18CrNiMo7-6 Steel

Steel name: 18CrNiMo7-6
Diagram No.: 84
DIN designation: 18CrNiMo7-6
Mat.No. (Wr.Nr.) designation: 1.6587
Chemical composition in weight %: 0.15-0.21% C, 0.40% Si, 0.50-0.90% Mn, 0.035% P, 0.035% S,
1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
Steel group: Alloy special structural steels
Applications: Plate wheels, driving pinions and highly stressed cog wheels
Comment: Heat-treated steels, alloy steels and free-cutting steels. Ball and
roller bearing steels. Ball and roller bearing steels for case hardening.
Reference: Not shown in this demo version.

Heat Treatment
Carburising: 880-980oC
Hardening: 860oC
Core hardening: 830-870oC
Surface hardening: 780-820oC
Tempering: 150-200oC
Note: End quench test: 860oC

Hardenability Diagram

Price: 20.00 US $
Buy Online Hardenability Diagram

Other Steel Data links:
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Transformation Diagrams of Non-Ferrous Alloys
Tempering Diagrams of Steels

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.