About Hardenability Diagrams of Steels v. 2.0

The database contains 2,121 experimental hardenability diagrams of steels collected from the journals, books, company prospects and web sites from the year 1948 to the year 2023. All information herein is a extracted from open literature, and is a orginally written by the authors, from the source references cited. Database is searchable with the usual keyword search - by steel name, or any other words. We hope that this database makes your professional life more productive and easily.