Citric Acid:H2O2 - GaAs - Wet Etchant by Chemical Composition

Material Name: GaAs
Recipe No.: 4942
Primary Chemical Element in Material: Ga
Sample Type: Wafer
Uses: Etching
Etchant Name: None
Etching Method: Wet etching
Etchant (Electrolyte) Composition: Citric acid:H2O2
Procedure (Condition): No data
Note: Wet etchant by chemical composition. GaAs etching; Ref. (Mukherjee, S.D., 1985).
Reference: A.R. Clawson, Guide to references on III-V semiconductor chemical etching, Materials Science and Engineering (Original Reference List), 31 (2001), p. 156.