Inclusions with Voids - CdZnTe
Material Name: CdZnTe
Record No.: 38
Primary Chemical Element in Material: Cd
Sample Type: Single crystal
Uses: Polishing, etching
Etchant Name: None
Etching Method: Wet etching
Etchant (Electrolyte) Composition: No data
Procedure (Condition): No data
Note: No data
Reference: Anwar Hossain, Etch pits in CdZnTe and other CdTe-based Crystals, Presented at the MRS Spring Meeting, April 1 – 5, 2013, Brookhaven National Laboratory, PowerPoint Presentation, pp. 1-27.

Figure 1: Inclusions with voids.