42CrMo4 Steel
Steel name: 42CrMo4
Table No.: 1742
DIN designation: 42CrMo4
Mat.No. (Wr.Nr.) designation: 1.7225
AISI/SAE designation: 4140
EN designation: 42CrMo4
UNI designation: 42CrMo4
AFNOR designation: 42CD4
BS designation: 708M40
GOST designation: 38ChM
GOST designation: ML42CrMo
Chemical composition in weight %: 0.38-0.45% C, max. 0.40% Si, 0.60-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
Steel group: Alloy steels
Applications: No data
Comment: Ac1=745 C, Ac3=790 C, Ms=335 C, Mf=120 C.
Reference: Not shown in this demo version.
Heat Treatment
Quenching: 860 C/oil, polymer
Tempering: 550-650 C
Hardenability test
Quenching: 840 C/water
Hardenability Table
Price: 20.00 US $
Buy Online Hardenability Table
Other Steel Data links:
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Transformation Diagrams of Non-Ferrous Alloys
Tempering Diagrams of Steels
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.