| Grit Number | Size (µm) | Grit Number | Size (µm) | Emery Grit |
| P60 | 269.0 | 60 | 268.0 | - |
| P80 | 201.0 | 80 | 188.0 | - |
| P100 | 162.0 | 100 | 148.0 | - |
| P120 | 127.0 | 120 | 116.0 | - |
| P180 | 78.0 | 180 | 78.0 | 3 |
| P240 | 58.5 | 220 | 66.0 | 2 |
| P280 | 52.2 | 240 | 51.8 | - |
| P320 | 46.2 | - | - | - |
| P360 | 40.5 | 280 | 42.3 | 1 |
| P400 | 35.0 | 320 | 34.3 | 0 |
| P500 | 30.2 | 360 | 27.3 | - |
| P600 | 25.8 | 400 | 22.1 | 00 |
| P800 | 21.8 | - | - | - |
| P1000 | 18.3 | 500 | 18.2 | 000 |
| P1200 | 15.3 | 600 | 14.5 | - |
| P1500 | 12.6 | 800 | 12.2 | 0000 |
| P2000 | 10.3 | 1000 | 9.2 | - |
| P2500 | 8.4 | 1200 | 6.5 | - |
| P4000* | 5.0* | - | - | - |