706 Alloy
Alloy name: 706
Diagram No.: 911
Type of diagram: TTH
Chemical composition in weight %: 36.9% Fe, 16.0% Cr, 3.02% Nb, 1.65% Ti, 0.19% Al, 0.01% C, 0.05% Si, 0.003% N, 0.001% S, balance is Ni.
Alloy group: Nickel-based alloys
Note: Hardness test results for 982% annealed then aged samples are shown in Figure. (1121 C annealed material showed similar results). Aging response is accelerated between 760 C and 816 C but peak hardness occurs at longer times between 704°C and 760°C. The T-T-T curves in Figure in Diagram No. 911 show that increases in hardness correlate with precipitation of Gamma’ and Gamma”. The highest isothermally generated hardnesses are associated with greater amounts of Gamma’ + Gamma” and the onset of Eta precipitation. In general, hardness decreases with increasing amounts of Eta, although slight hardening relative to the annealed state occurs where Eta (especially) and A2B precipitation thoroughly transform grains to Widmanstatten structure.
Additional links: No. 910, No. 911
Reference: Not shown in this demo version.
Transformation Diagram
Price: 20.00 US $
Buy Online Transformation Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT of Steels
Hardenability Diagrams of Steels
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Tempering Diagrams of Steels
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.