Silver Chloride - AgCl
Classification: Chloride
Atomic numbers: 47 & 17
Atomic weight: 143.34
Melting point (C): 455
Boiling point (C): 1550
Density (g/cm3): 5.552
Refractive index (n=): 2.0611
Hardness (Mosh-scratch): 1-1.5
Crystal structure: Isometric-normal: (100) cube
Color (solid): Pearl-grey
Cleavage: None