18CrNiMo7-6 Steel
Steel name: 18CrNiMo7-6
Table No.: 1722
DIN designation: 17CrNiMo6
Mat.No. (Wr.Nr.) designation: 1.6587
AISI/SAE designation: ~4820
EN designation: 18CrNiMo7-6
UNI designation: 18CrNiMo7-6
AFNOR designation: 18CND6
BS designation: ~822M17
Chemical composition in weight %: 0.15-0.21% C, max. 0.40% Si, 0.50-0.90% Mn, max. 0.025% P, max. 0.035% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
Steel group: Alloy steels
Applications: No data
Comment: Ac1-745 C, Ac3=825, Ms (core)=400 C, Ms (carburized surface)=170 C.
Reference: Not shown in this demo version.
Heat Treatment
Core hardening: 830-870 C/oil or polymer
Carburizing: 900-950 C
Hardening carburizing surface: 780-820 C/oil or polymer
Tempering: 15-200 C/air
Hardenability test
Quenching: 860 C/water
Hardenability Table
Click the image to enlarge the table.
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.