Home
Faceting
Material Name: Silicon
Record No.: 129
Primary Chemical Element in Material: Si
Sample Type: Wafer
Uses: Etching
Etchant Name: None
Etching Method: Dry etching
Etchant (Electrolyte) Composition: No data
Procedure (Condition): No data
Note: Generally due to increased yield per ion at a corner (dependent on ion energy/flux).
Reference: Steve Sirard, Introduction to Plasma Etching, Lam Research Corporation, PowerPoint Presentation, https://docplayer.net, 2020, pp. 1-58.

Figure 1: Faceting.