Citric Acid:H2O2 - InGaAs/AlGaAs/GaAs - Wet Etchant by Chemical Composition

Material Name: InGaAs/AlGaAs/GaAs
Recipe No.: 4957
Primary Chemical Element in Material: In, Al, Ga
Sample Type: Wafer
Uses: Etching
Etchant Name: None
Etching Method: Wet etching
Etchant (Electrolyte) Composition: Citric acid:H2O2:H2O (4:1:1)
Procedure (Condition): No data
Note: Wet etchant by chemical composition. Non-selective GaAs, AlGaAs etch rate ~4000 A/min; Ref. (Mao, B.-Y., 1994).
Reference: A.R. Clawson, Guide to references on III-V semiconductor chemical etching, Materials Science and Engineering (Original Reference List), 31 (2001), p. 158.