Chemical Composition of Steels in Weight %

0.002% C, 0.22% Mn, 0.018% P, 0.006% S, 0.037% Al-s, 0.047% Ti, <0.005% Nb, 0.002% N. High S: <0.002% C, 0.18% Mn, 0.018% P, 0.018% S, 0.029% Al-s, 0.049% Ti, <0.005% Nb, 0.003% N
0.0022% C, 0.11% Mn, 0.02% Si, 0.06% P, 0.01% S, 0.0355 Al (sol), 0.2% Cu, 0.0022% N
0.0026% C, 0.09% Si, 0.15% Mn, 0.043% al, 0.0057% S, 0.008% P, 0.071% Ti, 0.002% N, 0.040% SOAl, 0.0026% T[O]
0.003% C, 0.01% Si, 0.08% Mn, 0.004% P, 0.0003% S. Composition of refractory: 96.8% MgO, 1.8% CaO, 0.6% SiO2, 0.3% Fe2O3, 5.5% C
0.003% C, 0.01% Si, 0.08% Mn, 0.004% P, 0.0003% S. Composition of refractory: 96.8% MgO, 1.8% CaO, 0.6% SiO2, 0.3% Fe2O3, 5.5% C
0.003% C, 0.01% Si, 0.08% Mn, 0.004% P, 0.0003% S. Refractory material: Dol; Dol/Mag; Dol-C. MgO addition in slag: 0, 5, 8% MgO
0.003% C, 0.01% Si, 0.08% Mn, 0.004% P, 0.0003% S. Refractory material: Dol; Dol/Mag; Dol-C. MgO addition in slag: 0, 5, 8% MgO
0.003% C, 0.01% Si, 0.08% Mn, 0.004% P, 0.0003% S
0.003% C, 0.01% Si, 0.08% Mn, 0.004% P, 0.0003% S
0.0049% C, 0.091% S, 0.30% Mn, 0.33% Cu, 0.2457% Sn. Steel E2: 0.0046% C, 0.091% S, 0.40% Mn, 0.27% Cu, 0.6332% Sn. Steel E3: 0.0052% C, 0.087% S, 0.087% S, 0.30% Cu, 0.9455% Sn
0.0049% C, 0.091% S, 0.30% Mn, 0.33% Cu, 0.2457% Sn. Steel E2: 0.0046% C, 0.091% S, 0.40% Mn, 0.27% Cu, 0.6332% Sn. Steel E3: 0.0052% C, 0.087% S, 0.087% S, 0.30% Cu, 0.9455% Sn
0.005% C, 0.01% Si, 0.15% Mn, 0.015% P, 0.008% S, 0.03% Al, 0.03% Ti, 0.003% O
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.005% C, 0.25% Cu, 0.024% S, 0.0080% P, 0.0012% N
0.0058% C, 0.098% S, 0.88% Mn, 0.2431% Sn. Steel D2: 0.0052% C, 0.092% S, 0.83% Mn, 0.6437% Sn. Steel D3: 0.0055% C, 0.090% S, 0.78% Mn, 0.8814% Sn
0.006-0.010% C, 0.004-0.006% Si, 0.003-0.005% S, nil P, 0<Mn<1.25. (Second) 0.02-0.007% C, nil Mn, 0.001-0.006% P, 0.002-0.006% S, 0.002-1.175% Si
0.01% C, 19.80% Cr, 24.80% Ni, 6.18% Mo, 1.47% Mn, 0.003% S. Steel b: 0.01% C, 20.10% Cr, 25.00% Ni, 6.18% Mo, 1.46% Mn, 0.022% S
0.010% Al, 0.017% S
0.02% C, 0.37% Mn, 0.0186% N
0.02% C, 0.46% Si, 1.75% Mn, 9.15% Ni, 17.3% Cr, 0.36% Ti, 0.001% S, 0.01% N. AISI 319: 0.02% C, 0.65% Si, 1.68% Mn, 9.65% Ni, 17.4% Cr, 0.26% Ti, 0.026% S, 0.02% N
0.02% C, 16% Cr, 10% Ni, 2% Mo, 0.05% N, 300 ppm S, 50 ppm O2. Steel 2: 0.02% C, 22% Cr, 5% Ni, 3% Mo, 0.2% N, 50 ppm S, 30 ppm O2
0.02% C, 16% Cr, 10% Ni, 2% Mo, 0.05% N, 300 ppm S, 50 ppm O2. Steel 2: 0.02% C, 22% Cr, 5% Ni, 3% Mo, 0.2% N, 50 ppm S, 30 ppm O2
0.02% C, 16% Cr, 10% Ni, 2% Mo, 0.05% N, 300 ppm S, 50 ppm O2. Steel 2: 0.02% C, 22% Cr, 5% Ni, 3% Mo, 0.2% N, 50 ppm S, 30 ppm O2
0.02% C, 16% Cr, 10% Ni, 2% Mo, 0.05% N, 300 ppm S, 50 ppm O2. Steel 2: 0.02% C, 22% Cr, 5% Ni, 3% Mo, 0.2% N, 50 ppm S, 30 ppm O2
0.02% C, 16% Cr, 10% Ni, 2% Mo, 0.05% N, 300 ppm S, 50 ppm O2. Steel 2: 0.02% C, 22% Cr, 5% Ni, 3% Mo, 0.2% N, 50 ppm S, 30 ppm O2
0.02% C, 17.2% Cr, 10.1% Ni, 2.1% Mo
0.020 % C, 16.5 % Cr, 10.5 % Ni, 1.5 % Mn, 0.38 % Si, 0.041 % P, 0.025 % S
0.024-0.035% C, 0.48-0.44% Si, 1.45-1.55% Mn, 0.033-0.015% S, 17.95-18.19% Cr, 9.10-9.20% Ni, 0.30-0.35% Mo, 0.045-0.048% V, 0.090-0.095% Co, 0.19-0.22% Cu, 70-180 ppm Nb, 450-500 ppm N
0.024-0.035% C, 0.48-0.44% Si, 1.45-1.55% Mn, 0.033-0.015% S, 17.95-18.19% Cr, 9.10-9.20% Ni, 0.30-0.35% Mo, 0.045-0.048% V, 0.090-0.095% Co, 0.19-0.22% Cu, 70-180 ppm Nb, 450-500 ppm N
0.025% S, 0.02-0.04% Al
0.028% C, 0.20% Si, 66.0% Cr, 0.016% P, 0.004% S, 2850 ppm O, balance is Fe
0.028% C, 0.57% Si, 68.6% Cr, 0.014% P, 0.03% S, 1620-1750 ppm O, balance is Fe
0.03% C, 0.002% S, 0.19% Si, 19.4% Cr, 75.53% Ni, 2.28% Ti, 1.26% Al, 1.21% Fe, 0.07% Mo, 0.003% Zr, balance is Ni
0.03% C, 15% Mn, 21.5% Cr, 0.7% N
0.03% C, 15% Mn, 21.5% Cr, 0.7% N
0.03% C, 15% Mn, 21.5% Cr, 0.7% N
0.03% C, 16–18% Cr, 10–14% Ni, 2–3% Mo
0.03% C, 16–18% Cr, 10–14% Ni, 2–3% Mo
0.03% C, 73% Cr, rest is Fe
0.035% C, 1.7% Si, 0.83% Al, 0.2% Mn, 0.015% Cu, 0.0029% P, 0.028% S, 0.050% Se
0.037% C, 0.037% Al, 0.057% Ti, 0.120% Mn, 0.011% C, 0.021% Cr, 0.09% Ni. Slag composition in wt.%: 1.95% SiO2, 42.26% Al2O3, 51.33% CaO, 2.32% TiO2, <0.02% MnO, 0.13% MgO, 0.05% Cr2O3, 0.13% P2O5, 0.97% Fe
0.037% C, 0.64% Si, 1.22% Mn, 0.025% P, 0.009% S, 18.1% Cr, 9.0% Ni, 0.20% Mo, 0.0048% O, 0.024% N
0.04% C, 0.05% Mn, 0.01% P, 0.003% S, 0.03% Si, 0.1% Cu, 0.03% Ni, 0.03% Cr, 0.005% Mo, 0.004% Sn, 0.05% Al, 0.003% Nb, 0.002% V, 0.002% Ca, 0.0003% Pb, 0.06% Ti, 0.0005% B, 0.006% N
0.04% C, 0.14% Mn, 0.012% P, 0.015% S, 0.003% N
0.04% C, 0.22% Si, 1.54% Mn, 0.08% Nb, 0.08% Ti, 0.0024% P, 0.0075% S, 0.0085% O, 0.0043% N
0.04% C, 0.25% Si, 0.16% Mn, 0.003% Al, 0.006% S, 41 ppm N, 131 ppm O. HR steel: 0.15% C, 0.01% Si, 0.78% Mn, 0.034% Al, 0.005% S, 34 ppm N, 15 ppm O
0.04% C, 0.40% Si, 1.34% Mn, 18.5% Cr, 10.1% Ni, 0.50% Mo, 0.020% P, 0.005% S, 0.029% N
0.04% C, 0.74% Si, 0.26% Mn, 17.37% Cr, 10.09% Ni, 2.25% Mo
0.04% C, 17.5% Cr, 0.30% S
0.04% C, nil Si, 0.14% Mn, 0.012% P, 0.017% S, 0.003% N, 0.064% O
0.041% C, 0.83% Si, 0.82% Mn, 0.019% P, 0.006% S, 12.71% Cr, 3.70% Ni, 0.59% Mo
0.041% C, 0.83% Si, 0.82% Mn, 0.019% P, 0.006% S, 12.71% Cr, 3.70% Ni, 0.59% Mo
0.043% C, 0.021% Si, 0.17% Mn, 0.010% P, 0.004% S, 0.021% Al(total), 0.019% Al(s), 0.0022% Ca, 0.0036% [O], 0.0053% [N]
0.043% C, 0.40% Si, 1.34% Mn, 0.020% P, 0.005% S, 18.5% Cr, 10.1% Ni, 0.50% Mo, 0.029% N. Fig. 2: 0.18% C, 0.27% Si, 0.69% Mn, 0.009% P, 0.021% S, 0.009% N.
0.043% C, 0.40% Si, 1.34% Mn, 0.020% P, 0.005% S, 18.5% Cr, 10.1% Ni, 0.50% Mo, 0.029% N
0.043% C, 0.40% Si, 1.34% Mn, 0.020% P, 0.005% S, 18.5% Cr, 10.1% Ni, 0.50% Mo
0.045% C, 0.20% Al, 0.0086% O
0.05% C, 0.02% Si, 0.60% Mn, 0.008% Al
0.05% C, 0.25% Si, 1.85% Mn, 8.70% Ni, 17.7% Cr, >0.01% Ti, 0.319% S, 0.03% N
0.05% C, 0.25% Si, 1.85% Mn, 8.70% Ni, 17.7% Cr, >0.01% Ti, 0.319% S, 0.03% N
0.05% C, 0.29% Mn, 0.007% P, 0.030% S, 0.15% Cu, 0.07% Cr, 0.019% Sn
0.05% C, 0.43% Si, 0.95% Mn, 0.023% P, 0.012% Si, 18.0% Cr, 9.8% Ni, 0.50% Mo
0.05% C, 0.43% Si, 0.96% Mn, 0.023% P, 0.012% S, 18.0% Cr, 9.8% Ni, 0.50% Mo
0.05% C, 0.44% Mn
0.05% C, 0.54% Si, 1.27% Mn, 18.3% Cr, 9.1% Ni, 0.25% Mo, 0.035% P, 0.009% S, 0.050% N
0.05% C, 0.66% Si, 1.03% Mn, 17.8% Cr, 9.0% Ni
0.05% C, 0.67% Mn, 0.008% P, 0.035% S, 0.16% Si, 0.20% Cu, 0.051% Ni, 0.049% Cr
0.05% C, 0.67% Mn, 0.008% P, 0.035% S, 0.16% Si, 0.20% Cu, 0.051% Ni, 0.049% Cr
0.05% C, 0.67% Mn, 0.008% P, 0.035% S, 0.16% Si, 0.20% Cu, 0.051% Ni, 0.049% Cr
0.05% C, 0.80% Si, 1.65% Mn, 0.010% P, 0.011% S, 0.008% Al (total), 0.25% Ti, 35 ppm N, 20 ppm O. Steel B: 0.06% C, 0.68% Si, 2.00% Mn, 0.012% P, 0.015% S, 0.011% Al (total), 0.20% Ti, 40 ppm N, 20 ppm O
0.05% C, 0.80% Si, 1.65% Mn, 0.010% P, 0.011% S, 0.008% Al (total), 0.25% Ti, 35 ppm N, 20 ppm O
0.05% C, 1.25% Mn, 0.2% Si, >0.05% P+S, ~0.1% Al, ~0.1% Nb+Ti+V, ~0.4% Cu+Ni, >0.002% Ca, ~0.1% Cr, ~0.1% Mo
0.051% C, 0.52% Si, 0.90% Mn, 8.10% Ni, 18.06% Cr
0.051% C, 0.52% Si, 0.90% Mn, 8.10% Ni, 18.06% Cr
0.051% C, 0.52% Si, 0.90% Mn, 8.10% Ni, 18.06% Cr
0.051% C, 0.52% Si, 0.90% Mn, 8.10% Ni, 18.06% Cr
0.053% C, 0.21% Si, 1.22% Mn, 0.007% P, 0.0004% S, 0.046% Al, 0.0044% N, 0.0012% Ca, ~0.1%=Nb+V+Ti, ~0.25%=Cu+Ni
0.053% C, 0.21% Si, 1.22% Mn, 0.007% P, 0.0004% S, 0.046% Al, 0.1% Nb+V+Ti, 0.25% Cu+Ni, 0.0044% N, 0.0012% Ca
0.053% C, 0.54% Si, 1.30% Mn, 0.019% P, 0.006% S, 18.6% Cr, 9.2% Ni
0.057% C, 0.00419% O, 0.00260% N, 0.006% Si, 0.15% Mn, 0.011% P, 0.006% S, 0.043% Als, 0.032% Ti, 0.003% Nb
0.06% C, 0.04% Si, 2.07% Mn, 0.0108% P, 0.0015% S, 0.01% Al, 0.003% Ti, 0.0028% O, 0.0043% N. TRIP steel: 0.20% C, 0.28% Si, 1.52% Mn, 0.0078% P, 0.0004% S, 1.08% Al, 0.007% Ti, 0.0020% O, 0.0085% N
0.06% C, 0.04% Si, 2.07% Mn, 0.0108% P, 0.0015% S, 0.01% Al, 0.003% Ti, 0.0028% O, 0.0043% N. TRIP steel: 0.20% C, 0.28% Si, 1.52% Mn, 0.0078% P, 0.0004% S, 1.08% Al, 0.007% Ti, 0.0020% O, 0.0085% N
0.06% C, 0.05% Mn, 0.004% P, 0.010% S, 29.8% Cr, 0.03% Ni, 0.10% Mn, 0.01% Co, 0.01% Cu, 0.004% Al, 0.025% N, 0.045% O
0.06% C, 0.5% Si, 1% Mn, 0.02% S, 18% Cr, 8-9% Ni. Fig. 1b: 0.26% C, 0.48% Si, 0.84% Mn. Fig. 1c: 0.24% C, 0.30% Si, 1.40% Mn
0.06% C, 0.75-1.05% Mn, 0.40% Si, 0.015% P, 0.006% S, 3.35-3.65% Ni, 0.55-0.65% Mo, 0.45-0.75% Cr, 0.02-9.04% Al, 1.45-1.75% Cu
0.06% C, 1.80% Mn, 0.72% Si, 0.024% P, 0.016% S, 17.48% Cr, 10.63% Ni, 0.64% Ti, 0.005% O2, 0.020% N
0.06% C, max. 1.00% Si, max. 1.50% Mn, max. 0.060% P, 0.15-0.35% S, 16.50-18.50% Cr, 0.20-0.60% Mo
0.06-0.12% C, 0.15-0.35% Si, 0.25-0.50% Mn, 0.045% P, 0.045% S
0.06C–0.04S–0.35Mn–0.05P
0.07% C, 0.70% Si, 1.50% Mn, 16.00% Cr, 0.60% Mo, 4.00% Ni, 3.50% Cu
0.07% C, max. 1.00% Si, max. 2.00% Mn, max. 0.045% P, max. 0.030% S, 17.00-19.50% Cr, 8.00-10.50% Ni, max. 0.11% N
0.07-0.08% C, 1.4-1.5% Mn, 0.8-0.9% Si, max. 50 ppm N
0.07-0.08% C, 1.4-1.5% Mn, 0.8-0.9% Si, max. 50 ppm N
0.070% C, 0.051% Si, 0.39% Mn, 0.0010% S, 0.0084% Al(s), 0.0092% Al(t). Heat 3: 0.026% C, 0.053% Si, 0.34% Mn, 0.0006% S, 0.0090% Al(s), 0.011% Al(t)
0.070% C, 0.051% Si, 0.39% Mn, 0.0010% S, 0.0084% Al(s), 0.0092% Al(t). Heat 3: 0.026% C, 0.053% Si, 0.34% Mn, 0.0006% S, 0.0090% Al(s), 0.011% Al(t)
0.0702% C, 0.0022% S, 0.68% Mn, 0.098% Cu, 0.087% Sn. Steel G2: 0.0650% C, 0.0169% S, 0.68% Mn, 0.085% Cu, 0.090% Sn
0.0702% C, 0.0022% S, 0.68% Mn, 0.098% Cu, 0.087% Sn. Steel G2: 0.0650% C, 0.0169% S, 0.68% Mn, 0.085% Cu, 0.090% Sn
0.074% C, 0.22% Si, 1.00% Mn, 0.0072% P, 0.0094% S, 0.0011% Ti, 0.0017% Al, 0.0013% La, 0.0026% Ce, 0.0059% N and 0.0041% TO
0.075% C, 0.23% Si, 1.45% Mn, 0.024% Ti, 0.0001% B, 0.002% O. KT5 sample: 0.075% C, 0.23% Si, 1.46% Mn, 0.024% Ti, 0.001% B, 0.002% O
0.077% C, 1.46% Mn, 0.27% Si, 0.008% S, 0.007% P, 0.0028% Ti, 0.0081% N, 0.0460% O
0.078% C, 0.36% Si, 1.47% Mn, 18% Cr, 9% Ni, 0.22% S. Bottom Fig. 2: 0.83% C, 0.20% Si, 0.26% Mn, 0.020% S, 41.0% Cr, 5.25% Mo, 6.71% W, 0.22% Co, 2.0% V
0.079% C, 0.372% Si, 1.7763% Mn, 0.02% S, 0.011% P. Q690 steel: 0.089% C, 0.337% Si, 1.47% Mn, 0.426% Cr, 0.323% Mo, 0.258% Ni, 0.10% Ti, 0.009% S, 0.029% P. MK·G60-1 wire: 0.09% C, 0.69% Si, 1.64% Mn, 0.08% Cr, 0.11% Ti, 0.010% S, 0.015% P
0.079% C, 0.50% Si, 1.45% Mn, 0.017% P, 0.009% S, 30 ppm Al, 43 ppm Ti, 36 ppm N, 20 ppm O
0.08% C, <0.05% Si, 1.20% Mn, 0.07% P, 0.37% S
0.08% C, <1.00% Si, <2.00% Mn, 0.045% P, <0.030% S, 8-10.5% Ni, 18.00-20.00% Cr
0.08% C, <1.00% Si, <2.00% Mn, 0.045% P, <0.030% S, 8-10.5% Ni, 18.00-20.00% Cr
0.08% C, <1.00% Si, <2.00% Mn, 0.045% P, <0.030% S, 8-10.5% Ni, 18.00-20.00% Cr
0.08% C, 0.03% Si, 0.13% Mn
0.08% C, 0.03% Si, 0.13% Mn
0.08% C, 0.05% Si, 0.54% Mn, 0.12% P, 0.010% S, 0.07% Cu, 0.016% O. Steel B: 0.096% C, 0.26% Si, 0.61% Mn, 0.013% P, 0.016% S, 0.12% Cu, 0.004% O.
0.08% C, 0.05% Si, 0.54% Mn, 0.12% P, 0.010% S, 0.07% Cu, 0.016% O. Steel B: 0.096% C, 0.26% Si, 0.61% Mn, 0.013% P, 0.016% S, 0.12% Cu, 0.004% O.
0.08% C, 0.05% Si, 0.54% Mn, 0.12% P, 0.010% S, 0.07% Cu, 0.016% O. Steel B: 0.096% C, 0.26% Si, 0.61% Mn, 0.013% P, 0.016% S, 0.12% Cu, 0.004% O.
0.08% C, 0.05% Si, 0.54% Mn, 0.12% P, 0.010% S, 0.07% Cu, 0.016% O. Steel B: 0.096% C, 0.26% Si, 0.61% Mn, 0.013% P, 0.016% S, 0.12% Cu, 0.004% O.
0.08% C, 0.05% Si, 0.54% Mn, 0.12% P, 0.010% S, 0.07% Cu, 0.016% O. Steel B: 0.096% C, 0.26% Si, 0.61% Mn, 0.013% P, 0.016% S, 0.12% Cu, 0.004% O.
0.08% C, 0.05% Si, 0.54% Mn, 0.12% P, 0.010% S, 0.07% Cu, 0.016% O. Steel B: 0.096% C, 0.26% Si, 0.61% Mn, 0.013% P, 0.016% S, 0.12% Cu, 0.004% O.
0.08% C, 0.05% Si, 0.54% Mn, 0.12% P, 0.010% S, 0.07% Cu, 0.016% O. Steel B: 0.096% C, 0.26% Si, 0.61% Mn, 0.013% P, 0.016% S, 0.12% Cu, 0.004% O.
0.08% C, 0.14% Si, 0.34% Mn, 0.021% P, 0.018% S, 0.034% Al
0.08% C, 0.3% Si, 1.42% Mn, 0.008% P, 0.003% S, 0.034% Al, 0.31% Cu, 0.005% N, 0.003% Nb, 0.003% Ti, 0.132% V
0.08% C, 0.3% Si, 1.42% Mn, 0.008% P, 0.003% S, 0.034% Al, 0.31% Cu, 0.005% N, 0.003% Nb, 0.003% Ti, 0.132% V
0.08% C, 0.3% Si, 1.42% Mn, 0.008% P, 0.003% S, 0.034% Al, 0.31% Cu, 0.005% N, 0.003% Nb, 0.003% Ti, 0.132% V
0.08% C, 0.3% Si, 1.42% Mn, 0.008% P, 0.003% S, 0.034% Al, 0.31% Cu, 0.005% N, 0.003% Nb, 0.003% Ti, 0.132% V
0.08% C, 0.3% Si, 1.42% Mn, 0.008% P, 0.003% S, 0.034% Al, 0.31% Cu, 0.005% N, 0.003% Nb, 0.003% Ti, 0.132% V
0.08% C, 0.3% Si, 1.42% Mn, 0.008% P, 0.003% S, 0.034% Al, 0.31% Cu, 0.005% N, 0.003% Nb, 0.003% Ti, 0.132% V
0.08% C, 0.4-0.8% Mn, 0.33% Si, 0.02% P, 0.02% S, 0.01-0.045% Al, up to 0.08% Ti, up to 90 ppm N, 293-794 ppm O
0.08% C, 1.00% Si, 2.00% Mn, 17.50% Cr, 2.25% Mo, 12.00% Ni
0.08% C, 1.26% Mn, 0.01% P, 0.041% Al, 0.24% Si, 0.002% S
0.08% C, 1.4% Mn, 0.8% Si, 0.0035% Al, 0.005% S, 0.01% S, 0.02% P, 0.0020% Ca, 0.0001% Mg
0.08% C, 1.4% Mn, 0.8% Si, 0.0035% Al, 0.005% S, 0.01% S, 0.02% P, 0.0020% Ca, 0.0001% Mg
0.08% C, 1.46% Mn, 0.25% V, 0.0180% N, 0.016% Al, 0.007% Si, 0.001% S
0.08% C, 1.47% Mn, 0.004% S, 0.012% Ti, 0.026% Al, 0.004% N
0.08% C, 1.47% Mn, 0.004% S, 0.012% Ti, 0.026% Al, 0.004% N
0.08% C, 18.60% Cr, 11.70% Ni, 2.20% Mo, C < 0.08, Cr 18.60, Ni 11.70, Mo 2.20, Cu <0.4, 0.08% C, 3.66% Si, 0.15% Mn
0.081% C, 0.00453% O, 0.00314% N, 0.029% Si, 0.23% Mn, 0.016% P, 0.005% S, 0.036% Als, 0.005% Ti, 0.001% Nb
0.085% C, 0.37% Si, 1.75% Mn, 0.015% P, 0.006% S, 0.10% Mo, 0.015% Ti, 0.022% Nb, 0.0040% B, 0.035% Al, 0.048% O, 0.0041% N
0.085% C, 0.37% Si, 1.75% Mn, 0.035% Al, 0.015% Ti, 0.0040% B, 0.048% O, 0.0041% N
0.085% C, 0.37% Si, 1.75% Mn, 0.035% Al, 0.015% Ti, 0.0040% B, 0.048% O, 0.0041% N
0.085% C, 0.37% Si, 1.75% Mn, 0.035% Al, 0.015% Ti, 0.0040% B, 0.048% O, 0.0041% N
0.086% C, 0.39% Si, 1.81% Mn, 0.017% P, 0.006% S, 0.10% Mo, 0.013% Ti, 0.020% Nb, 0.0040% B, 0.073% Al, 0.048% O, 0.0035% N
0.086% C, 0.39% Si, 1.81% Mn, 0.073% Al, 0.013% Ti, 0.0040% B, 0.048% O, 0.0035% N
0.09% C, 0.18% Si, 0.32% Mn, 0.010% P, 0.010% S, 0.05% Ni, 0.20% Cr, 0.03% Mo, 0.015% Al, 0.0128% N
0.09% C, 0.55% Si, 1.2% Mn
0.09% C, 0.55% Si, 1.2% Mn
0.09% C, 0.60% Mn, 0.06% P, 0.30% S
0.09% C, trace Si, 0.53% Mn, 0.008% P, 0.024% S, 0.13% Cu
0.09% C - 0.07% Nb
0.090% C, 0.004% Si, 0.89% Mn, 0.030% P, 0.0018% S, 0.009% Al(s), 0.090% Ti(total), 0.087% Ti(s), 0.0019% N(total), 0.0016% [0]e, 0.0016% [N]
0.090% C, 0.35% Si, 1.72% Mn, 0.014% P, 0.005% S, 0.10% Mo, 0.014% Ti, 0.019% Nb, 0.0035% B, 0.022% Al, 0.046% O, 0.0042% N
0.090% C, 0.35% Si, 1.72% Mn, 0.022% Al, 0.014% Ti, 0.0035% B, 0.046% O, 0.0042% N
0.090% C, 0.35% Si, 1.72% Mn, 0.022% Al, 0.014% Ti, 0.0035% B, 0.046% O, 0.0042% N
0.10% C, <0.10% Si, 1.00% Mn, 270-290 ppm Ti, 20-25 ppm N, 1a: 98 ppm O, 64 ppm S, 1b: 68 ppm O, 371 ppm S
0.10% C, 0.046% S, 0.23% Si, 0.03% C, 0.04% Ni, 0.01% V, 0.01% W, 0.01% Co, 0.01% Al, 0.16% Cu, 0.50% Mn, 0.01% Mo, 0.009% P, 0.10% C, 0.25% Si, 1.55% Mn, 0.015% Al, 0.005% Zr, 0.015% Ti, 0.003% N, 0.006% S
0.10% C, 0.26% Si, 0.58% Mn, 0.019% P, 0.02% S, 12.40% Cr, 2.69% Ni, 1.62% Mo, 0.37% V, 0.08% Cu, 0.02% W, 0.005% Al, 0.001% Ti, 0.03% Co, 0.006% Sn, 0.013% Zr
0.10% C, 0.32% Si, 0.46% Mn, 0.009% P, 0.006% S, 2.20% Cr, 0.90% Ni, 1.04% Mo
0.10% C, 0.47% Mn, 0.08% Si, 0.014% P, 0.023% S, 0.08% Cr, 0.05% NI, 0.17% Cu, 0.014% Mo, 0.009% Sn, 0.006% B, 0.009% N
0.10% C, 0.47% Mn, 0.08% Si, 0.014% P, 0.023% S, 0.08% Cr, 0.05% NI, 0.17% Cu, 0.014% Mo, 0.009% Sn, 0.006% B, 0.009% N
0.10% C, 0.64% Mn, 0.01% P, 0.05% S, 0.13% Si, 0.31% Cu, 0.10% Ni, 0.04% Cr
0.10% C, 0.64% Mn, 0.01% P, 0.05% S, 0.13% Si, 0.31% Cu, 0.10% Ni, 0.04% Cr
0.10% C, 7.70% W, 2.00% V, 0.15% Ta, 0.02% Ti, 30 ppm N, 65 ppm O, 74 ppm Al, 10 ppm S
0.10% S
0.11% C, 0.09% Si, 0.36% Mn, 0.018% P, 0.0144% S, 0.067% Cu, 0.1% Al(sol), 0.0169% N, 0.0149% T.O
0.11% C, 0.09% Si, 0.36% Mn, 0.018% P, 0.0144% S, 0.067% Cu, 0.1% Al(sol), 0.0169% N, 0.0149% T.O
0.11% C, 0.09% Si, 0.36% Mn, 0.018% P, 0.0144% S, 0.067% Cu, 0.1% Al(sol), 0.0169% N, 0.0149% T.O
0.11% C, 0.09% Si, 0.36% Mn, 0.018% P, 0.0144% S, 0.067% Cu, 0.1% Al(sol), 0.0169% N, 0.0149% T.O
0.11% C, 0.09% Si, 0.36% Mn, 0.018% P, 0.0144% S, 0.067% Cu, 0.1% Al(sol), 0.0169% N, 0.0149% T.O
0.11% C, 0.09% Si, 0.36% Mn, 0.018% P, 0.0144% S, 0.067% Cu, 0.1% Al(sol), 0.0169% N, 0.0149% T.O
0.11% C, 0.09% Si, 0.50% Mn, 0.02% S, 0.02% P, 10.15% Ni, 17.87% Cr, 0.55% Ti. Steel B: 0.10% C, 0.08% Si, 1.54% Mn, 0.11% S, 0.02% P, 9.34% Ni, 18.65% Cr, 0.78% Ti, 1.97% Cu, 0.13% Bi
0.11% C, 0.09% Si, 0.50% Mn, 0.02% S, 0.02% P, 10.15% Ni, 17.87% Cr, 0.55% Ti. Steel B: 0.10% C, 0.08% Si, 1.54% Mn, 0.11% S, 0.02% P, 9.34% Ni, 18.65% Cr, 0.78% Ti, 1.97% Cu, 0.13% Bi
0.11% C, 0.09% Si, 0.50% Mn, 0.02% S, 0.02% P, 10.15% Ni, 17.87% Cr, 0.55% Ti. Steel B: 0.10% C, 0.08% Si, 1.54% Mn, 0.11% S, 0.02% P, 9.34% Ni, 18.65% Cr, 0.78% Ti, 1.97% Cu, 0.13% Bi
0.11% C, 0.09% Si, 0.50% Mn, 0.02% S, 0.02% P, 10.15% Ni, 17.87% Cr, 0.55% Ti. Steel B: 0.10% C, 0.08% Si, 1.54% Mn, 0.11% S, 0.02% P, 9.34% Ni, 18.65% Cr, 0.78% Ti, 1.97% Cu, 0.13% Bi
0.11% C, 0.09% Si, 0.50% Mn, 0.02% S, 0.02% P, 10.15% Ni, 17.87% Cr, 0.55% Ti. Steel B: 0.10% C, 0.08% Si, 1.54% Mn, 0.11% S, 0.02% P, 9.34% Ni, 18.65% Cr, 0.78% Ti, 1.97% Cu, 0.13% Bi
0.11% C, 0.18% Si, 0.70% Mn, 11.75% Cr, 1.75% Mo, 2.50% Ni, 0.33% V
0.11% C, 0.25% Si, 1.10% Mn, 0.004% P, 0.030% S, 0.006% N, 0.06% Cr, 0.05% Ni, 0.13% Cu, 0.022% Al (soluble), 0.04% Al (insoluble)
0.12% C, 0.20% Si, 0.70% Mn, 0.048% P, 0.046% S, 0.005% N
0.12% C, 0.29% Si, 1.01% Mn, 0.014% P, 0.025% S
0.12% C, 0.29% Si, 1.01% Mn, 0.014% P, 0.025% S
0.12% C, 0.29% Si, 1.01% Mn, 0.014% P, 0.025% S
0.12% C, 1.00% Si, 1.50% Mn, 12.50% Cr
0.12% C, 1.00% Si, 1.50% Mn, 12.50% Cr
0.12% C, 1.00% Si, 1.50% Mn, 12.50% Cr
0.12% C, 1.00% Si, 1.50% Mn, 13.00% Cr, 0.60% Mo
0.12% C, 1.00% Si, 1.50% Mn, 13.00% Cr, 0.60% Mo
0.12% C, max. 0.40% Si, 0.55% Mn, 2.25% Cr, 1.00% Mo, 0.50% Ni
0.125% C, 0.73% Mn, 0.41% Si, 0.016% P, 0.016% S, 0.13% Ni, 16.7% Cr, 0.10% Te, steel b: 0.10% C, 1.14% Mn, 0.025% Si, 0.074% P, 0.342% S, 0.040% Te
0.13% C, 0.039% S, 0.51% Mn
0.13% C, 0.31% Si, 0.51% Mn, 0.023% P, 0.009% S, 0.010% Al, 1.50% Cr, 0.06% Mo, 1.55% Ni, <0.01% V
0.13% C, 0.47% Mn, 0.19% Si, 0.29% Cr, 0.08% Ni, 0.49% Mo, 0.23% V
0.13% C, 0.98% Si, 1.08% Mn, 0.04% P, 0.030% Si, 0.11% Cr
0.13% C, 0.98% Si, 1.08% Mn, 0.04% P, 0.030% Si, 0.11% Cr
0.13% C, 0.98% Si, 1.08% Mn, 0.040% P, 0.030% S, 0.011% Cr
0.13% C, 0.98% Si, 1.08% Mn, 0.040% P, 0.030% S, 0.011% Cr
0.13% C, 0.98% Si, 1.08% Mn, 0.040% P, 0.030% S, 0.011% Cr
0.14% C, 0.040% Si, 1.10% Mn, 0.30% S
0.14% C, 0.05% Si, 1.10% Mn, 0.30% S
0.14% C, 0.07% Si, 1.0% Mn
0.14% C, 0.29% Si, 1.44% Mn, 0.001% P, 0.001% S, 0.0004% N, 0.002% O. SR steel: 0.13% C, 0.29% Si, 1.44% Mn, 0.001% P, 0.062% S, 0.0003% N, 0.002% O
0.14% C, 0.29% Si, 1.44% Mn, 0.001% P, 0.001% S, 0.0004% N, 0.002% O. SR steel: 0.13% C, 0.29% Si, 1.44% Mn, 0.001% P, 0.062% S, 0.0003% N, 0.002% O
0.14% C, 0.29% Si, 1.44% Mn, 0.001% P, 0.001% S, 0.0004% N, 0.002% O. SR steel: 0.13% C, 0.29% Si, 1.44% Mn, 0.001% P, 0.062% S, 0.0003% N, 0.002% O
0.14% C, 0.29% Si, 1.44% Mn, 0.001% P, 0.001% S, 0.0004% N, 0.002% O. SR steel: 0.13% C, 0.29% Si, 1.44% Mn, 0.001% P, 0.062% S, 0.0003% N, 0.002% O
0.14% C, 0.29% Si, 1.44% Mn, 0.001% P, 0.001% S, 0.0004% N, 0.002% O. SR steel: 0.13% C, 0.29% Si, 1.44% Mn, 0.001% P, 0.062% S, 0.0003% N, 0.002% O
0.14% C, 0.29% Si, 1.44% Mn, 0.001% P, 0.001% S, 0.0004% N, 0.002% O. SR steel: 0.13% C, 0.29% Si, 1.44% Mn, 0.001% P, 0.062% S, 0.0003% N, 0.002% O
0.14-0.19% C, max. 0.40% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% % S, 1.40-1.70% Cr, 1.40-1.70% Ni
0.145% C, 0.340% Mn, 0.009% S, 0.062% Si, 0.010% P, 0.027% Al, 0.0063% Ca, 0.0036% N
0.147% C, 0.051% Si, 0.53% Mn, 0.010% P, 0.005% S, 2.24% Cr, 0.090% Ni, 0.89% Mo
0.149% C, 0.003% S, 0.005% P, 0.64% Mn, 0.30% Si, 0.53% Al, 0.01% Ni, 0.058% Ti, 0.030% O, 0.033% N
0.149% C, 0.003% S, 0.005% P, 0.64% Mn, 0.30% Si, 0.53% Al, 0.01% Ni, 0.058% Ti, 0.030% O, 0.033% N
0.15% C, 0.05% Si, 0.84% Mn, 0.009% P, 0.033% S, 0.03% Cr, 0.05% Ni, 0.12% Cu, 0.004% N
0.15% C, 0.24% Si, 1.50% Mn, <0.007% S, 0.011-0.014% Ti, 80-120 ppm O, 4-10 ppm N. Bottom Fig.: 0.06% C, 0.14% Si, 1.48% Mn, 0.003% S, 0.0011% Ti, 0.033% Al, 40 ppm N
0.15% C, 0.29% Si, 0.75% Mn, 0.86% Cr, 1.45% Ni, 0.08% Mo
0.15% C, 0.29% Si, 0.75% Mn, 0.86% Cr, 1.45% Ni, 0.08% Mo
0.15% C, 0.3% Si, 1.0% Mn, 0.4% Cr, 0.1% Mo, 0.015% Ti, 0.0015% B
0.15% C, 0.36% Si, 1.43% Mn
0.15% C, 0.44% Si, 0.84% Mn, 0.023% P, 0.018% S, 0.21% Cr, 0.08% Cu
0.15% C, 1.0% Mn, 0.20% Si, 0.04% P, <0.04% P, 0.25% Cr, 0.40% Ni
0.15% C, 1.0% Mn, 0.20% Si, 0.04% S, <0.04% P, 0.25% Cr, 0.40% Ni
0.15-0.19% C, 0.23-0.29% Si, 1.10-1.16% Mn, 0.011-0.022 % P, 0.018-0.030% S, 0.85-1.15% Cr, 0.01-0.08 % Mo, 0.10-0.27% Cu, 0.011-0.035 %Sn, 0.015-0.043 % Al, 0.001-0.004% B
0.15-0.19% C, 0.23-0.29% Si, 1.10-1.16% Mn, 0.011-0.022 % P, 0.018-0.030% S, 0.85-1.15% Cr, 0.01-0.08 % Mo, 0.10-0.27% Cu, 0.011-0.035 %Sn, 0.015-0.043 % Al, 0.001-0.004% B
0.15–0.25% C, 0.01% Si, 0.05% Mn, 0.0006% Al
0.16% C, 0.06% Si, 1.00% Mn, 0.03% P, 0.015% S, 0.004% N
0.16% C, 0.071% Si, 0.7% Mn, 0.008% P, 0.008% S, 0.018% Al
0.16% C, 0.071% Si, 0.7% Mn, 0.008% P, 0.008% S, 0.018% Al
0.16% C, 0.071% Si, 0.7% Mn, 0.008% P, 0.008% S, 0.018% Al
0.16% C, 0.071% Si, 0.7% Mn, 0.008% P, 0.008% S, 0.018% Al
0.16% C, 0.071% Si, 0.7% Mn, 0.008% P, 0.008% S, 0.018% Al
0.16% C, 0.071% Si, 0.7% Mn, 0.008% P, 0.008% S, 0.018% Al
0.16% C, 0.071% Si, 0.7% Mn, 0.008% P, 0.008% S, 0.018% Al
0.16% C, 0.071% Si, 0.7% Mn, 0.008% P, 0.008% S, 0.018% Al
0.16% C, 0.299% Si, 1.355% Mn, 0.023% P, 0.0094% S, 0.002% Ti, 0.002% Nb, 0.003% V. Susceptible: 0.17% C, 0.219% Si, 1.395% Mn, 0.016% P, 0.0097% S, 0.002% Ti, 0.002% Nb, 0.003% V
0.16% C, 0.325%Si, 1.125%Mn, 0.015%P, 0.027%S, 1.25% Cr, 0.020% Mo, 0.065%Al, 0.0035%B
0.16% C, 0.35% Si, 0.67% Mn, 0.015% P, 0.017% S, 0.009% N, 100 ppm O, Al has not been found
0.16% C, 0.35% Si, 0.67% Mn, 0.015% P, 0.017% S, 0.009% N, 100 ppm O, Al has not been found
0.16% C, 0.35% Si, 0.67% Mn, 0.015% P, 0.017% S, 0.009% N, 100 ppm O, Al not detectable
0.16% C, 0.35% Si, 0.67% Mn, 0.015% P, 0.017% S, 0.009% N, 100 ppm O, no trace of Al
0.16% C, 0.35% Si, 0.67% Mn, 0.015% P, 0.017% S, 0.039% N, 100 ppm O, no trace of Al
0.16% C, 0.35% Si, 0.67% Mn, 0.015% P, 0.017% S, 0.039% N, 100 ppm O, no trace of Al
0.16% C, 0.35% Si, 0.67% Mn, 0.15% P, 0.017% S, 0.039% N, 100 ppm O, no trace of Al. Steel b: 0.12% C, 0.20% Si, 0.70% Mn, 0.048% P, 0.046% S, 0.10% Cr, 0.19% Cu, 0.005% N
0.16% C, 0.37% Si, 1.44% Mn, 0.018% P, 0.009% S, 0.031% Al, 0.009% N
0.16% C, 0.37% Si, 1.44% Mn, 0018% P, 0.009% S, 0.09% Cu, 0.02% Cr, 0.07% Ni, 0.031% Al (soluble), 0.009% N
0.16% C, 0.39% Si, 0.50% Mn, 0.011% P, 0.002% S, 2.19% Cr, 0.08% Ni, 0.92% Mo, 0.11% Cu
0.16% C, 0.50% Mn, 0.60% Si, 0.030% P, 0.020% S
0.16% C, 0.66% Mn, 0.008% P, 0.025% S, 0.17% Si, 0.19% Cu, 0.046% Ni, 0.060% Cr
0.16% C, 0.66% Mn, 0.008% P, 0.025% S, 0.17% Si, 0.19% Cu, 0.046% Ni, 0.060% Cr
0.16% C, 0.66% Mn, 0.008% P, 0.025% S, 0.17% Si, 0.19% Cu, 0.046% Ni, 0.060% Cr
0.16% C, 0.66% Mn, 0.008% P, 0.025% S, 0.17% Si, 0.19% Cu, 0.046% Ni, 0.060% Cr
0.16% C, 0.66% Mn, 0.008% P, 0.025% S, 0.17% Si, 0.19% Cu, 0.046% Ni, 0.060% Cr
0.16% C, 0.66% Mn, 0.008% P, 0.025% S, 0.17% Si, 0.19% Cu, 0.046% Ni, 0.060% Cr
0.16% C, 0.66% Mn, 0.008% P, 0.025% S, 0.17% Si, 0.19% Cu, 0.046% Ni, 0.060% Cr
0.16% C, 0.66% Mn, 0.008% P, 0.025% S, 0.17% Si, 0.19% Cu, 0.046% Ni, 0.060% Cr
0.16% C, 0.66% Mn, 0.008% P, 0.025% S, 0.17% Si, 0.19% Cu, 0.046% Ni, 0.060% Cr
0.16% C, 0.66% Mn, 0.008% P, 0.025% S, 0.17% Si, 0.19% Cu, 0.048% Ni, 0.060% Cr
0.16% C, 0.68% Mn, 0.01% P, 0.04% S, 0.19% Si, 0.31% Cu, 0.10% Ni, 0.04% Cr
0.16% C, 0.68% Mn, 0.01% P, 0.04% S, 0.19% Si, 0.31% Cu, 0.10% Ni, 0.04% Cr
0.16% C, 0.68% Mn, 0.01% P, 0.04% S, 0.19% Si, 0.31% Cu, 0.10% Ni, 0.04% Cr
0.16% C, 0.68% Mn, 0.01% P, 0.04% S, 0.19% Si, 0.31% Cu, 0.10% Ni, 0.04% Cr
0.16% C, 0.68% Mn, 0.010% P, 0.027% S, 0.18% Si, 0.19% Cu, 0.054% Ni, 0.056% Cr
0.16% C, 0.68% Mn, 0.010% P, 0.027% S, 0.18% Si, 0.19% Cu, 0.054% Ni, 0.056% Cr
0.16% C, 0.68% Mn, 0.010% P, 0.027% S, 0.18% Si, 0.19% Cu, 0.054% Ni, 0.056% Cr
0.16% C, max. 0.40% Si, 1.15% Mn, 0.95% Cr, 0.024% S
0.16% C, max. 0.40% Si, 1.15% Mn, 0.95% Cr
0.16% C, max. 0.40% Si, 1.15% Mn, 0.95% Cr
0.16% C, max. 0.40% Si, 1.15% Mn, 0.95% Cr
0.160% C, 0.68% Mn, 0.010% P, 0.027% S, 0.18% Si, 0.19% Cu, 0.054% Ni, 0.056% Cr
0.160% C, 0.68% Mn, 0.010% P, 0.027% S, 0.18% Si, 0.19% Cu, 0.054% Ni, 0.056% Cr
0.160% C, 0.68% Mn, 0.010% P, 0.027% S, 0.18% Si, 0.19% Cu, 0.054% Ni, 0.056% Cr
0.167% C, 0.68% Mn, 0.009% P, 0.028% S, 0.19% Si, 0.19% Cu, 0.054% Ni, 0.060% Cr
0.17% C, 0.19% Si, 0.72% Mn, 0.016% S, 1.05% Cr, 0.23% Mo, 0.024% Al, 0.0106% N
0.17% C, 0.40% Si, 1.50% Mn, 0.016% P, 0.015% S, 0.011% N, 0.035% Nbm 0.020% Al (soluble), 0.016% Al (indissoluble)
0.17% C, 0.74% Mn, 0.001% P, 0.03% S, 0.17% Si, 0.33% Cu, 0.09% Ni, 0.05% Cr
0.17% C, 0.74% Mn, 0.01% P, 0.03% S, 0.17% Si, 0.33% Cu, 0.09% Ni, 0.05% Cr
0.17% C, 0.74% Mn, 0.01% P, 0.03% S, 0.17% Si, 0.33% Cu, 0.09% Ni, 0.05% Cr
0.17% C, 1.20% Mn, 0.25% Si, 0.010% P, 0.012% S, 0.025% Al, 0.0025% Ca, 0.0045% O, 0.0070% N. Steel grade B: 0.08% C, 0.44% Mn, 0.23% Si, 0.010% P, 0.012% S, 0.030% Al, 0.0030% Ca, 0.0040% O, 0.0075% N
0.17% C, max. 1.40% Mn, max. 0.045% P, max. 0.045%S, max. 0.009% N
0.17-0.23% C, 0.30-0.60% Si, 1.30-1.60% Mn, max. 0.035% P, max. 0.035% S
0.18% C, 0.13% Si, 0.39% Mn, 0.023% P, 0.14% S, 13.6% Cr, 0.66% Ni
0.18% C, 0.13% Si, 0.39% Mn, 0.023% P, 0.14% S, 13.6% Cr, 0.66% Ni
0.18% C, 0.15% Si, 0.45% Mn, 0.014% P, 0.003% S, 11.30% Cr, 0.38% Ni, 0.83% Mo, 0.28% V, 0.10% Cu, 0.007% Al
0.18% C, 0.16% Si, 0.76% Mn, 0.03% S, 0.25% Ni, 1.25% Cr, 0.24% Mo
0.18% C, 0.16% Si, 0.76% Mn, 0.03% S, 0.25% Ni, 1.25% Cr, 0.24% Mo
0.18% C, 0.16% Si, 0.76% Mn, 0.03% S, 0.25% Ni, 1.25% Cr, 0.24% Mo
0.18% C, 0.18% Si, 1.46% Mn, 0.006% P, 0.002% S, 0.88% Ni, 0.12% Cr, 0.51% Mo, 0.01% V
0.18% C, 0.35% Si, 11.5% Cr, 0.60% Ni, 0.50% Mo, 0.25% V, 0.30% Nb
0.18% C, 0.4% Si, 1.5% Mn, 0.01% P, 0.001% S, others: Nb, Ti, B
0.18% C, 0.80% Mn, 0.01% P, 0.03% S, 0.18% Si, 0.33% Cu, 0.10% Ni, 0.05% Cr
0.18% C, 0.80% Mn, 0.01% P, 0.03% S, 0.18% Si, 0.33% Cu, 0.10% Ni, 0.05% Cr
0.18% C, 0.80% Mn, 0.01% P, 0.03% S, 0.18% Si, 0.33% Cu, 0.10% Ni, 0.05% Cr
0.18% C, 0.80% Mn, 0.01% P, 0.03% S, 0.18% Si, 0.33% Cu, 0.10% Ni, 0.05% Cr
0.18% C, 0.80% Mn, 0.01% P, 0.03% S, 0.18% Si, 0.33% Cu, 0.10% Ni, 0.05% Cr
0.18% C, 0.80% Mn, 0.01% P, 0.03% S, 0.18% Si, 0.33% Cu, 0.10% Ni, 0.05% Cr
0.18% C, 0.80% Mn, 0.01% P, 0.03% S, 0.18% Si, 0.33% Cu, 0.10% Ni, 0.05% Cr
0.18% C, 0.80% Si, 0.01% P, 0.03% S, 0.18% Si, 0.33% Cu, 0.10% Ni, 0.05% Cr
0.18% C, 0.80% Si, 0.01% P, 0.03% S, 0.18% Si, 0.33% Cu, 0.10% Ni, 0.05% Cr
0.18% C, 1.96% P
0.18-0.24% C, max. 0.50% Si, 0.40-0.80% Mn, max. 0.025% P, max. 0.015% S, 11-12.50% Cr, 0.80-1.20% Mo, 0.25-0.35% V
0.19% C, 0.06% Si, 0.13% Mn, 0.013% P, 0.01% S, 0.52% Ni, 11.01% Cr, 0.09% Mo, 3.45% W, 0.21% Co, 0.06% V, 0.03% N, 0.01% Nb
0.19% C, 0.14% Si, 0.54% Mn, 0.012% P, 0.003% S, 11.10% Cr, 0.44% Ni, 0.92% Mo, 0.27% V, 0.15% Cu
0.19% C, 0.25% Si, 0.30% Mn, 1.25% Cr, 0.20% Mo, 4.05% Ni
0.19% C, 0.25% Si, 0.30% Mn, 1.25% Cr, 0.20% Mo, 4.05% Ni
0.19% C, 0.26% Si, 1.36% Mn, 0.007% P, 0.007% S, 0.68% Ni, 0.19% Cr, 0.04% Cu, 0.48% Mo, trace V
0.19% C, 0.30% Si, 0.55% Mn, 10.75% Cr, 0.75% Mo, 0.55% Ni, 0.20% V, 0.33% Nb, 0.08% N, 0.0015% B
0.19% C, 0.30% Si, 0.55% Mn, 10.75% Cr, 0.75% Mo, 0.55% Ni, 0.20% V, 0.33% Nb, 0.08% N, 0.0015% B
0.20% C, 0.17% Si, 0.48% Mn, 0.020% P, 0.004% S, 10.40% Cr, 0.47% Ni, 0.54% Mo, 0.13% V, 0.05% Cu, 0.006% Al
0.20% C, 0.28% Si, 0.80% Mn
0.20% C, 0.40% Si, 0.80% Mn, 0.53% Cr, 0.20% Mo, 0.55% Ni
0.20% C, 0.50% Si, 1.00% Mn, 11.25% Cr, 1.00% Mo, 0.55% Ni, 0.30% V
0.20% C, 0.60% Mn, 0.44% Si, 0.028% S, 0.032% P, 1.25% Cr, 0.15% Mo, 0.16% Ni, 0.14% Cu, 0.080% Al, 0.038% Al, 0.038% O, 0.014% N
0.20% C, 0.60% Mn, 0.44% Si, 0.028% S, 0.032% P, 1.25% Cr, 0.15% Mo, 0.16% Ni, 0.14% Cu, 0.080% Al, 0.038% Al, 0.038% O, 0.014% N
0.20% C, 1.00% Si, 1.50% Mn, 13.00% Cr
0.20% C, 1.00% Si, 1.50% Mn, 13.00% Cr
0.20% Mn, 0.57% Ti. Steel 1b: 0.19% Mn, 0.06% Ti. Steel 1c: 0.20% Mn, 0.35% Ti. Steel 1d: 0.20% Mn, 0.57% Ti
0.20-0.25% C, 0.80-0.90% Mn, 0.10-0.90% Si, 0.010% S, 0.005% P, 0.090-0.16% Al(total), 0.005-0.0015% N
0.20-0.30% C, 0.035-0.080% Si, 0.40-1.50% Mn, 0.010-0.030% P, 0.002-0.012% S, 0.030-0.14%% Cr, 0.15-0.25% Ni, 0.020-0.030% Cu, 0.010-0.012% Nb, 28-40 ppm N
0.20-0.30% C, 0.035-0.080% Si, 0.40-1.50% Mn, 0.010-0.030% P, 0.002-0.012% S, 0.030-0.14%% Cr, 0.15-0.25% Ni, 0.020-0.030% Cu, 0.010-0.012% Nb, 28-40 ppm N
0.20-0.30% C, max. 1.00% Si, 8.00-10.00% Mn, max. 0.045% P, max. 0.015% S, 24.00-26.00% Cr, 6.00-8.00% Ni, 0.20-0.40% N
0.200% C, 0.2730% Si. 0.8710% Mn, 0.0140% P, 0.0300% S, 0.0025% Ca, 0.022% Al(tot), 0.0210% Al(sol), 0.0038% O
0.200% C, 0.2730% Si. 0.8710% Mn, 0.0140% P, 0.0300% S, 0.0025% Ca, 0.022% Al(tot), 0.0210% Al(sol), 0.0038% O
0.200% C, 0.2730% Si. 0.8710% Mn, 0.0140% P, 0.0300% S, 0.0025% Ca, 0.022% Al(tot), 0.0210% Al(sol), 0.0038% O
0.200% C, 0.2730% Si. 0.8710% Mn, 0.0140% P, 0.0300% S, 0.0025% Ca, 0.022% Al(tot), 0.0210% Al(sol), 0.0038% O
0.21% C, 0.069% S, 0.47% Mn, 0.045% P, 0.017% Si, 0.024% Cu, 0.0035% N, 0.013% O, Mn/S ratio: 6.8:1, Mn/C ratio: 2:1
0.21% C, 0.069% S, 0.47% Mn, 0.045% P, 0.017% Si, 0.024% Cu, 0.0035% N, 0.013% O, Mn/S ratio: 6.8:1, Mn/C ratio: 2:1
0.21% C, 0.069% S, 0.47% Mn, 0.045% P, 0.017% Si, 0.024% Cu, 0.0035% N, 0.013% O, Mn/S ratio: 6.8:1, Mn/C ratio: 2:1
0.21% C, 0.20% Si, 0.79% Mn, 0.038% P, 0.027% S, 0.01% Cr, 0.010% Cu
0.21% C, 0.22% Si, 0.53% Mn, 0.014% P, 0.002% S, 11.40% Cr, 0.58% Ni, 0.27% V, 0.04% Cu, 0.014% Al
0.21% C, 0.35% Si, 0.60% Mn, 13.00% Cr, 0.60% Mn
0.21% C, 0.35% Si, 0.60% Mn, 13.00% Cr, 0.60% Ni
0.21% C, 0.35% Si, 0.60% Mn, 13.00% Cr, 0.60% Ni
0.2180% C, 0.2370% Si. 0.8710% Mn, 0.015% P, 0.030% S, 0.0025% Ca, 0.019% Al(tot), 0.0140% Al(sol), 0.0048% O
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.011% P, 0.014% S, 0.029% Al, 0.26% Si, 1.01% Mn, 0.09% Ni, 0.11% Cr, 0.02% Mo, 0.17% Cu
0.22% C, 0.24% Si, 0.50% Mn, 0.032% P, 0.029% S
0.22% C, 0.28% Si, 0.89% Mn, 0.021% P, 0.013% S, 0.115% Al, 0.014% N
0.22% C, 0.54% Si, 1.29% Mn, 0.10% Ti, 0.025% Al
0.22% C, 0.55% Si, 1.60% Mn
0.22% C, 0.55% Si, 1.60% Mn
0.224% C, 1.046% Mn, 0.256% Si, 0.0019% S, 0.0035% B, 0.0395% Yi, 0.2185% Cr, 0.0044% N, 0.0370% Al
0.2270% C, 0.2490% Si. 0.8720% Mn, 0.0110% P, 0.0330% S, 0.0029% Ca, 0.019% Al(tot), 0.0150% Al(sol), 0.0030% O
0.23% C, 0.41% Si, 1.07% Mn, 0.021% P, 0.022% S, 0.007% Al, 40 ppm O
0.234% C, 0.003% S, 0.011% P, 0.50% Mn, 0.28% Si, 1.70% Al, 0.02% Ni, 0.003% Ti, 0.006% O, 0.064% N
0.234% C, 0.003% S, 0.011% P, 0.50% Mn, 0.28% Si, 1.70% Al, 0.02% Ni, 0.003% Ti, 0.006% O, 0.064% N
0.234% C, 0.003% S, 0.011% P, 0.50% Mn, 0.28% Si, 1.70% Al, 0.02% Ni, 0.003% Ti, 0.006% O, 0.064% N
0.234% C, 0.003% S, 0.011% P, 0.50% Mn, 0.28% Si, 1.70% Al, 0.02% Ni, 0.003% Ti, 0.006% O, 0.064% N
0.24% C, 0.05% Mn, 0.65% Si
0.24% C, 0.38% Si, 1.39% Mn, 0.030% P, 0.038% S
0.24% C, 0.38% Si, 1.39% Mn, 0.030% P, 0.038% S
0.24% C, 1.07% Mn, 0.26% Si, 0.010% P, 0.003% S, 0.12% Cu, 0.42% Ni, 0.29% Cr, 0.08% Mo
0.25% C, 0.40% Si, 0.75% Mn, <0.01% P, <0.020% S
0.25% C, 0.50% Mn
0.25% C, 1.01% Mn, 0.28% Si
0.25% C, 1.10% Mn, <0.03% Si, 0.019% S, 0.011% P
0.25% C, 1.10% Mn, <0.03% Si, 0.019% S, 0.011% P
0.2580% C, 0.2450% Si, 0.8020% Mn, 0.0100% P, 0.0270% S, 0.0013% Ca, 0.024% Al(tot), 0.0210% Al(sol), 0.0017% O
0.26% C, 0.43% Si, 0.74% Mn, 0.011% P, 0.006% S, 0.020% Al
0.26% C, 0.43% Si, 0.74% Mn, 0.011% P, 0.006% S, 0.020% Al
0.26% C, 0.48% Si, 0.84% Mn, 0.022% P, 0.001% Al, 74 ppm O
0.26% C, 0.48% Si, 0.84% Mn, 0.022% P, 0.011% S, 0.038% Al, 47 ppm O
0.26% C, 0.48% Si, 0.84% Mn, 0.022% P, 0.011% S, 0.038% Al, 47 ppm O
0.26-0.34% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.030% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.26-0.34% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.030% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.27% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.20% Mo
0.27% C, 0.51% Mn, 0.010% P, 0.007% S, 0.31% Si, 1.08% Cr, 0.24% Mo, 0.030% V, 0.032% V, 0.0032% B, 0.061% Ti, 0.056% Al, 0.010% N
0.27% C, 2.11% Si, 1.60% Mn, 0.013% P, 0.013% S, 0.49% Cr, 0.003% Mo, 0.233% Al, 0.002% B, 0.001% Ti, 0.011% N
0.278% C, 0.441% Si, 0.66% Mn, 0.049% Al
0.30% C, 0.22% Si, 1.03% Mn, 0.027% P, 0.018% S, 0.010% N
0.30% C, 0.24% Si, 0.47% Mn, 0.016% P, 0.003% S, 2.36% Cr, 0.12% Ni, 0.18% Mo, 0.13% V, 0.19% Cu
0.30% C, 0.40% Si, 0.45% Mn, 2.00% Cr, 0.40% Mo, 1.90% Ni
0.30% C, 0.40% Si, 0.45% Mn, 2.00% Cr, 0.40% Mo, 1.90% Ni
0.30% C, 0.40% Si, 0.45% Mn, 2.00% Cr, 0.40% Mo, 1.90% Ni
0.30% C, 0.40% Si, 0.45% Mn, 2.00% Cr, 0.40% Mo, 1.90% Ni
0.30% C, 0.40% Si, 0.45% Mn, 2.00% Cr, 0.40% Mo, 1.90% Ni
0.30% C, 0.40% Si, 0.55% Mn, 2.50% Cr, 0.20% Mo, 0.15% V
0.30% C, 0.86% Mn, 0.44% Si
0.30% C, 1% Mn, 4% Cr, 0.4% V, max. 0.2% S, max. 0.2% P. ESR (electro slag remelting): 0.28% C, 1.00% Mn, 4.20% Cr, 0.34% V, 1.01% Mo, 0.24% Si, 0.067% Al, 0.0161% N, 0.031% P, 0.011% S
0.30% Si: 0.65% C, 0.30% Si, 27.3% Mn, 8.36% Al, 0.42% Mo, balance is Fe. Steel with 0.82% C: 0.97% C, 0.82% Si, 29.87% Mn, 8.7% Al, 0.44% Mo, Fe is balance
0.31% C, 0.030% Si, 1.14% Mn, 0.011% P, 0.007% S, 0.15% Cu, 0.10% Ni, 0.08% Cr, 0.024% Al, 0.0035% Ca
0.31% C, 0.28% Si, 0.8% Mn
0.31% C, 0.40% Si, 0.38% Mn, 0.025% P, 0.010% S, 12.90% Cr, 0.19% Ni, 0.06% Cu, 0.011% Al
0.31% C, 0.68% Mn, 0.5% Si, 12.32% Cr, 0.21% Ni, 0.019% P, 0.06% S
0.32% C, 0.35% Si, 0.60% Mn, 3.00% Cr, 1.00% Mo, 0.30% V
0.32% C, 0.35% Si, 0.60% Mn, 3.00% Cr, 1.00% Mo, 0.30% V
0.32% C, 0.60-1.10% Si, max. 0.010% P, max. 0.003% S, 1.35% Cr, 0.80% Mo, 0.14% V, max. 1.00% Ni, 0.92-0.96% CEIIW, 0.55-0.57% CET
0.33% C, 0.25% Si, 0.60% Mn, 0.011% P, 0.023% S, 0.009% N
0.33% C, 0.25% Si, 0.60% Mn, 0.011% P, 0.023% S, 0.009% N
0.33% C, 0.34% Si, 0.60% Mn, 0.013% P, 0.018% S, 2.43% Cr, 0.12% Ni, 0.49% Mo, 0.05% Cu
0.33% C, 0.34% Si, 0.60% Mn, 0.013% P, 0.018% S, 2.43% Cr, 0.12% Ni, 0.49% Mo, 0.05% Cu
0.33% C, 0.34% Si, 0.60% Mn, 0.013% P, 0.018% S, 2.43% Cr, 0.12% Ni, 0.49% Mo, 0.05% Cu
0.33% C, 0.34% Si, 0.60% Mn, 0.013% P, 0.018% S, 2.43% Cr, 0.12% Ni, 0.49% Mo, 0.05% Cu
0.34% C, 0.32% Si, 1.42% Mn, 0.013% P, 0.056% S, 1.78% Cr, 0.16% Ni, 0.16% Mo, 0.01% V, 0.12% Cu, 0.022% Al
0.34% C, 0.40% Si, 0.65% Mn, 1.50% Cr, 0.23% Mo, 1.50% Ni
0.34% C, 0.40% Si, 0.65% Mn, 1.50% Cr, 0.23% Mo, 1.50% Ni
0.34% C, 0.40% Si, 0.75% Mn, 1.05% Cr, 0.23% Mo
0.34% C, 0.40% Si, 0.75% Mn, 1.05% Cr, 0.23% Mo
0.35% C, 0.20% Si, 0.53% Mn, 0.009% P, 0.001% S, 1.51% Cr, 1.65% Ni, 0.10% Cu, 0.007% Al
0.35% C, 0.25% Si, 0.40% Mn, 1.4% Cr, 3.0% Ni, 0.50% Mo
0.35% C, 0.25% Si, 0.40% Mn, 1.4% Cr, 3.0% Ni, 0.50% Mo
0.35% C, 0.25% Si, 0.40% Mn, 1.4% Cr, 3.0% Ni, 0.50% Mo
0.35% C, 0.25% Si, 0.40% Mn, 1.4% Cr, 3.0% Ni, 0.50% Mo
0.35–0.40% C, 0.01% Si, 0.0004% Al, 0.001% Mn
0.36% C, 1.00% Mn, 0.50% Cr, 1% Mn
0.37% C, 0.07% Si, 0.75% Mn, 0.009% P, 0.010% S, 0.008% Mo, 0.030% Cu, 0.036% Al, 0.0040% B, 0.0070% N. Steel 2: 0.38% C, 0.08% Si, 0.73% Mn, 0.010% P, 0.005% S, 0.006% Mo, 0.035% Ti, 0.0046% Cu, 0.042% Al, 0.0033% B, 0.0077% N
0.37% C, 0.20% Si, 0.50% Mn, 0.01% P, 0.001% S, 5.11% Cr, 0.06% Ni, 2.38% Mo, 0.017% Co, 0.53% V, 0.046% Cu, 0.001% W, 0.018% Al, 0.001% Ce, 0.0001% B, 0.0007% Ca
0.37% C, 0.23% Si, 0.74% Mn, 0.022% P, 0.045% S, 1.07% Cr, 0.09% Ni, 0.01% Mo, 0.12% Cu, 0.01% V
0.37% C, 0.30% Si, 0.79% Mn, 0.023% P, 0.003% Cr, 15.70% Cr, 0.80% Ni, 1.03% Mo, 0.13% Cu, 0.006% Al
0.37% C, 0.36% Si, 1.47% Mn, 0.019% P, 0.071% S, 1.91% Cr, 10.16% Ni, 0.18% Mo, 0.01% V, 0.16% Cu, 0.03% W, 0.015% Al
0.37% C, 0.36% Si, 1.47% Mn, 0.019% P, 0.071% S, 1.91% Cr, 10.16% Ni, 0.18% Mo, 0.01% V, 0.16% Cu, 0.03% W, 0.015% Al
0.37% C, 0.58% Si, 0.38% Mn, 0.01% P, 0.001% S, 5.08% Cr, 0.10% Ni, 1.16% Mo, 0.019% Co, 0.72% V, 0.078% Cu, 0.008% W, 0.001% Al, 0.002% Ce, 0.0002% B, <0.0006% Ca
0.37% C, 1.00% Si, 0.38% Mn, 5.15% Cr, 1.30% Mo, 0.40% V
0.37% C, 1.00% Si, 5.15% Cr, 1.30% Mo, 0.40% V
0.38% C, 0.22% Si, 1.5% Mn, 0.12% V, 0.035% Al, 0.02% S, 0.02% P, 0.3% Cr
0.38% C, 0.34% Si, 1.49% Mn, 0.011% P, 0.064% S, 1.82% Cr, 0.17% Ni, 0.17% Mo, 0.02% V, 0.14% Cu, 0.008% Al
0.38% C, 0.50% Si, 0.37% Mn, 0.01% P, 0.002% S, 5.05% Cr, 0.15% Ni, 1.09% Mo, 0.019% Co, 0.65% V, 0.072% Cu, 0.002% W, 0.001% Al, 0.001% Ce, 0.0001% B, 0.0007% Ca
0.38% C, 0.97% Si, 0.36% Mn, 0.009% P, 0.002% S, 5.05% Cr, 0.04% Ni, 1.21% Mo, 1.00% V, 0.04% Cu, 0.014% Al
0.38% C, 1.06% Si, 0.43% Mn, 0.019% P, 0.0006% S, 5.29% Cr, 0.13% Ni, 0.048% Co, 0.94% V, 0.011% Al, 0.007% N, 0.0001% B, 0.0004% Ca, 0.00028% O
0.38% C, 1.06% Si, 0.43% Mn, 0.019% P, 0.0006% S, 5.29% Cr, 0.13% Ni, 0.048% Co, 0.94% V, 0.011% Al, 0.007% N, 0.0001% B, 0.0004% Ca, 0.00028% O
0.38% C, 1.06% Si, 0.43% Mn, 0.019% P, 0.0006% S, 5.29% Cr, 0.13% Ni, 0.048% Co, 0.94% V, 0.011% Al, 0.007% N, 0.0001% B, 0.0004% Ca, 0.00028% O
0.39% C, 0.27% Si, 0.25% Mn, 0.55% Cr, 3.25% Mo, 0.14% Ni
0.39% C, 0.35% Si, 0.44% Mn, 0.007% P, 0.006% S, 1.39% Cr, 2.88% Ni, 0.61% Mo, 0.003% N
0.39% C, 0.36% Si, 0.28% Mn, 0.022% P, 0.002% S, 12.70% Cr, 0.19% Ni, 0.04% Mo, 0.02% V, 0.07% Cu, 0.012% Al
0.39% C, 0.45% Si, 0.26% Mn, 0.026% P, 0.003% S, 12.80% Cr, 0.20% Ni, 0.11% Mo, 0.06% Cu, 0.023% Al
0.39% C, 0.49% Si, 0.37% Mn, 0.02% P, 0.01% S, 5.35% Cr, 0.11% Ni, 1.05% Mo, 0.018% Co, 0.69% V, 0.071% Cu, 0.004% W, 0.001% Al, 0.001% Ce, 0.0001% B, 0.0006% Ca
0.39% C, 0.96% Si, 0.36% Mn, 0.01% P, <0.001% S, 5.21% Cr, 0.15% Ni, 1.28% Mo, 0.019% Co, 0.91% V, 0.074% Cu, 0.02% W, 0.041% Al, 0.003% Ce, 0.0001% B, 0.0007% Ca
0.39% C, 0.96% Si, 0.36% Mn, 0.01% P, <0.001% S, 5.21% Cr, 0.15% Ni, 1.28% Mo, 0.019% Co, 0.91% V, 0.074% Cu, 0.02% W, 0.041% Al, 0.003% Ce, 0.0001% B, 0.0007% Ca
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V. DIEVAR: 0.35% C, 0.2% Si, 0.5% Mn, 5.0% Cr, 2.3% Mo, 0.6% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V. DIEVAR: 0.35% C, 0.2% Si, 0.5% Mn, 5.0% Cr, 2.3% Mo, 0.6% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V. DIEVAR: 0.35% C, 0.2% Si, 0.5% Mn, 5.0% Cr, 2.3% Mo, 0.6% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.4% Mn, 5.3% Cr, 1.3% Mo, 0.9% V
0.39% C, 1.0% Si, 0.40% Mn, 5.3% Cr, 1.3% Mo, 0.9% V, 0.0005% S
0.39% C, 1.00% Si, 0.38% Mn, 5.15% Cr, 1.35% Cr, 1.00% V
0.39% C, 1.00% Si, 0.40% Mn, 0.0005% S, 5.30% Cr, 1.30% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 0.0005% S, 5.30% Cr, 1.30% Mo, 0.90% V
0.39% C, 1.03% Si, 0.37% Mn, 0.0005% S, 5.15% Cr, 0.20% Ni, 1.29% Mo, 0.039% W, 0.021% Co, 0.93% V, 0.027% Ti, 0.020% Al
0.39% C, 1.03% Si, 0.37% Mn, 0.0005% S, 5.15% Cr, 0.20% Ni, 1.29% Mo, 0.039% W, 0.021% Co, 0.93% V, 0.027% Ti, 0.020% Al
0.39% C, 1.03% Si, 0.37% Mn, 0.0005% S, 5.15% Cr, 0.20% Ni, 1.29% Mo, 0.039% W, 0.021% Co, 0.93% V, 0.027% Ti, 0.020% Al
0.39% C, 1.06% Si, 0.32% Mn, 0.019% P, 0.004% S, 4.91% Cr, 0.11% Ni, 1.17% Mo, 0.37% V, 0.011% Ti
0.39-0.40% C, 0.85-1.00% Si, 0.35-0.40% Mn, 4.80-5.30% Cr, 1.28-1.30% Mo
0.40% C, 0.21% Si, 0.79% Mn, 0.01% P, 0.02% S, 1.20% Cr, 0.21% Mo
0.40% C, 0.21% Si, 0.79% Mn, 0.01% P, 0.02% S, 1.20% Cr, 0.21% Mo
0.40% C, 0.30% Si, 1.45% Mn, 1.95% Cr, 0.20% Mo
0.40% C, 0.33% Mn, 0.32% Si, 0.001% S, 0.009% P, 3.20% Ni, 0.91% Cr, 0.61% Mo, 0.15% V, 0.006% Al, 0.009% Cu, 0.011% Sn, 0.009% Sb, 0.001% As, 1 ppm H2, 20 ppm O, 56 ppm N
0.40% C, 0.36% Si, 1.44% Mn, 0.015% P, 0.077% S, 1.82% Cr, 0.12% Ni, 0.19% Mo, 0.17% Cu, 0.013% Al
0.40% C, 0.40% Mn, 1.0% Si, 5.30% Cr, 0.10% Ni, 1.30% Mo, 0.90% V, 0.10% A
0.40% C, 0.40% Si, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 0.40% Si, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 0.85% Mn, 0.013% P, 0.077% S, 0.28% Si, 0.99% Cr, 0.010% Al, 0.15% Ni, 0.21% Mo, 0.23% Cu, 0.009% Sn. Low sulfur: 0.41% C, 0.94% Mn, 0.010% P, 0.012% S, 0.28% Si, 0.0094% N, 1.01% Cr, 0.028% Al, 0.15% Ni, 0.22% Mo, 0.17% Cu, 0.007% Sn.
0.40% C, 0.85% Mn, 0.013% P, 0.077% S, 0.28% Si, 0.99% Cr, 0.010% Al, 0.15% Ni, 0.21% Mo, 0.23% Cu, 0.009% Sn. Low sulfur: 0.41% C, 0.94% Mn, 0.010% P, 0.012% S, 0.28% Si, 0.0094% N, 1.01% Cr, 0.028% Al, 0.15% Ni, 0.22% Mo, 0.17% Cu, 0.007% Sn.
0.40% C, 0.85% Mn, 0.013% P, 0.077% S, 0.28% Si, 0.99% Cr, 0.010% Al, 0.15% Ni, 0.21% Mo, 0.23% Cu, 0.009% Sn. Low sulfur: 0.41% C, 0.94% Mn, 0.010% P, 0.012% S, 0.28% Si, 0.0094% N, 1.01% Cr, 0.028% Al, 0.15% Ni, 0.22% Mo, 0.17% Cu, 0.007% Sn.
0.40% C, 0.99% Si, 0.37% Mn, 0.01% P, 0.0003% S, 5.22% Cr, 0.10% Ni, 1.26% Mo, 0.019% Co, 0.92% V, 0.077% Cu, 0.001% W, 0.044% Al, 0.003% Ce, 0.0001% B, 0.0006% Ca
0.40% C, 1.02% Si, 0.38% Mn, 0.014% P, 0.002% S, 5.12% Cr, 0.10% Ni, 1.25% Mo, 1.02% V, 0.15% Cu, 0.0135 Al
0.40-0.50% C, 2.70-3.30% Si, max. 0.80% Mn, max. 0.040% P, max. 0.030% S, 8.00-10.00% Cr, max. 0.60% Ni
0.41% C, 0.20% Si, 0.75% Mn, 1.05% Cr, 0.23% Mo
0.41% C, 0.20% Si, 0.75% Mn, 1.05% Cr, 0.23% Mo
0.41% C, 0.20% Si, 0.75% Mn, 1.05% Cr, 0.23% Mo
0.41% C, 0.20% Si, 0.75% Mn, 1.05% Cr
0.41% C, 0.20% Si, 0.75% Mn, 1.05% Cr
0.41% C, 0.40% Si, 0.65% Mn, 1.65% Cr, 0.33% Mo, 1.00% Al
0.41% C, 0.40% Si, 0.65% Mn, 1.65% Cr, 0.33% Mo, 1.00% Al
0.41% C, 0.40% Si, 0.65% Mn, 1.65% Cr, 0.33% Mo, 1.00% Al
0.41% C, 0.40% Si, 0.75% Mn, 1.05% Cr, 0.28% Mo
0.42% C, 0.20% Si, 0.80% Mn, 0.025% S, 1.00% Cr, <10 ppm O
0.42% C, 0.25% Si, 0.65% Mn, 0.01% P, 0.002% S, 1.15% Cr, 0.2% Mo
0.42% C, 0.25% Si, 0.65% Mn, 0.01% P, 0.002% S, 1.15% Cr, 0.2% Mo
0.42% C, 0.25% Si, 0.65% Mn, 0.01% P, 0.002% S, 1.15% Cr, 0.2% Mo
0.42% C, 0.25% Si, 0.65% Mn, 0.01% P, 0.002% S, 1.15% Cr, 0.2% Mo
0.42% C, 0.25% Si, 0.65% Mn, 0.01% P, 0.002% S, 1.15% Cr, 0.2% Mo
0.42% C, 0.25% Si, 0.65% Mn, 0.01% P, 0.002% S, 1.15% Cr, 0.2% Mo
0.42% C, 0.25% Si, 0.65% Mn, 0.01% P, 0.002% S, 1.15% Cr, 0.2% Mo
0.42% C, 0.26% Si, 0.64% Mn, 0.01% P, 0.004% S, 0.0010% Ca, 0.0010% Mg, 1.14% Cr, 0.23% Mo
0.42% C, 0.26% Si, 0.64% Mn, 0.01% P, 0.004% S, 0.0010% Ca, 0.0010% Mg, 1.14% Cr, 0.23% Mo
0.42% C, 0.26% Si, 0.64% Mn, 0.01% P, 0.004% S, 0.0010% Ca, 0.0010% Mg, 1.14% Cr, 0.23% Mo
0.42% C, 0.26% Si, 0.64% Mn, 0.01% P, 0.004% S, 0.0010% Ca, 0.0010% Mg, 1.14% Cr, 0.23% Mo
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S
0.43% C, 0.14% Si, 0.30% Mn, 0.003% P, 0.001% S, 1.10% Cr, 0.52% Mo, 0.30% V, 0.03% Nb, 0.01% Al
0.44% C, 0.20% Si, 0.73% Mn, 0.023% P, 0.019% S
0.44% C, 0.28% Si, 0.72% Mn, 0.011% P, 0.051% S, 0.95% Cr, 0.11% Ni, 0.19% Mo, 0.14% Cu
0.44% C, 0.28% Si, 0.72% Mn, 0.011% P, 0.051% S, 0.95% Cr, 0.11% Ni, 0.19% Mo, 0.14% Cu
0.45 %C, 0.76%Mn, 0.38 % Si, 0.05 % S, 0.041 %P
0.45% C, 0.0037% N, 0.28% Si, 0.78% Mn, 0.014% P, 0.018% S, 0.002% Al, 0.0114% O
0.45% C, 0.18% Si, 0.82% Mn, 0.071% P, 0.15% S
0.45% C, 0.18% Si, 0.82% Mn, 0.071% P, 0.15% S
0.45% C, 0.18% Si, 0.82% Mn, 0.071% P, 0.15% S
0.45% C, 0.20% Si, 0.80% Mn, 0.02% P, 0.008% S, 0.94% Cr, 0.15% Mo, 0.07% Cu
0.45% C, 0.21% Si, 0.74% Mn, 0.011% S, 0.009% P
0.45% C, 0.21% Si, 0.74% Mn, 0.011% S, 0.009% P
0.45% C, 0.22% Si, 0.70% Mn, 0.034% S, 0.002% Al, 39 ppm O2
0.45% C, 0.22% Si, 0.70% Mn, 0.034% S, 0.002% Al, 39 ppm O2
0.45% C, 0.22% Si, 0.70% Mn, 0.034% S, 0.002% Al, 39 ppm O
0.45% C, 0.22% Si, 0.70% Mn, 0.034% S, 0.002% Al, 39 ppm O
0.45% C, 0.24% Si, 0.27% Mn, 0.011% P, 0.005% S, 1.31% Cr, 4.00% Ni, 0.18% Mo, 0.11% Cu, 0.008% Al
0.45% C
0.46% C, 0.22% Si, 0.67% Mn, 0.028% S
0.46% C, 0.22% Si, 0.67% Mn, 0.038% S
0.46% C, 0.31% Si, 0.36% Mn, 0.028% P, 0.003% S, 3.33% Cr, 0.17% Ni, 1.65% Mo, 0.25% V, 0.15% Cu, 0.014% Al
0.46% C, 0.40% Si, 0.65% Mn, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.47% C, 1.00% Si, 1.00% Mn, 13.50% Cr
0.47-0.55% C, 0.15-0.35% Si, 0.80-1.10% Mn, 0.030% P, 0.030% S, 0.90-1.20% Cr, 0.10-0.20% V
0.48% C, 0.32% Si, 0.34% Mn, 0.021% P, 0.004% S, 14.50% Cr, 0.10% Ni, 0.55% Mo, 0.11% V, 0.03% Cu, 0.007% Al
0.49% C, 0.27% Si, 0.67% Mn, 0.009% P, 0.003% S, 3.13% Cr, 0.13% Ni, 1.39% Mo, 0.22% V, 0.10% Cu, 0.020% Al
0.49% C, 0.31% Si, 0.69% Mn, 0.011% P, 0.009% S, 3.13% Cr, 0.15% Ni, 1.36% Mo, 0.23% V, 0.15% Cu, 0.009% Al
0.5-3% CaO, >85% MgO, 0.5-4% Al2O3, 1-3% SiO2, rest. 2-8%
0.50% C, 0.40% Si, 1.00% Mn, 0.020% P, 0.018% S, 1.10% Cr, 0.22% V
0.50% C, 0.50% Si, 0.70% Mn, 3.25% Cr, 0.25% V
0.50% C, 0.50% Si, 0.70% Mn, 3.25% Cr, 1.50% Mo, 0.25% V
0.50% C, 0.50% Si, 0.70% Mn, 3.25% Cr, 1.50% Mo, 0.25% V
0.50% C, 0.70% Mn, 0.40% Si, <0.02% P, <0.02% S, 2.5% Cr, 0.50% Mo
0.50% C, 0.91% Si, 0.41% Mn, 0.019% P, 0.0056% S, 7.91% Cr, 0.14% Ni, 0.019% Co, 0.39% V, 0.060% Al, 0.038% N, 0.0001% B, 0.0008% Ca, 0.00100% O
0.50% C
0.50% C
0.51% C, 0.34% Si, 0.96% Mn, 0.014% P, 0.003% S, 1.07% Cr, 0.06% Mo, 0.08% Ni, 0.012% Al, 0.13% Cu, 0.001% Nb, 0.004% Ti, 0.17% V, 0.01% Sn, 0.0009% Ca, 0.0002% B
0.52% C, 0.35% Si, 0.96% Mn, 0.93% Cr, 0.12% V, 0.007% S, 0.010% Al
0.52% C, 0.35% Si, 0.96% Mn, 0.93% Cr, 0.12% V, 0.007% S, 0.010% Al
0.52% C, 0.35% Si, 0.96% Mn, 0.93% Cr, 0.12% V, 0.007% S, 0.010% Al
0.52% C, 0.35% Si, 0.96% Mn, 0.93% Cr, 0.12% V, 0.007% S, 0.010% Al
0.55% C, 0.07% Si, 0.04% Mn, 0.018% P, 0.013% S
0.55% C, 0.07% Si, 0.04% Mn, 0.018% P, 0.013% S
0.55% C, 0.07% Si, 0.04% Mn, 0.018% P, 0.013% S
0.55% C, 1.5% Si, 0.7% Mn, 0.7% Cr
0.55% O
0.56% C, 0.81% Mn, 1.85% Si, 0.026% P, 0.024% S, 0.21% Cr, 0.15% Ni, 0.025% Mo
0.58% C, 0.39% S
0.59% C, 0.39% Si, 1.53% Mn, 0.023% P, 0.018% S, 0.008% N
0.59% C, 0.39% Si, 1.53% Mn, 0.023% P, 0.18% S, 0.08% N
0.59% C, 0.39% Si, 1.53% Mn
0.59% C, 0.60% Mn, 1.60% Si, 1.09% Cr, 0.11% V, 0.006% S, 0.009% O, 0.013% Al
0.59% C, nil Mn, 0.035% S, 0.010% O
0.60% C, 0.14% Si, 1.11% Mn, 0.029% S, 0.006% N
0.60% C, 0.30% Si, 0.60% Mn, 0.60% Cr
0.61% C, 1.79% Si, 0.93% Mn, 0.010% P, 0.008% S
0.61% C, 1.79% Si, 0.93% Mn, 0.010% P, 0.008% S
0.61% C, 1.79% Si, 0.93% Mn, 0.010% P, 0.008% S
0.62% C, 0.26% Si, 0.70% Mn, 0.015% P, 0.018% S, 0.65% Cr, 0.07% Ni
0.62% C, 0.26% Si, 0.79% Mn, 0.015% P, 0.018% S, 0.65% Cr, 0.07% Ni
0.62% C, 0.26% Si, 0.79% Mn, 0.015% P, 0.018% S, 0.65% Cr, 0.07% Ni
0.62% C, 0.47% Si, 1.78% Mn, 0.034% P, 0.018% S, 0.007% N
0.62% C, 0.47% Si, 1.78% Mn, 0.034% P, 0.018% S, 0.007% N
0.62% C, 0.47% Si, 1.78% Mn, 0.034% P, 0.018% S, 0.007% N
0.65% C, 0.30% Si, 3.05% Cr, 0.50% Mo, 0.13% V
0.68% C, 0.31% Si, 0.77% Mn, 0.014% O, 0.008% S, 3.15% Cr, 0.69% Mo, 0.07% Ni, 0.005% Sn, 0.009% As, 0.045% Cu, 0.003% Al
0.68% C, 1.05% Si, 0.60% Mn, 8.25% Cr, 1.40% Mo, 1.50% Ni, 1.00% V
0.70% C, 1.57% Mn, 0.45% Si, 0.006% S, 0.010% P, 390 ppm Ti, 39 ppm B, 13 ppm Al, 83 ppm N, 308 ppm O
0.70% C, 1.57% Mn, 0.45% Si, 0.006% S, 0.010% P, 390 ppm Ti, 39 ppm B, 13 ppm Al, 83 ppm N, 308 ppm O
0.70% C, 1.57% Mn, 0.45% Si, 0.006% S, 0.010% P, 390 ppm Ti, 39 ppm B, 13 ppm Al, 83 ppm N, 308 ppm O
0.70-0.80% C, 0.65-0.70% Mn, 0.16-0.30% Si, max. 0.020% P, max. 0.020% S, max. 60 ppm N
0.70-0.80% C, 0.65-0.70% Mn, 0.16-0.30% Si, max. 0.020% P, max. 0.020% S, max. 60 ppm N
0.70-0.80% C, 0.65-0.70% Mn, 0.16-0.30% Si, max. 0.020% P, max. 0.020% S, max. 60 ppm N
0.70-0.80% C, 0.65-0.70% Mn, 0.16-0.30% Si, max. 0.020% P, max. 0.020% S, max. 60 ppm N
0.71% C, 0.29% Si, 1.01% Mn, 0.026% P, 0.016% S, 1.00% Cr
0.72% C, 0.05% P, 0% S, 0.017% Cu, Mn: Lap
0.72% C, 1.56% Mn, 0.49% Si, 0.007% S, 0.010% P, 420 ppm Ti, 48 ppm B, 160 ppm Al, 67 ppm N, 438 ppm O
0.72% C, 1.56% Mn, 0.49% Si, 0.007% S, 0.010% P, 420 ppm Ti, 48 ppm B, 160 ppm Al, 67 ppm N, 438 ppm O
0.72% C, 1.56% Mn, 0.49% Si, 0.007% S, 0.010% P, 420 ppm Ti, 48 ppm B, 160 ppm Al, 67 ppm N, 438 ppm O
0.74% C, 0.27% Si, 0.99% Mn, 0.019% S, 0.016% Cr and 0.015% Ni
0.75% C, 0.18% Si, 0.48% Mn, 0.005% P, 0.008% S, 0.001% S-Al, 0.01% Ca, 0.003% O. Chemical composition of the slag: 20.7% Al2O3, 36.5% CaO, 42.8% SiO2
0.78% C, 1.44% Mn, 0.60% Si, 0.006% S, 0.007% P, 540 ppm Ti, 56 ppm B, 580 ppm Al, 41 ppm N, 336 ppm O
0.78% C, 1.44% Mn, 0.60% Si, 0.006% S, 0.007% P, 540 ppm Ti, 56 ppm B, 580 ppm Al, 41 ppm N, 336 ppm O
0.78% C, 1.44% Mn, 0.60% Si, 0.006% S, 0.007% P, 540 ppm Ti, 56 ppm B, 580 ppm Al, 41 ppm N, 336 ppm O
0.8% C, 1.43% Mn, 0.0238% S, 0.023% Al, 0.0012% Ca, 0.0090% N. Heat B2: 0.19% C, 1.49% C, 0.028% S, 0.025% Al, 0.0011% Ca, 0.0081% N
0.80% C, 0.34% Si, 0.35% Mn, 4.30% Cr, 4.90% Mo, 6.40% W, 2.03% V
0.80% C, 1.59% Si, 2.01% Mn, 1.00% Cr, 0.24% Mo, 1.15% Co, 0.002% P, 0.002% S
0.80% C
0.86% C, 0.33% Si, 0.36% Mn, 0.018% P, 0.003% S, 1.73% Cr, 0.29% Mo, 0.10% V, 0.24% Cu
0.87% C, 0.30% Si, 0.38% Mn, 1.75% Cr, 0.28% Mo, 0.13% Ni, 0.10% V
0.88% C, 0.19% Si, 1.95% Mn, 0.009% P, 0.004% S, 0.31% Cr, 0.06% Ni, 0.02% Mo, 0.09% V, 0.09% Cu, 0.009% Al
0.88% C, 0.30% Si, 0.38% Mn, 2.15% Cr, 0.28% Mo, 0.10% V
0.88% C, 0.31% Si, 0.35% Mn, 0.009% P, 0.01% S, 1.80% Cr, 0.13% Ni, 0.13% V, 0.24% Cu, 0.21% Mo
0.89% C, 30.1% Mn, 8.85% Al, 1.01% Si, 0.31% Mo, 0.006% P, <0.05% Ni, <0.05% Cr, <0.05% Cu
0.9-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, max. 0.030% P, max. 0.025% S, 1.35-1.65% Cr, max. 0.30% Ni, max. 0.30% Cu
0.9-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, max. 0.030% P, max. 0.025% S, 1.35-1.65% Cr, max. 0.30% Ni, max. 0.30% Cu
0.9-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, max. 0.030% P, max. 0.025% S, 1.35-1.65% Cr, max. 0.30% Ni, max. 0.30% Cu
0.9-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, max. 0.030% P, max. 0.025% S, 1.35-1.65% Cr, max. 0.30% Ni, max. 0.30% Cu
0.9-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, max. 0.030% P, max. 0.025% S, 1.35-1.65% Cr, max. 0.30% Ni, max. 0.30% Cu
0.9-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, max. 0.030% P, max. 0.025% S, 1.35-1.65% Cr, max. 0.30% Ni, max. 0.30% Cu
0.90% C, 0.2% Si, 0.3% Mn, 4.3% Cr, 3.3% Mo, 6.4% W, 2.1% V
0.90% C, 0.25% Si, 2.00% Mn, 0.35% Cr, 0.13% V
0.90% C, 0.25% Si, 2.00% Mn, 0.35% Cr, 0.13% V
0.90% C, 0.25% Si, 2.00% Mn, 0.35% Cr, 0.13% V
0.90% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 1.90% V, 6.60% W
0.90% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 4.95% Mo, 1.90% V, 6.60% W
0.90% C, 29.11% Mn, 9.25% Al, 1.07% Si, 0.37% Mo, 0.070% P, 0.09% Ni, 0.24% Cr, 0.10% Cu
0.90-1.03% C, 0.15-0.35% Si, 0.30-0.50% Mn, max. 0.04% P, max. 0.05% S
0.91% C, 1.34% Si, 0.77% Mn, 0.014% P, 0.013% S, 1.07% Cr, 0.10% Ni
0.92% C, 0.24% Mn, 0.009% Si, 1.526% P, 0.091% S
0.93-1.05% C, 0.45-0.75% Si, 1.00-1.20% Mn, max. 0.025% P, max. 0.015% S, 1.40-1.65% Cr, max. 0.30% Cu, max. 0.05% Al
0.95% C, 0.15% Si, 0.25% Mn, 1.35% Cr
0.95-1.10% C, 0.15-9.35% Si, max. 0.50% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Ni, 1.30-1.60% Cr, max. 0.25% Cu
0.95-1.10% C, 0.15-9.35% Si, max. 0.50% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Ni, 1.30-1.60% Cr, max. 0.25% Cu
0.97% C, 0.10% Si, 0.29% Mn, 0.015% P, 1.42% Cr, 0.13% Ni, 0.03% Mo, 0.17% Cu, 0.004% V, 0.027% Al, 0.0008% S
0.97% C, 0.10% Si, 0.29% Mn, 0.015% P, 1.42% Cr, 0.13% Ni, 0.03% Mo, 0.17% Cu, 0.004% V, 0.027% Al, 0.0008% S
0.97% C, 0.10% Si, 0.29% Mn, 0.015% P, 1.42% Cr, 0.13% Ni, 0.03% Mo, 0.17% Cu, 0.004% V, 0.027% Al, 0.0008% S
0.97% C, 0.23% Si, 1.13% Mn, 0.009% P, 0.001% S, 0.53% Cr, 0.15% Ni, 0.10% Mo, 0.09% V, 0.15% Cu, 0.51% W, 0.013% Al, 0.010% Co
0.97% C, 0.25% Si, 0.35% Mn, max. 0.0015% S, 1.50% Cr
0.97% C, 0.32% Si, 0.019% P, 0.017% S, 1.43% Cr, 0.31% Mn
0.98% C, 0.30% Si, 0.48% Mn, 0.017% P, 0.006% S, 5.01% Cr, 0.11% Ni, 0.93% Mo, 0.22% V, 0.24% Cu, 0.009% Al
1.0% C, 0.25% Si, 0.30% Mn, 1.4% Cr, 0.2% Ni, 0.25% Cu, 0.03% Al, 0.015% S
1.0% C, 0.25% Si, 0.30% Mn, 1.4% Cr, 0.2% Ni, 0.25% Cu, 0.03% Al, 0.015% S
1.0% C, 0.25% Si, 0.30% Mn, 1.4% Cr, 0.2% Ni, 0.25% Cu, 0.03% Al, 0.015% S
1.0% C, 0.25% Si, 0.30% Mn, 1.4% Cr, 0.2% Ni, 0.25% Cu, 0.03% Al, 0.015% S
1.0% C, 0.30% Si, 0.30% Mn, 1.50% Cr
1.00% C, 0.25% Si, 0.42% Mn, 0.023% P, 0.011% S, 4.90% Cr, 0.17% Ni, 0.95% Mo, 0.18% V, 0.09% Cu, 0.013% Al
1.00% C, 0.26% Si, 0.36% Mn, 1.44% Cr, 0.002% Ti, 6 ppm O
1.01% C, 0.31% Si, 0.69% Mn, 0.020% P, 0.018% S, 4.91% Cr, 0.16% Ni, 0.96% Mo, 0.18% V, 0.11% Cu, 0.018% Al
1.01% C, 1.46% Cr, 0.2% Si, 0.34% Mn, 0.015% P, 0.005% S, 0.09% Cu, 0.04% Ni, 0.01% Mo, 5 ppm O
1.19% C, 13.7% Mn, 0.61% Si, 0.62% Cr, 0.31% Mo, 0.12% Ni, 0.04% Al, 0.05% P, 0.004% S, 0.0265% N
1.19% C, 13.7% Mn, 0.61% Si, 0.62% Cr, 0.31% Mo, 0.12% Ni, 0.04% Al, 0.05% P, 0.004% S, 0.0265% N
1.19% C, 13.7% Mn, 0.61% Si, 0.62% Cr, 0.31% Mo, 0.12% Ni, 0.04% Al, 0.076% P, 0.004% S, 0.0265% N
1.19% C, 13.7% Mn, 0.61% Si, 0.62% Cr, 0.31% Mo, 0.12% Ni, 0.04% Al, 0.076% P, 0.004% S, 0.0265% N
1.28% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 0.85% Mo, 3.75% V, 12.00% W
1.28% C, 0.45% Si, 0.40% Mn, 4.15% Cr, 3.55% Mo, 3.25% V, 9.50% W, 10.00% Co
1.3% C, 0.3% Si, 18% Mn, 0.004% S and 0.005% O
1.4% C
1.43% C, 0.23% Si, 0.30% Mn, 0.35% Cr, 0.25% V, 3.05% W
1.50% C, 0.23% Si, 0.60% Mn, 1.40% Cr
1.51% C, 0.28% Si, 0.27% Mn, 0.022% P, 0.004% S, 11.50% Cr, 0.12% Ni, 0.73% Mo, 0.75% V, 0.05% Cu, 0.017% Al
1.52% C, 0.29% Si, 0.26% Mn, 0.022% P, 0.003% S, 11.80% Cr, 0.15% Ni, 0.78% Mo, 0.69% V, 0.06% Cu, 0.007% Al
1.53% C, 0.25% Si, 0.25% Mn, 4.90% Cr, 5.00% Ni, 6.50% V, 4.90% Co
1.53% C, 0.35% Si, 0.40% Mn, 12.00% Cr, 1.00% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.00% Cr, 1.00% Mo, 0.85% V
1.53% C, 0.35% Si, 0.40% Mn, 12.00% Cr, 1.00% Mo, 0.85% V
1.56% C, 0.26% Si, 0.28% Mn, 0.023% P, 0.007% S, 11.90% Cr, 0.18% Ni, 0.74% Mo, 0.99% V, 0.06% Cu, 0.006% Al
1.56% C, 0.30% Si, 0.38% Mn, 0.018% P, 0.006% S, 11.90% Cr, 0.85% Mo, 0.96% V, 0.010% Al, 0.22% Ni, 0.13% Cu, 0.18% W
1.60% C, 4.80% Cr, 2.00% Mo, 5.00% V, 10.50% W, 8.00% Co
1.60% C, 4.80% Cr, 2.00% Mo, 5.00% V, 10.50% W, 8.00% Co
1.60% C, 4.80% Cr, 2.00% Mo, 5.00% V, 10.50% W, 8.00% Co
1.9% P
1.96% C, 0.31% Si, 0.73% Mn, 13.4% Cr, 1.28% W, 0.011% P, 0.007% S
10.16% C, 0.66% Mn, 0.008% P, 0.025% S, 0.17% Si, 0.19% Cu, 0.048% Ni, 0.060% Cr. A529 tundish sample: 0.17% C, 0.74% Mn, 0.01% P, 0.03% S, 0.17% Si, 0.33% Cu, 0.09% Ni, 0.05% Cr
11.32% Cr, <0.5% Ni, 0.5% Mn, 0.39% Si, 0.209% Ti, 0.005% C, 0.007% N, 0.001% S, 0.025% P, 8 ppm Ca. Steel 409L AOD: 11.34% Cr, <0.5% Ni, 0.5% Mn, 0.55% Si, 0.141% Ti, 0.006% Al, 0.011% C, 0.009% N, 0.003% S, 0.025% P, 8 ppm Ca
11.32% Cr, <0.5% Ni, 0.5% Mn, 0.39% Si, 0.209% Ti, 0.005% C, 0.007% N, 0.001% S, 0.025% P, 8 ppm Ca. Steel 409L AOD: 11.34% Cr, <0.5% Ni, 0.5% Mn, 0.55% Si, 0.141% Ti, 0.006% Al, 0.011% C, 0.009% N, 0.003% S, 0.025% P, 8 ppm Ca
11.32% Cr, <0.5% Ni, 0.5% Mn, 0.39% Si, 0.209% Ti, 0.005% C, 0.007% N, 0.001% S, 0.025% P, 8 ppm Ca. Steel 409L AOD: 11.34% Cr, <0.5% Ni, 0.5% Mn, 0.55% Si, 0.141% Ti, 0.006% Al, 0.011% C, 0.009% N, 0.003% S, 0.025% P, 8 ppm Ca
11.5-13% Cr, max 1% Si, max 1% Mn, max 0.5% S, max 0.5% P
160 ppm, contact time: 30 s. Sample 2: 450 ppm, contact time: 1 s. Sample 3: 780 ppm, contact time: 1 s. Sample 4: 1800 ppm, contact time: 1 s. Sample 5: 1800 ppm, contact time: 5 s. Sample 6: 1800 ppm, contact time: 60 s
160 ppm, contact time: 30 s. Sample 2: 450 ppm, contact time: 1 s. Sample 3: 780 ppm, contact time: 1 s. Sample 4: 1800 ppm, contact time: 1 s. Sample 5: 1800 ppm, contact time: 5 s. Sample 6: 1800 ppm, contact time: 60 s
160 ppm, contact time: 30 s. Sample 2: 450 ppm, contact time: 1 s. Sample 3: 780 ppm, contact time: 1 s. Sample 4: 1800 ppm, contact time: 1 s. Sample 5: 1800 ppm, contact time: 5 s. Sample 6: 1800 ppm, contact time: 60 s
160 ppm, contact time: 30 s. Sample 2: 450 ppm, contact time: 1 s. Sample 3: 780 ppm, contact time: 1 s. Sample 4: 1800 ppm, contact time: 1 s. Sample 5: 1800 ppm, contact time: 5 s. Sample 6: 1800 ppm, contact time: 60 s
160 ppm, contact time: 30 s. Sample 2: 450 ppm, contact time: 1 s. Sample 3: 780 ppm, contact time: 1 s. Sample 4: 1800 ppm, contact time: 1 s. Sample 5: 1800 ppm, contact time: 5 s. Sample 6: 1800 ppm, contact time: 60 s
160 ppm, contact time: 30 s. Sample 2: 450 ppm, contact time: 1 s. Sample 3: 780 ppm, contact time: 1 s. Sample 4: 1800 ppm, contact time: 1 s. Sample 5: 1800 ppm, contact time: 5 s. Sample 6: 1800 ppm, contact time: 60 s
160 ppm, contact time: 30 s. Sample 2: 450 ppm, contact time: 1 s. Sample 3: 780 ppm, contact time: 1 s. Sample 4: 1800 ppm, contact time: 1 s. Sample 5: 1800 ppm, contact time: 5 s. Sample 6: 1800 ppm, contact time: 60 s
17.3% Cr, 8.7% Ni, 1.6% Mn, 0.78% Cu, 0.66% Si, 0.37% Mo, 0.34% S, 0.17% Co, 0.034% C, 0.032% N, and 0.028% P
18 ppm Al, 255 ppm Ti. Sample 2C: 32 ppm Al, 67 ppm Ti. Sample 5D: 1808 ppm Al, 866 ppm Ti
18 ppm C, 6 ppm S, less than 10 ppm P, less than 5 ppm Si, 1 ppm Mn, 1 ppm Cu, 8 ppm N, 80 ppm O and remaining Fe
18 ppm C, 6 ppm S, less than 10 ppm P, less than 5 ppm Si, 1 ppm Mn, 1 ppm Cu, 8 ppm N, 80 ppm O and remaining Fe
18 ppm C, 6 ppm S, less than 10 ppm P, less than 5 ppm Si, 1 ppm Mn, 1 ppm Cu, 8 ppm N, 80 ppm O and remaining Fe
18 ppm C, 6 ppm S, less than 10 ppm P, less than 5 ppm Si, 1 ppm Mn, 1 ppm Cu, 8 ppm N, 80 ppm O and remaining Fe
18 ppm C, 6 ppm S, less than 10 ppm P, less than 5 ppm Si, 1 ppm Mn, 1 ppm Cu, 8 ppm N, 80 ppm O and remaining Fe
18% Cr, 10% Ni, 0.3% Ti
18% Cr, 10% Ni, 0.3% Ti
18% Ni, 5.0% Mo, 9.0% Co, 0.7% Ti, 0.1% Al, <0.03% C
19-25 ppm C, 60-90 ppm S, 20 ppm N, 250-400 ppm O, 68 ppm Co, <10 ppm others
2.10% C, 0.21% Si, 0.24% Mn, 0.025% P, 0.005% S, 12.70% Cr, 0.16% Ni, 0.08% Mo, 0.07% V, 0.03% Cu, 0.007% l
21% Cr, 24.5% Ni, 3.3% Mo; 0.066% Ce metal added
21% Cr, 24.5% Ni, 3.3% Mo; 0.066% Ce metal added
25% Cr, 20% Ni, 1(-4)% Si, 0.5(-1)% Mn
27% Al2O3, 41% Cr2O3, 32% SiO2
29.8% SiO2
3 % of carbon, 1 – 10 % each of the main alloying element
3.53% C, 1.91% Si, 0.86% Mn, 0.011% P, 0.008% S, 0.02% Cr, 1.91% Ni
3.66% C, 2.31% Si, 0.15% Mn, 0.03% P, 0.01% S, 0.03% Cr, 0.27% Ni, 0.01% Mo, 0.11% Cu, 0.05% Mg
3.66% C, 2.31% Si, 0.15% Mn, 0.03% P, 0.01% S, 0.03% Cr, 0.27% Ni, 0.01% Mo, 0.11% Cu, 0.05% Mg
3.66% C, 2.31% Si, 0.15% Mn, 0.03% P, 0.01% S, 0.03% Cr, 0.27% Ni, 0.01% Mo, 0.11% Cu, 0.05% Mg
3.66% C, 2.31% Si, 0.15% Mn, 0.03% P, 0.01% S, 0.03% Cr, 0.27% Ni, 0.01% Mo, 0.11% Cu, 0.05% Mg
30% Al2O3, 5-6% MgO, 1-2% SiO2, <0.4% FeO
30Ni–19Cr–0.8Mn–0.5Al–0.5Ti–0.45Si–0.12C–0.01N, balance Fe
4% Si
400 ppm Ti and 290 ppm Al
5.3% Cr, 1.3% Mo, 0.9% V
5.3%Cr-1.3%Mo-0.9%V
5.3%Cr-1.3%Mo-0.9%V
50% Ti, 50% Fe
62% Cr, 1.89% Si, 7.33% Cr, 0.028% S, 0.01% P, 0.18% Mn, 0.13% Ti, 0.37% Ni, 0.13% V, 0.043% N,
64% FeS, ?% O
64.1% FeO, 3.2% Fe2O3, 31% SiO2
65% Fe, 19.5% Cr, 9.8% Ni, 1.13% Mn, 1.16% Si, 2.67% Mo, 0.030% Al
73% Cr, 0.03% C, 0.08% Si, balance is Fe
73% Cr, 0.03% C, 0.08% Si, balance is Fe
73% Cr, 0.03% C, 0.09% Si, balance is Fe
73% Cr, 0.03% C, 0.09% Si, balance is Fe
75% SiO2, 6.7% Pb, 8% Ca, 4.8% Al, 2.5% Na2O, 0.5% K2O, 0.5% Zn, Cu+Ba+Mg
76.2% Ti, 3.3% Al, 0.6% Si, >0.3% O, 0.07% Ca, <0.002% S)
81.2% V, 0.15% C, 0.50% Si, 0.020% P, 0.020% S, 0.020% As, 0.36% Al, 2050 ppm O, balance is Fe
82.2% Mn, 9.92% C, 0.38% Si, 0.18% P, 0.058% N, 0.17% O
9.79% Ni, 0.006% Al, 0.00% Ti, 0.0034% O
99.97% Fe
99.97% Fe
99.97% Fe
99.97% Fe
Fe - <0.15% C – 13% Cr - >0.15% S
Fe – 0.07% C – 0.06% Mn – 0.2% Si – 0.16% P – 0.02% S
Fe – 0.1% C - 0.8% Mn – 18.2% Cr – Fe – 0.35% C – 0.78% Mn – 1.74% Cr – 0.41% Mo – 0.050% Al – 57 ppm O
Fe-0.19% C
Fe-0.1C-0.0035S-1.45Mn-0.1Si-0.015Ti-0.0025O-0.03N+Mg
Fe-0.2% C
Fe-0.35% C-0.78% Mn-1.74% Cr-0.41% Mo-0.050% Al-57 ppm O
Fe-0.77C-0.24Si-0.63Mn
Fe-17Cr-8Ni-1.5Mn-0.04C-0.2Mo-0.3S
Fe-3% Si
Fe-3% Si
Fe-3.33%C-1.64%Si-0.31%Mn-1.37%P-0.107%S
Fe-3.62%C-2.03%Si-1.13%P-0.61%Mn-0.137%S-0.113%Cr-0.478%Ni-0.004%Al
Fe-30Mn-9Al-1Si-0.9C-0.5Mo
Fe-5Al
Fe-5Al
Fe-l.35Ti-0.025C-0.035N
Fe; 0.078-0.095C; 0.21-0.276Si; 1.35-1.42Mn; 0.011-0.012P; 0.003-0.005S; 0.019-0.039Cr; 0.01-0.012Ni; 0.014-0.017Cu; Fe–0.1C–1.5Mn–0.1Si–xTi–0.005O–0.007S
Fe–0.39C–1.0Si–0.4Mn–5.2Cr–1.4Mo–0.9V
Fe–10 mass% Ni alloy
Fe–10% Ni alloy
Fe–16 wt% Cr
Fe–16 wt% Cr
Fe–16 wt% Cr
Fe–16 wt% Cr
Fe–16 wt% Cr
Fe–16 wt% Cr