1040, 4140, 4340, 5140, 8640 Steels
Steel name: 1040, 4140, 4340, 5140, 8640
Diagram No.: 2080
AISI/SAE designation: 1040, 4140, 4340, 5140, 8640
Chemical composition in weight %: No data
Steel group: Steels
Applications: No data
Comment: Hardenability curves for five different steel alloys, each containing 0.4 wt% C. Approximate alloy compositions (wt%) are as follows: 4340–1.85 Ni, 0.80 Cr, and 0.25 Mo; 4140–1.0 Cr and 0.20 Mo; 8640–0.55 Ni, 0.50 Cr, and 0.20 Mo; 5140–0.85 Cr; and 1040 is an unalloyed steel. (Adapted from figure furnished courtesy Republic Steel Corporation).
Reference: Not shown in this demo version.
Heat Treatment
Hardening: No data
Hardenability Diagram
Price: 20.00 US $
Buy Online Hardenability Diagram
Other Steel Data links:
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Transformation Diagrams of Non-Ferrous Alloys
Tempering Diagrams of Steels
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.