M7C3 Carbides in Steels

(Cr, Fe)7C3 carbides in Cr-Co steel
(Cr, Fe)7C3 carbides in chromium cast iron
(Cr,Fe)7C3, Fe3C and Fe23(C,B)6 carbides in white cast irons
(Fe,Cr)3C and (Cr,Fe)7C3 carbides in air-hardening cast tool steel
(Fe,Cr)7C3 carbides in ferritic stainless steel
(Fe,Cr,Mo)7C3 and (Fe,Cr,Mo)3C carbides in Fe-3.3C-l6Cr-3Mo-lMn-0.5Si alloy
(Fe2Cr)C, M23C6 and M7C3 carbides in X20CrMoV121 steel
(FeCrMo)C and (FeCrMoMn)C carbides in 10CrMo9-10 steel
(Mo,Cr)2C carbides in Fe-1.7C-1.2Si-l.1Mn-0.8Ni-3.6Cr-1.7Mo-4.7V alloy
0.65C-5.62Cr-0.70V-1.26Mo steel - Electrolytic extraction of carbides
1.12C-11.12Cr-1.48V-2.27W-1.34Mo steel - Electrolytic extraction of carbides
1.12C-11.12Cr-1.48V-2.27W-1.34Mo steel - Electrolytic extraction of carbides
C2C, Cr3C2, Cr7C2, Cr7C3 and Cr23C6 carbides in AISI 446 steel
Carbide microstructure in PM tool steel
Carbide microstructures in cold work tool steels
Carbide phases in T25 and P91 creep resisting steels
Carbides distribution in cold work tool steels
Carbides in 1.2379 and UNIVERSAL steels (Acoustic Emission Test)
Carbides in 1.2379 and Universal steels
Carbides in 1.2379, 1.3202 and experimental steels
Carbides in 2.25Cr-1Mo steel
Carbides in AISI M42 steel
Carbides in Damascus steel
Carbides in HSS7 steel
Carbides in HiCr iron rolls
Carbides in NCWV/D3 steel
Carbides in Vanadis PM steel
Carbides in X155CrVMo121 steel
Carbides in coating layer on tool steels
Characteristic carbides (MC, M2C, M3C, M7C3, M23C6) in white cast iron
Chi carbides in 316L-type austenitic stainless steel
Chromium carbides in 100Cr6 steel
Cr7C3 and Cr23C6 carbides in D3 steel
Etchants for carbides in steels
Eutectic VC, NbC and M6C carbides in steel
Fe3C, (Cr,Fe)7C3 and Fe23(C,B)6 carbides in chromium white cast iron
Fe3C, Cr7C3, Mo2C, and (Mn,Mo)2C carbides in 20MoCrS4 steel
Fe3C, VC, M7C3 and M23C6 carbides in heat resistant 12Kh1MF steel
Fracture surface of four-point bending test samples of cold work tool steel
High-carbon carbides in 20Cr-25Ni steel
M23C6 and M7C3 carbides in 2.25Cr–1.0Mo steel
M23C6 and M7C3 carbides in 9%Cr–1%Mo–0.2%V steel
M23C6 carbides in AISI 420 steel
M23C6 carbides in AISI 420 steel - As-received samples
M23C6 carbides in AISI 420 steel - Sub-zero tempering followed by tempering
M23C6 carbides in AISI 420 steel - The effect of austenitising temperature on microstructure
M23C6 carbides in AISI 420 steel - The effect of austenitising temperature on the asquenched microstructure and properties of heats 1 and 2
M23C6 carbides in AISI 420 steel - The effect of double tempering on microstructure
M23C6 carbides in AISI 420 steel - The effect of sub-zero tempering on microstructure
M23C6 carbides in AISI 420 steel - The effect of tempering temperature on microstructure
M23C6 carbides in ASTM A351 steel
M23C6 carbides in grade 91 steel II
M23C6, M7C3 and M6C carbides in 2.25%Cr–Mo–V–Nb and 2.25%Cr–W–V–Nb steels
M23C6, M7C3 and VC carbides in 12X1M0 heat resistant steel
M23C6, M7C3 carbides in alloyed cast iron
M23C6, MC, M7C3 carbides and sigma phase in austenitic stainless steels
M23C6, NbC and M7C3 carbides in steels for nuclear industry
M2C and M23C6 carbides in 0.5Mo-0.5Cr-0.25V low alloy creep resistant steel
M2C and M7C3 carbides in high-chromium white iron
M2C, M3C and M7C3 carbides in Caldie hot work tool steel
M2C, M3C, M23C6 and M7C3 carbides in 13CrMo4-5 steel
M2C, M3C, M7C3 and M23C6 carbides in 1.25Cr–0.5Mo steel
M2C, M6C and M7C3 carbides in Fe3Al alloy
M2C, M6C, M7C3 and M23C6 carbides 2.25Cr1Mo steel
M2C, M6C, M7C3 carbides in Fe3Al-based alloy
M2C, M7C3, M23C6 and M6C carbides in 2.25Cr-1Mo steel
M2C, M7C3, M23C6 carbides in 2.25Cr1.5Mo and 3Cr1.5Mo steels
M3C and M7C3 carbides in 0.1C-0.9Cr-V steels
M3C and M7C3 carbides in 0.46C-5.22Cr steel
M3C and M7C3 carbides in 3Cr1.5Mo power plant steel
M3C and M7C3 carbides in white cast iron
M3C, M2C, M7C3 and M23C6 carbides in 3Cr1.5Mo and 21–4 Cr1Mo steels
M3C, M2C, M7C3 carbides in 6CrC cast steel
M3C, M6C, M7C3, M23C6 carbides in 2.25Cr-1.5W steel
M3C, M7C3 and M23C6 carbides in Cr white cast iron
M3C, M7C3 and M23C6 carbides in X150CrMoV12-1 steel
M3C, M7C3 and M23C6 carbides in X20CrMoV12-1 creep resistant steel
M3C, M7C3 and M4C3 carbides in X40CrMoV5-1 steel
M3C, M7C3 carbides in Fe-12Cr-1.6Mn-1.0Ni-0.5Si-4.1C white cast iron
M3C, M7C3 carbides in high-chromium white iron
M3C, M7C3, M23C6 carbides in alloyed tool steels
M3C, M7C3, MC, M6C carbides in steel rolls
M3C, VC and M7C3 carbides in Strømhard austenitic manganese steel
M3C/M7C3 carbides in 4CRMO steel
M6C and M7C3 carbides in 0.86%C, 7.6%Cr, 0.48%(Nb + V) semi high speed cast steel
M6C and M7C3 carbides in Cr and semi HSS steels for rolls
M6C carbides in Fe-Mo-C alloy
M6C, M23C6 and M7C3 carbides in 2.25Cr–1.6W–V–Nb steel
M6C, M2C, M23C6 and M7C3 carbides in T24 creep resistant steel
M6C, VC, (CrFeMoW)7C3 and M23C6 carbides in high speed steels
M7C3 and M23C6 carbides in 18% Cr cast iron
M7C3 and M23C6 carbides in 0.5C-25Cr-24.5Ni-1.8W-1.9Si-1.9Mn alloy
M7C3 and M23C6 carbides in 0.63C-12.7Cr martensitic stainless steel
M7C3 and M23C6 carbides in 2.25Cr-1.0Mo steel
M7C3 and M23C6 carbides in 2.25Cr-1.0Mo steel
M7C3 and M23C6 carbides in 2.4%C-30%Cr, 2.9% C-27%Cr steels
M7C3 and M23C6 carbides in AISI 440C stainless steel
M7C3 and M23C6 carbides in MANET steel
M7C3 and M23C6 carbides in Manet steel
M7C3 and M23C6 carbides in NCWV/D3 tool steel
M7C3 and M23C6 carbides in Stellites 6 and 21
M7C3 and M23C6 carbides in TENASTEEL steel
M7C3 and M23C6 carbides in high chromium cast iron I
M7C3 and M23C6 carbides in high chromium cast iron II
M7C3 and M23C6 carbides in high chromium cast iron III
M7C3 and M23C6 carbides in high chromium white iron
M7C3 and M3C carbides in Fe-1C-4.4Cr-l.6V alloy
M7C3 and M6C carbides in high Cr and semi high speed steels
M7C3 and M6C5 carbides in white cast Fe-Cr-C-V alloy
M7C3 and Mo2C carbides in Fe-0.9C-11.3Cr-0.7Mn-2.95Mo-0.3Si and Fe-1.33C-6.8Cr-2.4Mo-0.2Si steels
M7C3 and NbC carbides in Fe-2.1C-l4.7Cr-lNb alloy
M7C3 carbides in 1.2379 steel
M7C3 carbides in 1.2379 steel
M7C3 carbides in 15Cr-3Mo white cast iron
M7C3 carbides in 16% Cr white cast iron
M7C3 carbides in 2.25Cr1.5Mo steel
M7C3 carbides in 5CR steel
M7C3 carbides in 5CR80MO steel
M7C3 carbides in 5CRDH steel
M7C3 carbides in 5CRMO steel
M7C3 carbides in AISI 440C martensitic stainless steel
M7C3 carbides in AISI D2 steel (bar diameters of 25.4, 70 and 210 mm)
M7C3 carbides in AISI D3 steel
M7C3 carbides in Cr white cast iron
M7C3 carbides in D2 steel
M7C3 carbides in D3 steel
M7C3 carbides in D3 tool steel
M7C3 carbides in EutecticA white cast iron
M7C3 carbides in Fe-0.86C-23.8Cr-1.9Si-2.1 Ni alloy
M7C3 carbides in Fe-25Cr-3.1C-2.0Mn-0.7Si and Fe-25Cr-5.2C-2.1Mn-0.4Si high chromium cast irons
M7C3 carbides in Fe-2C-12Cr tool steel
M7C3 carbides in Fe-4.46C-33.6Cr-1.19Mn-0.78Si-0.022S-0.028P weld steels
M7C3 carbides in HyperA white cast iron
M7C3 carbides in HyperEXP white cast iron
M7C3 carbides in HypoA white cast iron
M7C3 carbides in SDS II steel
M7C3 carbides in SKD11 steel
M7C3 carbides in SS440C steel
M7C3 carbides in WeldoverlayA white cast iron
M7C3 carbides in WeldoverlayB white cast iron
M7C3 carbides in X155CrVMo12-1 steel
M7C3 carbides in X210CrW12 steel
M7C3 carbides in hardfacing alloy (Fe- 34Cr-4.5C)
M7C3 carbides in high-chromium white cast iron
M7C3 carbides in high-chromium white cast iron (17% Cr)
M7C3, (Fe,Cr)23C6 and Mo2C carbides in high alloyed chromium cast iron
M7C3, M23C6 and M6C carbides in 13HMF steel
M7C3, M23C6 and M6C carbides in 13HMF steel
M7C3, M23C6 carbides in AISI 440A steel
M7C3, M23C6, MC and M3C carbides in G21CrMoV4 – 6 (L21HMF) low alloy cast steel
M7C3, M23C6, VC and Mo2C carbides in forged steel rolls
M7C3, M2C and MC carbides in semi-HSS grades
M7C3, M3C, MX carbides in 31CrMo12 steel
M7C3, M8C7, M23C6 carbides in 4Cr5MoSiV1 steel
M7C3, MC and M2C carbides in hardfacing steel
M7C3, MC, M23C6 and M3C carbides in AISI H11 steel
MC and M6C carbides in AISI M2 steel
MC and M6C carbides in cast M2 high speed steel
MC and M6C carbides in high-carbon high speed steel roll
MC and M7C3 carbides in PM tool steel
MC and M7C3 carbides in Thyrospray 2399 PM steel
MC and M7C3 carbides in Vanadis 6 PM steel
MC and M7C3 carbides in Vanadis 6 PM steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in tool steels made by spray forming
MC, M23C6 carbides in hot work tool steel
MC, M2C and M7C3 carbides in Wear resistant cast iron for rolls
MC, M2C and M7C3 carbides in cast high speed steel roll
MC, M2C carbides in HSS7 steel for rolls
MC, M2C, M3C, M7C3 and M23C6 carbides in 2CrMoNiWV creep resistant steel III
MC, M2C, M3C, M7C3 and M23C6 carbides in G21CrMoV4 – 6 (L21HMF) cast steel
MC, M2C, M3C, M7C3, M23C6 and M6C carbides in 2CrMoNiWV creep resistant steel II
MC, M2C, M3C, M7C3, M23C6 and M6C carbides in 2CrMoNiWV creep resistant steel IV
MC, M2C, M3C, M7C3, M23C6 and M6C carbides in 2CrMoNiWV creep resistant steel V
MC, M2C, M6C and M7C3 carbides in 2%C–5%Cr–5%V–5%Mo–5%W–5%Co white cast iron
MC, M2C, M6C, M7C3 carbides in cast high speed steels (HSS) for rolls
MC, M2C, M7C3 and M23C6 carbides in Kosmos and Aurora steels
MC, M2C, M7C3 and M23C6 carbides in cast high speed roll
MC, M2C, M7C3 and M23C6 carbides in high speed steel roll
MC, M2C, M7C3 carbides in Fe-5%Cr-5%Mo-5%W-5%V-5%Co-2.0%C cast steel
MC, M2C, M7C3, M23C6 carbides in Aurora and Kosmos HSS steels
MC, M2C, M7C3, M23C6 carbides in cast HSS roll
MC, M3C and M7C3 carbides in high chromium cast iron
MC, M3C, M6C and M7C3 carbides in SS2541, THG2000, QRO90 and MCG 4M steels
MC, M6C, M7C3 and M23C6 carbides in 1.2690 steel
MC, M6C, M7C3, M23C6 carbides in HS 3-1-2, HS 6-5-2 steels
MC, M6C, M7C3, M23C6 carbides in HS3-1-2, HS6-5-2 steels
MC, M7C3 and M2C carbides in cast high speed steel roll
MC, M7C3 and M6C carbides in PM cold work tool steel
MC, M7C3 and M6C carbides in THG2000, MCG2006 and QRO90 steels
MC, M7C3 carbides in ROLTEC,TOUGHTEC, WEARTEC, AISI A2, D2 and D6 steels
MX, M2X, M7C3, M23C6 carbides in 1.7779 steel
MX, M3C and M7C3 phases in Cr-V low-alloyed steel
MX, M3C, M7C3, M23C6 carbides in 17CrMoV10 steel
Mat.No. 1.2312, DIN 40CrMnMoS8-6 steel - Electrolytic extraction of carbides
Mat.No. 1.2312, DIN 40CrMnMoS8-6 steel - Electrolytic extraction of carbides
Mat.No. 1.2343, DIN X38CrMoV5-1, AISI H11 steel - Electrolytic extraction of carbides
Mat.No. 1.2343, DIN X38CrMoV5-1, AISI H11 steel - Electrolytic extraction of carbides
Mat.No. 1.2344, DIN X40CrMoV51, AISI H13 steel - Electrolytic extraction of carbides
Mat.No. 1.2344, DIN X40CrMoV51, AISI H13 steel - Electrolytic extraction of carbides
Mat.No. 1.2345, DIN X50CrVMo51, AISI Approx. H11 steel - Electrolytic extraction of carbides
Mat.No. 1.2378, DIN X220CrVMo12-2 steel - Electrolytic extraction of carbides
Mat.No. 1.2379*, DIN X155CrVMo12-1, AISI D2 steel - Electrolytic extraction of carbides
Mat.No. 1.2379*, DIN X155CrVMo12-1, AISI D2 steel - Electrolytic extraction of carbides
Mat.No. 1.2606, DIN X37CrMoW5-1, AISI H12 steel - Electrolytic extraction of carbides
Mo2C and (Fe,Cr)7C3 carbides in high Cr white cast iron Fe-21Cr-3Ni-1.7Mo-2.4C
Mo2C carbides in Fe-C-Mo steel
Mo2C, (V,Ti)C, (Fe,Mo)6C, Fe7C3, Fe3C carbides in austempered ductile iron (ADI)
Mo2C, M7C3 and VC carbides in SHSS II steel
NbC, TiC, V4C3, ZrC, Mo2C, Fe3C, M7C3, M6C, M23C6 carbides in carbon steel and stainless steel
Precipitates in 10CrMo9-10 steel
SEM images of fracture surfaces in PM tool steel
Time–temperature–precipitation diagrams (TTP) for low alloyed steels
V4C3, C7C3 and VC carbides in K190 ISOMATRIX PM steel
V4C4 and Cr7C3 carbides in K190 ISOMATRIX PM steel
V8C7, M7C3 carbides in cast high speed steel for rolls
VC and M7C3 carbides in Fe-2.4C-5.4Cr-6V alloy
VC and W-Mo carbides in HSS rolls
VC, Fe3C, M7C3 and M23C6 carbides in 12X1MO steel
VC, M23C6 and M7C3 carbides in Dievar hot work tool steel
VC, M7C3 carbides in 1.8075 steel
VC, Mo2C, M7C3 and M23C6 carbides in forged high speed steel roll