17CrNiMo6 Steel

Steel name: 17CrNiMo6
Diagram No.: 689
DIN designation: 17CrNiMo6
Mat.No. (Wr.Nr.) designation: 1.6587
Chemical composition in weight %: 0.15-0.20% C, <0.40% Si, 0.40-0.60% Mn, <0.035% P, <0.035% S,
1.50-1.80% Cr, 1.40-1.70% Ni, 0.25-0.35% Mo
Steel group: Alloyed steel
Applications: No data
Comment: The legend: Harte in HRC - Hardness in HRC, Abstand von der abgeschrechten Stirnflache in mm - Distance from quenched end in mm.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 860–900oC/oil, polymer, water

Hardenability Diagram

Price: 20.00 US $
Buy Online Hardenability Diagram

Other Steel Data links:
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Transformation Diagrams of Non-Ferrous Alloys
Tempering Diagrams of Steels

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.