MC Carbides in Steels

(Cr) 23C6, V4C3 carbides in X190 CrVMo 20-4 steel - Annealed condition
(Cr) 7C3, V4C3 carbides in X190 CrVMo 20-4 steel - Quenched from 1200 C/5 min
(Cr,Fe)23C6 and VX carbides in X20CrMoV12-1 steel
(Cr,Fe)7C3 carbides in K110, PM steel K390 steels
(Cr,Fe)7C3, (Cr,Fe)23C6, NbC and Nb6C5 carbides in JIS SCH2 steel
(Cr15.58Fe7.42)23C6 and V8C7 carbides in PM AISI M2 steel
(FeCrMo)C and (FeCrMoMn)C carbides in 10CrMo9-10 steel
(Mo,V)2C, (Fe,Mo)6C and VC carbides in high speed steel produces by CDC process
(Ti,W)C and (Fe,W)6C carbides in LIME steel sample
(V,Ta)C, VC and TaC carbides in Fe-V-Ta-C alloy
Atom maps of manganese and carbon from 1045 steel after tempering at 300°C
Carbide microstructure in PM tool steel
Carbide microstructures in cold work tool steels
Carbide phases in high speed steels
Carbides distribution in cold work tool steels
Carbides in 1.2379 and UNIVERSAL steels (Acoustic Emission Test)
Carbides in 1.2379 and Universal steels
Carbides in 1.2379, 1.3202 and experimental steels
Carbides in AISI M1 high speed steels
Carbides in Fe-5Cr-5W-5Mo-V-C cast high speed steel
Carbides in HSS7 steel
Carbides in HiCr iron rolls
Carbides in M50 high speed steel
Carbides in Vanadis PM steel
Carbides in annealed microstructure of M4 high speed steel
Carbides in annealed microstructure of T15 high speed steel
Carbides in annealed, hardened and tempered S 6-5-2-5 high speed steel
Carbides in cast and hot-deformed S 6-5-2-5 high speed steel
Carbides in coating layer on tool steels
Carbides in high speed steel rolls
Carbides in semi-high-speed steel (HSS)
Carbides in the cryogenic treated AISI M2 steel
Carbides in tool steels with high chromium content
Cementite in 0.30% C carbon steel
Cementite in Dillidur 690 steel
Cementite phases in carbon steel
Characteristic carbides (MC, M2C, M3C, M7C3, M23C6) in white cast iron
Cr23C6, VC, Fe3C, Mo2C, Nb4C3 carbides in R7, R47, R102A, R147, R191, R192 and R206N steels
Cr3C6 and NbC carbides in 12% Cr ferritic steel
Cr7C3 and Cr23C6 carbides in D3 steel
Cr7C3 and NbC carbides in 2.50C-3.30Si-6.20Cr-1.42Ni-2.20Mo-2.60V-0.98W steel
Cr7C3, (Cr,Fe) 7C3 carbides in D2 steel - Annealed condition
Cr7C3, (Cr,Fe) 7C3 carbides in D2 steel - Quenched from 1150 C/15 min
Cr7C3, V4C3 carbides in X230CrVMo13 4 steel - Annealed condition
Cr7C3, V4C3 carbides in X230CrVMo13 4 steel - Quenched from 1150 C/5 min
Cr7C3, V4C3, V8C7 carbides in X150 CrVMo 8-4 steel - Quenched from 1150 C/15 min
Cr7C3, V4C3, V8C7 carbides in X290 VCrMo10-8 steel - Annealed condition
Cr7C3, V4C3, V8C7 carbides in X290 VCrMo10-8 steel - Quenched from 1200 C/5 min
Cr7C3, V8C7 carbides in X150 CrVMo 8-4 steel - Annealed condition
Cr7C3, V8C7, (Fe3W3)C-(Fe4W2)C carbides in HS10-2-5-8 steel - Annealed condition
Cr7C3, V8C7, (Fe3W3)C-(Fe4W2)C carbides in HS6-5-4 steel - Annealed condition
Cr7C3, V8C7, V4C3, (Fe3W3)C-(Fe4W2)C carbides in HS6-5-3-9 steel - Annealed condition
Cr7C3, V8C7, V4C3; Mo2C, (Fe3W3)C-(Fe4W2)C carbides in HS7-7-7-10 - Annealed condition
Dendritic primary carbide NbC in stainless steel
Epsilon and M3C carbides in 35MnCrMoV8-6-4-1 steel
Epsilon, M3C, M2C carbides in 30CrMoNiV10-25-6-2 steel
Epsilon, M3C, MC and M2C carbides in 0.30C-2.50Cr-2.60Mo-1.59Ni-0.18V hot work tool steel
Epsilon, M3C, MC and M2C carbides in 30CrMoNiV10-25-6-2 hot work tool steel
Epsilon, M3C, MC, M2C carbides in HS18-0-1 steel
Epsilon, MC and M2C carbides in HS18-0-1 and HS6-5-2 steels
Etchants for carbides in steels
Eutectic VC, NbC and M6C carbides in steel
Fe3C and NbC carbides in 0.14C-1.48Mn-0.78Si-0.052Nb steel
Fe3C and NbC carbides in 3.4C–0.9Si–0.7Mn–4.4Ni–1.8Cr–0.4Mo cast steel roll
Fe3C carbides in line pipe steel
Fe3C, M23C6 and VC carbides in X20CrMoV121 and P91 steels
Fe3C, VC, M7C3 and M23C6 carbides in heat resistant 12Kh1MF steel
Fe3Nb3C carbides in C-Cr-Nb-Ti steel
Fracture surface of four-point bending test samples of cold work tool steel
M23(C,B)6, TiC and NbC carbides in 18% Cr ferritic stainless steel
M23C6 VC and M6C carbides in Cr-Mo-W-V steel
M23C6 and M3C carbides in 12% chromium steel
M23C6 and TaC carbides in TAC1 creep resisting steel
M23C6 carbides in E911 steel
M23C6 carbides in P91 steel
M23C6, M6C and MC carbides in 2.25Cr–1Mo steel
M23C6, M6C and MC carbides in AISI 316, AISI 304, X6CrNiMoTi 17-12-2 steels
M23C6, M6C and MC carbides in AISI H13 steel
M23C6, M7C3 and M6C carbides in 2.25%Cr–Mo–V–Nb and 2.25%Cr–W–V–Nb steels
M23C6, M7C3 and VC carbides in 12X1M0 heat resistant steel
M23C6, MC, M7C3 carbides and sigma phase in austenitic stainless steels
M23C6, NbC and M7C3 carbides in steels for nuclear industry
M23C6, TiC and TaC carbides in stainless steels
M23C6, V8C7, MC and M2C carbides in spray formed AISI M2 steel
M2C and M23C6 carbides in 0.5Mo-0.5Cr-0.25V low alloy creep resistant steel
M2C, M3C, M23C6 and M7C3 carbides in 13CrMo4-5 steel
M2C, M6C, TiC, VC and NbC carbides in AISI M7 cast high speed steel
M2C, MC and M6C carbides in AISI M2 high speed steel
M3C, M7C3, MC, M6C carbides in steel rolls
M3C, VC and M7C3 carbides in Strømhard austenitic manganese steel
M6C and M7C3 carbides in 0.86%C, 7.6%Cr, 0.48%(Nb + V) semi high speed cast steel
M6C and M7C3 carbides in Cr and semi HSS steels for rolls
M6C and MC carbides in PM high speed steel
M6C, M23C6 and NbC carbides in 347, HR120 and NF709 steels
M6C, VC, (CrFeMoW)7C3 and M23C6 carbides in high speed steels
M7C3 and M23C6 carbides in MANET steel
M7C3 and M23C6 carbides in Manet steel
M7C3 and M6C carbides in high Cr and semi high speed steels
M7C3 and MC carbides in SHSS and HSS rolls
M7C3 and NbC carbides in Fe-2.1C-l4.7Cr-lNb alloy
M7C3 carbides in D2 steel
M7C3, M23C6 and M6C carbides in 13HMF steel
M7C3, M23C6 and M6C carbides in 13HMF steel
M7C3, M23C6, MC and M3C carbides in G21CrMoV4 – 6 (L21HMF) low alloy cast steel
M7C3, M23C6, VC and Mo2C carbides in forged steel rolls
M7C3, M2C and MC carbides in semi-HSS grades
M7C3, MC and M2C carbides in hardfacing steel
M7C3, MC, M23C6 and M3C carbides in AISI H11 steel
MC (or M4C3), M23C6 and M6C carbides in AISI M2 steel
MC and M23C6 carbides in Armour steel
MC and M23C6 carbides in P91 creep reistant steel
MC and M3C carbides in cast AISI D3 steel
MC and M6C carbides in M4 high speed steel
MC and M6C carbides in AISI M2 high speed steel
MC and M6C carbides in AISI M2 steel
MC and M6C carbides in HS 10-2-5-8 steel
MC and M6C carbides in HS 6-5-3 steel
MC and M6C carbides in M4 steel
MC and M6C carbides in PM Sinter 23 tool steel
MC and M6C carbides in SINTER 23 PM steel
MC and M6C carbides in cast M2 high speed steel
MC and M6C carbides in high-carbon high speed steel roll
MC and M7C3 carbides in PM tool steel
MC and M7C3 carbides in Thyrospray 2399 PM steel
MC and M7C3 carbides in Vanadis 6 PM steel
MC and M7C3 carbides in Vanadis 6 PM steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in tool steels made by spray forming
MC carbide segregation in H13 tool steel
MC carbides in 0.17C-1.37Mn-0.24Cr-0.48Mo steel
MC, M2C and M6C carbides in K390 steel
MC, M2C and M6C carbides in AISI M2 high speed steel manufactured by different casting technologies
MC, M2C and M6C carbides in S 6-5-2-5 high speed steel
MC, M2C and M6C carbides in semi high speed steel for rolls
MC, M2C and M7C3 carbides in Wear resistant cast iron for rolls
MC, M2C and M7C3 carbides in cast high speed steel roll
MC, M2C carbides in HSS7 steel for rolls
MC, M2C, M3C, M7C3 and M23C6 carbides in 2CrMoNiWV creep resistant steel III
MC, M2C, M3C, M7C3 and M23C6 carbides in G21CrMoV4 – 6 (L21HMF) cast steel
MC, M2C, M3C, M7C3, M23C6 and M6C carbides in 2CrMoNiWV creep resistant steel II
MC, M2C, M3C, M7C3, M23C6 and M6C carbides in 2CrMoNiWV creep resistant steel IV
MC, M2C, M3C, M7C3, M23C6 and M6C carbides in 2CrMoNiWV creep resistant steel V
MC, M2C, M6C and M7C3 carbides in 2%C–5%Cr–5%V–5%Mo–5%W–5%Co white cast iron
MC, M2C, M6C, M7C3 carbides in cast high speed steels (HSS) for rolls
MC, M2C, M7C3 and M23C6 carbides in Kosmos and Aurora steels
MC, M2C, M7C3 and M23C6 carbides in cast high speed roll
MC, M2C, M7C3 and M23C6 carbides in high speed steel roll
MC, M2C, M7C3, M23C6 carbides in Aurora and Kosmos HSS steels
MC, M2C, M7C3, M23C6 carbides in cast HSS roll
MC, M3C and M7C3 carbides in high chromium cast iron
MC, M3C, M6C and M7C3 carbides in SS2541, THG2000, QRO90 and MCG 4M steels
MC, M6C and M23C6 carbides in H13 hot work tool steel
MC, M6C and M23C6 carbides in AISI H13 hot work tool steel
MC, M6C and M23C6 carbides in AISI T1 steel
MC, M6C, M7C3 and M23C6 carbides in 1.2690 steel
MC, M7C3 and M2C carbides in cast high speed steel roll
MC, M7C3 and M6C carbides in PM cold work tool steel
MC, M7C3 and M6C carbides in THG2000, MCG2006 and QRO90 steels
MC, M7C3 carbides in ROLTEC,TOUGHTEC, WEARTEC, AISI A2, D2 and D6 steels
MX and M23C6 carbides in 100Cr creep resistant steel
Mo2C and NbC carbides in Fe–4Mo–0.1Nb–0.2C steel
Mo2C and VC carbides in Cr-Mo-V steel
Mo2C carbides in Fe–4Mo–0.2C steel
Mo2C, M7C3 and VC carbides in SHSS II steel
NbC and Cr23C6 carbides in high Cr (11 wt.%) tempered martensitic steel
NbC and M23C6 carbides in HR120 and AL20-25+Nb steels
NbC and NbMoC carbides in 0.2C–1.5Si–1.5Mn steel
NbC and TaC carbides in sintered 316L stainless steel
NbC carbide in Nb cast iron
NbC carbides in 12%CrNb steel
NbC carbides in 347 and AL347HP steels
NbC carbides in CF8C and CF8C-Plus steels
NbC carbides in CF8C-Plus cast austenitic stainless steel
NbC carbides in HSLA steel
NbC carbides in HTUPS4 and NF709 steels
NbC carbides in Nb-stabilized 18 Cr-8 Ni stainless steel
NbC carbides in Nb-stabilized 18 Cr-8 Ni stainless steel
NbC carbides in T347 stainless steel
NbC carbides in Weldox steel
NbC carbides in high-strength low-alloy steel with Nb
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC, M23C6 carbides in HR120, AL20-25+Nb steels
NbC, M6C, M23C6 carbides in NF709 steel
Niobium carbide powder
Primary MC carbide in 0-5-1-2Ti grade cast high speed steel
Primary carbide particles of MC type in H11 steel
SEM images of fracture surfaces in PM tool steel
Some properties of metallic hard materials
Tantalum carbide powder
TiC and M23C6 carbides in Ti stabilized 18 Cr-8 Ni stainless steel
TiC and M23C6 carbides in Ti stabilized 18 Cr-8 Ni stainless steel
TiC carbide in Ferro-Titanit steel
TiC carbides in 440C–TiC composite steel
TiC carbides in 0.42C–0.30Ti steel
TiC carbides in Ti stabilized 18 Cr-8 Ni stainless steel
TiC carbides in TiNb and IF steels
TiC in Fe-10% TiC composite
TiC in Fe-10% TiC composite
TiC in Fe-10% TiC composite
Time–temperature–precipitation diagrams (TTP) for low alloyed steels
V4C3 carbides in 2CrMoNiWV creep resistant steel I
V4C3, C7C3 and VC carbides in K190 ISOMATRIX PM steel
V4C4 and Cr7C3 carbides in K190 ISOMATRIX PM steel
V6C5 carbides in microalloyed steel
V8C7, (Fe3W3)C- (Fe4W2)C carbides in HS6-5-4 steel - Quenched from 1200 C/5 min
V8C7, (Fe3W3)C-(Fe4W2)C carbides in HS10-2-5-8 steel - Quenched from 1200 C/5 min
V8C7, Mo2C, (Fe3W3)C – (Fe4W2)C carbides in 1.3344 steel - Annealed condition
V8C7, V4C3, (Fe3W3)C-(Fe4W2)C carbides in 1.3344 steel - Quenched from 1200 C/5 min
V8C7, V4C3, (Fe3W3)C-(Fe4W2)C carbides in HS6-5-3-9 steel - Quenched from 1200 C/5 min
V8C7, V4C3, (Fe3W3)C-(Fe4W2)C carbides in HS7-7-7-10 - Quenched from 1200 C/5 min
VC and M23C6 carbides in HCM12 steel
VC and M3C carbides in JIS SKS3 and BSBO1 steels
VC and M7C3 carbides in Fe-2.4C-5.4Cr-6V alloy
VC and Mo2C carbides in Cr-Mo-W-V steel
VC and Mo2C carbides in Cr-Mo-W-V steel
VC and TiC carbides in Fe-0.049C-0.3Mn-0.126V, Fe-0.38C-1.5Mn-0.5Si-O.1V, Fe-0.052C-0.18Mn-0.12Ti steels
VC and W3Fe3C carbides in HSS6-5-2C high speed steel
VC cabides in microalloyed steel
VC carbides in Cr-Mo-V steel
VC carbides in Cr-Mo-V steel
VC carbides in Cr-Mo-V steel
VC carbides in Cr-Mo-V steel
VC carbides in Cr-Mo-V steel
VC carbides in Cr-Mo-V steel
VC carbides in Cr-Mo-V-W steel
VC carbides in Cr-Mo-V-W steel
VC carbides in Cr-Mo-W-V steel
VC carbides in Cr-Mo-W-V steel
VC carbides in Fe-2.4C-0.9Si-0.9Mn-0.1 Ni-2.9Cr-3.4Mo-5-9V alloy
VC carbides in Fe-3.3C-9.2V-2Si steel
VC carbides in Fe–0.25V–0.05C steel
VC carbides in Fe–0.75V–0.15C steel
VC carbides in Fe–1V–0.2C steels
VC carbides in Fe–V–C stel
VC carbides in cast high speed steel
VC carbides in high speed steel
VC carbides in high vanadium cast iron
VC carbides in medium carbon steel with higher V
VC carbides in vanadium steel
VC, Fe3C, M7C3 and M23C6 carbides in 12X1MO steel
VC, M23C6 and M7C3 carbides in Dievar hot work tool steel
VC, Mo2C, (Fe,Cr)3C and (Cr,Fe)7C3 carbides in a new hot work tool steel
VC, Mo2C, M7C3 and M23C6 carbides in forged high speed steel roll
Vanadium rich carbides in cast high speed steels

Copyright © 2018 by Steel Data. All Rights Reserved.