20Cr3 Steel

Steel name: 20Cr3
Diagram No.: 889
DIN designation: 20Cr3
Mat.No. (Wr.Nr.) designation: 1.3559
Chemical composition in weight %: 0.17-0.23% C, max. 0.40% Si, 0.60-1.60% Mn, max. 0.025% P, max. 0.015% S, 0.60-1.00% Cr, max. 0.30% Cu, 0.050% Al
Steel group: Ball and roller bearing steels - case hardening steel
Applications: No data
Comment: No data
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 895-905oC

Hardenability Diagram

Price: 20.00 US $
Buy Online Hardenability Diagram

Other Steel Data links:
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Transformation Diagrams of Non-Ferrous Alloys
Tempering Diagrams of Steels

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.