Particles on Chips: Hair I
Material Name: No data
Record No.: 13
Primary Chemical Element in Material: No data
Sample Type: Wafer
Uses: Etching
Etchant Name: None
Etching Method: No data
Etchant (Electrolyte) Composition: No data
Procedure (Condition): No data
Note: No data
Reference: Website https://www.tf.uni-kiel.de/matwis/amat/elmat_en/kap_5/illustr/hair.html, 2020.

Figure 1: Large size picture of a hair (from a female) on a 256 kbit memory chip. Just one of the little flakes of the
hair would be enough to cover one memory cell.