Firmodur 6582 Steel

Steel name: Firmodur 6582
Diagram No.: 2027
Mat.No. (Wr.Nr.) designation: 1.6582
DIN designation: 34CrNiMo6
AFNOR designation: 34CrNiMo8
AISI/SAE designation: 4337 / 4340
AFNOR designation: 34CrNiMo8
BS designation: 816M40
JIS designation: SNCM447
Chemical composition in weight %: 0.30-0.38% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
Steel group: Alloyed steels
Applications: Firmodur 6582 is used for through-hardened components such as fasteners in the automotive and mechanical engineering industry with high demands on strength and toughness.
Comment: No data
Reference: Not shown in this demo version.

Heat Treatment
Hardening: Hardening temperature 850°C.

Hardenability Diagram

Price: 20.00 US $
Buy Online Hardenability Diagram

Other Steel Data links:
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Transformation Diagrams of Non-Ferrous Alloys
Tempering Diagrams of Steels

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.