Name | Chemical formula | Stoichiometric composition, wt. % |
Corundum | Al2O3 | 100% Al2O3 |
Cristobalite | SiO2 | 100% SiO2 |
Tridymite | SiO2 | 100% SiO2 |
Quartz | SiO2 | 100% SiO2 |
Wustite | FeO | 100% FeO |
Mullite | 3Al2O3 x 2SiO2 | 28% SiO2, 72% Al2O3 |
Grunerite | FeO x SiO2 | 55% FeO, 45% SiO2 |
Fayalite | 2FeO x SiO2 | 71% FeO, 29% SiO2 |
Hercynite | FeO x Al2O3 | 41% FeO, 59% Al2O3 |
Almandine | 3FeO x Al2O3 x 3SiO2 | 43% FeO, 37% SiO2, 20% Al2O3 |
Fe-cordierite | 2FeO x 2Al2O3 x 5SiO2 | 22% FeO, 47% SiO2, 31% Al2O3 |