Fe-Mo Alloy - Alloys with 12-20 at.% Mo

Material Name: Fe-Mo alloys
Recipe No.: 1953
Primary Chemical Element in Material: Fe
Sample Type: Thin foil
Uses: Etching
Etchant Name: None
Etching Method: Electrolytic thinning
Etchant (Electrolyte) Composition: 30% sulphuric acid, 70% methanol.
Procedure (Condition): Temperature: 220 K.
Note: Alloys with 12-20 at.% Mo.
Reference: T.Miyakaki, et al., Acta Met., Vol.28, No.8, August 1980, p. 1143.