max. 0.030% P, max. 0.030% S, 0.70-1.00% Cr, 0.25-0.35% Mo
0.56-0.64% C, 0.70-1.20% Si, 0.65-1.10% Mn, max. 0.040% P, max. 0.030% S, 0.45-0.65% Cr, 0.35% Cu, 0.06% Mo, 0.25% Ni
0.56-0.64% C, max. 0.40% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.70-1.00% Cr, 0.06-0.15% Mo
0.57% C, 0.30% Si, 0.85% Mn
0.57% C, 1.00% Si, 0.95% Mn, 0.12% Mo, 0.16% V
0.57-0.63% C, 0.50-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr, 0.07-0.25% V
0.57-0.63% C, 0.50-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr, 0.07-0.25% V
0.57-0.64% C, 1.60-2.00% Si, 0.70-1.00% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr
0.57-0.64% C, 1.60-2.00% Si, 0.70-1.00% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr
0.57-0.64% C, 1.60-2.00% Si, 0.70-1.00% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr
0.57-0.64% C, 1.70-2.20% Si, 0.70-1.00% Mn, max. 0.035% P, max. 0.035% S, 0.25-0.40% Cr
0.57-0.65% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63
0.57-0.65% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63
0.57-0.65% C, <0.40% Si, 0.60-0.90% Mn, <0.045% P, <0.040% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=<0.63
0.57-0.65% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S
0.57-0.65% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.57-0.65% C, 0.60-2.00% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.20-0.45% Cr
0.57-0.65% C, 1.50-2.00% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.30% Cr, 0.25% Ni, 0.20% Cu
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V, + Pb
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V. +Pb
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V
0.58% C, 0.29% Si, 0.91% Mn, 0.014% P, 0.016% S, 0.78% Cr, 0.07% Ni, 0.01% Mo, 0.05% Cu, 0.023% Al
0.58% C, 0.90% Si, 1.00% Mn, +Pb
0.58% C, 0.90% Si, 1.00% Mn
0.58% C, 1.75% Si, 0.75% Mn, 0.40% Cr
0.58% C, 1.75% Si, 0.75% Mn, 0.40% Cr
0.58% C, 1.75% Si, 0.80% Mn
0.58-0.61% C, 0.11-0.55% Si, 0.55-0.65% Mn, max. 0.020% P, max. 0.007% S, 0.15-0.22% Cr, max. 0.15% Ni, max. 0.08% Mo
0.59% C, 0.25% Mn, 3.90% Ni
0.59% C, 0.34% Si, 0.66% Mn, 0.012% S, 0.020% P, 0.17% Ni, 0.65% Cr, 0.02% Mo
0.59% C, 0.89% Mn, 0.53% Ni, 0.64% Cr, 0.22% Mo
0.59-0.64% C, 1.60-1.80% Si, 0.70-0.90% Mn, 0.035% P, 0.025% S, 0.20-0.40% Cr
0.60% C, 0.25% Si, 0.75% Mn, <0.03% S, +Pb. Cm60: 0.60% C, 0.25% Si, 0.75% Mn, 0.020-0.035% S, +Pb
0.60% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
0.60% C, 0.50% Si, 1.20% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.08% Mo, 0.30% Ni, 0.020% Al, 0.012% N
0.60% C, 0.52% Mn, 5.00% Ni
0.60% C, 0.80% Cr, and 0.20% V
0.60% C, 1.88% Mn
0.60% C, 2.00% Si, 0.85% Mn, 0.25% Cr, 0.25% Mo, 0.20% V. Steel 2: 0.57% C, 1.90% Si, 0.85% Mn, 0.25% Cr, 0.33% Mo
0.60-0.70% C, 1.50-1.80% Si, 0.70-1.00% Mn, max. 0.035% P, max. 0.035% S
0.60-0.70% C, 1.50-1.80% Si, 0.70-1.00% Mn, max. 0.035% P, max. 0.035% S
0.61% C, <0.40% Si, 0.75% Mn, <0.40% Cr, <0.10% Mo, <0.40% Ni
0.61% C, 0.27% Mn, 0.99% Ni
0.62% C, 0.26% Si, 0.69% Mn, 0.026% S, 0.019% P, 0.45% Ni, 0.15% Cr, 0.10% Mo
0.62% C, 0.64% Mn, 0.67% Si, 1.79% Ni, 0.60% Cr, 0.32% Mo
0.62% C, 0.82% Mn, 2.01% Si, 0.07% Cr
0.62% C, 0.86% Mn, 2.13% Si, 0.33% Cr
0.62% C, 0.95% Mn, 2.01% Si, 0.15% Cr
0.63% C, 0.87% Mn
0.63% C, 0.87% Mn
0.63-0.70% C, 0.20-0.35% S, 0.75-1.00% Mn, max. 0.040% P, max. 0.040% S
0.63-0.70% C, 0.20-0.35% Si, 0.75-1.00% Mn, max. 0.040% P, max. 0.040% S, 0.20-0.30% Mo
0.63-0.70% C, 1.40-1.60% Si, 1.35-1.55% Mn, 0.025% P, 0.002% S, 1.00-1.20% Cr, 0.23-0.27% Mo, 0.25% Ni
0.64% C, 0.87% Mn, 0.0018% B. 0.63% C, 0.87% Mn, B-none
0.64% C, 1.13% Mn
0.65% C, 0.25% Si, 0.75% Mn, 0.020-0.035% S, + Pb
0.65% C, 0.68% Mn, 0.10% Mo. Blue line: 0.64% C, 0.68% Mn, 0.00% Mn
0.65% C, 1.75% Si, 0.80% Mn
0.65% C, 1.75% Si, 0.80% Mn
0.65% C, 1.75% Si, 0.80% Mn
0.65-0.75% C, <0.40% Si, 0.60-1.10% Mn, <0.035% P, <0.035% S
0.65-0.75% C, <0.40% Si, 0.60-1.10% Mn, <0.035% P, <0.035% S
0.65-0.75% C, 0.15-0.35% Si, 0.20-1.10% Mn, <0.025% P, <0.035% S
0.65-0.75% C, 0.15-0.35% Si, 0.20-1.10% Mn, <0.025% P, <0.035% S
0.67% C, 1.31% Si, 0.49% Mn, 0.016% P, 0.024% S, 0.48% Cr, 0.47% Ni, 0.25% Cu, 0.08% Mo, 0.024% Sn
0.68% C, 0.25% Si, 0.60% Mn, 0.65% Cr, 1.40% Ni, 0.20% Mo
0.68% C, 0.87% Mn, 0.24% Mo
0.68-0.75% C, 0.15-0.35% Si, 0.20-0.35% Mn, max. 0.025% P, max. 0.035% S
0.68-0.75% C, 0.15-0.35% Si, 0.20-0.35% Mn, max. 0.025% P, max. 0.035% S
0.68-0.75% C, 0.15-0.35% Si, 0.20-0.35% Mn, max. 0.025% P, max. 0.035% S
0.7% C, 0.80% Cr, and 0.20% V
0.70% C, 0.25% Si, 0.30% Mn
0.70% C, 0.28% Si, 0.41% Mn, 0.28% Cr, 0.91% Ni, 0.11% Mo
0.70% C, 0.55% Mn, 0.85% Cr, 1.40% Ni, and 0.25% Mo
0.72-0.80% C, 0.15-0.58% Si, 0.70-1.20% Mn, <0.020% P, 0.08-0.025% S, <0.15% Cr, <0.02% Mo, <0.10% Ni, <0.030% V, <0.004% Al
0.73% C, 1.62% Si, 0.73% Mn, 0.019% P, 0.018% S, 0.10% Cr, 0.19% Cu, 0.12% Ni, 0.01% V
0.75% C, 0.25% Si, 0.70% Mn, <0.035% S
0.75-0.85% C, 0.20-0.30% Si, 0.45-0.55% Mn, max. 0.025% P, max. 0.025% S, 0.10-0.20% Cr, 0.10-02.0% Ni, 0.05% V
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.79% C, 0.76% Mn
0.80% C, 0.80% Cr, and 0.20% V
0.80% C, 2.04% Mn, 0.0015% B. Blue lines: 0.80% C, 1.88% Mn, B-none
0.80% Mn, 0.55% Ni, 0.5% Cr, 0.2% Mo
0.80-0.90% C, 0.15-0.35% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.025% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.80-0.90% C, 0.20-0.30% Si, 0.50-0.85% Mn, max. 0.025% P, max. 0.025% S, 0.10-0.20% Cr, 0.10-0.20% Ni, 0.05% V
0.85% C, 0.25% Si, 0.65% Mn
0.85% C, 0.25% Si, 0.65% Mn
0.86% C, 0.24% Si, 2.06% Mn, 0.023% P, 0.010% S, 0.28% Cr, 0.079% V
0.87% C, 0.30% Mn, 0.27% V. Blue lines: 0.87% C, 0.30% Mn, 0.27% V
0.87% C, 0.30% Mn, 0.27% V. Blue lines: 0.89% C, 0.29% Mn
0.89% C, 0.19% Si, 0.39% Mn, 1.58% Cr, 4.00% Ni. Core: 0.15% C, 0.20% Si, 0.45% Mn, 1.54% Cr, 4.03% Ni
0.89% C, 0.29% Mn
0.90% C, 0.21% Si, 0.50% Mn, 3.36% Ni. Core: 0.13% C, 0.21% Si, 0.50% Mn, 3.36% Ni
0.90-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, max. 0.030% P, max. 0.025% S, 0.40-0.60% Cr
0.90-1.05% C, 0.50-0.70% Si, 1.00-1.20% Mn, max. 0.030% P, max. 0.025% S, 1.40-1.65% Cr, max. 0.30% Ni, max. 0.30% Cu
0.91% C, 0.23% Si, 0.65% Mn, 0.60% Cr, 1.35% Ni. Core: 0.21% C, 0.24% Si, 0.61% Mn, 0.67% Cr, 1.35% Ni
0.92% C, 0.80% Cr, and 0.20% V
0.93% C, 0.11% Si, 0.31% Mn, 0.010% S, 0.012% P, 0.20% Ni, 0.12% Cr
0.93-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, max. 0.025% P, max. 0.015% S, 1.35-1.60% Cr, max. 0.10% Mo, max. 0.050% Al, max. 0.30% Cu
0.93-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, max. 0.030% P, max. 0.030% S, 1.35-1.65% Cr
0.93-1.05% C, 0.15-0.35% Si, 0.60-.80% Mn, max. 0.025% P, max. 0.015% S, 1.65-1.95% Cr, 0.20-0.35% Mo, max. 0.30% Cu, max. 0.050% Al
0.93-1.05% C, 0.15-0.35% Si, 0.60-0.80% Mn, max. 0.025% P, max. 0.015% S, 1.65-1.95% Cr, 0.20-0.35% Mo, max. 0.30% Cu, max. 0.050% Al
0.93-1.05% C, 0.45-0.75% Si, 1.00-1.20% Mn, max. 0.025% P, max. 0.015% S, 1.45-1.65% Cr, max. 0.10% Mo, max. 0.30% Ni, max. 0.050% Al
0.94-1.00% C, 0.10-0.15% Si, 0.25-0.45% Mn, max. 0.018% P, max. 0.010% S, 1.30-1.50% Cr, max. 0.15% Ni, 0.20-0.23% Mo
0.95% C, 0.22% Si, 0.60% Mn, 1.23% Cr, 3.27% Ni, 0.13% Mo
0.95% C, 0.23% Si, 0.82% Mn, 0.52% Cr, 0.56% Ni, 0.19% Mo
0.95% C, 0.24% Si, 0.58% Mn, 1.79% Ni, 0.25% Mo
0.95% C, 0.30% Si, 0.84% Mn, 0.55% Ni, 0.66% Cr, 0.11% Mo
0.95% C, 0.30% Si, 1.20% Mn, 0.50% W, 0.50% Cr, and 0.20% V
0.95-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, max. 0.025% P, max. 0.015% S, 1.35-1.60% Cr, max. 0.10% Mo, max. 0.30% Cu, max. 0.050% Al
0.95-1.10% C, 0.15-0.35% Si, 0.25-0.45% Mn, max. 0.015% P, max. 0.015% S, 1.35-1.65% Cr, max. 0.40% Ni
0.97% C, 0.52% Mn, 3.36% Ni, 0.19% Mo
0.97% C, 1.04% Mn, 0.32% Mo. Blue lines: 0.97% C, 1.04% Mn, 0.32% Mo
0.97% C, 1.04% Mn, 0.32% Mo
0.98% C, 0.20% Si, 0.70% Mn, 0.60% Cr, 0.68% Mo, 0.12% Ni
0.98-1.05% C, 0.15-0.25% Si, 0.35-0.45% Mn, max. 0.035% P, max. 0.035% S
1.00% C, 0.25% Si, 0.35% Mn, 0.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.30% Si, 0.70% Mn, 1.80% Cr, 0.30% Mo
1.00% C, 0.30% Si, 0.70% Mn, 1.80% Cr, 0.30% Mo
1.00% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
1.00% C, 0.52% Mn, 5.00% Ni
1.00% C, 0.60% Si, 1.10% Mn, 1.50% Cr
1.00% C, 0.60% Si, 1.10% Mn, 1.50% Cr
1.00% C, 0.90% Cr, 0.20% V. L6 steel: 0.70% C, 0.75% Cr, 1.50% Ni, 0.25% Mo
1.00% C, 1.40% Cr, and 0.20% V
1.00% C, 1.88% Mn
1.00% nickel steel
1.00-1.10% C, 0.15-0.35% Si, 0.20-0.40% Mn, max. 0.030% P, max. 0.030% S, 0.90-1.10% Cr
1.02% C, 0.36% Mn, 0.20% Ni, 1.41% Cr. Blue lines: 1.02% C, 0.36% Mn, 0.20% Ni, 1.41% Cr
1.02% C, 0.36% Mn, 0.20% Ni, 1.41% Cr
1.05% C, 0.30% Si, 0.35% Mn, 1.50% Cr
1.08% C, 0.25% Si, 0.53% Mn, 0.015% S, 0.022% P, 0.33% Ni, 1.46% Cr, 0.06% Mo
1.10% C, 0.19% Si, 0.81% Mn, 0.55% Ni, 0.63% Cr, 0.11% Mo
1.13% C, 0.30% Mn
1.20% C, 0.30% Mn, 0.26% Si, 0.70% Cr, 0.25% Mo, 1.56% W, and 0.20% V
1.50% C, 0.3% Si, 0.4% Mn, 12.0% Cr, 0.9% Mo, 0.3% V. SGT steel: 1.0% C, 0.3% Si, 1.0% Mn, 0.7% Cr. YXR7 steel: 0.8% C, 0.8% Si, 0.3% Mn, 4.7% Cr, 1.3% W, 5.5% Mo, 1.3% V. YXM1 steel: 0.9% C, 0.3% Si, 0.4% Mn, 4.2% Cr, 6.5% W, 5.0% Mo, 2.0% V.
1.50% C, 0.35% Si, 0.40% Mn, 12.00% Cr, 1.00% Mo, 0.85% V. Steel O1: 0.95% C, 0.25% Si, 1.20% Mn, 0.48% Cr, 0.13% V, 0.55% W. Steel W1: 1.00% C, 0.20% Si, 0.25% Mn.
1.50% Ni ??? Cr ??? Mo steel
1.53% C, 0.35% Si, 0.40% Mn, 12.00% Cr, 1.00% Mo, 0.85% V
1.80% C, 0.56% Mn, 0.30% Si, 0.09% Ni, 0.14% Cr, 0.98% Mo
2.59C-0.7Si-0.91Mn-18.54Cr-0.002P-0.001S-Fe
3.57% C, 2.31% Si, 0.39% Mn, 0.020% P, 0.007% S, 0.54% Cu
3.65% C, 2.85% Si, 0.31% Mn, 0.016% P, 0.006% S, 0.002% Cu
3.68% C, 2.24% Si, 0.39% Mn, 0.015% P, 0.002% S, 1.25% Cu