Cf45 Steel

Steel name: Cf45
Diagram No.: 454
DIN designation: Cf45
Mat.No. (Wr.Nr.) designation: 1.1193
Chemical composition in weight %: 0.43-0.49% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S
Steel group: Non alloy special steels
Applications: No data
Comment: No data
Reference: Not shown in this demo version.

Heat Treatment
Hardening in water: 820-850oC
Hardening in oil: 830-860oC
Tempering: 550-660oC

Hardenability Diagram


Click the image to enlarge the diagram.


Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.