TiO2 Nanotube Synthesis - Wet Etching
Material Name: TiO2
Recipe No.: 10318
Primary Chemical Element in Material: Ti
Sample Type: Nano
Uses: Etching
Etchant Name: None
Etching Method: Wet etching
Etchant (Electrolyte) Composition: See the data file.
Procedure (Condition): No data
Note: Fluoride etching of Ti metal substrate to form TiO2 nanotubes.
Reference: TiO2 Nanotube Synthesis, Source not known, 2020.