Citric Acid:H2O2 - InGaAs/AlGaAs/GaAs - Wet Etchant by Chemical Composition

Material Name: InGaAs/AlGaAs/GaAs
Recipe No.: 4966
Primary Chemical Element in Material: In, Al, Ga
Sample Type: Wafer
Uses: Etching
Etchant Name: None
Etching Method: Wet etching
Etchant (Electrolyte) Composition: Citric acid:H2O2
Procedure (Condition): No data
Note: Wet etchant by chemical composition. Selective removal of GaAs substrate from Al0.7Ga0.3As etch stop layer; Ref. (Zhang, C., 1999).
Reference: A.R. Clawson, Guide to references on III-V semiconductor chemical etching, Materials Science and Engineering (Original Reference List), 31 (2001), p. 158.