39NiCrMo3+H, 39NiCrMo3+HH, 39NiCrMo3+HL Steels

Steel name: 39NiCrMo3+H, 39NiCrMo3+HH, 39NiCrMo3+HL
Diagram No.: 1980
DIN designation: 39NiCrMo3
Mat.No. (Wr.Nr.) designation: 1.6510
Chemical composition in weight %: See the chemical composition table
Steel group: Alloy steels
Applications: No data
Comment: Scatter bands for the Rockwell - C hardness in the end quench hardenability test.
Reference: Not shown in this demo version.

Heat Treatment
End quench test: 850 +/-5 C

Hardenability Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.