1.8159 Steel
Steel name: 1.8159
Diagram No.: 829
DIN designation: 50CrV4
Mat.No. (Wr.Nr.) designation: 1.8159
AISI/SAE designation: 6145/6150
Chemical composition in weight %: 0.51% C, <0.40% Si, 0.90% Mn, 1.05% Cr, 0.18% V
Steel group: Alloyed steel
Applications: Permanently stressed machine, engine and vehicle parts when high strength and
toughness are required.Most severely stressed springs for trucks, torsion springs.
Comment: No data
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 820-860oC/oil
Hardenability Diagram
Click the image to enlarge the diagram.
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.