22MnB5 Steel
Steel name: 22MnB5
Diagram No.: 1524
DIN designation: 22MnB5
Chemical composition in weight %: 0.22-0.28% C, 0.15-0.35% Si, 1.20-1.40% Mn, max. 0.035% P, max. 0.035% S, 0.10-0.30% Cr, 0.0010-0.0060% B
Steel group: Alloyed stels, boron steels
Applications: Grade SB24M13B is a boron steel for general purposes without any specified mechanical properties.Its closest equivalent is found in the standard number 22MnB5.This grade is suitable to serve as chains (side-links) in materials handling equipment of various kinds that are exposed to heavy wear and varying stresses (bending, tensile, fatigue).
Comment: Ms=400 C, Ac1=719 C, Ac3=790 C.
Reference: Not shown in this demo version.
Heat Treatment
Hardenability Diagram
Price: 20.00 US $
Buy Online Hardenability Diagram
Other Steel Data links:
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Transformation Diagrams of Non-Ferrous Alloys
Tempering Diagrams of Steels
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.