Manganese silicates in low carbon Si-killed steel


Figure 1: Oxide inclusions in low carbon Si-killed steel, SEM, scale bars: 10, 20 µm.

Inclusion name: Oxide inclusions
Record No.: 1050
Inclusion formula: See the figure 1.
Inclusion type (Macro/Micro/Nano): Macro
Inclusion type (Exogenous/Indigenous): Indigenous
Inclusion classification: Oxide
Inclusion composition in weight %: No data
Sample: Si-killed steel
Steel composition in weight %: 0.09% C, 0.55% Si, 1.2% Mn.
Note: No data